A Threshold-Adaptive Framework for Quantitative Diagnosis of Internal Short Circuits in LiFePO4 Batteries Using Multi-Feature Incremental Capacity Curves

,
,
,
,
and
1
School of Artificial Intelligence, Wuhan University of Technology, Wuhan 430070, China
2
State Grid Hubei Electric Power Co., Ltd. Wuhan Power Supply Company Qingshan Power Supply Center, Wuhan 430080, China
3
School of New Energy and Electrical Engineering, Wuhan University of Technology, Wuhan 430070, China
4
Hubei Key Laboratory of Advanced Technology for Automotive Components, Wuhan University of Technology, Wuhan 430070, China

Abstract

Although incremental capacity (IC) curve analysis is promising for early internal short circuit (ISC) detection, its diagnostic accuracy degrades significantly across a wide resistance range, especially for low-resistance events dominated by leakage currents. To overcome this limitation, we propose a threshold-adaptive ISC diagnostic framework that dynamically integrates quantitative resistance calculation (for high resistance, R ≥ 100 Ω) with Gaussian process regression (GPR)-based leakage current analysis (for low resistance, R < 100 Ω). Validated on 20 Ah LiFePO4 batteries, this approach achieves <6% error for 100–300 Ω and <8% error for <100 Ω (after GPR correction), demonstrating robust, implementation-ready solutions for real-world battery safety monitoring.

1. Introduction

Owing to their long cycle life and high energy density, lithium-ion batteries have become the dominant energy storage technology for electric vehicles (EVs), following their initial success in consumer electronics. In recent years, governments around the world have increased investment in the new energy industry [1], especially in the field of electric vehicles [2,3], and the global lithium battery market has therefore grown rapidly [4]. Due to the comprehensive consideration of vehicle speed, range, life, safety and cost, at present, the vast majority of pure electric vehicles have chosen lithium-ion batteries as their energy source [5,6].
However, lithium-ion batteries have potential safety issues that pose a threat to the personal and property safety of consumers [7,8]. An ISC occurs when mechanical, thermal, or electrical abuse (e.g., nail penetration, overheating, or overcharging) induces unintended contact between positive and negative electrodes, triggering uncontrolled discharge and heat generation [9,10]. As the specific energy of the battery system increases, the electrode material of the lithium-ion battery thickens [11,12,13] and the separator becomes thinner [14], elevating ISC probability. Therefore, it has become more important to clarify the triggering mechanism and hazards of internal short circuits in lithium-ion batteries and to develop an internal short circuit diagnostic algorithm [15,16].
The evolution of an internal short circuit can be divided into three stages: initial, intermediate and final [17]. The initial stage exhibits minimal electrothermal signatures due to low current density, rendering early detection challenging. To address this, existing ISC diagnosis methods primarily exploit battery state differentials—namely, capacity fade, voltage relaxation, state of charge deviation, and internal resistance change. Kong et al. [18] judged whether a lithium-ion battery had an internal short circuit fault by experimentally measuring and analyzing the remaining charge capacity of the battery. Feng et al. [19] proposed an electrochemical model to convert the measured cell voltage and temperature into the inherent electrochemical state of the cell, thereby achieving online internal short circuit fault diagnosis. Duan et al. [20] proposed a data-driven fault diagnosis based on information entropy to diagnose battery pack faults by analyzing the inconsistencies of different battery packs. Zheng et al. [21] developed a purely data-driven method using machine learning algorithms to diagnose early ISC faults based on different relaxation voltage features. An extended Kalman filter algorithm was used to estimate the SOC based on the features of the battery cells, and then the cell capacity was estimated. Finally, the fault was diagnosed quantitatively during a complete charge and discharge cycle at a specific threshold.
The IC curve has emerged as an effective means of diagnosing short-circuit faults within the battery [22]. By analyzing the changes in the incremental capacity peaks of faulty batteries and normal batteries, key information on changes in battery characteristics can be obtained, thereby establishing a correspondence between the external features of the battery and its electrochemical features.
Guo et al. [23] used the IC curve to diagnose micro-short circuits in ternary 18,650 batteries. The root mean square error between the IC curves of batteries with different degrees of short circuit and normal batteries were calculated to amplify the difference in internal short circuits and thereby diagnose micro-short circuits. The short circuit resistance can be calculated quantitatively based on the difference in charging capacity. Zhang et al. [24] studied in depth the changing laws of the difference between the IC curve and the charging capacity and proposed a micro-short circuit diagnosis for ternary lithium-ion batteries. They found that the peak of the IC curve corresponds uniquely to the SOC of the battery, so the difference in SOC between the internally short-circuited battery and the normal one is described using the difference in charging capacity and the resistance is quantified. Zhang et al. [25] proposed a local outlier factor method for ternary lithium-ion batteries that targets IC curves. This effectively identifies early short circuit faults in the battery, accurately locates the faulty single cell in the battery pack and describes the severity of the fault but does not quantitatively analyze the resistance. Sun et al. [26] chose ternary lithium-ion batteries and used the characteristic changes in the IC curve to qualitatively distinguish between ISC batteries and aged batteries. They then established an equivalent circuit model for the ISC battery and combined it with extended Kalman filtering and the forgetting factor recursive least squares (FFRLS) to jointly estimate the internal short-circuit resistance and SOC of the faulty battery. Zhao et al. [27] found that the fault voltage curve of the parallel module has a smaller deviation than the standard voltage curve, so a fault simulation model of the parallel battery module was established for the ternary lithium battery. At the same time, by analyzing the relationship between the Peak III and Peak IV amplitudes of the IC curve, features of the parallel battery module and the short circuit resistance are obtained. Finally, a model-driven online calculation process for short circuit resistance is proposed in the application, and its robustness is verified. Liao et al. [28] proposed a fault diagnosis based on the IC curve for ternary lithium batteries, aiming to identify aging batteries and batteries affected by micro-short circuits (MSC). The method used feature parameters of the IC curve to find aging batteries. The study highlights a clear link between the IC Peak and the SOC. To estimate the leakage current, the approach involves analyzing the variation in the time each battery takes to hit its peak point. This method can estimate the MSC resistance to quantify the degree of short circuit failure, and the average diagnostic error of MSC resistance within 510 Ω is always kept below 10%. Qiao et al. [29] also proposed an online quantitative diagnosis for internal short circuits in batteries based on the incremental capacity, which uses the IC curve to compare the area difference between the internally short-circuited battery and the normal battery for diagnosis. It can successfully calculate the ISC resistance with small errors and calculation.
As shown above, existing IC-based methods are predominantly limited to ternary (NMC) cells and exhibit resistance-dependent accuracy degradation. The present work extends IC-based ISC diagnosis to LiFePO4 cells and introduces a threshold-adaptive mechanism that maintains accuracy across the full resistance range, complementing and advancing the current state of the art. To bridge these gaps, this work establishes three contributions:
(1)
First, an IC curve-based ISC diagnostic framework for LiFePO4 batteries is developed through systematic experiments.
(2)
Second, the framework is rigorously validated across a comprehensive range of resistance values, ensuring robust diagnostic performance across diverse internal short-circuit scenarios.
(3)
Third, leakage current and its normalized proportion are introduced as novel ISC resistance predictors, achieving significant accuracy improvements for low-resistance faults.

