Numerical Investigation of Unbonded Post-Tensioned Concrete Slabs Reinforced with CFRP Tendons

,
,
,
and
1
Department of Structural Engineering, Faculty of Engineering, Zagazig University, Zagazig 44519, Egypt
2
Civil and Environmental Engineering, University of Missouri, Columbia, MO 65211, USA
*
Author to whom correspondence should be addressed.

Abstract

This study investigates the behavior of unbonded post-tensioned two-way concrete slabs reinforced with either steel or FRP tendons. An initial comparison was conducted to evaluate the effect of different FRP tendon materials, including AFRP, GFRP, and CFRP. Based on the outcomes of this comparison, CFRP tendons were selected for a detailed performance comparison with steel tendons. A three-dimensional finite element model was developed using ANSYS Workbench 2023 R1 and validated against available experimental results. Subsequently, a comprehensive parametric study was carried out to examine the influence of tendon material, tendon profile, tendon arrangement, slab thickness, tendon spacing, and post-tensioning level. The results indicate that the use of unbonded CFRP tendons resulted in lower mid-span deflection compared with steel tendons. Additionally, changing the tendon profile from straight to parabolic reduced mid-span deflection by approximately 44.5% for steel tendons and 64.4% for CFRP tendons. For the parabolic tendon profile, the use of CFRP tendons reduced mid-span deflection by approximately 48% compared with steel tendons.

1. Introduction

Concrete defects are imperfections that occur during mixing, casting, curing, or service life and can reduce concrete strength and durability. These defects are mainly caused by poor materials, improper workmanship, or environmental effects [1].
Cracking is the most common concrete defect and results from shrinkage, temperature changes, or loading. Honeycombing and segregation occur due to insufficient compaction, leading to weak and permeable concrete [2].
Durability-related defects develop over time, especially reinforcement corrosion caused by chloride penetration and carbonation. Proper mix design, adequate curing, and good construction practices help reduce these defects [1,3]. Therefore, to overcome these defects and improve the structural performance and durability of concrete members, post-tensioning has been widely adopted as an effective construction technique.
Post-tensioning is a form of prestressing in which high-strength steel tendons are placed in concrete and stressed after the concrete has hardened using hydraulic jacks, then anchored mechanically to introduce compressive forces into the member. This technique is widely used in buildings, parking structures, foundations, bridges, tanks, and other structural applications.
Post-tensioning makes it possible to achieve longer spans, thinner sections, and structural solutions that are often not feasible with conventional reinforced concrete [4,5].
G. Mohamed et al. conducted a numerical study to investigate the structural and economic performance of post-tensioned (PT) floor systems in the Egyptian market. The study demonstrated that PT floor systems provide structural and economic advantages over conventional reinforced concrete (RC) flat slabs, particularly for long-span and multi-story buildings. Furthermore, the results indicated that PT floors become more economical than RC flat slabs for spans exceeding 8.3 m under Egyptian market conditions [6].
E. Ellobody and C.G. Bailey conducted an experimental and numerical investigation on the behavior of unbonded post-tensioned one-way concrete slabs. A nonlinear finite element model was developed and validated against the experimental results, showing good agreement in terms of load-deflection response and failure modes. The parametric study demonstrated that increasing the concrete strength improved the ultimate load capacity of the slabs. Experimentally, increasing the concrete strength from 44.4 MPa to 48.2 MPa increased the ultimate load by 13.8% [7].
Corrosion of steel tendons is a major problem for post-tensioned concrete, especially because corrosion is often hard to detect inside grouted ducts. While research continues to develop better means to protect steel tendons against corrosion, considerable effort is devoted to finding suitable non-metallic tendons for post-tensioning applications. Fiber-reinforced polymer (FRP) composite offers a viable alternative to steel tendons. In addition to their superior durability, FRP tendons may result in lower relaxation losses as compared with steel [5]. FRP tendons may be made with different types of fibers. Due to their higher strength, elastic modulus, and excellent durability, Carbon Fiber-Reinforced Polymer (CFRP) tendons are the most practical option. The advantages of post-tensioning are multiplied when combined with prefabrication so as to reduce on-site construction time. FRP materials are classified by fiber type. Glass Fiber-Reinforced Polymer (GFRP) is the most widely used due to its low cost and good corrosion resistance. Aramid Fiber-Reinforced Polymer (AFRP) is distinguished by high toughness and impact resistance, while CFRP offers the highest strength and stiffness at low weight for advanced structural applications [8,9]. CFRP offers several advantages, including high rigidity and high strength, which provide an excellent strength-to-weight ratio compared to conventional materials. Its low density significantly reduces structural weight, while its corrosion resistance ensures durability in hard environmental conditions. CFRP also exhibits high fatigue strength, making it suitable for applications subjected to repeated loading, and its low thermal expansion allows it to maintain dimensional stability under temperature variations. In addition, CFRP has good constructible characteristics, as it can be easily molded into complex shapes and tailored to meet specific design and performance requirements [10].
Post-tensioned CFRP tendons were used to increase the slab stiffness through prestressing action; in addition to improved serviceability, post-tensioning increased the design shear capacity by more than 70% [11].
Gąćkowski investigated the feasibility of replacing conventional steel tendons with CFCC composite tendons in prestressed precast beams used in densely ribbed floor systems. The study considered C50/60 concrete for the precast beams and C25/30 concrete for the supplementary topping and composite ribs. Five three-dimensional numerical models were developed with spans ranging from 6 to 15 m and one to five beams per rib. The models were assessed under the ultimate limit state (ULS) in bending and serviceability limit states (SLS), including crack width and deflection. The results confirmed that CFCC tendons provided comparable structural performance to steel tendons and were feasible for long-span prestressed floor systems [12].
Nassif et al. investigated the flexural strength of concrete members prestressed with bonded and unbonded steel and CFRP tendons. A closed-form analytical approach based on the modified deformation-based approach was developed to predict the stress in unbonded prestressed tendons and the nominal flexural strength. The proposed approach was assessed using a database of 330 beams and slabs prestressed with steel and/or CFRP tendons, based on experimental test results from the authors and the literature. The results showed excellent agreement with the existing ACI provisions and demonstrated the applicability of the proposed approach to different combinations of bonded and unbonded steel and CFRP tendons [13].
Alsuwaidi et al. conducted an experimental field study on the rehabilitation of partially corroded post-tensioned concrete structures. The study evaluated the structural condition and implemented a rehabilitation strategy incorporating CFRP strengthening and waterproofing. The results showed that CFRP strengthening increased the slab flexural strength by 30% and reduced crack width by 23%, improving the overall structural performance [14].
Abdel-Jaber et al. conducted an experimental study to evaluate the effectiveness of CFRP grids in strengthening and repairing reinforced concrete slabs exposed to high temperatures. Laboratory tests showed that CFRP reinforcement significantly improved the structural performance of the slabs, increasing their ultimate load capacity by up to 41.4% and enhancing stiffness while reducing deflection [15].
Grace et al. conducted an experimental and numerical study to investigate the flexural behavior of precast prestressed decked bulb T-beams reinforced with CFRP tendons. The results showed that the CFRP-prestressed beam achieved 88% of the flexural load-carrying capacity and 103% of the maximum deflection of the steel-prestressed beam, demonstrating comparable overall flexural performance with the added advantage of corrosion resistance [16].
Lee et al. conducted an experimental and numerical study on the flexural behavior of simply supported concrete beams prestressed with unbonded CFRP tendons under four-point loading. The developed numerical model showed good agreement with the experimental load–deflection responses. The parametric study demonstrated that increasing the concrete compressive strength, the amount of unbonded CFRP tendons, and the initial prestressing level improved both the initial cracking and ultimate flexural strengths [17].
Elbelbisi et al. conducted a numerical study to investigate the flexural behavior of steel–concrete composite beams reinforced with externally post-tensioned CFRP tendons using a three-dimensional finite element model. The results showed that CFRP tendons provided the highest flexural capacity, increasing the beam capacity by 50%, while a 20–30% post-tensioning level achieved the optimum structural performance [18].
Tan D. Le et al. conducted an experimental study on the flexural behavior of precast segmental concrete beams prestressed with bonded and unbonded CFRP tendons under four-point loading. The results demonstrated that CFRP tendons can effectively replace steel tendons due to their excellent load-carrying capacity and ductility. Beams prestressed with bonded CFRP tendons exhibited an average ultimate load capacity of 167 kN, which was 41.5% higher than that of beams prestressed with unbonded CFRP tendons (118 kN). In contrast, beams with unbonded CFRP tendons exhibited significantly greater ductility and a less brittle failure mode [19].
Although previous studies have demonstrated the effectiveness of post-tensioned concrete systems and the advantages of CFRP tendons in improving the structural performance of concrete members, most investigations focused either on conventional steel tendons in post-tensioned slabs or on CFRP tendons in beams. In addition, the available studies on slabs mainly investigated CFRP as an external strengthening material rather than as post-tensioning tendons. Furthermore, a comprehensive comparison between steel, GFRP, AFRP, and CFRP tendons in post-tensioned concrete slabs has not been sufficiently addressed. Therefore, this study first compares the structural performance of post-tensioned concrete slabs reinforced with steel, GFRP, AFRP, and CFRP tendons to identify the most suitable FRP tendon type. Subsequently, the selected CFRP tendon is directly compared with conventional steel tendons using a validated nonlinear finite element model based on the load–deflection response.
Accordingly, this study aims to fill these research gaps by first evaluating the performance of different FRP tendon types and then investigating the structural behavior of post-tensioned concrete slabs reinforced with the selected CFRP tendon in comparison with conventional steel tendons using a validated nonlinear finite element model.
The study does not only examine the expected effects of the investigated design variables (tendon profile, tendon arrangement, tendon distribution, slab thickness, and prestressing level) individually; rather, it evaluates their effects on the structural response for different tendon materials, providing insight into the material-dependent structural behavior of CFRP and conventional steel tendons.
In this paper, a nonlinear finite element (FE) model was developed in ANSYS Workbench 2023 R1 to investigate the structural behavior of post-tensioned concrete slabs. Initially, the structural performance of slabs reinforced with conventional steel, GFRP, AFRP, and CFRP tendons was compared to identify the most suitable FRP tendon type. Subsequently, a detailed comparison was carried out between the selected CFRP tendon and conventional steel tendons. The developed FE model was validated against experimental results available in the literature to ensure its accuracy in predicting the structural response. A parametric study comprising 48 finite element models was then performed to evaluate the influence of key design parameters, including tendon material, prestress level, tendon profile, tendon arrangement, tendon spacing, and slab thickness, on the load–deflection behavior of post-tensioned concrete slabs.

