Skip to Content
You are currently on the new version of our website. Access the old version .
MaterialsMaterials
  • Article
  • Open Access

8 January 2025

18 Pages

Laser Powder Bed Fusion of a Novel Crack-Free γ′ Phase-Strengthened Ni-Based Alloy

,
,
,
,
and
1
Shenzhen Research Institute of Shandong University, Shenzhen 518057, China
2
Key Laboratory of High Efficiency and Clean Mechanical Manufacture of Ministry of Education, School of Mechanical Engineering, Shandong University, Jinan 250061, China
3
School of Automotive Engineering, Weifang Vocational College, Weifang 262737, China
*
Authors to whom correspondence should be addressed.

Abstract

Laser powder bed fusion (LPBF)-fabricated Ni-based alloys with high γ′ phase fractions generally suffer from cracking that limits their applications. This study presents SD247, a novel alloy that overcomes the challenge of cracking issues and exhibits superior mechanical properties after heat treatment. Compared to CM247LC, SD247 exhibited a lower cracking tendency due to alloying element modification. After heat treatment, SD247 features primary γ′ phases with an average diameter of 306 nm and secondary γ′ phases averaging 25 nm, with few Ta- and Ti-rich MC-type carbides. The columnar grain structure in as-built specimens largely disappeared, and the fraction of grains in soft orientations decreased by 12.8%. The microhardness and ultimate tensile strength increased by 30% and 20%, respectively. These findings demonstrate that the superior LPBF fabrication of Ni-based alloys with a high γ′ fraction can be achieved. Because of the excellent mechanical properties and acceptable cost, LPBF-fabricated SD247 shows great potential in aerospace hot-end components.