2. Proposed Diagnostic Framework

2.1. Incremental Capacity Curve Analysis for LiFePO4 Batteries

The lithium-ion battery incremental capacity method is widely used in the study of battery aging and degradation mechanisms [30]. It converts the voltage platform into the peak value in the incremental capacity. By studying the IC curve, the electrochemical change features of the battery can be reflected [31], thereby establishing a correspondence between the external charging and discharging characteristics of the battery and the characteristics inside the battery.
Figure 1 illustrates the voltage–capacity curve and IC curve of a 20 Ah LiFePO4 battery charged at 0.1 C. The anode material, graphite, undergoes lithium-ion intercalation during charging, transitioning carbon into LiC6 through five distinct electrochemical reaction stages (1–5). These stages manifest as voltage plateaus in the voltage–capacity curve, with three prominent plateaus (1*II, 2*II, and 5*II) corresponding to peaks in the IC curve [32]. Simultaneously, the cathode material alternates between FePO4 and LiFePO4. This phase transition involves a single-phase solid-solution reaction and a two-phase coexistence region, where the latter dominates more than 95% of the battery’s capacity change. The two-phase region (Phase II) establishes a stable reference potential for the anode reactions, ensuring minimal voltage hysteresis.
Figure 1. LiFePO4 battery voltage–capacity curve compared with IC curve.
The internal dynamics of a lithium-ion battery constitute a complex nonlinear system, where conventional time-domain analysis of charge/discharge curves fails to capture its nonlinear behavior. Incremental capacity (IC) analysis overcomes this limitation by transforming voltage plateaus in the terminal voltage curve into distinct peaks. These IC Peaks serve as critical diagnostic features for battery aging assessment and internal short circuit detection [28]. Consequently, we employ the IC curve to investigate short-circuit mechanisms in lithium-ion batteries.
The principle of incremental capacity analysis involves computing the first derivative of the terminal voltage–capacity (V-Q) curve under constant current charging/discharging conditions to obtain the incremental capacity curve. The IC curve quantifies the amount of charge/discharge per unit voltage of the battery, as defined in Equations (1) and (2)
Q = ∫ I × d t
d Q / d V = I × d t / d V
where t and I represent time and current in the constant-current charging mode, respectively.
However, practical IC curves suffer from measurement noise, necessitating smoothing. After comparing multiple smoothing techniques, Gaussian smoothing is adopted here due to its noise suppression capability while preserving critical features [33]. The Gaussian smoothing method has the characteristics of a Gaussian distribution, as expressed below [34]:
G ( x ) = 1 σ 2 π e x p ( ( − ( x − μ ) 2 ) / ( 2 σ 2 ) )
where μ and σ represent the mean and standard deviation of the observed signal x, respectively.
In this IC curve processing, linear interpolation with 1200 interpolation points is used to enhance resolution, and the IC curve is obtained by further differentiating and taking the standard deviation σ to be 17.5.
Justification of parameter choices: The LiFePO4 charging curve spans approximately ΔV ≈ 1.65 V (2.0–3.65 V); with 1200 interpolation points the voltage resolution is about 1.4 mV/point, sufficient to resolve the narrow Peak ③ (spanning ~50 mV) while avoiding over-interpolation artifacts. The Gaussian smoothing standard deviation σ = 17.5 was selected based on a systematic sensitivity analysis (Table 1), reprocessing the IC curves with σ ∈ [5, 40] and interpolation points N ∈ {600, 1200, 2400}.
Table 1. Sensitivity of Peak ③ position and height to Gaussian smoothing parameter σ and interpolation-point number N.
Peak ③ position is extremely stable: ≤1.1 mV shift for σ ∈ [15, 25] and ≤0.4 mV for N ∈ {1200, 2400}. Although Peak ③ height varies more with σ (±18% for σ ∈ [15, 25]), the diagnostic method primarily depends on peak position and relative area differences, both of which remain stable within the identified range; σ = 17.5 was selected as the midpoint of the stable interval [15, 25]. A supplementary figure comparing IC curves at different σ values is provided in Figure 2.
Figure 2. IC curves processed with different σ values and N values. (a) IC curves at different sigma (N = 1200); (b) IC curves at different N (sigma = 17.5).

