Multiscale Damage Evolution and Load-Transfer Mechanisms of a Millennium-Old Stone Arch Bridge: A Case Study of the Guanyin Bridge

,
,
,
,
,
and
1
Hunan Provincial Engineering Research Center for Immovable Cultural Heritage Health Monitoring and Smart Utilization, Hunan Institute of Science and Engineering, Yongzhou 425199, China
2
Institute of Concrete Science and Technology (ICITECH), Universitat Politècnica de València, 46022 València, Spain
3
Nuclear Industry Huzhou Survey, Planning, Design and Research Institute Co., Ltd., Huzhou 313000, China
4
School of Civil Engineering, Longdong University, Qingyang 745000, China

Abstract

Ancient stone arch bridges are a significant scientific challenge for cultural heritage preservation worldwide, with the core difficulty lying in the fact that, over the course of centuries, they have been subjected to damage from numerous unpredictable factors. Taking a millennium-old stone arch bridge as an example, this paper employs a comparative analysis of a load-damage model developed under multi-factor and multi-constraint conditions and a three-dimensional finite element simulation model—covering both global and local aspects—to reveal the energy transfer patterns of the bridge’s overall and local mortise-and-tenon structures, as well as the intrinsic characteristics of deformation and stress propagation. Research data indicate that, under the action of overall external loads, stress in stone arch bridges is primarily concentrated at the abutments; for individual mortise-and-tenon structures, the regions of maximum stress are concentrated at the abutments of the main arch rings on the north and south sides; the energy transfer pathways within both structures differ from theoretical calculations, and abrupt changes in local stress occur. The comprehensive analysis results are generally consistent with the on-site damage observed in the stone arch bridges. Multiple sets of samples collected from the damaged areas were subjected to microscopic testing and analysis, which further confirmed that long-term environmental erosion is also a contributing factor to the deterioration of stone arch bridges. This study conducted a detailed investigation ranging from theoretical modeling to finite element simulation and microscopic testing. The research models and data obtained will provide a scientific basis for the preservation of millennia-old cultural relics and offer strong support for preventive restoration efforts.

1. Introduction

Historic architectural cultural relics around the world are subject to erosion, weathering, and various forms of deterioration and damage caused by the natural environment. To ensure the long-term inheritance, the restoration and conservation of this cultural heritage has become a major focus of international heritage conservation research [1]. Due to their complex structures, stone arch bridges are subject to diverse uncertain loads and constraints imposed by the natural environment, so it is necessary to strengthen their construction techniques and carry out comprehensive investigation and research on their damage conditions [2]. In recent years, safety incidents involving stone arch bridges in China have occurred frequently.
Especially for long-span stone arch bridges, once there is a local instability in the main arch ring, it will trigger progressive collapse failures, leading to a sudden concentration of stress in the most unfavorable areas of the overall structure (Figure 1, Figure 2 and Figure 3) [3], and eventually resulting in complete collapse of the bridge. Given the unique dynamic structural characteristics of such bridges, there is an urgent need to study how to achieve reliable, safe, and effective continuous preventive conservation [4].
Figure 1. North side of the stone arch bridge.
Figure 2. South side of the stone arch bridge.
Figure 3. Deck of the stone arch bridge.
Some scholars have conducted thorough research on the safety, reliability, stability and dynamic characteristics of long-span bridges. Song He Zhao et al. [5] carried out a modal analysis of stone arch bridges, and derived characteristic parameters of stone arch bridges that more closely reflect their actual operating conditions using the engineering back analysis method; Zhao Ruofan et al. [6], drawing on practical experience, analyzed the theories of various stone arch bridges, providing a reliable basis for the results of load tests on stone arch bridges; and Choi, Won Jin et al. [7] determined the modal parameters of masonry bridges based on the operational modal analysis, and carried out a nonlinear rating analysis, providing a reference for the load-carrying capacity of masonry arch bridges. For the research on modeling and simulation of stone arch bridges, Matsuno, Takashi et al. [8] established a global finite element model for long-span open-spandrel stone arch bridges, and simulated the performance indexes of the old stone arch ring and the newly reinforced concrete arch ring using the dual-element method; Chen X et al. [9] analyzed the ultimate load-bearing capacity and failure characteristics of a three-span sandstone masonry arch bridge under ultimate loads using the 3D elastoplastic finite element method; and Zhiwu Zhou et al. [10] conducted a comprehensive optimization assessment of bridges using 3D finite element coupling analysis, achieving a coupled study for sustainable development. Kim TM et al. [11] established a 3D finite element model of the bridge and analyzed its dynamic characteristics, seismic action effects and seismic stress responses; Chun Zhu et al. [12] investigated the spatial seismic response of the structure using the time-history analysis and the Pushover method, and evaluated the seismic performance of long-span stone arch bridges by establishing a finite element model of spandrel reinforcement with fiber-reinforced polymer (FRP); and Zhou Shi Hua et al. [13] assessed the bridge’s response to man-induced vibrations through modal finite element analysis and field test.
Ma Xiaotong et al. [14] conducted a detailed investigation into the stone arrangement of ancient stone arch bridges, established finite element models of typical arches with four kinds of stone materials, and analyzed the collapse modes and load-bearing capacity of the arches. For research on deterioration, damage and reinforcement of stone arch bridges, Ma Feng Bo et al. [15] conducted a detailed investigation into the deterioration of existing long-span stone arch bridges and performed a verification based on principles of structural mechanics, providing a systematic method and framework for assessing the load-carrying capacity of similar bridges; Wang Yanqi et al. [16] carried out a case study on a multi-span continuous open-spandrel stone arch bridge to investigate and analyze its deterioration, conduct reinforcement and restoration, and verify the reinforcement effect; Mueller, Christine H and Meyer Renate [17] conducted laboratory tests on the 3D response of masonry arch bridges, drawing conclusions regarding damage accumulation in such bridges; and Marco Zucca et al. [18] evaluated its seismic performance through linear and nonlinear finite element analyses, and these measures significantly improved the seismic performance of the building.
Based on a comprehensive literature review, it is necessary to conduct 3D detailed simulation and a comprehensive evaluation of the static equivalent response (both global and local), load-carrying capacity transfer efficiency, local energy concentration effects, and ultimate load-carrying capacity of a stone arch bridge under the disturbance of uncertain influencing factors, as well as a thorough analysis of their current damage characteristics. In this paper, the Guanyin Bridge, a famous ancient bridge with a thousand years of history, was investigated. Physical 3D scanning was conducted to establish a research system of “static equivalent response assessment + 3D modeling of mortise-and-tenon structure + exploration of reliability and damage mechanism” (a LEICA ScanStation P40 3D laser scanner was used. The distance from the scanner station to the scanning subject was less than 21 m. Targets were used for inter-station connection, with no fewer than three targets simultaneously in adjacent areas, and the effective data overlap was greater than 30%. The point spacing of the 3D point cloud model was no greater than 2 mm, and the single-point accuracy was no less than 1 mm). The laws of dynamic load response of the overall structure and individual components of the stone arch bridge under the disturbance of multiple uncertain influencing factors were analyzed, and the changes in the interaction force transfer of individual mortise-and-tenon structures were investigated, providing sufficient theoretical data support for the preventive conservation and intelligent monitoring of stone arch bridges.
This paper has five parts: Section 1 introduces the research focus and innovation points through a literature review; Section 2 introduces the key theoretical mathematical models of methods; Section 3 introduces the case testing process and basic data analysis; Section 4 compares the stress distribution of stone arch bridges and the analysis of simulation model data; and Section 5 highlights the shortcomings and future research prospects in this field.

2. Methods

The structural stress analysis of ancient stone arch bridges requires the integration of on-site investigations and surveying data. By comprehensively considering the field survey records and geological conditions, a structural stress analysis model—specifically, a 3D finite element model established to analyze the bridge structure’s stress characteristics and failure mechanisms [19]. Based on the field survey data, the bridge structure primarily consists of the arch ring, abutments, the upper spandrel layer, the bridge deck, and the railings. Under vertical loading, since the arch ring serves as the primary load-bearing component, contact modeling is applied between the individual stone blocks within the arch ring during both the stress analysis and the model construction phases [20]. The bridge structure is composed primarily of fine-grained monzogranite. The boundary conditions for the stone arch bridge are defined along the three-dimensional axes x (west to east), y (northward and perpendicular to the x-axis), and z. In the stress analysis of the global and theoretical models of the stone arch bridge, normal contact is assumed at the contact surfaces to account for the transmission of axial forces and the friction forces generated by gravity; the friction coefficient is set to 0.45 in accordance with code requirements. In the individual analysis of mortise-and-tenon joints, shear forces and friction forces are treated according to the assumptions. Based on the bridge’s actual functional usage, the primary load considered in the analysis is gravitational load (the value of μ = 0.45 for the rock-to-rock interface is adopted based on the following considerations: the stone-to-stone contact in the stone arch bridge features relatively flat surfaces without mortar filling, with localized weathering and microcracks present at the interface; nevertheless, no interfacial shear slip occurs in the arch ring, and the structure does not experience any failure mode) [21]. According to the field survey data, varying degrees of cracks and damage were observed at the base of the stone arch bridge’s arch ring; these cracks are non-penetrating and do not result in localized changes to the stress distribution. During the overall structural safety assessment, to account for the impact of this damage [22], the number of damaged stones is not considered, and the load-bearing area of the structure is measured according to the actual geometric dimensions.
This study proposes the following hypotheses: 1. Regarding structural loads, the analysis primarily considers static loads and equivalent pedestrian loads (like heavy dynamic loads, such as vehicle traffic, are strictly prohibited in the scenic area). Since the stone arch bridge is located between shallow valleys, the wind loads considered are based on on-site observations of wind direction and wind exposure angle; dynamic modal responses caused by extreme weather conditions are not taken into account. 2. In the overall stress analysis of the stone arch bridge, the friction and sliding between the side walls, main arch, bridge deck, and abutments and the bedrock on the eastern and western slopes are taken into account. The relative sliding of the model during the analysis generates shear forces and bending moments. However, relative frictional shear forces between individual mortise-and-tenon joints are not considered, as local voids prevent full contact, and the shear forces in these areas are relatively small. 3. In the overall finite element simulation analysis, the applied forces are consistent with those in the global structural analysis, with shear forces generated by applied friction and relative slippage. However, in the simulation analysis of individual mortise-and-tenon units, friction is considered, but unit slippage is not; the units are assumed to be in a stable state under actual operating conditions. 4. Four mortise-and-tenon units—Nos. 15, 53, 54, and 76—were selected as they represent the four most common types of mortise-and-tenon connections in the entire stone arch bridge. These four units are located in the regions of highest stress in both the overall stress analysis and the simulation analysis and thus hold significant analytical value for understanding stress transfer and deformation in the global model.

