Ultrasonic Pulse-Echo Evaluation of Resistance Spot-Welded Joints in Thin Car-Body Steel Sheets

,
,
,
,
,
and
1
Faculty of Civil and Transport Engineering, Poznan University of Technology, 61-131 Poznan, Poland
2
Faculty of Mechanical Engineering, Poznan University of Technology, 60-131 Poznan, Poland
3
Department of Transport Engineering and Logistics Systems,Abylkas Saginov Karaganda Technical University, 56 N. Nazarbayev Avenue, 100027 Karaganda, Kazakhstan
*
Author to whom correspondence should be addressed.
Appl. Sci.2026, 16(22), 11503;https://doi.org/10.3390/app162211503 
(registering DOI)
This article belongs to the Special Issue Applications of Ultrasonic Waves for Non-Destructive Testing

Abstract

Resistance spot welding is the principal joining process for car bodies, and the condition of several thousand welds per vehicle has to be confirmed without destroying the product. This study examined to what extent the ultrasonic pulse-echo technique, applied with a universal flaw detector, identifies the condition of spot welds in thin car-body steel sheet. In total, 150 lap joints of 0.7 mm sheet were welded at constant electrode force with 15 combinations of voltage (2.10, 2.94 and 4.22 V) and weld time (0.2–1.0 s). Each weld was tested three times with a 20 MHz delay-line probe. The numbers of back-wall and intermediate echoes as well as the residual joint thickness (RWS) were recorded. Welds made at 2.10 V showed intermediate echoes from the unfused sheet interface and an RWS of 1.27–1.30 mm, consistent with an undersized nugget. At 2.94 V, no intermediate echoes were recorded at welding times of 0.2 and 0.4 s, whereas some readings at 0.6 s contained intermediate echoes, resulting in mixed ultrasonic indications for series h. Excess heat input (4.22 V, or 2.94 V for 0.8–1.0 s) reduced the number of back-wall echoes to about one per reading and often caused a complete loss of signal. Used jointly, the three indications distinguished echo patterns interpreted as undersized, correctly formed and overheated welds, and suggested a preliminary parameter range of 2.94 V and 0.2–0.6 s for the tested set-up, which requires verification by destructive testing.