2.2. High-Resistance ISC Diagnosis Using IC Curve Area Difference

In order to simulate internal short circuit conditions [35], external resistors of varying values are connected to the battery terminals [36]. Although external short circuits do not strictly replicate internal short circuits, they effectively emulate early-stage ISC scenarios [37,38]. We first propose a method to quantify short-circuit resistance by calculating the area difference between the ISC and normal incremental capacity curves.
Applicability of the external-resistor substitution method: External parallel resistors replicate the primary electrical signature of an ISC—a continuous parasitic current path that bypasses the normal electrochemical reaction. For early-to-moderate ISC (R ≥ 5.5 Ω), the dominant diagnostic signal is the additional charge (leakage current) drawn during constant-current charging, which manifests as IC curve elevation and is faithfully reproduced by external resistors. The method targets ISC regimes where the resistance is sufficiently high that thermal runaway has not yet been triggered; for severe ISC at very low resistance (e.g., <5 Ω), thermal effects dominate and the method’s applicability diminishes. We note the key differences from real ISC; in a real ISC, heat is generated internally at the short-circuit site, leading to localized hot spots and potentially non-uniform current distribution, whereas external resistors generate heat outside the cell with more uniform thermal conditions, and the current path flows through the terminals rather than the electrode/separator interface. Prior studies [35,36] have systematically compared external and internal short-circuit triggering methods and confirmed that external methods are suitable for studying the electrical response of early-stage ISC. This limitation is also stated in the Conclusions.
Connecting resistors of varying resistances in parallel with the battery induces ohmic voltage drop and polarization effects during charging. At high C-rates, the voltage plateau of LiFePO4 batteries diminishes significantly, causing IC Peak features to merge and increasing resistance calculation errors. Thus, a uniform 0.1C constant-current charging protocol is adopted [39]. Taking a low-resistance external short circuit as an example:
As shown in Figure 3a, the ISC IC curve is divided into four segments based on peaks, and find the Peak ① and Peak ②, the Peak ② and Peak ③, and the lowest value point X1_ISC, X2_ISC, X3_ISC between Peak ③ and Peak ④, respectively. We also take points X0_ISC and X4_ISC, where
X 0 _ I S C = X 1 _ I S C − 0.05 V
X 4 _ I S C = X 3 _ I S C + 0.05 V
Figure 3. Segmentation of IC curves for (a) ISC and (b) normal states.
Similarly, as shown in Figure 3b, the normal IC curve is divided into four parts according to the peaks. The Peak ① and Peak ②, the Peak ② and Peak③, and the lowest value points X1_nor, X2_nor, and X3_nor between Peak ③ and Peak ④ are found, respectively. The points X0_nor and X4_nor are also taken, where
X 0 _   n o r = X 1 _   n o r − 0.05 V
X 4 _   n o r = X 3 _   n o r + 0.05 V
Sensitivity to the voltage-window offset: The 0.05 V offset defining the Peak ③ integration window was chosen to capture the full Peak ③ area without including adjacent peaks while providing a consistent boundary across all resistance conditions, as is shown in Table 2.
Table 2. Sensitivity of the Peak ③ integrated area to the voltage-window offset.
For offsets <0.05 V the window is too narrow to capture the full Peak ③ structure, causing rapid area reduction; for offsets >0.05 V the area continues to grow as adjacent features are included. The 0.05 V offset represents the transition point where the full Peak ③ lobe is captured while minimizing contamination from adjacent peaks and valleys. Because the area-difference method computes the difference between ISC and normal IC curves within this window, a consistent window definition across all resistance conditions ensures that the diagnostic result reflects ISC severity rather than window artifacts.
At low C rates, the amount of charge ΔQ delivered by an ISC cell in the same voltage range ΔV will exceed that of a regular cell, causing the ISC IC curve to exhibit higher peaks. The total charge delivered by each cell corresponds to the area under its IC curve, and the difference between the ISC and normal IC curves represents the short-circuit leakage charge (LEQ). Taking Peak ① as an example, the internal short-circuit resistance RISC is calculated as follows:
Normal curve ΔQ:
Δ Q ( ① _ n o r ) =   ∫ X 0 _ n o r X 1 _ n o r d Q d V d V
ISC curve ΔQ:
Δ Q ( ① _ I S C ) =   ∫ X 0 _ I S C X 1 _ I S C d Q d V d V
Electric leakage ΔQ at ①:
Δ Q L E Q ① = Δ Q ( ① _ I S C ) − Δ Q ( ① _ n o r )
As shown in Figure 4, the charging time between voltages X 0 _ I S C ( t 1 A ) and X 1 _ I S C ( t 2 B ) of the charging voltage curve Δt2(AB) is shown in the figure below. The leakage current ILEQ① between the two voltages can therefore be expressed as:
I L E Q ① = Δ Q L E Q ① Δ t 2 A B
Figure 4. Charging curve of ISC battery and normal battery.
After obtaining the leakage current ILEQ, the ISC resistance (RISC) is calculated using Ohm’s law. In this study, IISC is the average leakage current between voltage points A (X0_ISC) and B (X1_ISC), and the corresponding average terminal voltage U A B ¯ is shown in Figure 4. The formula for IISC is as follows:
U A B ¯ = ∫ t 1 A t 2 B V d t t 2 B − t 1 A
R I S C = U A B ¯ I L E Q ①
The short-circuit resistances under different peak intervals can be calculated, and the accuracy of Peak ①–④ is validated by comparing the calculated values against the externally applied test resistances.
In addition, lower external short-circuit resistance induces a more pronounced leftward voltage shift in the charging IC curve. This occurs because a resistor with a lower resistance not only generates heat itself but also causes the battery to heat up. The increase in temperature will reduce the polarization effect of the battery and reduce the voltage hysteresis. This also means that, at lower voltages, the electrochemical reactions in the battery will proceed more easily. Therefore, during the charging process, lithium ions may migrate from the positive electrode to the negative electrode at a lower voltage. Secondly, the rise in temperature also accelerates the diffusion of lithium ions in the electrode material, allowing the reaction to occur at a lower voltage. Finally, this causes the IC curve to shift to the left, which is why the ISC curve in Figure 3 is offset to the left compared to the normal curve.
It is important to note that the IC curve area difference method (Section 4.1) does not perform uniformly across all resistance levels. Specifically, it is suitable for high-resistance scenarios but yields large errors for low-resistance cases and vice versa. Consequently, based on literature analysis, the area difference method is prioritized for high-resistance diagnosis due to its broader applicability across resistance ranges. Low-resistance diagnosis will be addressed in the following section.