2. Numerical Modeling

In this research, ANSYS Workbench 2023 R1 software was used to simulate a two-way post-tensioned concrete slab reinforced either with conventional steel tendons or FRP tendons [18,20]. The two-way post-tensioned concrete slab has plan dimensions of 9 m × 9 m and is supported by four columns with fixed column bases. The slab is structurally reinforced with internal conventional steel reinforcement and post-tensioning tendons made of different advanced materials. The post-tensioning system incorporated multi-strand tendons, where each tendon contains seven 0.5-inch (12.7 mm) seven-wire strands to provide the required cross-sectional area. Furthermore, the parametric study evaluated three distinct slab thicknesses designated as T1 (220 mm), T2 (240 mm), and T3 (260 mm). Only one-quarter of the slab was modeled using symmetry boundary conditions along the mid-planes to take advantage of structural symmetry, thereby reducing the computational effort while maintaining accuracy. Symmetry boundary conditions have been applied. Figure 1 illustrates the finite element model for one-quarter of the post-tensioned slab cross-section.
Figure 1. The FEM of one-quarter of the post-tensioned slab cross-section.
The finite element model incorporates the concrete slab, internal steel reinforcement, and various post-tensioning tendons (steel, AFRP, GFRP, and CFRP). To ensure accurate force transfer, the interface behaviors and interaction profiles between the concrete matrix and the different types of tendons were rigorously defined.
Concrete was modeled using a nonlinear constitutive model to capture realistic behavior under loading. FRP tendons were modeled as linear elastic materials, while steel tendons were defined as bilinear elastic–plastic materials.
The applied loads included the slab self-weight, live load (5.0 kN/m2) and post tensioning forces.
SOLID 65 element was employed to simulate the concrete, featuring eight nodes with three degrees of freedom for each node, encompassing translations in the nodal directions x, y, and z. This element is adept at simulating plastic deformation, cracking in three orthogonal directions, and crushing [20]. For the reinforcing bars and post-tensioning tendons, the model utilized a LINK 180 3D spar element. This element, with two nodes and three degrees of freedom each, was chosen [21]. The unbonded tendons were modeled using LINK180 elements with nodes separate from the concrete mesh. A frictionless tendon–duct interface allowed longitudinal sliding while preventing penetration through the duct wall. This interaction provided transverse guidance along the curved tendon path and transferred the corresponding normal forces to the concrete. No perfect-bond constraints were imposed along the free tendon length. At the physical anchorages, the tendon ends were connected to the anchorage regions, with anchorage slip neglected. In contrast, the ordinary reinforcing bars were assumed perfectly bonded to the concrete.

2.1. Real Constants

In order to simulate the initial post-tensioning force a temperature load effect was used. The initial temperature determined using Equation (1) determines the relationship between the temperature load and the tension force. The phrase “initial temperature” refers to the corresponding temperature change required to obtain the necessary post-tensioning force.
Initial temperature = F/α E Ap
where
F: The post tension force.
E: Tendon modulus of elasticity.
α: Coefficient of thermal expansion.
Ap: Cross section of the tendon [22].

2.2. Modeling of Materials Behavior

Concrete was assumed to be homogeneous and isotropic. Its nonlinear compressive behavior was represented in ANSYS Workbench 2023 R1 using a multilinear isotropic hardening model. The uniaxial compressive stress–strain relationship was defined by nine points connected by linear segments, as shown in Figure 2a [23,24].
Figure 2. Modeling of material: (a) compression stress–strain curve for concrete and (b) model for steel material.
The nonlinear behavior of the steel reinforcement was modeled using a bilinear isotropic hardening model. The material properties, including the elastic modulus and yield strength, were obtained from the experimental study as shown in Figure 2b.
To simulate the brittle behavior of the FRP material, a linear elastic material model was utilized. Figure 3 illustrates the stress–strain relationship of the utilized materials in comparison to that of steel.
Figure 3. Stress–strain behavior of the tendon materials.
A mesh-sensitivity study was conducted using element sizes ranging from 80 to 150 mm. Figure 4 shows the influence of mesh size on the predicted maximum deflection. Refinement from 100 to 80 mm changed the maximum deflection by approximately 6%, while increasing the element count from 26,002 to 41,641. The 100 mm mesh was therefore selected for the subsequent analyses, providing a balance between prediction stability and computational effort with 37.6% fewer elements than the finest mesh investigated.
Figure 4. Mesh-sensitivity study.

2.3. Validation

Experimental data selected from the literature were chosen based on their recognized accuracy and relevance to the study parameters, ensuring comprehensive validation across various conditions and rigorous benchmarking against established standards in the field to enhance the credibility and applicability of our findings. Therefore, experimental data from Ellobody and Bailey [7] and Lee et al. [17] were selected from the literature to validate the FEM.
Experimental data reported by Ellobody and Bailey (2008) [7] were utilized to validate the accuracy of the proposed numerical model. The laboratory program tested a full-scale, simply supported one-way concrete slab measuring 4300 mm in length with a clear span of 4000 mm, a width of 1600 mm, and a thickness of 160 mm. The slab was post-tensioned using three longitudinal parabolic unbonded steel tendons with a nominal diameter of 15.7 mm and an area of 150 mm2, stressed to 70% of their ultimate breaking load. Under ultimate static loading, the reference specimen, achieved an ultimate failure load of 178.2 kN at a maximum mid-span deflection of 93.5 mm. The structural failure mechanism was characterized by a ductile combination of concrete crushing in the compression zone and tendon yielding. Figure 5a,b illustrates the dimensions, specifics, and configurations of the post-tensioned tendons used in the examined slab.
Figure 5. General layout of the unbonded post-tensioned slabs tested by Ellobody and Bailey [7] (dimensions in mm).
Detailed material properties of all slab components can be found in Table 1. A finite element model was developed in ANSYS Workbench 2023 R1 to simulate the experimentally tested slab. The numerical results showed good agreement with the experimental results as demonstrated in Table 2 and Figure 6.
Table 1. Overview of material properties for the Ellobody and Bailey experiment [7].
Table 2. Loads and deflections from experimental and finite element analysis [7].
Figure 6. Mid-span load–deflection curves: a comparison between Ellobody and Bailey [7] and FEM.
Experimental data reported by Lee et al. (2015) [17] were also utilized to validate the accuracy of the proposed numerical model. The laboratory program tested a simply supported rectangular concrete beam measuring 3200 mm in length with a clear span of 2700 mm, a width of 150 mm, and a total depth of 250 mm. The beam was internally prestressed using one longitudinal straight unbonded CFRP tendon with a nominal diameter of 10.5 mm and an area of 55.7 mm2, stressed to 50% of its ultimate tensile strength. Under ultimate static loading, the tested specimen achieved an ultimate failure load of 47.2 kN at a maximum mid-span deflection of 28.6 mm. The specimen underwent quasi-static testing using a four-point bending setup. Figure 7 illustrates the dimensions, specifics, and configurations of the internally unbonded tendon used in the examined beam.
Figure 7. Geometrical properties of the simply supported beam tested by Lee et al. [17] (a) cross-section and (b) elevation of the beam (dimensions in mm).
Detailed material properties of all beam components can be found in Table 3. A finite element model (FEM) was developed in ANSYS Workbench 2023 R1 to simulate the experimental specimen. Comparing the FEM results with the experimental data, good agreement was observed between the numerical and experimental results as demonstrated in Table 4 and Figure 8.
Table 3. Overview of material properties for the Lee et al. experiment [17].
Table 4. Loads and deflections from experimental and finite element analysis [17].
Figure 8. Mid-span load–deflection curve comparison between: lee et al. [17] and FEM.
Finally, it can be confidently concluded that the developed finite element model (FEM) is highly able to predict the full structural response and flexural behavior of post-tensioned concrete elements reinforced with either steel or advanced CFRP tendons.