2.1. Principle of Dynamic and Static Loads

Under dynamic loads, the structural response of long-span stone arch bridges differs significantly from that under static loads. It is necessary to consider the effects of inertial moments and frictional resistance. The stress, displacement and acceleration within the structure exhibit cumulative superposition with the variation in internal and external loads. According to D’Alembert’s principle [23], inertial forces are introduced in the dynamic analysis of structures, and the static equivalent response is transformed into an instantaneous static problem; subsequently, internal forces and displacements in structural dynamics are analyzed using static methods [24]. The dynamic balance equation (Eq.) of the long-span stone arch bridge is:
M u ¨   +   C u ˙   +   Ku   =   F
where u is the displacement vector (m) of the bridge; u ¨ is the acceleration vector (m/s2) of the bridge; u ˙   is the velocity vector (m/s) of the bridge; M is the mass matrix of the arch bridge; C is the damping matrix (N·s/m) of the arch bridge; K is the stiffness matrix (N/m) of the arch bridge; and F is the dynamic load vector (N) of the arch bridge.
Displacement   calculation :   δ = q L 2 8 E I · 1 1 + 4 f 2 / L 2
where δ is the displacement (m); f / L is the rise-to-span ratio (the ratio of the vertical distance from the crown of the arch to the line connecting the springings to the horizontal distance between the springings); E is the modulus of elasticity (Pa); and I is the moment of inertia (m4).
Stress   calculation :   σ = M h 2 I
where σ is the stress (Pa); M is the bending moment (N·m); and h is the thickness (m) of the arch ring.

2.2. Load Conditions

Large stone arch bridges are classified as statically indeterminate floating structures that maintain equilibrium under the combined effects of their own weight and various external loads. The loads acting on them are [25]:
F = ∑ i = 1 n ( λ 1 F 1   +   λ 2 F 2   +   λ 3 F 3   +   ⋯   +   λ n F n )
where F is the total load (N) borne by the structure; λ i is the influence coefficient; and F i is the external load force (N) of an individual structural element.
The main loads to be considered are determined in accordance with relevant bridge codes and on-site investigations, including effects of structural gravity [26], pedestrian load, wind load, and temperature action.
G = γ ∑ o = 1 6 V o                                                                             Gravity   load   F pedestrian = L Q                                                                                               Pedestrian   load F wind = 1 2 ρ U g ∑ i   = 1 ,   j   = 1 4 C i S j                                           Wind   load           H t = α ∆ t l δ 22                                                                                   Temperature   load
where   G is the gravity load (N); γ is the material density (kg/m3); V o is the structural volume (m3); F pedestrian is the pedestrian load (N); L is the total length of the bridge (m); Q is the standard value of pedestrian load (kN/m2); F wind is the wind load (N); ρ is the air density (kg/m3); U g is the equivalent static array wind speed (m/s); C i is the wind force coefficient; and S j is the calculation quantity of different forces exerted by the wind on the bridge (kN/m2). H t is the horizontal force at the elastic center (N); α is linear thermal expansion coefficient of the material (for stone masonry, typically taken as 8 × 106/°C); ∆ t is calculated temperature difference (°C); l is calculated span of the arch (m); and δ 22 is flexibility coefficient at the elastic center. The temperature range is ±20 °C, and 0.8 MPa is taken.

2.3. Structural Forces and Finite Element Modeling

2.3.1. Structural Discretization

1. Abutment and Foundation
Abutments and foundations are subjected to stress concentration due to the combined action of arch thrust, self-weight, subgrade reaction and other forces. A 3D solid element discrete model was established for abutments and foundations [27]. The node displacement vector δ s of solid elements contains three degrees of freedom of translation at each node, and the stiffness matrix K s is:
K e   =   ∫ V s B T DdV
where B is the strain–displacement matrix; D is the elastic matrix of the material; and V s is the volume (m3) of the solid element.
2. Arch Ring and Spandrel Structure
Beam elements can effectively simulate the bending and axial deformation of the structure under load. The main structures of the stone arch bridge, such as the arch ring and spandrel columns, are discretized using spatial beam elements and divided into n elements with each element length of l i ( i = 1, 2, …, n ). The node displacement vector δ e is [28]:
δ e   =   [ u 1 v 1 w 1         θ x 1 θ y 1 θ z 1   ⋯   u n v n w n           θ x n θ y n θ z n ] T
where u , v , and w are the parallel displacements of the node in the x , y , and z directions respectively (m); θ x , θ y , and θ z are the torsional displacements of the x , y , and z axes respectively (m), with the subscripts indicating the element nodes.
The stiffness matrix K e of the beam element is a 12 × 12 matrix, expressed as:
K e   =   12 0 0 6 l 0 0 − 12 0 0 6 l 0 0 0 12 0 0 − 6 l 0 0 − 12 0 0 − 6 l 0 0 0 E A E I l 2 0 0 0 0 0 − E A E I l 2 0 0 0 6 l 0 0 4 l 2 0 0 − 6 l 0 0 2 l 2 0 0 0 − 6 l 0 0 4 l 2 0 0 6 l 0 0 2 l 2 0 0 0 0 0 0 G J E I l 2 0 0 0 0 0 − G J E I l 2 − 12 0 0 − 6 l 0 0 12 0 0 − 6 l 0 0 0 − 12 0 0 6 l 0 0 12 0 0 6 l 0 0 0 − E A E I l 2 0 0 0 0 0 E A E I l 2 0 0 0 6 l 0 0 2 l 2 0 0 − 6 l 0 0 4 l 20 0 0 0 − 6 l 0 0 2 l 2 0 0 6 l 0 0 4 l 2 0 0 0 0 0 0 − G J E I l 2 0 0 0 0 0 G J E I l 2
where E is the modulus of elasticity of the material (Pa); I is the moment of inertia of the cross-section (m4); A is the cross-sectional area (m2); G is the shear modulus (Pa); J is the torsional moment of inertia (m4); and l is the length of the beam element (m).

2.3.2. Elastoplastic Analysis

The stone arch bridge is a stone masonry structure, and its material properties are analyzed based on linear elastic–plastic characteristics.
A linear elastic constitutive model is adopted, and the stress–strain relationship of the material satisfies Hooke’s law [29]:
σ   =   D ε
where σ is the stress vector; ε is the strain vector; and D is the elastic matrix.
Stone is an isotropic material, and its elastic matrix D is [30]:
D   =   E ( 1 − v ) ( 1 − 2 v ) 1   −   v v v 0 0 0 v 1   −   v v 0 0 0 v v 1   −   v 0 0 0 0 0 0 1 − 2 v 2 0 0 0 0 0 0 1 − 2 v 2 0 0 0 0 0 0 1 − 2 v 2
where E is the modulus of elasticity of stone masonry (Pa); v is the Poisson’s ratio.
Constitutive damage model for rock in stone arch bridges: The rock mass in stone arch bridges consists of granite. A constitutive model was established using statistical damage theory to analyze the mechanical properties and characteristic stresses of the rock mass [31]. The rock mass is divided into undamaged and damaged materials; the undamaged material obeys the generalized Hooke’s law, which states:
σ i =   E ε i 1 − D +   μ σ g + σ k
where E and µ represent the elastic modulus and Poisson’s ratio of the rock, respectively; ε i (i = 1, 2, 3, or 2, 3, 1, or 3, 2, 1) represents the macroscopic strain of the rock; σ g (where g has the same value as i ) represents the macroscopic nominal stress of the rock in the g direction; and σ k (where k has the same value as i ) represents the macroscopic nominal stress of the rock in the k direction.
The F d p model for measuring the strength of rock microelements using the Drucker–Plague criteria are as follows:
F d p =   α 1 I 1 +   J 2   −   k 1
where α 1 and I 1 are constants related to the cohesion c y and the angle of internal friction ∅ y , respectively, at the rock’s yield point; and I 1 and J 2 are the first invariant of the stress tensor and the second invariant of the stress displacement, respectively.
Assuming that the strength F of an infinitesimal element follows a Weibull distribution, we obtain the rock damage evolution model, namely:
D   =   1 − e x p − F 0 F m F ≥ 0 0 F < 0
In the equation, F 0 and m are parameters of the Weibull distribution. Substituting Equation (13) into Equation (11) yields the statistical damage constitutive model for rock, namely:
σ i =   E ε i e x p − F 0 F m + μ σ g + σ k F ≥ 0 E ε i + μ σ g + σ k F < 0
Under loading, a rock mass transitions from an initial fully elastic state to one characterized by gradual degradation of stiffness, increased ductility, and enhanced nonlinear hysteretic behavior; as it approaches the damage-collapse stage, it exhibits highly nonlinear behavior. By defining elastoplastic constitutive models at the material level, the finite element model is enabled to exhibit superior nonlinear hysteretic capabilities during the large-deformation stage. In ABAQUS 2021 software, the general contact algorithm automatically searches for contact surfaces to perform calculations, simulating the collision and contact behavior of rock mass members and reproducing the structural damage patterns.

