Degradation of Anion Exchange Membrane Water Electrolyzers Under Shutdown and Open-Circuit Transients: Protocols, Mechanisms, Diagnostics, and Mitigation

and
Department of Energy (DENERG), Politecnico di Torino, Corso Duca Degli Abruzzi 24, 10129 Torino, Italy
*
Author to whom correspondence should be addressed.
Hydrogen2026, 7(4), 195;https://doi.org/10.3390/hydrogen7040195 
(registering DOI)

Abstract

Anion exchange membrane water electrolyzers (AEMELs) are attractive for direct coupling to variable renewable supply, but their durability under the resulting transients is poorly constrained. This review examines AEMEL degradation under the intermittent test protocols reported at cell and stack level, focusing on the shutdown and open-circuit portions of those protocols. We classify the protocols by the electrical route through which the stop is imposed and set out what each reproduces of renewable-driven operation and what it does not. Reported degradation figures are re-expressed on a common per-cycle basis so that studies using different metrics, current densities and cycle counts can be compared. Three recurring losses emerge: oxidation and dissolution of non-noble hydrogen-evolution catalysts, ohmic drift of the membrane and ionomer after dry stops, and structural reorganization of the electrode under repeated reverse current. In the single cells resolved so far, open-circuit and reverse-current stops load the cathode, with a loss that scales with the cathode metal’s stability; severity is set by the boundary conditions at the stop rather than by intermittency as such. Diagnostics and mitigation are assessed on that basis. The evidence base remains small, dominated by single cells, and rarely electrode-resolved, with one anode chemistry tested.

Article Metrics

Citations

Article Access Statistics

Multiple requests from the same IP address are counted as one view.