Abstract
This study investigated the salt-coated high-temperature corrosion behavior and post-corrosion mechanical properties of 316L stainless-steel joints vacuum-brazed with three typical nickel-based filler metals: Ni-Cr-B, Ni-Cr-B-Si and Ni-Cr-Si. Salt-coated corrosion tests were conducted at 850 °C in air with NaCl deposition for up to eight cycles. In B-containing joints, CrB precipitates formed in the diffusion-affected zone, and corrosion propagated inward along their distribution paths. In the Ni-Cr-Si joint, selective oxidation of the continuously distributed Ni₃Si phase induced volume expansion and cracking, accelerating localized corrosion. This continuous Ni₃Si network was suppressed in the Ni-Cr-B-Si joint, as B preferentially reacts with Cr to form boride precipitates, which alters the solidification path and solute segregation behavior and reduces the continuity of Si-rich intermetallic phases at the seam center. The corrosion resistance follows the order Ni-Cr-B > Ni-Cr-B-Si > Ni-Cr-Si. After eight cycles, the Ni-Cr-Si joint reaches a relative corrosion depth of approximately 145 μm, approximately 32% higher than that of the Ni-Cr-B joint. The Ni-Cr-B joint retains the highest post-corrosion tensile strength (339 MPa, 38% decrease from the as-brazed state), while the Ni-Cr-Si joint suffers the most severe degradation (130 MPa, 78% decrease). These findings provide a reference for filler metal selection in high-temperature chloride-laden service environments.