2.4. Parametric Investigation

A comprehensive parametric study involving variations in geometric and material characteristics was conducted to evaluate the structural behavior, ultimate load, and deformation response of two-way post-tensioned concrete slabs prestressed with either steel or FRP tendons (CFRP, GFRP, and AFRP).
Based on the initial analysis, Carbon Fiber-Reinforced Polymer (CFRP) tendons emerged as the most effective alternative within the FRP group to replace conventional steel tendons. Consequently, all remaining parametric models were compared against both the conventional steel and the selected CFRP configurations to evaluate their relative structural performance.
The geometric variations incorporated three distinct slab thicknesses, designated as T1 (220 mm), T2 (240 mm), and T3 (260 mm), to analyze the strict effect of structural depth and stiffness increments.
Concurrently, the material parameters investigated the structural efficiency of utilizing different types of advanced post-tensioning tendons, including conventional steel and CFRP tendons, which were evaluated under distinct post-tensioning (PT) levels up to 50% of their ultimate tensile strength.
Forty-eight models, categorized into eight groups (labeled A to H), were constructed to study the effect of different parameters on the deflection of the post-tensioned slab. Details of this parametric investigation are provided in Table 5.
Table 5. Parametric study details and limitations.
Group A investigated the effect of tendon material, including steel, CFRP, AFRP, and GFRP, by developing four finite element models: SDD4T3-50, CDD4T3-50, ADD4T3-50, and GDD4T3-50, respectively. Meanwhile, Group B investigated the effect of tendon profile by comparing steel and CFRP tendons with both straight and parabolic tendon profiles. Four models were developed for this purpose: SDD4T3-50S and SDD4T3-50, representing steel tendons with straight and parabolic profiles, respectively, and CDD4T3-50S and CDD4T3-50, representing CFRP tendons with straight and parabolic profiles, respectively, as shown in Figure 9. Each pair of models was compared to evaluate the influence of tendon profile for the same tendon material.
Figure 9. The geometry of group (B) models: (a) Parabola tendon and (b) Straight tendon.
Group C investigated the effect of tendon arrangement by comparing steel and CFRP tendons with three different tendon layouts: distributed–distributed (DD), banded–distributed (BD), and banded–banded (BB) as shown in Figure 10. Six models were developed for this purpose: SDD4T3-50, SBD4T3-50, and SBB4T3-50, representing steel tendons with DD, BD, and BB layouts, respectively, and CDD4T3-50, CBD4T3-50, and CBB4T3-50, representing CFRP tendons with DD, BD, and BB layouts, respectively.
Figure 10. Tendon Arrangement (a) Banded–Distributed tendons, (b) Banded–Banded tendons, (c) Distributed–Distributed tendons.
Group D investigated the effect of slab thickness by comparing steel and CFRP tendons with three different slab thicknesses: T1 (220 mm), T2 (240 mm), and T3 (260 mm). Six models were developed for this purpose: SDD4T1-50, SDD4T2-50, and SDD4T3-50, representing steel tendons with slab thicknesses of 220 mm, 240 mm, and 260 mm, respectively, and CDD4T1-50, CDD4T2-50, and CDD4T3-50, representing CFRP tendons with the same slab thicknesses, respectively.
Group E investigated the effect of tendon distribution distance (4ts, 5ts, and 6ts) by comparing steel and CFRP tendons under a slab thickness of 240 mm. Six models were developed for this purpose: SDD4T2-50, SDD5T2-50, and SDD6T2-50, representing steel tendons, and CDD4T2-50, CDD5T2-50, and CDD6T2-50, representing CFRP tendons, where ts denotes the slab thickness.
Group F investigated the effect of tendon distribution distance (4ts, 5ts, and 6ts) by comparing steel and CFRP tendons under a slab thickness of 260 mm. Six models were developed for this purpose: SDD4T3-50, SDD5T3-50, and SDD6T3-50, representing steel tendons, and CDD4T3-50, CDD5T3-50, and CDD6T3-50, representing CFRP tendons, where ts denotes the slab thickness.
Group G investigated the effect of prestress level (20%, 30%, 40%, and 50% of the ultimate tendon strength, (Pu) by comparing steel and CFRP tendons under a slab thickness of 240 mm. Eight models were developed for this purpose: SDD4T2-20, SDD4T2-30, SDD4T2-40, and SDD4T2-50, representing steel tendon models, and CDD4T2-20, CDD4T2-30, CDD4T2-40, and CDD4T2-50, representing CFRP tendon models.
Group H investigated the effect of prestress level (20%, 30%, 40%, and 50% of the ultimate tendon strength, (Pu) by comparing steel and CFRP tendons under a slab thickness of 260 mm. Eight models were developed for this purpose: SDD4T3-20, SDD4T3-30, SDD4T3-40, and SDD4T3-50, representing steel tendon models, and CDD4T3-20, CDD4T3-30, CDD4T3-40, and CDD4T3-50, representing CFRP tendon models, as presented in Table 5.

2.5. Loading

There are two steps in the loading procedure. In the first step, the slab was subjected to the post-tensioning force in addition to its self-weight (dead load only), without applying any live load, where this prestressing force was calculated as a specific percentage of the tendon’s ultimate strength, which is presented in Table 6. In the second step, the live load of 5.0 kN/m2 was gradually applied until the required ultimate loading level was reached.
Table 6. Overview of material properties of the post-tensioning tendons for the numerical study.
The live load was applied as a uniformly distributed surface load of 5.0 kN/m2 over the slab area. The load values presented in the load–deflection curves represent the reaction force obtained from the numerical model during the application of the distributed live load.

2.6. Material Properties

The material properties of the post-tensioning tendons, conventional reinforcing steel and concrete utilized in this study are summarized in Table 6 and Table 7, including the concrete compressive strength and the specific mechanical properties of the steel and different FRP tendons.
Table 7. Overview of material properties of the conventional reinforcing steel and concrete for the numerical study.
For the finite element models, the seven strands of each tendon were represented by a single equivalent circular tendon with a diameter of 29.8 mm (radius = 14.9 mm), corresponding to an equivalent cross-sectional area of approximately 697.4 mm2. The same equivalent tendon geometry was adopted for all tendon materials to maintain consistency in the numerical comparison. The (Ap) values reported in the material-properties table represent the cross-sectional area of an individual strand obtained from the corresponding literature and manufacturer data.
The constitutive behavior of the materials was defined according to their respective mechanical characteristics. Concrete was modeled using SOLID65 with a nonlinear stress–strain relationship based on the adopted nine-point compressive stress–strain curve. Conventional reinforcing steel and steel post-tensioning tendons were modeled using elastic–plastic stress–strain relationships, while CFRP, AFRP, and GFRP tendons were modeled as linear-elastic materials up to failure.

3. Results

In this section, the numerical results obtained from the parametric study are comprehensively discussed, focusing primarily on the evaluation of the mid-span load-deflection response, with consideration of the ultimate load of the two-way post-tensioned concrete slabs.