2.3.3. Boundary Conditions

The base of the abutment and the foundation are regarded as fixed constraints [32], i.e., the three degrees of freedom of translation and three degrees of freedom of rotation at each node are all zero:
u   =   0 ,   v   =   0 ,   w   =   0 ,   θ x   =   0 ,   θ y   =   0 ,   θ z   =   0

2.3.4. Global Finite Element Equation

By modeling the stiffness matrix, mass matrix and load vector of all elements, the global finite element equation of Guanyin Bridge is obtained:
M δ   ¨ +   C δ   ˙ +   K δ   =   F ( t )
where M   is the structural mass matrix (kg·m2); C is the damping matrix (kg/s), adopting the Rayleigh damping form C   =   α M   +   β K ; K is the structural stiffness matrix [33]; δ is the node displacement vector (m); δ ˙ is the node velocity vector (m/s); δ ¨ is the node acceleration vector (m/s2); and F ( t ) is the load vector that varies with time (N).
α and β are Rayleigh damping coefficients, which can be calculated from the first two natural frequencies ω 1 and ω 2 and damping ratios ξ 1 and ξ 2 of the known structure [34]:
ξ 1   =   α 2 ω 1 +   β ω 1 2 ξ 2   =   α 2 ω 2 +   β ω 2 2
A global finite element coupling model was used to analyze the dynamic characteristics of stone arch bridges, providing a theoretical basis for safety maintenance and sustainable conservation.

3. Results

3.1. Overview

Guanyin Bridge, located in Bailu Town, Xingzi County, Jiujiang City, Jiangxi Province, was built in the seventh year of the Dazhong Xiangfu reign of the Song Dynasty (1014 AD), and was designated as an Important Heritage Site under State Protection in the third batch by the State Council in 1988. Featuring a unique and exquisite design, Guanyin Bridge boasts an ingenious and robust structure with a simple yet elegant architectural form, embodying the superb craftsmanship and outstanding creativity of ancient working people. It was included on the World Heritage List as part of Lushan Mountain in 1996 [26]. The arch bridge is a single-span stone arch bridge with a total length of 21.671 m, a width of 4.563 m, a span of 7.204 m, a rise of 3.337 m, and a vertical distance of 7.015 m from the deck to the base of the abutment (Figure 4). In this study, the bridge body is divided into five parts (Figure 5).
Figure 4. Three-dimensional view of Guanyin Bridge.
Figure 5. North elevation view of Guanyin Bridge.
Guanyin Bridge is a stone arch bridge constructed using a parallel single-arch masonry technique; the bridge structure is composed of five distinct layers. Arranged from bottom to top, these layers consist of the eastern and western abutments, the arch ring layer, the spandrel layer, the bridge deck, and the railings.

3.1.1. Abutment

The eastern and western bridge abutments are situated upon stable, massive rock foundations flanking the banks of the Three Gorges Ravine. Due to a vertical elevation difference of 1.55 m between the two sides—with the western side being lower and the eastern side higher—a 1.98 m tall abutment was constructed on the western side, whereas the eastern abutment consists of a masonry structure merely three courses (0.88 m) in height. The construction material utilized is fine-grained metamorphic monzogranite. The western abutment is designed in the style of a ‘Sumeru’ pedestal featuring corner columns: its lowest tier consists of a single course of convex-profiled bricks; the two tiers immediately above feature corbeling; surmounting these are three tiers of bricks forming ‘Humen’ (ogee-arch) motifs, flanked by corner columns, which are in turn topped by two additional tiers of corbeling (Figure 6).
Figure 6. Scour and erosion of the stone arch bridge foundation.

3.1.2. Arch Layer

The upper section of the bridge abutment consists of the arch ring, the primary load-bearing structure—composed of seven parallel rows of voussoirs made of granite. Of these seven rows, two rows each contain 16 voussoirs, while the remaining five rows consist of 15 voussoirs each; in total, 107 voussoirs were laid to form the bridge arch. Each voussoir feature carved interlocking tenons and mortises on its upper and lower surfaces, allowing them to engage end-to-end and wedge tightly together, thereby ensuring a close fit between adjacent stones (Figure 7).
Figure 7. Arch layer of load-bearing structure.

3.1.3. Impact Coupon Layer

Situated between the arch layer and the bridge deck is the spandrel layer. The masonry stones used in the eastern and western sections differ in size; specifically, in the sections above the third course of voussoirs, the stones on both ends of each layer are uniform and symmetrical, whereas in the sections below the third course, the stones on both ends of each layer are no longer symmetrical. Nevertheless, within the eastern section, the dimensions of the stones in each layer on the north and south sides remain generally symmetrical, as do the dimensions of the stones in each layer on the north and south sides of the western section (Figure 8).
Figure 8. Detailed overlapping structure.

3.2. The Stress of the Structure

Given the thousands of years of exposure to natural environments and applied loads, the priority is to conduct an ultimate safety load analysis on the stone arch bridge. The Guanyin Bridge spans the Sanxia Stream, with its entire foundation constructed between the cliffs of the Lushan gorge. The bridge deck is situated at an elevation of approximately 340 m above sea level. To its northwest lies the Hanyang Peak (maximum elevation 1474 m), and to its northeast, the remaining range of the Wulao Peak (maximum elevation 1436 m). Prevailing northeasterly winds are observed with the highest frequency annually, persisting for about six months, generally at magnitudes of 3 to 5 (wind speeds ranging from 3.4 to 10.7 m/s). The wind attack angle varies from +5° to +15° (positive attack angle). Owing to the topographic constraint imposed by the surrounding mountains on three sides, the airflow is forced to ascend along the valley floor, resulting in a substantial upward vertical component (ranging from 0.087 F w i n d ~0.259 F w i n d ) in the actual inflow direction (Figure 9 and Figure 10).
Figure 9. Sectional division view.
Figure 10. Force view.
Through force analysis, the stress concentration areas of the structure were identified, and targeted protection measures were taken to enhance safety and durability during operation and maintenance. An arch utilizes curved structural elements to serve as its load-bearing framework [35]. Under the influence of vertical loads, the structure relies primarily on compressive forces between the masonry units to transmit the load, resulting predominantly in horizontal thrust at the arch springing [36]. As the bridge structure is continuously subjected to various forms of deterioration, it has gradually sustained damage. Based on data derived from on-site inspections, instances where the arch axis exhibits out-of-plane displacement—with a maximum deviation of 80 mm observed in a single masonry unit—occur in a structure where the average width of the masonry blocks is approximately 620 mm. Under the action of vertical loads (specifically, the structure’s self-weight), the resulting out-of-plane bending moment acting upon the centerline of the masonry blocks is relatively minor [37]; consequently, the overall structural deformation remains limited. This allows for sufficient contact between adjacent masonry blocks to effectively transmit compressive forces, thereby ensuring the overall structural stability of the stone arch bridge. The calculated loads are listed below (Table 1).
Table 1. Load summary table.

3.2.1. Load Analysis

A global model was established for the stone arch bridge. The self-weight of the bridge and the pedestrian load were applied to the deck as uniformly distributed loads. The included angle α between the wind load and the arch vault was defined as the wind angle of attack, generating friction and disturbing forces on the bridge surface. Additionally, the bridge is subjected to reaction forces from the supports and interaction forces between the bridge structure on both sides and the supporting structures. The entire arch bridge maintains a state of static equilibrium under the action of multiple loads (Figure 10). Under gravitational loading, the zones of high structural stress within the arch are concentrated in its lower-to-middle sections [38], with the maximum stress occurring at the roots of the arch at its eastern and western extremities. The relatively lower stress observed in the arch at the damaged location within the central column row is attributable to the structural impairment of the central arch itself; this damage has diminished its load-bearing capacity, resulting in a redistribution of stress within the arch system, whereby the arches on either side have assumed the supporting function [39], with the undamaged arches serving as the primary load-bearing elements.

3.2.2. Force Analysis

1. Overall Force Analysis
The arch springing is regarded as a fixed-hinged support. Given G + F pedestrian = 5,160,394.31 N, q = 238,124.42 N/m can be yielded. The magnitude of the support reaction is F R 1 = 3,906,682.98 N, and F R 2 = 1,186,964.65 N. Combined with the force diagram and structural mechanics, the shear force and bending moment equations of the arch bridge are derived respectively as follows:
V =       − q x                                                         ( 0 ≤ x < 6.97 ) F R 1 − q x                                         ( 6.97 ≤ x < 17.491 ) q ( 21.671 − x )               ( 19.575 ≤ x ≤ 21.671 )
M =       − 1 2 q x 2                                                                       ( 0 ≤ x < 6.97 ) F R 1 ( x − 6.97 ) − 1 2 q x 2                   ( 6.97 ≤ x < 17.491 ) − 1 2 q ( 21.671 − x ) 2                         ( 19.575 ≤ x ≤ 21.671 )
Based on Equations (18) and (19) and relevant data, the shear force and bending moment are calculated and plotted (Figure 9Figure 11 and Figure 12). According to Equation (19), the maximum bending moment occurs at 15.03 m (marked in red in Figure 9), with a maximum value of 1,941,509.15 N·m.
Figure 11. Shear force view.
Figure 12. Bending moment view.
2. Structural Discretization:
Guanyin Bridge has a total length of 21.671 m, which is divided into several sections using the slice method with one section per meter (Figure 9). According to Equations (18) and (19), the shear forces and bending moments of these sections are calculated (Table 2).
Table 2. Summary of section shear force and bending table.
3. Local Force Analysis
As shown in Figure 11 and Figure 12, there are significant changes in shear force and bending moment at the arch springing and mid-span. To further analyze the force characteristics of the detailed structure of the arch bridge, the masonry elements marked in Figure 6 were selected for a coupled analysis.
4. The spatial form of the structure is presented through “3D diagrams”, while the force distribution is illustrated by “shear force diagrams (V-diagrams)” and “bending moment diagrams (M-diagrams)”. The magnitude and variation in stress and displacement are intuitively reflected using “finite element stress diagrams” and “finite element displacement diagrams” through colors (such as red, blue, etc.), quantifying the forces acting on the structure and its deformation.
5. Regarding the stress distribution within the stone tenons of the arch ring, an analysis was conducted using a solid model established for the basal regions at both ends of the arch, specifically incorporating the tenon-and-mortise connections between the voussoirs. The friction coefficient between the masonry units was set at 0.45. Table 3 presents the stress distribution at the tenon-and-mortise joints of the voussoirs at the base of the arch ring under gravitational loading. As illustrated by the data, stress concentration phenomena are evident within the voussoirs of the Guanyin Bridge arch ring; specifically, this concentration is predominantly localized at the interlocking tenon-and-mortise interfaces along the inner face of the arch. This condition renders these specific areas highly susceptible to damage and structural failure, potentially resulting in a loss of load-bearing capacity.
Table 3. Local shear force, bending moment view.

