Evaluation of Self-Healing and Microstructure of Nano-Silica Engineered Cementitious Composites Reinforced with Glass Fiber

and
Civil Engineering Department, University of Technology-Iraq, Baghdad 10066, Iraq
*
Authors to whom correspondence should be addressed.
Eng2026, 7(12), 666;https://doi.org/10.3390/eng7120666 
(registering DOI)
This article belongs to the Section Materials Engineering

Abstract

This experimental work has investigated the effect of adding nano-silica (NS) at percentages of (1.5, 2.0, 2.5)% by weight of the total cementitious binder (CB) as a replacement on the self-healing and microstructure of engineered cementitious composites (ECC). A flow table test was conducted for fresh properties evaluation, and physical tests including density, porosity, and absorption were carried out. Besides that, mechanical tests were conducted, involving compression, flexural, and direct tension tests. Also, self-healing was evaluated by pre-cracking (50 × 50 × 50) mm cube specimens using a concentrated load under uniaxial compression, forming cracks with maximum widths ranging between 0.40 and 0.63 mm. Tests were conducted, including crack width measurement and closure monitoring over time, measurement of electrical resistivity change during the healing process, and measurement of compressive strength after 28 days under different types of curing conditions, namely moisture curing and carbonation curing. X-ray diffraction (XRD), scanning electron microscopy (SEM), and energy-dispersive X-ray (EDX) were performed for microstructural analysis for the REF mix and NS2.0 for both wet- and carbonation-cured specimens. The results show improvement in compressive, flexural, and direct tension strength for smart ECC containing nano-silica at 2.0%. The results revealed that the best average compressive strength of pre-cracked specimens under wet curing conditions was obtained from a mix containing 2% nano-silica, at 35.8 MPa. The best average compressive strength of pre-cracked specimens under carbonation curing conditions was obtained from a mix containing 2.0% nano-silica with 1% glass fiber, at 47.96 MPa. The best crack closure rate was obtained from the 2.0% NS mixture under wet curing conditions, with the maximum sealed crack width of 0.47 mm. Also, the highest compressive strength improvement (25.44%) and direct tensile strength improvement (45.18%) were obtained from the 2.0% NS mixture; the flexural strength improvement (87.19%) was obtained from the 2.5% NS mixture.

Article Metrics

Citations

Article Access Statistics

Article metric data becomes available approximately 24 hours after publication online.