3.1. Effect of Tendon Material

The results of Group A evaluate the structural impact of different tendon materials (steel, CFRP, AFRP, and GFRP) on the mid-span deflection, using the steel configuration as the benchmark reference. Figure 11a illustrates that at a load of 208 kN, the reference steel tendon exhibited a deflection of 17.6 mm. In comparison, the CFRP tendons demonstrated the highest structural efficiency, experiencing a deflection of only 9.2 mm, which represents a 48% deflection reduction relative to the steel. Conversely, alternative fiber materials resulted in increased deformations; the AFRP tendons produced a deflection of 29 mm, indicating a 65% increase in deflection compared to steel. The poorest performance was observed in the GFRP tendons, which registered a massive deflection of 104 mm, representing an increase of approximately 491% over the steel reference. This superior performance of the CFRP model is primarily attributed to its higher ultimate tensile strength and elastic modulus compared with the other FRP tendon materials considered in this study. While deflection differences between CFRP and steel are minor under low service loads, they become increasingly significant at higher load levels. Under elevated loads, steel tendons may reach the yield point, resulting in a rapid increase in deflection. In contrast, CFRP tendons exhibit no yield plateau and preserve a linear-elastic response up to failure with a constant modulus of elasticity, contributing to the lower deflection observed at high load levels.
Figure 11. Mid-span load–deflection curves for (a) group A and (b) group B.
Regarding the maximum load-carrying capacity, the models were compared for the four tendon materials. The steel tendon model reached a maximum load-carrying capacity of 224 kN, while the CFRP, AFRP, and GFRP tendon models reached maximum capacities of 231 kN, 210 kN, and 208 kN, respectively. Compared with the steel tendon model, the CFRP tendon model exhibited an increase of approximately 3.1%, while the AFRP and GFRP tendon models exhibited decreases of approximately 6.3% and 7.1%, respectively, in their maximum load-carrying capacities.
The typical deformation obtained from the finite element model are illustrated in Figure 12.
Figure 12. Total deformation of quarter of the slab.

3.2. Effect of Tendon Profile

In group B the PT concrete slab is analyzed to compare the effect of tendon profile on mid-span deflection for steel and CFRP tendons as shown in Figure 11b.
For steel tendons, the straight tendon profile in model SDD4T3-50S produced a mid-span deflection of 37.5 mm at a load of 224 kN. Changing to a parabolic tendon profile in model SDD4T3-50 reduced the mid-span deflection to 20.8 mm at the same load, corresponding to a reduction of approximately 44.5%. The parabolic tendon profile provides a better prestress distribution along the span, applying more prestress where bending moments are highest, which increases the effective stiffness of the slab and reduces mid-span deflection. For CFRP tendons, the straight tendon profile in model CDD4T3-50S produced a mid-span deflection of 30.3 mm at a load of 224 kN. Changing to a parabolic tendon profile in model CDD4T3-50 reduced the mid-span deflection to 10.8 mm at the same load, corresponding to a reduction of approximately 64.4%.
Furthermore, at the same applied load, the parabolic CFRP tendon profile reduced the mid-span deflection by approximately 48% compared with the parabolic steel tendon profile.
The parabolic tendon profile reduces mid-span deflection compared with the straight profile due to the curvature of the tendon, which introduces an upward balancing action along the span. This effect contributes to the more favorable load–deflection response and lower mid-span deflection observed for the parabolic profile.
Overall, the best-performing model in Group B is the CFRP tendon slab with a parabolic tendon profile (CDD4T3-50). It achieved the lowest mid-span deflection of 10.8 mm at a load of 224 kN, indicating a more favorable load–deflection response compared with the steel tendon models.
To compare the structural performance of the post-tensioned slab reinforced with steel tendons against CFRP tendons under the same prestressing force, both systems were analyzed. The results are summarized in Table 8.
Table 8. Comparison between steel and CFRP tendons under the same prestressing force.
Under the same prestressing force, the slab reinforced with CFRP tendons exhibited 19.5% higher maximum mid-span deflection than the corresponding slab reinforced with steel tendons. However, at the same prestressing level (50% of Pu), the slab reinforced with CFRP tendons showed a 48% lower maximum mid-span deflection than the slab reinforced with steel tendons. Therefore, the subsequent comparisons were conducted at the same prestressing level (%Pu).

3.3. Effect of Tendons Arrangement

In Group C, the effect of tendon arrangements on slab deflection is compared for CFRP and steel tendons as shown in Figure 13a.
Figure 13. Mid-span Load–deflection curves for (a) group C and (b) group D.
For CFRP tendons, the three studied models CDD4T3-50, CBD4T3-50, and CBB4T3-50 show different performances depending on the tendon layout. The banded–banded arrangement (CBB4T3-50) produced the highest mid-span deflection of 15.4 mm at a load of 183 kN, making it the least effective tendon distribution. Changing to a banded–distributed arrangement (CBD4T3-50) reduced the mid-span deflection to 9.95 mm, representing a reduction of approximately 35.4% compared to CBB4T3-50. The distributed–distributed arrangement (CDD4T3-50) showed the best performance, giving the lowest mid-span deflection of 8.5 mm at the same load, which corresponds to a 14.6% reduction from CBD4T3-50 and a 44.8% reduction from CBB4T3-50, making it the most effective tendon configuration in minimizing mid-span slab deflection.
The observed differences in mid-span deflection are primarily due to the location of the prestressing tendons and their influence on the overall load–deflection response of the slab. In the distributed–distributed layout (CDD4T3-50), the prestressing tendons are distributed across the slab, resulting in the lowest mid-span deflection and a more favorable load–deflection response. In the banded–distributed layout (CBD4T3-50), prestress is less effectively distributed at mid-span, leading to a slightly higher deflection compared with the distributed–distributed layout. The banded–banded layout (CBB4T3-50) places prestress away from mid-span, resulting in the largest mid-span deflection among the three configurations.
For steel tendons, the three studied models were SDD4T3-50, SBD4T3-50, and SBB4T3-50. The banded–banded arrangement (SBB4T3-50) produced the highest mid-span deflection of 19.1 mm at a load of 183 kN, making it the least effective configuration. Changing to a banded–distributed arrangement (SBD4T3-50) reduced the mid-span deflection to 12.9 mm, representing a reduction of approximately 32.5% compared to SBB4T3-50. The distributed–distributed arrangement (SDD4T3-50) exhibited the lowest mid-span deflection of 11.97 mm at the same load, corresponding to a 37.3% reduction from SBB4T3-50, making it the most effective tendon distribution in minimizing slab deflection.
The differences in mid-span deflection for steel tendons are mainly due to the tendon location and its effect on the overall load–deflection response. In the distributed–distributed layout (SDD4T3-50), the prestressing tendons are distributed across the slab, resulting in the lowest mid-span deflection. In the banded–distributed layout (SBD4T3-50), the prestressing tendons are less effectively distributed at mid-span, resulting in a moderately higher mid-span deflection compared with the distributed–distributed layout. The banded–banded layout (SBB4T3-50) places the prestressing tendons in the regions around the columns, away from the mid-span, resulting in the highest mid-span deflection among the steel tendon configurations.
The comparison is made for a reinforced concrete slab prestressed either with steel tendons (SDD4T3-50, SBD4T3-50, SBB4T3-50) or CFRP tendons (CDD4T3-50, CBD4T3-50, CBB4T3-50) at the same load of 183 kN. CFRP tendons consistently achieve lower mid-span deflections than steel tendons for all tendon layouts. For the distributed–distributed layout, CDD4T3-50 reduced the deflection to 8.5 mm compared to 11.97 mm for SDD4T3-50, a reduction of approximately 29%. In the banded–distributed layout, CBD4T3-50 achieved 9.95 mm versus 12.9 mm for SBD4T3-50, about 23% lower. For the banded–banded layout, CBB4T3-50) gave 15.4 mm compared to 19.1 mm for SBB4T3-50, a 19.4% reduction. Overall, the distributed–distributed layout with CFRP tendons (CDD4T3-50) provides the best performance at this load, minimizing mid-span deflection and demonstrating the most effective tendon type and distribution among all studied configurations.
At lower loads, CFRP tendons can produce higher mid-span deflections than steel tendons because CFRP has a lower modulus of elasticity, making the slab initially more flexible. Steel tendons, with their higher modulus of elasticity, resist deflection more effectively at these low loads. However, at higher loads, CFRP tendons outperform steel, producing lower mid-span deflections. This occurs because CFRP can sustain high tensile stresses while maintaining a linear-elastic response, allowing the prestressing force to remain effective at higher load levels and contributing to better control of slab deflection. In contrast, steel tendons may reach their yield stress at higher load levels, after which their post-yield behavior is associated with a more pronounced increase in slab deflection.
Regarding the maximum load-carrying capacity, the CFRP tendon arrangements DD, BD, and BB reached 231, 212, and 185 kN, respectively, corresponding to increases of approximately 24.9% and 14.6% for DD and BD, respectively, relative to BB. For steel tendons, the corresponding capacities were 224, 210, and 183 kN, with increases of approximately 22.4% and 14.8% for DD and BD, respectively, relative to BB. Overall, the CFRP tendon models exhibited higher maximum load-carrying capacities than the corresponding steel tendon models, with increases of approximately 3.1%, 1.0%, and 1.1% for the DD, BD, and BB arrangements, respectively.