4. Discussion

In this study, a full-bridge model was established using the finite element software ABAQUS. The finite element model was discretized into 59,800 elements with a mesh size of 0.1 m; the meshes are all in a hybrid hexahedral–tetrahedral configuration (Figure 13a). The bridge body is primarily composed of fine-grained monzogranite. All masonry materials are modeled with an elastic constitutive law, adopting an elastic modulus of 80 GPa and a Poisson’s ratio of 0.241. Since the stone arch bridge serves exclusively as a pedestrian sightseeing passage, the damping ratio is considered in accordance with the half-U-shaped rock damping behavior under constant-amplitude cyclic loading, with a range of 0.020 to 0.050 [30].
Figure 13. Distribution diagram of finite element model. (a) Finite element model. (b) x-axis. (c) y-axis. (d) z-axis.
Stress distribution diagrams for a stone arch bridge under gravitational loading—specifically in the absence of structural damage—reveal that the high-stress zone is situated within the lower-to-middle section of the arch ring, with the maximum stress occurring at the arch springing. When the bridge is subjected to gravitational loads, the high-stress zone in the undamaged sections of the arch ring remains concentrated in the lower-to-middle region—again with maximum stress at the springing—whereas the stress within the damaged sections of the arch ring is comparatively lower. This phenomenon is primarily attributable to the damage sustained by the central portion of the arch ring; as this damage diminishes its load-bearing capacity, the internal stresses undergo redistribution, causing the undamaged sections of the arch ring to assume the primary load-supporting role.

4.1. Structural Finite Element Analysis

As shown in Figure 13, the maximum displacement in the y-direction is greater than those in the x- and z-directions, reaching a peak value of −8.052 × 10−2 m. As shown in Figure 13c, the displacement is symmetrically distributed from the mid-span toward both ends. The maximum displacement in the x-direction is −2.115 × 10−2 m, which is larger than that in the z-direction of 2.9 × 10−3 m, indicating that the deformation in the x-direction is greater than that in the z-direction. Figure 13b,d show that deformation and the likelihood of deformation failure are relatively high in the right half of the arch.
As shown in Figure 14 and Figure 15, the overall deformation of the arch bridge is symmetrical, the maximum stress at the arch springing of the bridge is 9.929 × 107 Pa, and the probability of failure at this location is higher than that at other parts of the bridge; the maximum displacement at the mid-span of the bridge is 8.05 × 10−2 m, making it the most prone to deformation; the displacement at the arch springing is minimal, with a value of 0, making it the least prone to deformation.
Figure 14. Overall stress distribution diagram.
Figure 15. Overall displacement distribution view.
As shown in Figure 16 and Figure 17, the deformation of the arch bridge exhibits a symmetrical distribution, with the maximum displacement occurring at mid-span; both stress and displacement values decrease gradually along the direction of the arrow. As shown in Figure 16 and Figure 17, the displacement variations in the bridge deck and the bridge base are identical, both exhibiting the maximum displacement at mid-span and the minimum displacement at the arch springing. Based on the above data, the deformation trend of the bridge structure can be determined. As shown in Figure 18, the maximum stress on the bridge deck in the y-direction is 4.483 × 105 Pa; the minimum stress at the mid-span of the bridge deck in the x-direction is 7.806 × 107 Pa; and the maximum stress on the bridge deck in the z-direction is 1.374 × 107 Pa, which is smaller than the maximum stresses in the x and y directions. It is determined that this direction has the lowest risk of failure.
Figure 16. Distribution of bridge deck displacement view.
Figure 17. Distribution of bridge bottom displacement view.
Figure 18. Distribution of bridge deck stress view. (a) Total stress distribution diagram of the bridge deck. (b) x-axis. (c) y-axis. (d) z-axis.
As shown in Figure 19, all datasets exhibit substantial fluctuations, with the maximum principal stress reaching S m a x = 99,288.55 Kpa. The stress transfer process displays five distinct wave crests, with mean values exceeding 60,000 kPa, and no fixed linear trend is observed. Under external loading, the internal deformation and stress response of the structure exhibit nonlinearity and instability. Similarly, during the process of nonlinear deformation, the variation in internal energy of the structure also presents a nonlinear pattern, with E m a x = 1004.57 KJ. The energy transfer process corroborates the deformation behavior and load distribution within the structure; apart from localized extreme values induced by concentrated loading, the remaining regions manifest a sequential load-transfer effect. Furthermore, the numerical results confirm that the adopted dynamic model—which excludes local damage (e.g., cracking and phase transformation) and deformation mechanisms (e.g., elastic-to-plastic and brittle-to-ductile transitions). This model satisfactorily captures both the force-transfer characteristics of individual arch blocks and the overall structural response curve. The “critical deformation states” of the structure, such as unstable crack propagation and structural buckling, are not triggered, indicating that the arch bridge remains in a stable condition.
Figure 19. Finite element analysis diagram view. (a) Displacement–stress. (b) Strain–energy. (c) Strain–stress–displacement. (d) Energy–strain–displacement. (e) Energy–displacement–strain.
When “high stress and large deformation” occur simultaneously at the mechanical peak value points, the peak value of the energy corresponds to the critical state. Deformation and energy transfer reflect the coupling between external force-induced deformation and the effective transfer of internal microscopic energy. The binomial fitting analysis was performed on the collected data to obtain R s s d 2 = 0.9978, R e s d 2 = 0.7830, and R e d s 2 = 0.7453, and the comparison shows that the stress–strain data analysis is more in line with the actual working conditions, accurately verifying the robustness of the simulation analysis data (Figure 19c–e).

4.2. Finite Element Analysis of an Individual Element

The main arch of a stone arch bridge adopts a direct interlocking structure using male–female tenons (mortise-and-tenon joints), whose core characteristics lie in the combination of “rigidity with flexibility” and “collaborative load transfer”.
1. Achieving a “flexible” connection with brittle stone: Stone has high compressive strength but low tensile strength. The design of the male–female tenons transfers forces through direct compression between the stone components, thereby avoiding tensile stresses that would pull on the tenon at the joint.
2. Pursuing “gapless insertion” of the male–female tenon in stone arch bridges: This form of “locking” is achieved jointly by gravity and the lateral thrust of the arch, firmly pressing the tenon into the mortise.
3. Fine finite element simulation of the male–female tenon structure: The simulation uses 3D high-order solid elements to finely mesh the tenon and mortise and sets up “contact pairs” to model their complex mechanical behavior (Figure 20) [40].
Figure 20. Structural stress analysis and mess division. (a) 15. (b) 53 and 54. (c) 76. (d) Orthophoto unwrapped view of the bottom surface.

4.2.1. Main Arch No. 15

As shown in Figure 20 and Figure 21, the stress values reach their peak in both the early and late stages. The stress values in the later stage are relatively concentrated, while the energy values decrease, indicating an unstable deformation response in the material and an uneven force distribution of the internal mortise-and-tenon structure. With the continuous increase in displacement and strain, the stress distribution tends to concentrate, leading to complex interactions between stress transfer and damage development. In the middle and late stages, energy increases with strain, and there are locally discrete points. Material deformation gradually becomes more regular. However, due to internal damage (such as microcracks and local losses), local anisotropic energy transfer persists. The points where stress and energy reach their maximum values approach the critical state of the deformation (e.g., structural instability); the decrease in stress corresponds to energy transfer and dissipation, demonstrating the phenomena of “energy consumption through plastic deformation” and “energy release via damage propagation” in statically indeterminate structures.
Figure 21. Finite element analysis of views 15. (a) Stress analysis. (b) Strain analysis. (c) Logarithmic strain. (d) Reaction force. (e) Displacement–stress. (f) Strain–energy. (g) Analysis of LS. (h) Analysis of RF.
The analysis data indicate that the maximum stress occurs at the joint interface of the stone tenon and arch shoe, specifically: S n 1 = 236,531.36 Pa > S n 2 = 230,504.23 Pa > S n 3 = 222,300.02 Pa > S n 4 = 221,074.28 Pa > S n 5 = 219,119.94 Pa > S n 6 = 212,038.88 Pa > S n 7 = 205,698.56 Pa. The mean stress exceeds 0.2 MPa; despite the relatively high compressive strength of the material, an uneven transmission and distribution of forces has occurred—a phenomenon identified as one of the causes of localized damage. The only observed change occurred in a direction precisely opposite to that of the stress; specifically, significant displacement variations were noted at the interlocking mortise-and-tenon interfaces, measuring: D n 1 = 0.0347 mm > D n 2 = 0.0303 mm > D n 3 = 0.0291 mm > D n 4 = 0.0287 mm > D n 5 = 0.0280 mm > D n 6 = 0.0278 mm. While the mean displacement is less than 0.1 mm, on-site observations clearly reveal the presence of cracks, as well as localized misalignment and delamination. The distribution of strain differs significantly from that of stress; it is concentrated at the interface and exhibits a largely symmetrical distribution on the left and right sides, with values ranking as follows: S t 1 = 0.00000141µƐ > S t 2 = 0.00000136 µƐ > S t 3 = 0.00000131 µƐ > S t 4 = 0.00000121 µƐ > S t 5 = 0.0000008 µƐ > S t 6 = 0.0000007 µƐ. Concurrently, the energy loss values vary as follows: E t 1 = 7.008 J > E t 1 = 6.286 J > E t 2 = 6.125 J > E t 1 = 5.998 J > E t 1 = 5.641 J > E t 1 = 5.361 J. The distribution ranges for both parameters remain essentially consistent. As a stone arch bridge undergoes large deformation, it falls into the category of nonlinear deformation. The internal forces of the superstructure are transferred sequentially through the mortise-and-tenon joints, so the true strain (LE, Logarithmic Strain) needs to be analyzed. Analysis of 35 selected points shows that S L S 1 = 0.00000141 µƐ > S L S 2 = 0.00000136 µƐ > S L S 3 = 0.00000135 µƐ > S t 4 = 0.00000131 µƐ > S t 5 = 0.00000129 µƐ. The average value of the first ten groups is larger than the originally measured strain values, indicating that the true strain exhibits an accumulation effect after geometric nonlinearity is activated in the structural analysis (Figure 21c,g). At the boundary of point 15#, the reaction forces are concentrated on the upper side, with magnitudes of F R F 1 = 1155.21 Pa > F R F 2 = 1044.00 Pa > F R F 3 = 1017.82 Pa > F R F 4 = 991.09 Pa > F R F 5 = 668.08 Pa. The reaction force accounts for only 0.49% of the internally transferred stress, demonstrating that load transfer through the mortise-and-tenon joints is dominated by compression (Figure 21d,h).