2.3. Low-Resistance ISC Diagnosis with Multi-Feature IC Parameters

A large set of resistances was tested and calculated using the method in Section 2.2. It was found that, when the resistance is below 100 Ω, the error increases to a maximum of 15.71%, and all calculated resistances are lower than the actual values. This indicates that the method in Section 2.2 is inapplicable in this case.
Note that the specific value of internal short resistance is directly related to the tested battery’s capacity. In order to quantify the dividing line that can be applied to a wider range of batteries and to determine when further discrimination is required, the dimensionless value α R and threshold judgement method are proposed.
In Section 4.1, later calculations and the results of experiments with other capacities, it is found that the average voltage of Peak ① to ④ is close to and between 3.2 V and 3.4 V and the average voltage for the most accurate case of diagnostic accuracy results is around 3.33 V (Uaver). Battery capacity may fluctuate slightly during charge–discharge cycles, but minor variations do not significantly affect the results unless the battery has undergone severe aging. So, in the calculation of the dimensionless value for the relevant value can be uniformly used in the calculation of nominal capacity. The charging current of a battery with a capacity of 20 Ah is 2A (Irate) at 0.1C, and the calculated direct current resistance is. When the external resistance is lower than 100 Ω (Rtest), the diagnostic error is larger, and then we have:
α R = R t e s t U a v e r / I r a t e = 100   Ω 1.665   Ω ≈ 60.06
Therefore, the threshold judgement is as follows: a suspected short-circuited resistor is first diagnosed using the IC curve area difference method, and the dimensionless value is calculated from the obtained resistance. When α R ≥ 60.06, the IC curve area-difference method can be directly used to determine the resistance. When α R < 60.06, the Gaussian process regression (GPR) method is required for further analysis. The boundary case α R = 60.06 (corresponding to R = 100 Ω) is assigned to the IC-curve area-difference method, consistent with the experimental observation that the area-difference approach yields <6% error at this resistance. The dimensionless threshold α R = 60.06 is theoretically applicable to LiFePO4/graphite cells of different capacities. However, the current experimental validation is limited to 20 Ah pouch cells; validation on cells with different capacities, form factors, and aging states is an important direction for future work.
In the next step, a feasible dataset is trained using the GPR by capturing the feature parameters of its IC curve, such as slope and leakage current as a percentage of the ratio to achieve a better prediction of the resistance in the case of low resistances. Figure 5 shows the specific methodology flowchart.
Figure 5. Resistance diagnostics flowchart based on threshold judgement.

