Abstract
Polymer concrete (PC) is widely recognized for its high strength, rapid curing, and superior durability; however, its inherently brittle behavior limits its performance under flexural loading. Fiber-reinforcement is commonly used to enhance toughness and crack resistance, yet high fiber contents often result in workability loss, fiber agglomeration, and increased material heterogeneity. In this study, the mechanical behavior of PC incorporating low dosages of chopped polypropylene (PP) fibers was investigated, complemented by qualitative fracture-surface observations. A Box–Behnken experimental design was employed in which the dosages of 6 mm PP fibers (F6) and 12 mm PP fibers (F12) were independently varied from 0 to 0.30 wt% of the fiber-free base mixture, while the resin content ranged from 18 to 22 wt%, to evaluate their effects on density, flexural strength, compressive strength, and ultrasonic pulse velocity (UPV). Mechanical tests were complemented by ultrasonic pulse velocity (UPV) measurements, and selected fracture surfaces were examined by digital microscopy to qualitatively document visible fracture features and localized fiber-crack interactions, without quantitative microstructural measurements. The principal quantitative findings were: (i) density ranged from 1700 to 1890 kg/m3, with resin content producing the dominant statistically significant effect; (ii) flexural strength ranged from 18.18 to 23.21 MPa, and the investigated factors did not yield a meaningful predictive model for this response; and (iii) compressive strength ranged from 53.99 to 60.94 MPa, with resin content the only statistically significant factor (p = 0.0012), while the F12 term approached but did not reach statistical significance (p = 0.0635). The overall compressive strength model was significant (p = 0.0045) and exhibited limited predictive capability (predicted R2 = 0.442). UPV showed a statistically significant resin content effect (p = 0.0028), but the UPV model had limited predictive capability (predicted R2 = 0.229). Qualitative fracture-surface observations showed matrix cracking together with localized fiber bridging and pullout. Within the investigated low fiber design space, these local interactions were not accompanied by a systematic enhancement of the measured global strength responses.