Abstract
High-CaCO3-content polymer composites suffer from particle agglomeration and limited flowability. Here, a processable CaCO3-rich material (TP-CaCO3) was prepared without a polymer matrix using citric acid (CA), glycerol (Gly), and twin-screw thermomechanical processing. CA treatment influenced aggregation and redispersion, reducing the Z-average hydrodynamic diameter from 4773 to 311.1 nm. TP-CaCO3 retained the calcite structure but exhibited altered surface chemistry and multistep thermal mass loss. Acid-induced CO2 analysis yielded an apparent CaCO3-equivalent content of 53.01 ± 4.42%. A CaCO3/CA/Gly ratio of 100:40:20 processed at 180 °C yielded a compressive strength of 73.4 MPa. Increasing Gly content from 20 to 30 wt% relative to initial CaCO3 increased the melt flow rate from 5.05 to 9.73 g/10 min, with reduced compressive strength. Isothermal TGA revealed mass loss at 180 and 190 °C, requiring caution when interpreting flow behavior. DSC heating scans differed, without a conventional melting peak. Compared with direct hot pressing of the unextruded mixture, extrusion improved forming quality and compressive strength. After two additional extrusion passes, TP-CaCO3 retained 96.42% of its initial compressive strength. Composites containing 60–90 wt% TP-CaCO3 were obtained by melt blending with linear low-density polyethylene (LLDPE).