2.4. Gaussian Process Regression for Leakage Current Predictions

Gaussian process regression predicts the resistance by using the feature parameters of the IC curve as training data and establishing a relationship between them.
The GPR is similar to a set of finite random variables obeying a Gaussian distribution. For each data point x in the input set [x1, x2, …, xn], the probability distribution of the corresponding function value f(x) obeys a Gaussian distribution, denoted as f(x)~GP(m(x),kf(x,x′)) [34]. Therefore, the properties of f(x) are determined by its mean m(x) and covariance function kf(x,x′), which are given by the following equations:
m ( x ) = E ( f ( x ) )
k f ( x , x ′ ) = E [ ( m ( x ) − f ( x ) ) ( m ( x ′ ) − f ( x ′ ) ) ]
The choice of the covariance function kf(x,x′) depends on the actual application. The covariance between each feature variable can be represented by a Gaussian process kernel function. In this paper, the Matérn kernel function is selected, and its general form is:
k ( x p , x q ) = σ f 2 1 + 3 | x p − x q | λ exp − 3 | x p − x q | λ
where xp and xq represent the input sets of the pth and qth types, respectively.
The regression problem can be expressed as the output value of the function f(x) being affected by noise and the observed value y being the sum of the output value of f(x) and the noise magnitude, which is expressed as follows:
y = f ( x ) + ε
where ε is the noise and obeys a Gaussian distribution as shown in Equation (19)
ε ~ N ( 0 , σ n ) 2
The prior distribution of the observations satisfies:
y ~ N ( 0 , K f ( x , x ) + σ n I 2 )
where y is the observed sequence; x represents the input set [x1, x2, …,xn]; and Kf(x,x′) = (kij)n×n. Here, k i j = σ f exp 2 − x p − x q 2 2 λ 2 , I is the n-dimensional identity matrix, and σ n I 2 is the noise covariance matrix.
In Equation (17), the kernel function is determined by two parameters, σ f and λ , and the noise variance σ n . The unknown parameters θ = [ σ f , σ n , λ ] are called hyperparameters, and the hyperparameters can be determined using the maximum likelihood method. After the kernel function form and hyperparameters are determined, the GPR model is determined. By calculating the posterior distribution p ( y * | x , y , x * ) , the GPR model can predict the test sample. For a new data set x * , the estimated value y * also obeys a Gaussian distribution. Then the joint Gaussian distribution of the observed value y and the estimated value y * is
y y * ~ N 0 , K f ( x , x ) + σ n I 2 K f ( x , x * ) K f ( x , x * ) T K f ( x * , x * )
According to the priori distribution, it can be deduced that p ( y * | x , y , x * ) also obeys a Gaussian distribution, as shown in Equation (22):
p ( y * | x , y , x * ) = N ( y * | y ¯ * , cov ( y * ) )
and
y ¯ * = K f ( x , x * ) T K f ( x , x ) + σ n I 2 − 1 y
cov ( y * ) = K f ( x * , x * ) − K f ( x , x * ) T [ K f ( x , x ) + σ n I 2 ] − 1 K f ( x , x * )
where y ¯ * is the mean of y * and cov ( y * ) is the variance matrix of the test data, which reflects the reliability of the estimate.
This paper uses a GPR model, which uses I3 (the leakage current at Peak ③) and the leakage proportion (I3/I_rate × 100%) as features, and the reciprocal of resistance (1/R) as the prediction target. A Matérn kernel (Equation (17)) is adopted, with hyperparameters optimized by maximum likelihood estimation (MLE). Prediction yields a Bayesian posterior distribution with 95% prediction intervals, providing inherent uncertainty quantification.

3. Experimental Setup

The cells under test are LiFePO4/graphite pouch cells manufactured by Zhuhai Penghui Energy Co., Ltd. (Zhuhai, China). Three independent cells of the same batch and specification were used to support cross-unit validation. The basic specifications are shown in Table 3.
Table 3. Basic parameters of the experimental cells.
After capacity calibration, the capacity of this batch of batteries is generally around 20.5 Ah, and the 0.1C charging current is 2.05 A. Charging and discharging are performed using the NEWARE battery testing system, model CT-4002-5V300A-NTFA (Shenzhen Neware Technology Co., Ltd., Shenzhen, China; measurement accuracy: voltage ±0.05% FS + ±0.05% RD, full scale 5 V; current ±0.05% FS + ±0.05% RD, full scale 300 A). The ambient temperature in the experimental chamber is maintained at 24 ± 1 °C. The test platform is shown in Figure 6.
Figure 6. Schematic of the external-resistor substitution test platform: LiFePO4 pouch cell, external resistor R_ext in parallel (via a switch), and NEWARE CT-4002 wiring for V and I acquisition.