3.4. Effect of Slab Thickness

Group D examines the influence of slab thickness on deflection behavior using steel tendons or CFRP tendons as shown in Figure 13b. For steel tendons the slab with a thickness of 220 mm (SDD4T1-50) exhibited the largest deflection of 40.5 mm under a load of 180 kN, representing the poorest performance within this group. Increasing the slab thickness to 240 mm (SDD4T2-50) reduced the deflection to 16.9 mm, corresponding to an improvement of approximately 58.3% compared to the 220 mm slab. A further increase in slab thickness to 260 mm in the post-tensioned slab (SDD4T3-50) resulted in a significant reduction in deflection to 11.3 mm at the same load, achieving an additional improvement of about 72.1%relative to the 220 mm slab. Overall, model SDD4T3-50 exhibited the best deflection performance among all the investigated slab thicknesses, demonstrating that increasing the slab thickness significantly enhanced the flexural stiffness and effectively controlled the mid-span deflection under high load levels.
The pronounced reduction in deflection with increasing slab thickness is primarily attributed to the increased flexural stiffness resulting from the higher moment of inertia of the thicker slab, together with the greater tendon eccentricity. Consequently, the 260 mm slab exhibited a significant reduction in mid-span deflection compared with the thinner slab configurations. Subsequently, slabs reinforced with CFRP tendons were investigated to evaluate the influence of slab thickness on deflection behavior. At the same load level of 180 kN, the slab with a thickness of 220 mm (CDD4T1-50) exhibited a deflection of 37.2 mm, representing the highest deflection within this section. Increasing the slab thickness to 240 mm (CDD4T2-50) reduced the deflection to 15.7 mm under the same load, corresponding to an improvement of approximately 57.8% compared to the 220 mm slab. A further increase in slab thickness to 260 mm (CDD4T3-50) resulted in a deflection of only 8.4 mm at the same load level, achieving a reduction of about 77.4% relative to the 220 mm slab. Overall, model CDD4T3-50 achieved the minimum deflection among the investigated slab thicknesses, confirming that the 260 mm slab represents the configuration producing the minimum deflection within the investigated parameter range under identical loading conditions.
In slabs reinforced with CFRP tendons, the substantial decrease in deflection with increasing slab thickness is primarily attributed to the higher flexural stiffness resulting from the increased moment of inertia, together with the greater tendon eccentricity. The increased slab depth enhances the contribution of prestressing to the overall flexural response, resulting in a lower mid-span deflection under the applied load. In addition, the stable linear-elastic behavior of CFRP tendons, which maintain their stiffness without yielding, contributes to the consistent load–deflection response of the slab. Consequently, the 260 mm CFRP slab represents the configuration producing the minimum deflection within the investigated parameter range under high load levels.
A systematic comparison between slabs reinforced with steel tendons and CFRP tendons in Group D highlights the combined influence of tendon material and slab thickness on deflection control. At a thickness of 220 mm, the steel-reinforced slab (SDD4T1-50) exhibited a deflection of 40.5 mm under 180 kN, while the CFRP-reinforced slab (CDD4T1-50) deflected slightly less, at 37.2 mm under the same load, achieving an 8.15% reduction in deflection. Increasing the slab thickness to 240 mm produced a substantial reduction in deflection for both materials: the steel-reinforced slab (SDD4T2-50) deflected 16.9 mm, whereas the CFRP-reinforced slab (CDD4T2-50) reached 15.7 mm, achieving a 7.1% reduction in deflection. For the 260 mm slabs, the deflection decreased dramatically, with the steel-reinforced slab (SDD4T3-50) at 11.3 and the CFRP-reinforced slab (CDD4T3-50) at 8.4 mm achieving a 25.7% reduction in deflection This confirms that the 260 mm configuration represents the configuration producing the minimum deflection within the investigated parameter range for both materials. Overall, CFRP-reinforced slabs exhibited lower deflection than their steel-reinforced counterparts, with the 260 mm CFRP slab providing the most effective deflection control under elevated loading conditions.
Under low loads, CFRP-reinforced slabs may show higher deflection than steel-reinforced slabs due to CFRP’s lower modulus of elasticity. However, as the applied load increases, steel tendons may reach the yield point, resulting in a rapid rise in deflection. In contrast, CFRP tendons do not exhibit a yield plateau and maintain a linear-elastic response up to failure with a constant modulus of elasticity. This enables CFRP-reinforced slabs to sustain higher load levels while maintaining lower deflection, particularly under elevated loading conditions.
Regarding the maximum load-carrying capacity, the CFRP models with slab thicknesses of 220, 240, and 260 mm reached 187, 215, and 231 kN, respectively, corresponding to increases of approximately 15.0% and 23.5% for the 240 mm and 260 mm slabs, respectively, relative to the 220 mm slab. For steel tendons, the corresponding capacities were 180, 210, and 224 kN, with increases of approximately 16.7% and 24.4%, respectively. Overall, the CFRP tendon models exhibited higher maximum load-carrying capacities than the corresponding steel tendon models, with increases of approximately 3.9%, 2.4%, and 3.1% for slab thicknesses of 220, 240, and 260 mm, respectively.