4.2.2. Main Arch No. 53

As shown in Figure 20 and Figure 22, at an initial displacement of 0, the stress reaches a peak value of 141,566.83 Pa. As the displacement gradually increases, the stress exhibits an overall downward trend with reduced discreteness, corresponding to a specific deformation stage of the material, and marking a transition from high stress concentration to damage evolution and a decline in load-bearing capacity. During the low strain stage, the energy values are concentrated and generally low. When the strain exceeds 5 × 106 με, the energy gradually increases as the strain continues to rise, with high values of 2.03, 1.28, and 2.17 observed. Dynamic changes in energy accumulation and dissipation occur during material deformation. The high-energy points correspond to complex internal deformations of the structure (plastic deformation and microstructural energy equilibrium). Under small deformation, high stress corresponds to high energy propagation; under large deformation, stress decreases due to losses, while energy continues to dissipate via plastic deformation, presenting a chained mapping of “force → deformation → energy” [27]. The analysis reveals the complex behavior of materials from elastic rigidity to plastic damage and highlights multiscale uncertainties and differences in mechanisms across deformation stages, providing a multidimensional reference for studying constitutive laws and optimizing design.
Figure 22. Finite element analysis of views 53. (a) Stress analysis. (b) Strain analysis. (c) Logarithmic strain. (d) Reaction force. (e) Displacement–stress. (f) Strain–energy. (g) Analysis of LS. (h) Analysis of RF.
53# features a bidirectional tenon-and-mortise joint structure, situated precisely at the crown of the main arch; 53# and 54# are connected via an interlocking joint. Analysis data indicate that the maximum stress occurs at the interface between the stone tenon and the arch shoe, specifically: S n 1 = 141,566.83 Pa > S n 2 = 140,875.39 Pa > S n 3 = 126,891.90 Pa > S n 4 = 126,148.09 Pa > S n 5 = 124,547.14 Pa > S n 6 = 123,740.61 Pa > S n 7 = 121,327.56 Pa. The mean stress value exceeds 0.12 MPa. The compressive strength at this location is lower than that of 15#; however, the transmission and distribution of forces exhibit a uniform pattern, with essentially no damage or cracking observed. As this structural component directly bears the bridge deck loads, the transmission of forces is relatively uniform. Displacement variations at the tenon-and-mortise joints are insignificant, specifically: D n 1 = 0.0145 mm > D n 2 = 0.0133 mm > D n 3 = 0.0133 mm > D n 4 = 0.0132 mm > D n 5 = 0.0131 mm > D n 6 = 0.0130 mm. The mean displacement value exceeds 0.13 mm; field observations reveal no significant cracking, and there is an absence of localized misalignment or delamination. The strain distribution differs significantly from that of stress; it is concentrated at the lower insertion interface and exhibits an essentially symmetrical distribution on the left and right sides, with values of S t 1 = 0.000262 µƐ > S t 2 = 0.000260 µƐ > S t 3 = 0.000235 µƐ > S t 4 = 0.000234 µƐ > S t 5 = 0.000225 µƐ > S t 6 = 0.000197 µƐ. Concurrently, the energy loss values are E t 1 = 2.172 J > E t 2 = 2.172 J > E t 3 = 2.151 J > E t 4 = 2.030 J > E t 5 = 2.008 J > E t 6 = 1.737 J (Figure 22c,d,g,h). The distribution ranges for both remain essentially consistent.

4.2.3. Main Arch No. 54

As shown in Figure 20 and Figure 23, at the initial stage, the responses are unstable, and stress concentrates when the displacement approaches 0, reaching a peak value of 131,721.25 Pa. Energy is concentrated in the low-strain range, indicating that the initial force of the material is affected by microstructural defects and structural inhomogeneities, and that the evolution of deformation exhibits synergy; as displacement gradually increases, the overall stress attenuates while its dispersion rises. After the strain increases, energy grows orderly with strain and its dispersion decreases. The coupling of “stress attenuation → energy increase” reflects the transition of the material from “an unstable deformation process dominated by initial defects” to “a synergistic evolution process of macroscopic deformation and energy”. The points where stress and energy reach their maximum values correspond to the critical state of damage.
Figure 23. Finite element analysis of views 54. (a) Stress analysis. (b) Strain analysis. (c) Logarithmic strain. (d) Reaction force. (e) Displacement–stress. (f) Strain–energy. (g) Analysis of LS. (h) Analysis of RF.
54# features a bidirectional concave-recessed joint structure, situated precisely at the crown of the main arch; it connects with Unit 53# via an interlocking configuration. Analysis data indicate that the maximum stress occurs at the interface between the stone tenon and the arch shoe, with values ranking as follows: S n 1 = 127,499.44 Pa > S n 2 = 126,771.09 Pa > S n 3 = 123,604.76 Pa > S n 4 = 106,544.31 Pa > S n 5 = 104,509.62 Pa > S n 6 = 104,746.13 Pa > S n 7 = 100,072.18 Pa. The mean stress value exceeds 0.10 MPa; however, the compressive strength is lower than that of 53#. Consequently, under the compressive load from the main bridge deck, the direction of force transmission shifts toward the western side. Field observations indicate that the elevations are essentially consistent; furthermore, the structural integrity of Unit #54 is superior to that of 53#, exhibiting neither damage nor cracks. The displacements at the tenon-and-mortise concave joints are recorded as follows: D n 1 = 0.0105 mm > D n 1 = 0.0099 mm > D n 1 = 0.0087 mm > D n 1 = 0.0086 mm > D n 1 = 0.0077 mm > D n 1 = 0.0074 mm (Figure 23c,d,g,h).
The mean displacement value exceeds 0.007 mm; however, field observations reveal no discernible cracks, and there is an absence of localized misalignment or delamination, indicating that the structural connection remains tight. The strain distribution differs significantly from that of stress; it is concentrated at the lower insertion interface and exhibits a largely symmetrical distribution on the left and right sides, with values of S t 1 = 0.000022 µƐ > S t 2 = 0.000021 µƐ > S t 1 = 0.000020 µƐ > S t 1 = 0.000019 µƐ > S t 1 = 0.000017 µƐ > S t 1 = 0.000016 µƐ. Concurrently, the energy loss values are E t 1 = 1.554 J > E t 1 = 1.537 J > E t 2 = 1.536 J > E t 1 = 1.138 J > E t 1 = 1.121 J > E t 1 = 1.112 J. The distribution ranges remain essentially consistent.

4.2.4. Main Arch No. 76

As shown in Figure 20 and Figure 24, stress and energy accumulate under small deformations, while the response decays under large deformations; in the initial stage of displacement and strain, the stress values are discrete and the energy values vary significantly, reflecting the influence of microscopic defects and uneven distribution on the initial deformation of materials, and resulting in poor response stability. As displacement and strain increase, the energy exhibits fluctuations before gradually stabilizing. In the medium and high strain areas, the energy increases with strain and exhibits low values (0.34 J, 0.43 J), indicating that the material deformation tends to be regular, while local instability persists due to internal damage (e.g., microcracks).
Figure 24. Finite element analysis of views 76. (a) Stress analysis. (b) Strain analysis. (c) Logarithmic strain. (d) Reaction force. (e) Displacement–stress. (f) Strain–energy. (g) Analysis of LS. (h) Analysis of RF.
76# features a unidirectional mortise-and-tenon joint structure and is situated precisely at the western arch abutment. It is responsible for transmitting forces and providing load-bearing capacity for the first main arch ring. Analysis data indicate that the maximum stress occurs at the interface of the stone tenon grooves, with values ranking as follows: S n 1 = 123,294.25 Pa > S n 2 = 122,793.58 Pa > S n 3 = 112,737.06 Pa > S n 4 = 109,051.54 Pa > S n 5 = 107,453.95 Pa > S n 6 = 107,861.21 Pa > S n 7 = 104,193.09 Pa. The average stress value is less than 0.20 MPa, and the compressive strength is lower than that of 15#. Consequently, it is determined that under the load of the main bridge deck, the direction of force transmission shifts toward the eastern side; the load-bearing capacity of the eastern half is approximately twice that of the western half. 76# exhibits minor localized damage and cracking.
The displacements at the mortise-and-tenon joint interfaces are recorded as follows: D n 1 = 0.0069 mm > D n 1 = 0.0068 mm > D n 1 = 0.0061 mm > D n 1 = 0.0060 mm > D n 1 = 0.0058 mm > D n 1 = 0.0057 mm. The average displacement exceeds 0.005 mm; however, field observations indicate that any cracks are inconspicuous, and the magnitude of displacement is merely one-twentieth of that observed in Unit #15, thereby demonstrating that the structure remains fundamentally stable with its connections intact. The strain distribution differs significantly from that of stress; it is concentrated at the groove interfaces and exhibits an essentially symmetrical distribution on both the left and right sides, corresponding to the values: S t 1 = 0.000012 µƐ > S t 2 = 0.000012 µƐ > S t 1 = 0.000011 µƐ > S t 1 = 0.000010 µƐ > S t 1 = 0.000007 µƐ > S t 1 = 0.000005 µƐ. Concurrently, the energy dissipation values vary as follows: E t 1 = 1.653 J > E t 1 = 1.656 J > E t 2 = 1.317 J > E t 1 = 1.202 J > E t 1 = 1.145 J > E t 1 = 1.202 J (Figure 24c,d,g,h). A comparison between cases 76# and 15# reveals a difference of 20%, while their distribution ranges remain essentially consistent.
To sum up, with the increase in displacement and strain, the stress fluctuates with displacement before gradually stabilizing. In the medium and high strain areas, the energy increases with strain but exhibits local instability, reflecting an uneven distribution within the structure and the presence of certain damage (such as cracks or defects).