4. Results and Discussion

4.1. Diagnostic Performance of IC Curve Area Difference

Following the methodology outlined in Section 2.2, controlled external short-circuit experiments were conducted across 12 resistance conditions: 300 Ω, 250 Ω, 200 Ω, 150 Ω, 100 Ω, 83 Ω, 65 Ω, 50 Ω, 20 Ω, 10 Ω, 5.5 Ω, and normal conditions. For each test case, the incremental capacity curve was first processed using Gaussian smoothing to suppress measurement noise while preserving critical peak features. Subsequently, the internal short-circuit resistance values corresponding to characteristic Peaks ① through ④ were independently calculated using the area-difference approach described in Section 2.2. The diagnostic results for each resistance condition and peak position are presented in Table 4 and analyzed below.
Table 4. Error distribution across characteristic peaks for different short-circuit resistances.
Analysis of Table 4 reveals that Peaks ①, ②, and ④ consistently yield high diagnostic errors across all resistance values, whereas Peak ③ maintains significantly lower errors. Specifically, for resistances ≥100 Ω, Peak ③ delivers resistance calculations with errors below 6%, which aligns with the accuracy threshold established in the literature [29]. Conversely, when resistance falls below 100 Ω, errors increase substantially, reaching a maximum of 15.71%. Notably, in the sub-100 Ω range, the calculated resistance values are systematically underestimated relative to actual values.
To understand the poor diagnostic performance of Peaks ①, ②, and ④, two key mechanisms must be considered. First, Peaks ① and ② occur during early-stage charging phases with inherently short durations. Under ISC conditions, this limited timeframe restricts the development of measurable leakage currents through the shorting resistance, introducing significant errors into the area-difference calculations. Second, as documented in the literature, Peak ④ exhibits diagnostic ambiguity at high initial states of charge, where its signature overlaps with both ISC and normal operational conditions. Consequently, Peaks ①, ②, and ④ collectively demonstrate insufficient reliability for resistance quantification.
In addition, the literature [32] demonstrates that Peak ③ (corresponding to Peaks 5*II and 2*II in their notation) exhibits superior robustness against variations in charging rate, ambient temperature, and battery aging compared to other characteristic peaks. Given its alignment with typical operational SOC ranges, strong anti-interference capability, and association with the most significant capacity change rate (dQ/dV) in the IC curve, Peak ③ is readily identifiable in practical applications. These properties establish Peak ③ as the optimal feature for ISC fault detection.
In summary, Peak ③ is selected as the diagnostic feature because: (1) it produces the largest dQ/dV magnitude among all characteristic peaks, so ISC-induced leakage current produces the most pronounced absolute change in its area, maximizing the signal-to-noise ratio; (2) it occurs in the mid-charge region where the cell voltage is stable (~3.33 V) and the ISC leakage current has accumulated a measurable cumulative effect, unlike Peaks ① and ②, which occur during early charging phases with inherently short durations; (3) it is robust to charging rate, ambient temperature, and aging [32], making it the most reliable feature across diverse operating conditions; and (4) it is well-separated from adjacent peaks at 0.1C, ensuring reliable identification and integration, unlike Peak ④, which may merge with Peak ③ under high-C-rate or aged conditions.
Regarding curve selection for Figure 7, because LiFePO4 battery IC curves exhibit minimal distortion at very high resistances (>300 Ω), we selected representative resistance cases (10 Ω, 83 Ω, 100 Ω, and 200 Ω). These span the critical transition range where ISC-induced changes are clearly observable while maintaining diagnostic relevance.
Figure 7. 10 Ω, 83 Ω, 100 Ω, and 200 Ω compared with the normal IC curve.
Figure 7 demonstrates that lower short-circuit resistances generate larger leakage currents, requiring additional charge capacity to compensate and thereby increasing both the peak magnitude and integrated area of the IC curve. Consequently, the 10 Ω case exhibits IC curve characteristics significantly exceeding those of other test conditions. As the parallel resistance increases (83 Ω, 100 Ω, and 200 Ω), the ISC-induced IC curves progressively converge with the normal-state curve. To establish a robust discrimination criterion, we adopt 100 Ω (corresponding to a dimensionless threshold of 60.06) as the critical boundary; when the threshold value is <60.06, IC curves display pronounced visual deviations from normal operation, yet require GPR for accurate quantification due to area-difference method limitations; when the threshold is ≥60.06, subtle but quantifiable curve shifts permit reliable resistance calculation via the area-difference approach. As for the phenomenon of relatively smaller results for low resistances, the mechanisms are explained as follows:
The increased diagnostic error in the low-resistance region (R < 100 Ω) may be partially attributed to factors that violate the constant-impedance assumption underlying the area-difference method. We hypothesize that temperature rise and dynamic impedance variation are contributing factors—as lower resistances draw larger leakage currents and generate more ohmic heating—but direct temperature and impedance measurements were not performed in this study. Therefore, this explanation should be regarded as a working hypothesis. Future work incorporating in situ temperature monitoring and electrochemical impedance spectroscopy (EIS) would provide direct evidence to confirm or refine this mechanism.
The algorithm for calculating external resistance assumes that the equivalent internal resistance and internal short circuit characteristics of the battery are constant over a certain range. This assumption is relatively valid for high resistances, whereas at low resistances it may no longer be applicable due to dynamic changes in the internal chemical properties of the battery (e.g., enhanced thermal effects), which can lead to increased errors in the calculation of low resistances. It can be further illustrated with the help of the equivalent circuit model in the literature [40]:
For the sake of illustration, components such as the equivalent capacitance are omitted, so that the main equivalent model of a normal battery can be referred to as shown in Figure 8a The relationship between the terminal voltage and the terminal current of the equivalent circuit model of the battery is shown in Equation (25), where U is the terminal voltage of the battery, E is the open-circuit voltage (OCV) of the battery, I is the terminal current of the battery, and R is the internal resistance of the battery.
U = E − I R
Figure 8. Battery equivalent circuit model and internal short circuit equivalent circuit model. (a) Normal battery; (b) short-circuit battery.
Because the electrical characteristics of an internally short-circuited battery are comparable to those of an externally short-circuited one, the equivalent circuit model of Figure 8b can also be used to describe the internal short-circuit case. The RISC representative is a resistor connected in parallel to the outside. According to Figure 8b, Equation (26) can be obtained:
E − I R ⋅ R = I I S C ⋅ R I S C I R − I I S C = I
where IR is the current flowing through the original battery circuit and IISC is the internal short-circuit current. The internal short-circuit current IISC can be obtained by solving Equation (26) as Equation (27)
I I S C = E − I ⋅ R R + R I S C
Combining Equation (26) and Equation (27) and Ohm’s law, the relationship between the terminal voltage and terminal current of the equivalent circuit model of the internal short-circuited battery in Figure 8b can be obtained as Equation (28)
U = R I S C R + R I S C ⋅ E − I ⋅ R I S C R + R I S C ⋅ R
Comparing Equations (25) and (28), it can be found that the equations of short-circuit battery and normal battery have a similar structure; the difference is what the open-circuit voltage E and the internal resistance R of the normal battery become and in the relation equation of the short-circuit battery, respectively, it is called the equivalent open-circuit voltage of the short-circuit battery and is called the equivalent internal resistance of the short-circuit battery, and both are the equivalent parameter of the internal short-circuit battery. When the resistance is small, it will trigger the warming of the battery itself, and the warming of the battery makes its internal resistance decrease, i.e., R decreases, leading to an overall decrease in the equivalent internal resistance, i.e., of the internal short-circuit battery. However, for the IC curve area difference calculation method, especially for the normal battery, we assume that its internal resistance is relatively stable under Peak ③, which directly leads to the calculated short-circuit resistance RISC; resistance is relatively small, due to the temperature rise of the battery being more pronounced at low resistances, while the temperature rise of the high resistances is not so drastic, so the thermal effect produced by the high resistance is weak, and has little effect on the physicochemical characteristics of the battery, so the algorithm can calculate the high resistance more accurately.

