- Article
AISI 5120 steel, which underwent 30 min single-surface nanocrystallization via supersonic fine particle bombarding (SFPB), was pre-boronized at 600 °C for 2 h, and then final-boronized at 800 °C or 900 °C for 2–6 h, i.e., two-step p...
AISI 5120 steel, which underwent 30 min single-surface nanocrystallization via supersonic fine particle bombarding (SFPB), was pre-boronized at 600 °C for 2 h, and then final-boronized at 800 °C or 900 °C for 2–6 h, i.e., two-step p...
In this study, a two-step pack cementation process (preboronizing and then chromizing) was employed to prepare the B-Cr duplex-alloyed coating on the steel. After the first step of preboronizing (PB sample), box-type furnace chromizing (BC-1 sample)...
The use of molybdenum-based alloys as materials for components operating under high temperatures and significant mechanical loads is widely recognized due to their excellent mechanical properties. However, their low high-temperature resistance remain...
Boron and arsenic triiodides (BI3 and AsI3, respectively) are similar molecules that differ mainly in their geometries. BI3 is a planar trigonal molecule with D3h symmetry, while AsI3 exhibits a trigonal pyramidal shape with C3v symmetry. Consequentl...