4.3. Coupled Analysis

The finite element simulation results are compared with the theoretical analysis results to deduce the differences and coupling characteristics.

4.3.1. Global Structural Coupling

1. In the theoretical calculation of mid-span displacement, the displacement is obtained by Equation (2):
δ = q L 2 8 E I · 1 1 + 4 f 2 / L 2   = 238,124.42   ×   7.20 4 2 8   ×   3   ×   1 0 7 ×   0.0476 · 1 1 + 4   ×   0.7069 2 / 7.204 2 = 0.0625   m .
The maximum mid-span displacement obtained from the finite element model is 8.05 × 102 m (Figure 14), with a deviation of 28.80% from the theoretical value because the theoretical model neglects the elastoplastic damage of stone masonry and does not account for the nonlinear large-deformation effect of the material. In contrast, the finite element model adopts a linear elastic-damage constitutive model ( σ   =   ( 1 − D ) D ε ), in which damage and failure (variable D ) occur when the stress exceeds the limit threshold, aligning with the crack behavior of the masonry.
2. Arch Springing Stress
In the theoretical model, the bending moment at the arch springing is 5,784,149.32 N·m. Through Equation (3), it can yield: σ   =   M h 2 I   =   5,784,149.32   ×   0.5 2   ×   0.0476   ≈ 3.04 × 107 Pa.
Based on the finite element mess data, the maximum stress at the arch springing is 9.929 × 107 Pa (Figure 23 and Figure 24), with a deviation of 69.4% from the theoretical value because the theoretical model simplifies the arch springing as a hinged joint and does not account for the 3D stress concentration effect. In contrast, the finite element simulation adopts solid elements and foundation constraints to model rigid connections, making the arch springing constraints closer to the actual connection system and more consistent with the superposed state of compressive and shear forces.
According to the structural dynamic modeling analysis, the mode shape of Guanyin Bridge in the y-direction is overall vertical bending of the arch, that in the x-direction is lateral swing bending, and that in the z-direction is torsional vibration; regarding yxz , the finite element analysis results are consistent with the theoretical mode shapes, but there are differences in the magnitude of local deformation: the y   data from finite element analysis of the mode shape in the y-direction show that the vertical displacement at the arch crown is 28.80% higher than the theoretical value because the theoretical model neglects the coupling transfer effect of high-order mode shapes. In contrast, the discrete nature of the finite element model results in significant coupling effects among the vibration modes [41,42,43,44].
A comparison of the two reveals that while the mode shapes obtained from the theoretical model and the finite element simulation are consistent, there are relatively significant deviations in the static equivalent response data. In the optimization of bridge maintenance design, it is necessary to integrate the strengths of both approaches and establish a design framework combining “theoretical estimation and finite element simulation” to enhance the robustness of safety assessments and maintenance for long-span stone arch bridges.

4.3.2. Local Structural Coupling

Considering the different stress conditions between the local and global areas, the displacement generated locally should be shear displacement. The innovative displacement correction model is:
δ = VL AG
where V is the shear force (N); A is the cross-sectional area (m2); G is the shear modulus (Pa); G   =   E 2 ( 1 + μ ) ; and μ is the Poisson’s ratio.
Combined with Table 3, the maximum displacement of the main arch is obtained using Equation (20):
δ 15 max   =   VL AG   =   41,970.55   ×   0.609 0.383   ×   11,811,023.62 =   5.650   ×   10 − 3   m ;   δ 53 max   =   VL AG     =   13,135   ×   0.638   0.487   ×   11,811,023.62 = 1.457 × 10 − 3   m ;   δ 54 max = VL AG   = 16,749.05   ×   0.638 0.487   ×   11,811,023.62 = 1.858   ×   10 − 3   m ;   δ 76 max = VL AG = 27,047.84   ×   0.659   0.402   ×   11,811,023.62 = 3.754 × 10 − 3   m .
The maximum stress of the individual element is obtained using Equation (3):
σ 15 max   =   M 15 h 15 2 I 15   =   12,780.03   ×   0.629 2   ×   0.02   ≈   2.010   ×   10 5 Pa ;   σ 53 max   =   M 53 h 53 2 I 53   =   11,190.16   ×   0.763 2   ×   0.03   ≈   1.423   ×   10 5   Pa ; σ 54 max   =   M 54 h 54 2 I 54   =   11,879.73   ×   0.763 2   ×   0.03   ≈   1.511   ×   10 5   Pa ;   σ 76 max   =   M 76 h 76 2 I 76 = 31,625.13   ×   0.61 2   ×   0.02   ≈   4.823   × 10 5   Pa .
As shown in Table 3, the maximum displacement value of an individual element from the finite element model data is 3.469 × 10−5 m, 1.708 × 10−5 m, 1.079 × 10−5 m, and 6.998 × 10−6 m, with deviations of 98.5%, 95.1%, 99.4%, and 99.8% from the theoretical values respectively (the deviation comparison ratio of the maximum values); the maximum stress value of an individual element from the finite element model data is 2.365 × 105 Pa, 1.416 × 105 Pa, 1.317 × 105 Pa, and 1.223 × 105 Pa, with deviations of 85.0%, 84.7%, 82.8%, and 74.6% from the theoretical values respectively (the deviation comparison ratio of the maximum values). Analysis of the main causes of deviations: A theoretical analysis of the forces acting within the planar contact surface was conducted. The arch springing and arch shoe in the finite element solid model were simulated by rigid connection, which resulted in 3D stress concentration (compression–shear interaction) and amplified local deformation, highlighting the actual stress state; the theoretical analysis showed the contact effects of local components (such as stone friction and joint slippage) and the evolution of damage at contact surfaces, but it cannot reflect the influence of the friction coefficient between individual arch springing on force transfer. The elastoplastic constitutive model (Equations (9)–(12)) adopted for finite element solid model demonstrated the superiority of local refined analysis; the theoretical model exhibited uniform bending deformation at mid-span and failed to account for the local eccentric torque induced by bridge deck loads. In contrast, the finite element simulation completed the modeling and analysis of stress dispersion caused by uneven internal forces of individual elements at mid-span and the mutual constraints between the arch structures; therefore, there was discrepancy between the 3D simulation analysis of the individual arch springing and the theoretical model.
As shown in Figure 25, based on optimization analysis using polynomial surface fitting, R 15 2 = 0.998, R 53 2 = 0.978, R 54 2 = 0.993, and R 76 2 = 0.994 . All values of R 2 are significantly greater than 0.5, indicating that the conclusions of the theoretical analysis and the finite element simulation are consistent with the coupling effects, further demonstrating the robustness of the results obtained through the combined study of both approaches.
Figure 25. Fitting analysis of four structural parameters (displacement, stress, and energy). (a) No. 15. (b) No. 53. (c) No. 54. (d) No. 76.

4.3.3. Microscopic Analysis of Damage Sampling

To accurately assess the health status of the Guanyin Bridge, this study adopted a combination of focused field sampling in deteriorated areas and advanced materials analysis techniques (XRF, XRD) to analyze and quantify the causes of deterioration and conduct damage assessment. A total of 27 marked samples were collected from different locations in the field, focusing on the following aspects: biological lichen and moss erosion, long-term uneven deformation due to microcracks and local through-cracks, rock surface weathering and spalling dissolution, vegetation growth damage, and river water scouring (Figure 26).
Figure 26. Field sampling and microscopic analysis. (a) Moss-induced erosion. (b) Microcracks and locally penetrating cracks. (c) Rock surface weathering, exfoliation and dissolution. (d) Damage induced by vegetation growth.

4.3.4. Chemical Composition Analysis of Samples

A total of 16 rock samples (Nos. 1–16), three moss samples, three vegetation root samples, and three water samples were collected in the field.
The sampling locations were recorded for each sample. The samples were analyzed for major element concentrations using X-ray fluorescence spectrometry (XRF) (Figure 26).
1. Calcium (Ca) Content
There was significant spatial variability in Ca content in the stone arch bridge. The Ca content at sampling points on the west elevation was notably lower than that on the east elevation, indicating that the west elevation had experienced more severe rainwater scouring and biological erosion than the east elevation. Sample No. 14 from the bridge deck had a lower Ca content than the other two bridge deck samples, suggesting longer rainwater retention time and consequently more severe dissolution effects. Sample No. 16 from the arch springing exhibited a much lower Ca content than other samples, indicating frequent and rapid water scouring at this location. Relatively high Ca contents were detected in both water samples and root samples, demonstrating that water scouring and plant erosion are the main factors contributing to rock deterioration (Figure 27a).
Figure 27. Chemical composition analysis of samples. (a) Rock samples 1–16. (b) Moss, vegetation roots, water samples 1–9.
2. Impurity Elements Such as Silicon (Si), Iron (Fe), and Aluminum (Al)
The average contents of Si, Fe, and Al in samples Nos. 1–6 from the west elevation were higher than those in samples Nos. 7–12 from the east elevation, indicating that the west elevation was more strongly affected by wind-blown sand than the east elevation. Sample No. 16 from the arch springing had the highest impurity content, demonstrating that this area was severely affected by water-borne sand deposition and iron oxidation. The contents of Si, Fe, and Al in root samples were higher than those in rock samples, indicating that plant roots enriched sand particles from the natural environment (Figure 27a).
3. Enrichment of Si–al–fe and Weathering Degree
Comparison of the contents of Si, Fe, Al, K, and S with the observed field weathering degree showed a positive correlation. The average total impurity element content was 6.63% for the west elevation (Nos. 1–6), classified as weak weathering; 4.2% for the east elevation (Nos. 7–12), classified as very weak weathering; 6.89% for the bridge deck (Nos. 13–15), classified as weak weathering; and as high as 37.66% for the arch springing (No. 16), classified as severe weathering. These results demonstrate that the degree of enrichment of impurity elements such as Si, Fe, and Al can serve as a quantitative indicator for evaluating the weathering degree of stone (Figure 27).