4.2. Leakage Current Features and Threshold Determination

In the calculation, it is found that the leakage current I3 of the Peak ③ is more accurate than the leakage currents of other peaks, and the average voltage of the Peak ③ is around 3.33 V. We use the leakage current I3 of each resistor Peak ③ and the proportion of its leakage current to the total charging current as input for Gaussian regression training, corresponding to their respective resistances, to achieve prediction for different resistances. Among them, I3, U3 and R3 are all rounded to four decimal places. Since the device itself cannot stabilize the charging current at a strictly constant value during the charging process, the average value is taken, as shown in Table 5. We use the threshold determination method: when α R < 60.06, we use the characteristic variables of the leakage current for training and prediction.
Table 5. Feature parameters of Peak ③ under different resistances.
The I3 and leakage current ratios are extracted as the training volume, and the corresponding resistances were tested, with the following Table 6.
Table 6. Prediction results using I3 and the leakage current ratio.
The errors of the predicted resistances in Table 6 are greatly reduced compared with the area-difference method, with a maximum error of 7.89%. This also confirms the feasibility of using the leakage current I3 and its proportion to the total charging current as indicators for ISC resistance prediction. In order to investigate the applicability of this method, we used the data in Table 3 to randomly select resistance pairs and conduct an external short circuit replacement test on similar soft package LiFePO4 batteries. The results are as follows:
Leave-One-Out cross-validation (LOO-CV) was performed on the seven training points to assess generalization. The results are summarized in Table 7.
Table 7. Leave-One-Out cross-validation results of the GPR model with 95% prediction intervals.
For R ≥ 10 Ω the maximum LOO-CV error is 8.45% (at 20 Ω, mean 3.69%), and for R ≥ 50 Ω all errors are below 3% (max 2.65%). The 95% prediction interval covers the true value in all seven cases (100% coverage). The 5.5 Ω point shows a larger LOO-CV error (21.65%) because removing it leaves no low-resistance training data for extrapolation, yet the 95% PI still correctly covers the true value. Compared with the full-training-set predictions, the LOO-CV errors at 50–83 Ω are even lower, confirming that the model is not overfitting. The GPR model therefore demonstrates genuine predictive power beyond simple interpolation, with reliable uncertainty quantification.
As shown in Figure 9, the black curve is for battery No. 2 and the red curve is for battery No. 3. For battery No. 2, an external short-circuit experiment was performed by connecting 300 Ω, 200 Ω, 150 Ω, 100 Ω, 65 Ω, 50 Ω, 20 Ω, and 15 Ω resistors in parallel. The maximum error for resistors below 100 Ω is 7.08% (Corresponding to 20 Ω), and the maximum error for resistors above 100 Ω is 5.47%. For battery No. 3, it was connected in parallel with 283 Ω, 233 Ω, 183 Ω, 133 Ω, 100 Ω, 83 Ω, 50 Ω, and 33 Ω resistors. The maximum error for resistors under 100 Ω is 4.10% (corresponding to 83 Ω), and the maximum error occurs at 233 Ω, with an error of 5.79%.
Figure 9. High-to-low resistance error test for similar soft-packed LiFePO4 batteries.
The results for batteries No. 2 and No. 3 under random resistance tests are excellent; the errors of the short-circuit resistance, both within and outside the dimensionless threshold, are all below 8%, which proves the effectiveness of this method.

