Abstract
Fluorocarbon (FC)/Pd/Mg multilayer thin films have attracted considerable attention as hydrogen-responsive optical materials. However, their performance is strongly limited by interfacial instability and structural degradation during deposition and hydrogen cycling. In this study, Pt/FC/Pd/Mg multilayer thin films were obtained during focused ion beam (FIB) sample preparation, and transmission electron microscopy (TEM) was employed to investigate the FC layer–mediated interfacial effects. The results reveal that Pt deposition on FC leads to the formation of a confined nanocrystalline interfacial region accompanied by a reduced apparent FC thickness and the development of a Pt–FC intermixing zone. This behavior indicates that the FC layer functions as a “soft landing” medium, dissipating kinetic energy and modifying nucleation and growth behavior. Motivated by this finding, the mechanical properties of FC films and their influence on hydrogen-cycling performance in FC/Pd/Mg/FC structures are further examined. The hardness of FC layers can be tuned from 3.03 MPa to 42.8 MPa by adjusting sputtering parameters. Hydrogen-cycling experiments reveal a strong and non-monotonic dependence on FC mechanical properties. When the FC buffer layer is relatively hard, the initial hydrogenation kinetics are improved; however, prolonged cycling leads to poor adhesion and interfacial degradation. In contrast, when the FC buffer layer is soft, hydrogenation kinetics degrade rapidly during cycling, while long-term interfacial adhesion and structural integrity are significantly improved. These results demonstrate a dual and competing role of FC layers in governing hydrogen transport and mechanical stability, highlighting a critical trade-off for the design of durable hydrogen-responsive multilayer thin films.