Enhancing Durability and Resistance to Wear and Corrosion of AISI 431 Martensitic Stainless Steel for Sustainable Engineering Applications

,
,
,
,
,
and
Escola Politécnica de Enxeñaría de Ferrol, Centro de Investigacións en Tecnoloxías Navais e Industriais (CITENI), Campus Industrial de Ferrol, Universidade da Coruña, 15403 Ferrol, Spain
*
Author to whom correspondence should be addressed.
This article belongs to the Section Corrosion and Protection

Abstract

This study investigates the influence of heat treatment on the wear resistance and corrosion behavior of AISI 431 martensitic stainless steel, with the aim of enhancing durability and extending service life in demanding applications, thereby supporting more resource-efficient material use. Two single austenitizing treatments (1000 °C and 1070 °C) and one double austenitizing treatment were evaluated. The evolution of hardness, microstructure, wear resistance, and corrosion behavior was determined as a function of the applied heat treatment. Hardness was measured using the Rockwell C method, wear behavior was evaluated by Pin-on-Disk testing, and corrosion resistance was assessed by anodic potentiodynamic polarization tests. The untreated (as-received condition) steel exhibited the lowest wear mass loss. Among the heat-treated samples, the double austenitized condition exhibited the best wear performance. The highest hardness was obtained after single austenitization at 1070 °C (approximately 50 HRC), while double austenitization and single austenitization at 1000 °C resulted in hardness values of approximately 45 HRC. Corrosion testing revealed open-circuit potentials of −0.25 V, −0.27 V, −0.13 V, and −0.14 V for the untreated, SA1000, SA1070, and double-austenitized conditions, respectively. The results show that while SA1070 and DA exhibit more noble open-circuit potentials and extend the stability window against abrupt localized collapse, the DA condition operates under a high-rate non-passive regime with an elevated current density (1.38 mA/cm2). This thermal treatment shifts the degradation mechanism away from localized intergranular vulnerability at the expense of a higher continuous dissolution rate. Consequently, while DA provides favorable wear behavior among the heat-treated conditions, its elevated current density must be carefully considered for applications in marine environments.

Article Metrics

Citations

Article Access Statistics

Article metric data becomes available approximately 24 hours after publication online.