Skip to Content
MaterialsMaterials
  • Article
  • Open Access

25 November 2026

25 Pages

Mechanistic Understanding of Early Strength Development and Shrinkage Mitigation in Low-Clinker High-Volume Slag Binders: Further Performance Enhancement Through Particle Packing Optimization Under Desulfurization Gypsum Activation

and
1
Department of Highway and Railway Engineering, Liaoning Provincial College of Communications, Shenyang 110122, China
2
Liaoning Key Laboratory of Bridge Safety Engineering, Liaoning Provincial College of Communications, Shenyang 110122, China
3
School of Civil Engineering, Shenyang Jianzhu University, Shenyang 110168, China
*
Author to whom correspondence should be addressed.
This article belongs to the Section Construction and Building Materials

Abstract

Low-clinker high-volume slag binders offer considerable potential for reducing Portland cement consumption and associated carbon emissions, but their early-age strength development and drying shrinkage remain challenging under mild activation conditions. This study investigates the combined use of hemihydrate flue gas desulfurization gypsum (HFGD gypsum) activation and particle size distribution adjustment of ground granulated blast-furnace slag (GGBFS) to improve binder performance without strong alkaline activators. The effects of HFGD gypsum dosage were evaluated, and GGBFS gradation was adjusted using the modified Andreasen–Andersen model. Results indicate that 10% HFGD gypsum provides favorable early strength development by promoting ettringite (AFt) formation, whereas excessive gypsum addition leads to increased residual gypsum and reduced strength. At identical binder compositions, particle size distribution adjustment increased the maximum wet-packing solid volume concentration from 61.58% to 63.56% and enhanced 3-day compressive strength from 10.8 to 19.9 MPa, representing an increase of 84.3%. Isothermal calorimetry revealed accelerated early hydration, with the optimized mixture exhibiting 27.946 J/g higher cumulative heat release at 72 h. Meanwhile, mercury intrusion porosimetry showed that 3-day porosity decreased from 14.17% to 7.66%, while 40-day drying shrinkage was reduced by approximately 11.4%. Combined QXRD and SEM–EDS analyses suggest that the enhanced performance was associated with improved initial particle packing, accelerated hydration, and a more favorable distribution of hydration products, rather than increased AFt content alone. These findings highlight particle size distribution adjustment under moderate sulfate activation as an effective strategy for improving early strength, pore structure, and dimensional stability in low-clinker high-volume slag binders.