Abstract
Electrodeposition of coarse-grit diamond tools with complex profiles is affected by nonuniform current distribution and coating-thickness variations. This study investigated a conformal anode combined with stepwise-increasing current for a 20° inclined working surface. COMSOL Multiphysics 6.4 simulations were performed to evaluate current-density distributions, while grit-free electrodeposition experiments were conducted to assess coating-thickness dispersion. Three current-loading schedules were compared using independently prepared specimens (n = 3 per schedule) under approximately matched nominal charge input. In the simulations, the conformal anode reduced the current-density mirror-asymmetry coefficient (AJ) from 11.51% to 1.87%, while the experiments showed a reduction in the coating-thickness coefficient of variation (CVT) from 4.54% to 2.74% within the measured inner region. Among the three schedules, stepwise-increasing current yielded the lowest mean coefficient of variation in grit number (CVN, 2.04 ± 0.21%) and regional grit-height range (ΔHR, 95.64 ± 1.00 μm). Compared with the constant-current schedule, the stepwise-increasing-current schedule reduced the grit-fixation duration from 120 to 80.4 min, corresponding to a reduction of approximately 33%. A double-working-surface diamond dressing roller fabricated using the combined process exhibited CVN values of 1.40% and 1.15% on its two working surfaces and a representative ΔHR of 95.45 μm. These results support the feasibility of the proposed approach for the investigated geometry, while further evaluation is needed to establish its effects on dressing performance.