3.5. Effect of Distribution Distance

The section of Group E (with a 240 mm slab thickness) and Group F (with a 260 mm slab thickness) investigates the effect of tendon distribution distance on the deflection behavior of slabs reinforced with steel or CFRP tendons, as shown in Figure 14.
Figure 14. Mid-span load–deflection curves for (a) group E and (b) group F.
Group E, for steel tendons, the slab with the closest tendon spacing of 4ts (SDD4T2-50) exhibited the lowest deflection of 33.2 mm at a load of 210 kN, representing the best performance among the steel-reinforced slabs in this section as shown in Figure 14a. Increasing the distribution distance to 5ts (SDD5T2-50) resulted in a deflection of 63.9 mm at the same load, corresponding to an increase of approximately 92.5% compared to SDD4T2-50. Further widening the tendon spacing to 6ts (SDD6T2-50) led to a deflection of 110 mm at the same load, corresponding to an increase of 231.3 relative to SDD4T2-50. The increase in deflection resulting from larger tendon spacing is primarily caused by the reduced prestressing efficiency due to the wider spacing. As the tendons are placed farther apart, the prestressing force is applied over fewer locations, lowering the distribution of internal counteracting moments along the slab. This reduces the slab’s ability to resist bending, leading to higher curvature and greater overall deflection under the same applied load. Therefore, closer tendon spacing improves prestress effectiveness, enhances slab stiffness, and helps control deflection in post-tensioned slabs. Subsequently, slabs reinforced with CFRP tendons were analyzed to investigate the effect of tendon distribution distance on deflection behavior. Model CDD4T2-50, with the closest tendon spacing of 4ts, exhibited the lowest deflection of 21.1 mm at a load of 210 kN. Increasing the spacing to 5ts in the next model, CDD5T2-50, resulted in a deflection of 28.7 mm at the same load, corresponding to an increase of approximately 36% compared to CDD4T2-50. Further widening the tendon spacing to 6ts in CDD6T2-50 led to a deflection of 63 mm at the same load, corresponding to an increase of 198.6% relative to CDD4T2-50.
A comparative analysis between the slab reinforced with steel tendons and the slab reinforced with CFRP tendons clearly demonstrates the superior performance of CFRP tendons in controlling deflection. For the closest tendon spacing of 4ts, the steel tendon slab SDD4T2-50 exhibited a deflection of 33.2 mm at a load of 210 kN, while the corresponding CFRP tendon slab CDD4T2-50 deflected only 21.1 mm under the same load, achieving a reduction of approximately 36.4% in deflection. At the 5ts spacing, the steel tendon slab SDD5T2-50 deflected 63.9 mm compared to 28.7 mm in the CFRP tendon slab CDD5T2-50, a reduction of about 55.1%. For the widest spacing of 6ts, the steel tendon slab SDD6T2-50 reached 110 mm, whereas the CFRP tendon slab CDD6T2-50 deflected 63 mm, representing a reduction of roughly 42.73%. The lower deflection observed in slabs reinforced with CFRP tendons is associated with the stable linear-elastic behavior of CFRP and its ability to maintain high tensile stresses without yielding, contributing to improved deflection control under elevated loading conditions. In contrast, slabs reinforced with steel tendons may experience post-yield behavior at higher load levels, which is associated with a more pronounced increase in deflection. Overall, the slab reinforced with CFRP tendons consistently exhibited lower deflection than the slab reinforced with steel tendons across all tendon spacings, with CDD4T2-50 (4ts) showing the lowest deflection in this group.
Group F, for steel tendons, the slab with the closest tendon spacing of 4ts (SDD4T3-50) exhibited the lowest deflection of 17.6 mm at a load of 210 kN, representing the best performance among the steel-reinforced slabs in this group as shown in Figure 14b. Increasing the distribution distance to 5ts (SDD5T3-50) resulted in a deflection of 23.9 mm at the same load, corresponding to an increase of approximately 35.8% compared to SDD4T3-50. Further widening the tendon spacing to 6ts (SDD6T3-50) led to a deflection of 33.5 mm at the same load, corresponding to an increase of about 90.3% relative to SDD4T3-50. The increase in deflection resulting from larger tendon spacing is primarily caused by the reduced prestressing efficiency due to the wider spacing. As the tendon spacing increases, the prestressing force is distributed over a smaller number of tendon locations across the slab, resulting in less effective distribution of the prestressing effect. Consequently, the slab exhibits greater deflection under the same applied load. Therefore, closer tendon spacing provides a more effective distribution of the prestressing force and contributes to improved deflection control in post-tensioned slabs. Subsequently, slabs reinforced with CFRP tendons were analyzed to investigate the effect of tendon distribution distance on deflection behavior. Model CDD4T3-50, with the closest tendon spacing of 4ts, exhibited the lowest deflection of 9.2 mm at a load of 210 kN. Increasing the spacing to 5ts in the next model, CDD5T3-50, resulted in a deflection of 19.1 mm at the same load, corresponding to an increase of approximately107.6% compared to CDD4T3-50. Further widening the tendon spacing to 6ts in CDD6T3-50 led to a deflection of 22.4 mm at the same load, corresponding to an increase of about 143.5% relative to CDD4T3-50.
A comparative analysis between the slab reinforced with steel tendons and the slab reinforced with CFRP tendons clearly demonstrates the superior performance of CFRP tendons in controlling deflection. For the closest tendon spacing of 4ts, the steel tendon slab SDD4T3-50 exhibited a deflection of 17.6 mm at a load of 210 kN, while the corresponding CFRP tendon slab CDD4T3-50 deflected only 9.2 mm under the same load, achieving a reduction of approximately 47.7% in deflection. At the 5ts spacing, the steel tendon slab SDD5T3-50 deflected 23.9 mm compared to 19.1 mm in the CFRP tendon slab CDD5T3-50, a reduction of about 20.1%. For the widest spacing of 6ts, the steel tendon slab SDD6T3-50 reached 33.5 mm, whereas the CFRP tendon slab CDD6T3-50 deflected 22.4 mm, representing a reduction of roughly 33.1%. The reduction in mid-span deflection is attributed to the combined effects of tendon distribution distance, slab thickness, and tendon material behavior. A closer tendon distribution provides more effective control of slab deflection, while the greater slab thickness contributes to greater resistance to deformation. In addition, the stable linear-elastic behavior of CFRP allows the tendons to maintain their tensile resistance without yielding. In contrast, steel tendons may experience post-yield behavior at higher load levels, resulting in a more pronounced increase in mid-span deflection. Overall, the slab reinforced with CFRP tendons consistently outperforms the slab reinforced with steel tendons across all tendon spacings, with CDD4T3-50 (4ts) exhibiting the best performance and the lowest deflection among all analyzed slabs.

