Skip to Content
EntropyEntropy
  • Article
  • Open Access

26 November 2026

16 Pages

Effects of Composition Adjustment on Soft Magnetic Properties and Microstructure in Fe-Co-Ni Medium-Entropy Alloys

,
,
,
,
and
1
State Key Laboratory of Materials for Advanced Nuclear Energy, Shanghai University, Shanghai 200444, China
2
Suzhou Wave Vector Advanced Materials Technology Co., Ltd., Suzhou 215331, China
*
Author to whom correspondence should be addressed.
Entropy2026, 28(12), 1313;https://doi.org/10.3390/e28121313 
(registering DOI)
This article belongs to the Special Issue Recent Advances in High Entropy Alloys, 2nd Edition

Abstract

Fe-Co-Ni medium-entropy alloys (MEAs) show great soft-magnetic potential, yet the effect of intrinsic Fe-Co-Ni ratio adjustment (without extra alloying additions) on microstructure and magnetic behaviors is poorly clarified. In this study, Fe100−x(Co0.5Ni0.5)x (x = 10–80 at%) alloys were prepared by vacuum arc melting and characterized by X-ray diffraction (XRD), scanning electron microscopy-energy dispersive X-ray spectroscopy (SEM-EDS), electron backscatter diffraction (EBSD), vibrating sample magnetometer (VSM) and direct current (DC) soft magnetic measurements to reveal the influences of composition tuning on phase, microstructure, mechanical and soft-magnetic properties. With increasing x, the alloys transform from single BCC, through BCC+FCC dual-phase, to single FCC structure. Notably, all alloys with x ≤ 40 possess high saturation magnetization (Ms) exceeding 200 Am2/kg. This high Ms is attributed to a Fe-Co-enriched BCC phase. Across the whole composition range, Ms monotonically decreases from 220 Am2/kg to 138 Am2/kg, while coercivity (Hc) varies non-monotonically and peaks at x = 40. The maximum Hc originates from Ni grain-boundary segregation, fine grains, high fraction of low-angle grain boundaries (LAGBs) and severe local strain concentration. The x = 70 single FCC alloy delivers optimal DC soft-magnetic properties: initial permeability (μi) of 539, maximum permeability (μm) of 1464, low Hc of 36 A/m and saturation flux density (Bm) of 1.60 T. This work clarifies how phase constitution, grain features and strain govern magnetic responses and provides practical guidelines for designing high performance soft-magnetic MEAs.