Abstract
Aggressive ions attack reinforcing steel in saline soil environments, and once the passive film on HRB400 steel destabilizes, localized corrosion spreads rapidly. Most studies vary the concentration of a single ion; how the SO42−/Cl− ratio governs film breakdown remains unclear. HRB400 specimens were immersed in simulated concrete pore solution and dosed stepwise with solid salts. Single-chloride and single-sulfate systems were used as controls; combined systems had SO42−/Cl− ratios of 1, 3 and 5. OCP, LPR and EIS were recorded at every step, with SEM/EDS on selected specimens. With chloride alone the passive film destabilized at 0.03–0.04 mol/L Cl− (mean OCP); with sulfate alone the corrosion current density fell up to 0.05 mol/L SO42−, and the destabilization occurred only at 0.11–0.12 mol/L. Raising the ratio shifted destabilization to 0.05–0.06, 0.06–0.07 and 0.11–0.12 mol/L, about 1.57, 1.86 and 3.29 times the chloride-only value, and at 0.10 mol/L Cl− (240 h) mean icorr fell from 7.71 to 5.98, 3.19 and 1.26 μA/cm2 (n = 3). Na+ and K+ were not varied independently; the concentrations refer to the pore solution. Sulfate therefore delays rather than prevents destabilization, and the ratio, not the chloride concentration alone, determines when the film fails.