3.6. Effect of Prestress Level

Group G (with a 240 mm slab thickness) investigates the effect of prestressing levels on mid-span deflection for both steel and CFRP tendons, as shown in Figure 15, evaluating prestress levels of 20%, 30%, 40% and 50% of the tendon’s ultimate strength. Similarly, Groups H (with a 260 mm slab thickness) examines the same parameters as shown in Figure 16, covering prestress levels of 20%, 30%, 40%, and 50% of the tendon’s ultimate strength.
Figure 15. Mid-span load–deflection curves for group G: (a) steel tendons, (b) CFRP tendons, (c) only the 50% prestress level for steel and CFRP tendons.
Figure 16. Mid-span load–deflection curves for group H: (a) steel tendons, (b) CFRP tendons, (c) only the 50% prestress level for steel and CFRP tendons.
For Group G, representing the 240 mm slab thickness, the deflection behavior of steel tendons was evaluated under different prestressing levels. Model SDD4T2-20, with a prestressing level of 20%, produced a mid-span deflection of 180 mm at a load of 208 kN. Increasing the prestressing level to 30% in model SDD4T2-30 reduced the mid-span deflection to 165.4 mm at the same load, corresponding to a reduction of approximately 8.1% relative to the 20% prestressing level. Further increasing the prestressing level to 40% in model SDD4T2-40 reduced the mid-span deflection to 135.7 mm, corresponding to a reduction of approximately 24.6% relative to the 20% prestressing level. Increasing the prestressing level to 50% in model SDD4T2-50 further reduced the mid-span deflection to 33.3 mm at the same load, corresponding to a reduction of approximately 81.5% relative to the 20% prestressing level, as shown in Figure 15a.
Model SDD4T2-50, with a prestressing level of 50% of the ultimate tendon strength (Pu), exhibited the best deflection performance among the investigated steel tendon models in this group. This demonstrates that increasing the prestressing level improves the slab’s resistance to deformation and effectively reduces the mid-span deflection.
For CFRP tendons, model CDD4T2-20, with a prestressing level of 20%, produced a mid-span deflection of 155.3 mm at a load of 208 kN. Increasing the prestressing level to 30% in model CDD4T2-30 reduced the mid-span deflection to 123.0 mm at the same load, corresponding to a reduction of approximately 20.8% relative to the 20% prestressing level. Further increasing the prestressing level to 40% in model CDD4T2-40 reduced the mid-span deflection to 74.6 mm at the same load, corresponding to a reduction of approximately 52.0% relative to the 20% prestressing level. Increasing the prestressing level to 50% in model CDD4T2-50 further reduced the mid-span deflection to 21.1 mm at the same load, corresponding to a reduction of approximately 86.4% relative to the 20% prestressing level, as shown in Figure 15b.
Model CDD4T2-50, corresponding to a prestressing level of 50% of the ultimate tendon strength (Pu), exhibited the best deflection performance among the investigated CFRP tendon models in this section.
A comparison is made between steel tendons and CFRP tendons for the reinforced concrete slab. For prestressing levels of 20%, 30%, 40%, and 50%, CFRP tendons (CDD4T2-20, CDD4T2-30, CDD4T2-40, and CDD4T2-50) produced mid-span deflections of 155.3 mm, 123 mm, 74.6 mm, and 21.1 mm, respectively, which are significantly lower than the corresponding steel tendon deflections of 180 mm, 165.4 mm, 135.7 mm, and 33.3 mm for models SDD4T2-20, SDD4T2-30, SDD4T2-40, and SDD4T2-50. This corresponds to a reduction in mid-span deflection of approximately 13.7% at a prestressing level of 20%, 25.6% at a prestressing level of 30%, 45% at a prestressing level of 40%, and 36.6% at a prestressing level of 50%. Overall, the best-performing model in this section is the CFRP tendon slab with the prestressing level of 50% (CDD4T2-50) as shown in Figure 15c. This model achieved the lowest mid-span deflection, demonstrating better performance compared with the steel tendon models. The lower deflection can be attributed primarily to the higher prestressing level, which provides greater resistance to deformation and contributes to improved deflection control. In addition, the stable linear-elastic behavior of CFRP tendons allows them to maintain their tensile resistance at higher load levels. In contrast, steel tendons may approach the yield stress at higher load levels, resulting in a more pronounced increase in mid-span deflection.
Regarding the maximum load-carrying capacity, increasing the prestressing level from 20% to 30%, 40%, and 50% increase the capacity of CFRP tendon models from 213 kN to 215, 220, and 225 kN, corresponding to increases of approximately 0.9%, 3.3%, and 5.6%, respectively, relative to the 20% level. For steel tendons, the corresponding capacities increased from 208 kN to 210, 212, and 216 kN, with increases of approximately 1.0%, 1.9%, and 3.8%, respectively. Overall, the CFRP tendon models exhibited higher maximum load-carrying capacities than the corresponding steel tendon models, with increases of approximately 2.4%, 2.4%, 3.8%, and 4.2% at 20%, 30%, 40%, and 50% prestressing levels, respectively.
For Group H, representing the 260 mm slab thickness, the deflection behavior of steel tendons was evaluated under different prestressing levels as shown in Figure 16a. Model SDD4T3-20, with a prestressing level of 20%, produced a mid-span deflection of 62 mm at a load of 210 kN. Increasing the prestressing level to 30% in model SDD4T3-30 reduced the mid-span deflection to 56.8 mm at the same load, corresponding to a reduction of approximately 8.4% relative to the 20% prestressing level. Further increasing the prestressing level to 40% in model SDD4T3-40 reduced the mid-span deflection to 50.7 mm at the same load, corresponding to a reduction of approximately 18.2% relative to the 20% prestressing level. Increasing the prestressing level to 50% in model SDD4T3-50 further reduced the mid-span deflection to 17.6 mm at the same load, corresponding to a reduction of approximately 71.6% relative to the 20% prestressing level. Model SDD4T3-50, with a prestressing level of 50% of the ultimate tendon strength (Pu), exhibited the best deflection performance among the investigated steel tendon models.
For CFRP tendons, model CDD4T3-20, with a prestressing level of 20%, produced a mid-span deflection of 43.5 mm at a load of 210 kN. Increasing the prestressing level to 30% in model CDD4T3-30 reduced the mid-span deflection to 30 mm at the same load, corresponding to a reduction of approximately 31% relative to the 20% prestressing level. Further increasing the prestressing level to 40% in model CDD4T3-40 reduced the mid-span deflection to 25.7 mm at the same load, corresponding to a reduction of approximately 40.9% relative to the 20% prestressing level. Increasing the prestressing level to 50% in model CDD4T3-50 further reduced the mid-span deflection to 9.2 mm at the same load, corresponding to a reduction of approximately 78.9% relative to the 20% prestressing level, as shown in Figure 16b. Model CDD4T3-50, corresponding to a prestressing level of 50% of the ultimate tendon strength (Pu), exhibited the best deflection performance among the investigated CFRP tendon models in this section.
A comparison is made between steel tendons and CFRP tendons for the reinforced concrete slab. For prestressing levels of 20%, 30%, 40%, and 50%, CFRP tendons (CDD4T3-20, CDD4T3-30, CDD4T3-40, and CDD4T3-50) produced mid-span deflections of 43.5 mm, 30 mm, 25.7 mm, and 9.2 mm, respectively, which are significantly lower than the corresponding steel tendon deflections of 62 mm, 56.8 mm, 50.7 mm, and 17.6 mm for models SDD4T3-20, SDD4T3-30, SDD4T3-40, and SDD4T3-50. This corresponds to a reduction in mid-span deflection of approximately 29.8% at a prestressing level of 20%, 47.2% at a prestressing level of 30%, 49.3% at a prestressing level of 40%, and 47.7% at a prestressing level of 50%.
Overall, the best-performing model in this group is the CFRP tendon slab with the prestressing level of 50% (CDD4T3-50) as shown in Figure 16c. This model achieved the lowest mid-span deflection, demonstrating better performance compared with the steel tendon models. The lower deflection can be attributed primarily to the higher prestressing level, while the greater slab thickness also contributes to greater resistance to deformation and improved deflection control. In addition, the stable linear-elastic behavior of CFRP tendons allows them to maintain their tensile resistance at higher load levels. In contrast, steel tendons may approach the yield stress at higher load levels, resulting in a more pronounced increase in mid-span deflection.
Regarding the maximum load-carrying capacity, increasing the prestressing level from 20% to 30%, 40%, and 50% increased the maximum load-carrying capacity of CFRP tendon models from 217 kN to 220, 225, and 231 kN, respectively, corresponding to increases of approximately 1.4%, 3.7%, and 6.5%, respectively, compared with the 20% prestressing level. For steel tendons, the corresponding capacity increased from 210 kN to 218, 222, and 224 kN, with increases of approximately 3.8%, 5.7%, and 6.7%, respectively. Overall, the CFRP tendon models exhibited higher maximum load-carrying capacities than the corresponding steel tendon models at the different prestressing levels, with increases of approximately 3.3%, 0.9%, 1.4%, and 3.1% at the 20%, 30%, 40%, and 50% prestressing levels, respectively.
Based on the overall results, model CDD4T3-50, incorporating CFRP tendons with a distributed–distributed tendon arrangement, a parabolic tendon profile, a prestressing level of 50% of the ultimate tendon strength (Pu), and a slab thickness of 260 mm, exhibited the best overall structural performance and achieved the lowest mid-span deflection among all the investigated models.
The main advantage of CFRP tendons over conventional steel tendons is their higher ultimate tensile strength. This higher tensile strength enables CFRP tendons to sustain higher tensile stresses before reaching their ultimate capacity and is the primary factor contributing to their improved structural performance in the present numerical investigation.

4. Conclusions

In this research, a nonlinear parametric finite element analysis was conducted to investigate two-way unbonded post-tensioned concrete slabs prestressed with either conventional steel or FRP tendons, with particular emphasis on CFRP tendons. The developed FE model was validated against experimental results reported in the literature. A comprehensive parametric study was then conducted to evaluate the effects of tendon material, tendon profile, tendon arrangement, tendon distribution, slab thickness, and prestressing level on the structural response of the post-tensioned slabs. The main conclusions are as follows:
  • Effect of tendon material: Slabs reinforced with CFRP tendons exhibited 48% lower mid-span deflection compared to steel tendons within the investigated tendon systems. This difference is influenced by the combined effects of the tendon material and the applied initial prestressing force. In particular, the higher ultimate tensile strength of CFRP tendons resulted in a higher initial prestressing force when the prestressing level was defined as 50% of the corresponding ultimate tendon strength. Therefore, the observed reduction in deflection reflects the combined influence of the tendon material and prestressing force rather than the intrinsic mechanical properties of CFRP alone.
  • Effect of tendon profile: Slabs with parabolic tendon profiles demonstrated lower mid-span deflection than those with straight tendon profiles, with reductions of approximately 44.5% for steel tendons and 64.4% for CFRP tendons, indicating the greater effectiveness of the parabolic profile in reducing mid-span deflection.
  • Effect of tendon arrangement: Slabs with a distributed–distributed tendon layout showed better control of mid-span deflection compared with the other tendon arrangements, with reductions of approximately 44.8% for CFRP tendons and 37.3% for steel tendons compared with the banded–banded arrangement, demonstrating its effectiveness in minimizing mid-span deflection.
  • Effect of slab thickness: Thicker slabs exhibited reduced mid-span deflection under the applied loading conditions. For the increase in slab thickness from 220 mm to 260 mm, the mid-span deflection was reduced by approximately 72.1% for steel tendons and 77.4% for CFRP tendons. This reduction indicates that greater slab thickness provides higher resistance to deformation, resulting in improved control of mid-span deflection compared with thinner slabs.
  • Effect of distribution distance: Slabs with closer tendon spacing exhibited lower mid-span deflection under the same applied load. Reducing the distribution distance from 6ts to 4ts resulted in a reduction in mid-span deflection of approximately 47.5% for steel tendons and 58.9% for CFRP tendons.
  • Effect of prestressing level: Slabs with a prestressing level of 50% exhibited lower mid-span deflection within the investigated models. Increasing the prestressing level from 20% to 50% reduced the mid-span deflection by approximately 71.6% for steel tendons and 78.9% for CFRP tendons. The higher prestressing level provides a greater prestressing force, which improves the slab’s resistance to deformation and results in better control of mid-span deflection compared with lower prestressing levels.
  • The maximum load-carrying capacity increased with increasing slab thickness and with a distributed–distributed tendon arrangement. Increasing the slab thickness from 220 to 260 mm increased the maximum load-carrying capacity by approximately 23.5% for CFRP tendons and 24.4% for steel tendons, while changing the tendon arrangement from banded–banded to distributed–distributed increased the capacity by approximately 24.9% for CFRP tendons and 22.4% for steel tendons. In the comparison between CFRP and steel tendons, the CFRP models achieved increases in maximum load-carrying capacity of up to approximately 3.9%.
  • Combined effects of all parameters: Slabs with CFRP tendons arranged in a distributed–distributed configuration, subjected to a prestressing level of 50%, with a parabolic tendon profile and increased slab thickness, achieved the lowest mid-span deflection. This combination of tendon material, arrangement, prestressing level, tendon profile, and slab thickness resulted in the most favorable overall flexural performance within the investigated parameter range.
  • CFRP tendons offer superior structural performance compared to steel. Although they may show slightly higher initial deflection due to lower stiffness, they maintain a linear-elastic response without yielding, ensuring better stiffness retention under higher loads. In contrast, steel tendons may reach their yield stress at higher load levels, leading to increased deflection under the same loading conditions. Overall, CFRP provides improved deflection control and more reliable performance under elevated loading conditions.
  • CFRP tendons offer several advantages over conventional steel tendons, primarily attributed to their higher ultimate tensile strength, which allows them to withstand higher tensile stresses before failure.

