Abstract
DD5 Ni-based single-crystal superalloy was diffusion-brazed using Ni-based (NB) and Co-based (CB) filler alloys to systematically investigate the effects of filler alloy composition on joint microstructure, secondary phase formation, microhardness, and high-temperature tensile properties at 870 °C. The relationship between microstructural characteristics and fracture behavior was also examined. Both filler alloys produced sound metallurgical joints without obvious pores or cracks. The CB joint exhibited a brazed seam width of approximately 353.1 μm, slightly larger than that of the NB joint (348.0 μm), while significant differences were observed in grain size and secondary phase distribution. The CB joint exhibited a finer polycrystalline microstructure, with an average grain size of 56.3 μm, compared with 79.5 μm for the NB joint. Microstructural characterization revealed that the CB joint consisted primarily of a NiCo-rich γ matrix and skeletal WCo-rich and WCr-rich secondary phases, with area fractions of approximately 3.1% and 0.2%, respectively. In contrast, the NB joint contained WCr-rich and Cr-rich σ phases, with corresponding area fractions of 1.6% and 0.9%. The CB joint exhibited a higher peak microhardness of approximately 690 HV0.2 compared with 610 HV0.2 for the NB joint, which may be associated with the strengthening contribution of the WCo-rich phase. At 870 °C, the CB joint achieved an average tensile strength of 630 MPa, representing an improvement of approximately 34% over the NB joint (470 MPa). Fractographic analysis revealed that the CB joint exhibited a mixed fracture mode characterized by dimples and localized cleavage-like steps, whereas the NB joint displayed predominantly cleavage-like fracture features, with cracks preferentially initiating and propagating near the WCr-rich and Cr-rich σ phases. In comparison, the WCo-rich phase in the CB joint may contribute to enhanced local deformation resistance and reduced susceptibility to rapid crack propagation. These findings indicate that the nature, morphology, and spatial distribution of secondary phases play important roles in governing the high-temperature tensile behavior of brazed joints, highlighting the potential of Co-based filler alloys for improving the high-temperature load-bearing capability of DD5 single-crystal superalloy joints.