5. Conclusions

5.1. Research Conclusions

Through the coupled analysis of the dynamic characteristics of Guanyin Bridge, the core conclusion can be drawn as follows:
The static equivalent response of long-span stone arch bridges exhibits significant spatial variations. The arch springing is subjected to concentrated combined compression–shear stress (with a maximum stress of 9.929 × 107 Pa determined by the finite element analysis), while the mid-span area exhibits bending deformation and serves as a displacement-sensitive area (with a maximum displacement of 8.05 × 10−2 m). Furthermore, the response in the y-direction (vertical) is greater than that in the x- and z-directions.
Structural discretization and slice division of cross-sections show that the maximum bending moment (1,941,509.15 N·m) occurs at 15.03 m, which is consistent with the location of the high-stress area at the mid-span in the finite element model, validating the accuracy of the internal force distribution in the arch structure as modeled by the shear Equation (18) and the bending moment Equation (19).
The theoretical model and finite element simulation are complementary. The theoretical model yields macroscopic responses suitable for preliminary design analysis, while the finite element simulation achieves the detailed analysis of local stress concentrations and material damage. Cross-comparison between the two approaches enhances robustness (with maximum deviations of 28.80% for displacement and 69.4% for stress).
The coupled analysis of individual elements reveals that the stress deviation caused by the 3D constraints at the arch springings (15, 76) is higher than that at mid-span elements (53, 54), indicating that the contact effect of node constraints has a significant impact on the local responses. The comprehensive coupled study of stress, displacement, strain, and energy identifies the “multi-index collaborative localization” of structural defects.

5.2. Innovations and Shortcomings

A research model system integrating “static equivalent response assessment + 3D modeling of mortise-and-tenon structure + exploration of reliability and damage mechanism” was established. A comprehensive study and analysis were conducted on the millennial ancient stone arch bridge for the first time, and the internal energy variation laws of complex static equivalent responses were compared systematically, providing valuable insights for research on the complex dynamic characteristics of stone arch bridges worldwide.
Research data show that the high-stress, high-displacement, and high-energy areas of long-span stone arch bridges tend to be concentrated, but these patterns do not always align with the internal energy variation in some individual elements. Therefore, it is necessary to conduct more refined modeling and analysis, and to carry out assessments on deterioration prevention and maintenance using multiple approaches. Based on research into the characteristic parameters of the Guanyin Qiao Bridge, a refined model has been developed that enhances the robustness of stress and displacement calculations for crystal block components (arch springings 15# and 76# and mid-span elements 53, 54) in multi-span stone arch bridges, filling the gap of insufficient force analysis of local components in traditional theoretical models.
The theoretical model only adopts the linear elastic–plastic model, without considering the actual brittle fracture properties and heterogeneity of the material, resulting in slight differences between the local stress results and the finite element simulation results. There are certain discrepancies between the boundary conditions set in finite element modeling and the actual conditions, and the influence of the elastic deformation of the supporting structure on the static equivalent response of the stone arch bridge is not fully considered. It is concluded that the interacting contact bodies, which have endured for thousands of years, may have altered their constraint properties, which is one of the reasons for the discrepancies between the calculated model analysis and the data from the physical structure.
When performing a detailed stress analysis of the local structures of the mortise-and-tenon joints (Nos. 15, 53, 54, and 76), due to the presence of minute gaps in some contact surfaces between the individual components—gaps that were filled with debris—the interactions between the components were not considered, and the frictional forces at the contact surfaces were ignored. Consequently, some of the analysis data did not accurately reflect the stress transfer characteristics caused by joint slippage and local elastic deformation. In contrast, the simulation analysis was based on full-contact loading; therefore, a comparison of the resulting data reveals certain discrepancies in the stress transfer between components 15# and 76# at the actual arch foot.

5.3. Follow-Up Work

It is necessary to improve the comprehensive theoretical model and conduct a phased analysis of the elastoplastic damage evolution of materials to enhance the accuracy of local stress research. Moreover, combined with on-site intelligent testing, the durability and reliability of stone arch bridges can be comprehensively evaluated.
Furthermore, it is necessary to explore the dynamic effects of multi-load combinations on stone arch bridges under different temperature gradients, and establish a comprehensive assessment system for safety, protection, operation, and maintenance.
Finally, an intelligent monitoring system can be established based on the IoT cloud platform, and advanced monitoring equipment such as fiber-optic sensors can be installed in the structurally vulnerable areas of the bridge to realize dynamic safety warning and sustainable protection, inheriting and carrying forward China’s millennial architectural techniques.

Author Contributions

Conceptualization, Z.Z., Q.J., Y.L., H.Y., J.A. and V.Y.; Data curation, Z.Z.; Formal analysis, Z.Z., Y.Y., J.A. and V.Y.; Funding acquisition, Z.Z. and V.Y.; Investigation, Z.Z., Y.L. and V.Y.; Methodology, Z.Z.; Software, Z.Z.; Writing—original draft, Z.Z. and J.A.; Writing—review and editing, Z.Z.; Resources, Y.L., H.Y. and J.A.; Project administration, Y.L., H.Y., J.A. and V.Y.; Validation, Y.Y.; Supervision, J.A. and V.Y.; Visualization, H.Y., J.A. and V.Y. All authors have read and agreed to the published version of the manuscript.

Funding

The authors gratefully acknowledge the funding received from the following research projects: Grant PID2023-150003OB-100, funded by MCIN/AEI/10.13039/501100011033 and by “ERDF A way of making Europe”; the newly launched doctoral research project, issued by Xiang Ke University [2023] No. 75; Natural Science Foundation of Hunan Province, Number 2025JJ50288; the science and technology innovation Program of Hunan Province, Number 2026RC9006; and the Hunan Province Undergraduate Innovation Training Program, Number 6591,6615.

Data Availability Statement

All data supporting the findings of this study are available within the paper.

Conflicts of Interest

Authors Hongping Yang and Yang Yang were employed by the company Nuclear Industry Huzhou Survey, Planning, Design and Research Institute Co., Ltd. The remaining authors declare that the research was conducted in the absence of any commercial or financial relationships that could be construed as a potential conflict of interest.

