Skip to Content
  • Proceeding Paper
  • Open Access

13 November 2026

Assessment of the Impact of Accelerated Ageing on the Fire Behaviour of Interior Finishing Materials in Public Transport †

,
,
,
,
and
1
Faculty of Civil and Mechanical Engineering, Universidad Técnica de Ambato, Av. Los Chasquis y Río Payamino, Ambato 180207, Ecuador
2
Department of Mechanical and Production Engineering, Federal University of São João del-Rei (UFSJ), Praça Frei Orlando 170, São João del-Rei 36307-352, MG, Brazil
3
Faculty of Engineering and Applied Sciences, Universidad Técnica de Cotopaxi, Av. Simón Rodríguez s/n, Barrio El Ejido, Latacunga 050108, Ecuador
*
Author to whom correspondence should be addressed.
Eng. Proc.2026, 165(1), 4;https://doi.org/10.3390/engproc2026165004 
(registering DOI)

Abstract

The impact of artificial aging on PRANNA and VINYL was evaluated. Bus interior materials are exposed to UV radiation and humidity, yet regulations assess only pristine materials. This study evaluates both after 0, 125, and 250 h of xenon-arc aging. Analysis revealed surface degradation and an SSIM collapse of 0.73 for fabric and 0.55 for VINYL. Mechanically, VINYL underwent softening from 83.5 to 80.1 and increased stiffness to 490.22 µN·m. This change did not alter its burn rate but caused mass transfer occlusion, which triggered CO emissions at 250 h; PRANNA exhibited a nonlinear response, with softening from 68.0 to 60.4 and a loss of stiffness followed by delayed stiffening (1578 µN·m), accelerating flame spread at 250 h and tripling NO2 release.