Author Contributions

Conceptualization, H.A.M., A.E. (Ahmed Elbelbisi), and S.E.; methodology, H.A.M.; software, A.E. (Ahmed Elbelbisi) and S.E.; validation, A.E. (Ahmed Elbelbisi) and S.E.; formal analysis, A.E. (Ahmed Elbelbisi) and S.E.; investigation, H.A.M., A.E. (Ahmed Elbelbisi), and S.E.; data curation, A.E. (Ahmed Elbelbisi) and S.E.; writing—original draft preparation, S.E.; writing—review and editing, H.A.M., H.A., A.E. (Ahmed Elbelbisi), and A.E. (Ahmed Elkilani); visualization, A.E. (Ahmed Elbelbisi), A.E. (Ahmed Elkilani), and S.E.; supervision, H.A.M., H.A., and A.E. (Ahmed Elbelbisi). All authors have read and agreed to the published version of the manuscript.

Funding

This research received no external funding.

Data Availability Statement

The data that supported the findings of this study are available from the corresponding author upon reasonable request.

Conflicts of Interest

The authors declare no conflict of interest.

References

  1. Concrete, A.M. Properties of Concrete, 5th ed.; Longman: London, UK, 1995. [Google Scholar]
  2. Mehta, P.K.; Monteiro, P.J.M. Concrete Microstructure, Properties, and Materials; McGraw-Hill: New York, NY, USA, 2006. [Google Scholar]
  3. Committee, A.C.I. Guide to Durable Concrete; American Concrete Institute: Farmington Hills, MI, USA, 2001. [Google Scholar]
  4. Darwin, D.; Dolan, C.W.; Nilson, A.H. Design of Concrete Structures; McGraw-Hill Education: New York, NY, USA, 2016. [Google Scholar]
  5. Dolan, C.W.; Hamilton, H.R., III; Bakis, C.E.; Nanni, A. Design Recommendations for Concrete Structures Prestressed with FRP Tendons; Federal Highway Administration, FHWA: Washington, DC, USA, 2001.
  6. Mohamed, G.; Sakr, T.; Mohamed, G.H. Post tensioned floors as an economic alternative in Egyptian market (case study). Egypt. Int. J. Eng. Sci. Technol. 2015, 18, 2–3. [Google Scholar] [CrossRef] [Scilit]
  7. Ellobody, E.; Bailey, C.G. Behaviour of unbonded post-tensioned one-way concrete slabs. Adv. Struct. Eng. 2008, 11, 107–120. [Google Scholar] [CrossRef] [Scilit]
  8. Bank, L.C. Composites for Construction: Structural Design With FRP Materials; John Wiley & Sons: Hoboken, NJ, USA, 2006. [Google Scholar]
  9. Abaza, E.; Elshazli, M.T.; Elbelbisi, A.; Shehab, H.; Zaghlal, M. Punching Strengthening of Lightweight Aggregate Reinforced Concrete Flat Slabs Using Fiber-Reinforced Polymers. J. Compos. Sci. 2025, 9, 485. [Google Scholar] [CrossRef] [Scilit]
  10. Vijayan, D.S.; Sivasuriyan, A.; Devarajan, P.; Stefańska, A.; Wodzyński, Ł.; Koda, E. Carbon fibre-Reinforced Polymer (CFRP) Composites in Civil Engineering Application—A Comprehensive Review. Buildings 2023, 13, 1509. [Google Scholar] [CrossRef] [Scilit]
  11. Fico, R.; Galati, N.; Prota, A.; Nanni, A. Design and construction of a bridge deck using mild and post-tensioned FRP bars. Spec. Publ. 2005, 230, 1121–1138. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  12. Gąćkowski, R. Determination of limit states of precast beams with large spans in densely ribbed floors, reinforced with CFCC composite tendons. Mater. Bud. 2025, 638, 214–223. [Google Scholar] [CrossRef] [Scilit]
  13. Nassif, H.; Nasreddine, W.; Ünal, G.; Harajli, M. Nominal Flexural Strength of Concrete Members Prestressed with Hybrid Tendons. ACI Struct. J. 2026, 123, 133. [Google Scholar] [CrossRef] [Scilit]
  14. Alsuwaidi, H.; Habib, A.; Al-Sadoon, Z.A.; Maalej, M.; Altoubat, S.; Barakat, S.; Junaid, M.T. Rehabilitation of Partially Corrosion-Damaged Post-Tensioned Concrete Structures using Carbon Fiber Reinforced Polymer. Civ. Eng. J. 2025, 11, 2170–2188. [Google Scholar] [CrossRef] [Scilit]
  15. Abdel-Jaber, M.; Magharbeh, L.; Shhabat, M.; Ashteyat, A. Strengthening and repairing of a one-way solid slab exposed to thermal effect using CFRP Grid. Compos. Part C Open Access 2026, 19, 100694. [Google Scholar] [CrossRef] [Scilit]
  16. Grace, N.; Enomoto, T.; Baah, P.; Bebawy, M. Flexural behavior of CFRP precast prestressed decked bulb T-beams. J. Compos. Constr. 2012, 16, 225–234. [Google Scholar] [CrossRef] [Scilit]
  17. Lee, C.; Shin, S.; Lee, S. Modelling of load–deflection of concrete beams internally prestressed with unbonded CFRP tendons. Mag. Concr. Res. 2015, 67, 730–746. [Google Scholar] [CrossRef] [Scilit]
  18. Elbelbisi, A.H.; El-Sisi, A.A.; Hassan, H.A.; Salim, H.A.; Shabaan, H.F. Parametric study on steel–concrete composite beams strengthened with post-tensioned CFRP tendons. Sustainability 2022, 14, 15792. [Google Scholar] [CrossRef] [Scilit]
  19. Le, T.D.; Pham, T.M.; Hao, H.; Yuan, C. Performance of precast segmental concrete beams posttensioned with carbon fiber-reinforced polymer (CFRP) tendons. Compos. Struct. 2019, 208, 56–69. [Google Scholar] [CrossRef] [Scilit]
  20. El-Belbisi, A. Strengthening of Pre-stressed Steel–Concrete Composite Beams Using Carbon Fiber Tendons–A Parametric Study. Arch. Med. 2018, 4. [Google Scholar] [CrossRef] [Scilit]
  21. Alsharari, F.; El-Zohairy, A.; Salim, H.; El-Sisi, A.E.-D. Pre-damage effect on the residual behavior of externally post-tensioned fatigued steel-concrete composite beams. Structures 2021, 4, 578–587. [Google Scholar] [CrossRef] [Scilit]
  22. Elgholmy, L.; Salim, H.; Elsisi, A.; Salama, A.; Shaaban, H.; Elbelbisi, A. Prestressed CFRP Plates and Tendon Strengthening of Steel–Concrete Composite Beams. J. Compos. Sci. 2024, 8, 301. [Google Scholar] [CrossRef] [Scilit]
  23. Alsharari, F.; El-Sisi, A.E.-D.; Mutnbak, M.; Salim, H.; El-Zohairy, A. Effect of the progressive failure of shear connectors on the behavior of steel-reinforced concrete composite girders. Buildings 2022, 12, 596. [Google Scholar] [CrossRef] [Scilit]
  24. El-Sisi, A.E.; Saucier, A.; Salim, H.A.; Hoemann, J.M. Experimental and numerical evaluation of reinforced concrete walls retrofit systems for blast mitigation. J. Perform. Constr. Facil. 2019, 33, 04018113. [Google Scholar] [CrossRef] [Scilit]
Disclaimer/Publisher’s Note: The statements, opinions and data contained in all publications are solely those of the individual author(s) and contributor(s) and not of MDPI and/or the editor(s). MDPI and/or the editor(s) disclaim responsibility for any injury to people or property resulting from any ideas, methods, instructions or products referred to in the content.

Article Metrics

Citations

Article Access Statistics

Multiple requests from the same IP address are counted as one view.