References

  1. Pagani, C. Embedding the Protection of Cultural Heritage into a Security Agenda: China’s and Russia’s Heritage Diplomacy. Int. J. Cult. Policy 2025, 1–22. [Google Scholar] [CrossRef] [Scilit]
  2. Deng, Y.; Jia, Y.; Li, Y.; Li, A. Structural Parameter Identification of Ancient Stone Arch Bridge via Three-Dimensional Laser Ranger Scanning. J. Perform. Constr. Facil. 2022, 36, 04022041. [Google Scholar] [CrossRef] [Scilit]
  3. Diaz, C.; Cornadó, C.; Albareda, A. Damage in Face-Brick Facades Placed between Concrete Slabs. J. Build. Eng. 2020, 30, 101312. [Google Scholar] [CrossRef] [Scilit]
  4. Olivieri, C.; Fortunato, A.; DeJong, M. A New Membrane Equilibrium Solution for Masonry Railway Bridges: The Case Study of Marsh Lane Bridge. Int. J. Mason. Res. Innov. 2021, 6, 446. [Google Scholar] [CrossRef] [Scilit]
  5. Zhang, Y.; Jiang, P.; Song, H.; Leng, J.; Chen, R.; Jiang, Z. Experimental Study on the Eccentrically Compressive Performance of Square Masonry Columns Repaired with UHPC Jackets. Front. Mater. 2023, 10, 1232768. [Google Scholar] [CrossRef] [Scilit]
  6. Li, G.; Ji, Y.; Zhao, R.; Xue, L.; Zhang, Y.; Zheng, K.; Cui, Y. Stable-Wavelength Perovskite Nanoplatelet Laser via Mixed-Phase Engineering. Sci. China Mater. 2025, 68, 4025–4031. [Google Scholar] [CrossRef] [Scilit]
  7. Choi, W.J.; Kim, J.-Y.; Hwang, M.; Lim, C.M.; Park, B.C.; Emre, A.; Lee, S.H.; Kotov, N.A. Highly Elliptic Circular Dichroism of Copper Aspartate One-Dimensional Nanostructures across the Ultraviolet to Terahertz Ranges. Nano Lett. 2025, 25, 7699–7706. [Google Scholar] [CrossRef] [Scilit]
  8. Matsuno, T.; Kinoshita, N.; Shimizu, K.; Shoji, H.; Ohata, M. Microstructural Feature-Driven Post-Mortem Analysis of Plastic Strain and Stress Triaxiality in Ductile-Fractured Ferrite-Martensite Dual-Phase Steel: Integrating Microstructural Observations and Mesoscale Finite Element Simulations. J. Mater. Res. Technol. 2025, 39, 3087–3102. [Google Scholar] [CrossRef] [Scilit]
  9. Chen, X.; Liu, H.; Wei, P. Extended Multiscale FEM-Based Concurrent Optimization of Three-Dimensional Graded Lattice Structures with Multiple Microstructure Configurations. Compos. Struct. 2024, 341, 118186. [Google Scholar] [CrossRef] [Scilit]
  10. Zhou, Z.W.; Alcalá, J.; Yepes, V. Regional Sustainable Development Impact through Sustainable Bridge Optimization. Structures 2022, 41, 1061–1076. [Google Scholar] [CrossRef] [Scilit]
  11. Kim, T.M.; Kim, D.-H.; Kim, M.K.; Lim, Y.M. Flexural Behaviour of a Half-Decked Bulb Tee Pre-Stressed Concrete Girder: Full-Scale Test and Nonlinear Finite Element Analysis. Struct. Infrastruct. Eng. 2017, 13, 665–682. [Google Scholar] [CrossRef] [Scilit]
  12. Zhu, C.; Li, Z.; Bao, Y.; Ning, P.; Zhou, X.; Wang, M.; Wang, H.; Shi, W.; Chen, B. Dynamic Analysis of a Long Run-Out Rockslide Considering Dynamic Fragmentation Behavior in Jichang Town: Insights from the Three-Dimensional Coupled Finite-Discrete Element Method. Remote Sens. 2023, 15, 5708. [Google Scholar] [CrossRef] [Scilit]
  13. Zhou, S.; Zhang, D.; Hou, B.; Ren, Z. Vibration Isolation Performance Analysis of a Bilateral Supported Bio-Inspired Anti-Vibration Control System. Appl. Math. Mech. 2023, 44, 759–772. [Google Scholar] [CrossRef] [Scilit]
  14. Ma, X.; Bao, C.; Wang, H.; Long, H.; Peng, L.; Lim, K.S. Study on the Performance of Base-Isolated Structures against Progressive Collapse and Parametric Analysis. Structures 2025, 80, 109850. [Google Scholar] [CrossRef] [Scilit]
  15. Ma, F.; Zhang, L.; Cui, M.; Cheng, X.; Zou, Y.; Cui, Y.; Wu, G. Investigation and Treatment of Bearing Diseases for Typical Expressway and High-Speed Railway Bridges in Eastern China: A Field Practice Campaign. Struct. Infrastruct. Eng. 2024, 20, 13–35. [Google Scholar] [CrossRef] [Scilit]
  16. Wang, Y.; Sun, Q.; Ding, H.; Leng, S.; Cui, H.; Xu, B.; Cui, H. Investigation of Interfacial Bonding Properties of Polyurethane Concrete and Cement Concrete/Steel Reinforcement. Adv. Mater. Sci. Eng. 2022, 2022, 5644468. [Google Scholar] [CrossRef] [Scilit]
  17. Muller, C.H.; Meyer, R. Inference of Intensity-Based Models for Load-Sharing Systems with Damage Accumulation. IEEE Trans. Reliab. 2022, 71, 539–554. [Google Scholar] [CrossRef] [Scilit]
  18. Zucca, M.; Reccia, E.; Longarini, N.; Cazzani, A. Seismic Assessment and Retrofitting of an Historical Masonry Building Damaged during the 2016 Centro Italia Seismic Event. Appl. Sci. 2022, 12, 11789. [Google Scholar] [CrossRef] [Scilit]
  19. Thiagarajan, G.; Kadambi, A.V.; Robert, S.; Johnson, C.F. Experimental and Finite Element Analysis of Doubly Reinforced Concrete Slabs Subjected to Blast Loads. Int. J. Impact Eng. 2015, 75, 162–173. [Google Scholar] [CrossRef] [Scilit]
  20. Zhang, G.; Liu, Y.; Liu, J.; Lan, S.; Yang, J. Causes and Statistical Characteristics of Bridge Failures: A Review. J. Traffic Transp. Eng. 2022, 9, 388–406. [Google Scholar] [CrossRef] [Scilit]
  21. Liu, H.; Zhang, W.; Gao, T. Structural Topology Optimization under Rotating Load. Struct. Multidiscip. Optim. 2016, 53, 847–859. [Google Scholar] [CrossRef] [Scilit]
  22. Dai, Z.; Tang, H.; Wu, S.; Habibi, M.; Moradi, Z.; Ali, H.E. Nonlinear Consecutive Dynamic Instabilities of Thermally Shocked Composite Circular Plates on the Softening Elastic Foundation. Thin-Walled Struct. 2023, 186, 110645. [Google Scholar] [CrossRef] [Scilit]
  23. Yang, Y.; Zhong, L.; Guo, Y.; Sun, Y.; Fang, G.; Shen, H. Theoretical and Experimental Study of Rigid Rapier Weft Insertion Vibration. Mod. Phys. Lett. B 2025, 39, 2442020. [Google Scholar] [CrossRef] [Scilit]
  24. Luo, K.; He, X.; Jing, H. Topology Optimization of Bridges under Random Traffic Loading Using Stochastic Reduced-Order Models. Probabilistic Eng. Mech. 2024, 75, 103583. [Google Scholar] [CrossRef] [Scilit]
  25. Chen, X.; Geng, X.; Fu, W.; Tan, L.; Guan, J.; Liu, T. Vibration Serviceability Assessment of Ribbon-Shaped Large-Span Footbridge at High Altitudes under Wind-Pedestrians Coupling Effects. Structures 2024, 66, 106885. [Google Scholar] [CrossRef] [Scilit]
  26. Jia, Q.; Xu, D.; Zou, Y.; Bao, Z.; Wang, T. Optimized Analysis and Reinforcement Design Model for RC/SCC Box-Section Bridges Using Developed Advanced Design Framework. Eng. Struct. 2024, 317, 118625. [Google Scholar] [CrossRef] [Scilit]
  27. Zhou, Z.; Zhou, J.; Alcalá, J.; Yepes, V. Thermal Coupling Optimization of Bridge Environmental Impact under Natural Conditions. Environ. Impact Assess. Rev. 2024, 104, 107316. [Google Scholar] [CrossRef] [Scilit]
  28. Pan, D.; Yu, X.; Zhou, Y. Cradle-to-Grave Lifecycle Carbon Footprint Analysis and Frontier Decarbonization Pathways of District Buildings in Subtropical Guangzhou, China. J. Clean. Prod. 2023, 416, 137921. [Google Scholar] [CrossRef] [Scilit]
  29. Farooq, H.; Nimbalkar, S.; Sheng, D. Geotechnical Rheological Modelling of Integrated Train-Track-Bridge System Using a Viscoelastoplastic Approach. Comput. Geotech. 2026, 191, 107829. [Google Scholar] [CrossRef] [Scilit]
  30. Fu, G.; Zhou, S.; Qi, L. On the Strain Gradient Elasticity Theory for Isotropic Materials. Int. J. Eng. Sci. 2020, 154, 103348. [Google Scholar] [CrossRef] [Scilit]
  31. Zhao, J.; Wang, C. Robust Topology Optimization under Loading Uncertainty Based on Linear Elastic Theory and Orthogonal Diagonalization of Symmetric Matrices. Comput. Methods Appl. Mech. Eng. 2014, 273, 204–218. [Google Scholar] [CrossRef] [Scilit]
  32. Ito, K.; Kashima, K. Maximum Entropy Optimal Density Control of Discrete-Time Linear Systems and Schrödinger Bridges. IEEE Trans. Autom. Control 2024, 69, 1536–1551. [Google Scholar] [CrossRef] [Scilit]
  33. Xu, S.; Wang, J.; Wang, X. Transfer from Defective Bridge Information Model to Defect Analysis Model Based on Industry Foundation Classes. Struct. Infrastruct. Eng. 2024, 22, 1143–1158. [Google Scholar] [CrossRef] [Scilit]
  34. Jiang, T.; Rønnquist, A.; Song, Y.; Frøseth, G.T.; Nåvik, P. A Detailed Investigation of Uplift and Damping of a Railway Catenary Span in Traffic Using a Vision-Based Line-Tracking System. J. Sound Vib. 2022, 527, 116875. [Google Scholar] [CrossRef] [Scilit]
  35. Wang, T.; Zou, S.; Ling, T.; Zhao, D.; Liu, W. Time-Variant Reliability Assessment for Determining Truck Axle Weight Limit of RC Bridges: A Hybrid Machine Learning-Based Framework. Structures 2025, 80, 110126. [Google Scholar] [CrossRef] [Scilit]
  36. Chai, S.; Zhang, J.; Wang, X. Basic Static Behaviours of an Arch-Cable Composite Bridge. Structures 2023, 47, 1548–1557. [Google Scholar] [CrossRef] [Scilit]
  37. Ram, I.; Senderovich, S.; Brodsky, A. Experimental and Numerical Study on the Impact of Geometrical and Mechanical Properties of Joints on the Out-of-Plane Behaviour of Masonry Walls. Structures 2025, 75, 108849. [Google Scholar] [CrossRef] [Scilit]
  38. Guzman-Acevedo, G.M.; Vazquez-Becerra, G.E.; Quintana-Rodriguez, J.A.; Gaxiola-Camacho, J.R.; Anaya-Diaz, M.; Mediano-Martinez, J.C.; Carrión Viramontes, F.J. Structural Health Monitoring and Risk Assessment of Bridges Integrating InSAR and a Calibrated FE Model. Structures 2024, 63, 106353. [Google Scholar] [CrossRef] [Scilit]
  39. Chinnaboon, B.; Panyatong, M.; Chucheepsakul, S. Influences of Surface Effects on Bending of Nanoplates with Complex Elastic Boundary Supports: A BE-RBFs Method. Comput. Math. Appl. 2026, 202, 170–195. [Google Scholar] [CrossRef] [Scilit]
  40. Ramani, V.; Zhang, L. Impacts of Climate Change on Long-Term Reliability of Reinforced Concrete Structures Due to Chloride Ingress. Constr. Build. Mater. 2022, 354, 129091. [Google Scholar] [CrossRef] [Scilit]
  41. Zhou, Z.; Zhao, Z.; Alcalá, J.; Yepes, V. Intelligent Operation Monitoring and Finite Element Coupled Identification of Hyperstatic Structures. Results Eng. 2025, 27, 106990. [Google Scholar] [CrossRef] [Scilit]
  42. Zhou, Z.; Zhou, J.; Zhang, B.; Alcalá, J.; Yepes, V. The Centennial Sustainable Assessment of Regional Construction Industry under the Multidisciplinary Coupling Model. Sustain. Cities Soc. 2024, 101, 105201. [Google Scholar] [CrossRef] [Scilit]
  43. Zhou, Z.W.; Alcalá, J.; Yepes, V. Experimental Research on Diseases of Emulsified Asphalt Mortar Board for Ballastless Tracks. J. Mater. Civ. Eng. 2023, 35, 04023156. [Google Scholar] [CrossRef] [Scilit]
  44. Navarro, I.J.; Penadés-Plà, V.; Martínez-Muñoz, D.; Rempling, R.; Yepes, V. Life Cycle Sustainability Assessment for Multi-Criteria Decision Making in Bridge Design: A Review. J. Civ. Eng. Manag. 2020, 26, 690–704. [Google Scholar] [CrossRef] [Scilit]
Disclaimer/Publisher’s Note: The statements, opinions and data contained in all publications are solely those of the individual author(s) and contributor(s) and not of MDPI and/or the editor(s). MDPI and/or the editor(s) disclaim responsibility for any injury to people or property resulting from any ideas, methods, instructions or products referred to in the content.

Article Metrics

Citations

Article Access Statistics

Multiple requests from the same IP address are counted as one view.