5. Conclusions

Internal short circuits in LiFePO4 batteries cause abnormal energy dissipation during charging, which can be detected as distinct deviations in their IC curves. While conventional IC-based resistance estimation fails for low-resistance ISCs (<100 Ω), this work establishes a threshold-adaptive quantitative diagnosis framework that leverages multi-feature analysis of IC curves to achieve robust ISC resistance quantification. The framework employs a dimensionless threshold to dynamically switch between resistance estimation (error < 6% for 100–300 Ω when α R ≥ 60.06) and GPR refinement (error < 8% for R < 100 Ω when α R < 60.06). The proposed threshold-adaptive framework achieves <8% diagnostic error across the full resistance range, demonstrating that multi-feature IC curve analysis enables precise quantification of ISC resistance using an adaptive dimensionless threshold.
Although the proposed framework achieves <8% diagnostic error across the full resistance range, several limitations should be acknowledged. The method requires a controlled 0.1C constant-current charging protocol. Peak ③ and its leakage-current feature I3 correspond to one of the graphite anode intercalation stages described in Section 2.1, which are common to LiFePO4/graphite cells; the feature is therefore expected to be transferable, but the exact peak position and shape may vary with electrode loading and cell design, potentially requiring GPR model recalibration. Current validation is limited to 20 Ah pouch cells at 24 ± 1 °C in a laboratory environment, and external-resistor substitution approximates the electrical signature of ISC but does not replicate its thermal and mechanical aspects. Future work will validate the method on cells with different capacities, form factors, and aging states; investigate performance under dynamic temperature and variable C-rate conditions; extend the framework to pack-level diagnosis; and incorporate in situ temperature and impedance measurements to refine the low-resistance mechanism.

Author Contributions

R.X.: writing—original draft preparation; L.Q.: software, data curation; J.V.W.: validation, writing—review and editing; Z.G.: formal analysis, writing—review and editing; Q.W.: methodology, supervision; J.K.: conceptualization, funding acquisition. All authors have read and agreed to the published version of the manuscript.

Funding

This work was supported by the National Natural Science Foundation of China under Grants No. 52277224 and No. 52407217.

Data Availability Statement

Dataset available on request from the authors.

Conflicts of Interest

Author Lizi Qu was employed by State Grid Hubei Electric Power Co., Ltd., Wuhan, China. Authors Zhichao Gong and Jianqiang Kang were employed by Hubei Collaborative Innovation Center for Automotive Components Technology, Wuhan, China. The remaining authors declare that the research was conducted in the absence of any commercial or financial relationships that could be construed as a potential conflict of interest.

References

  1. Bao, Y.; Guo, X.; Wei, L.; Siqin, Z.; Chao, H. Research progress on cathode materials for lithium-ion batteries. J. Solid State Electrochem. 2025, 29, 3595–3619. [Google Scholar] [CrossRef] [Scilit]
  2. Balaouras, V.; Kelaidis, N.; Daskalopulu, A.; Kuganathan, N.; Chroneos, A. Ionic diffusion in post-lithium batteries. J. Solid State Electrochem. 2025, 29, 3553–3565. [Google Scholar] [CrossRef] [Scilit]
  3. Wang, Z.; Jiang, W.; Zhao, Y.; Hu, L.; Wang, Y.; Ma, Z. Chemo-mechanical coupling phase-field modeling of lithium dendrite growth within solid electrolyte. J. Solid State Electrochem. 2023, 27, 245–253. [Google Scholar]
  4. Xia, G.; Jiang, W.; Li, H.; Zheng, Z. In-situ detection of electrolyte defects in lithium-ion batteries using ultrasonic imaging and analysis of formation patterns. Energy Rep. 2024, 12, 4686–4695. [Google Scholar] [CrossRef] [Scilit]
  5. Belov, D.; Shieh, D.T. GBL-based electrolyte for Li-ion battery: Thermal and electrochemical performance. J. Solid State Electrochem. 2012, 16, 603–615. [Google Scholar]
  6. Lu, D.; Lin, S.; Hu, S.; Cui, W.; Fang, T.; Iqbal, A.; Zhang, Z.; Peng, W. Thermal behavior and failure mechanism of large format lithium-ion battery. J. Solid State Electrochem. 2021, 25, 315–325. [Google Scholar]
  7. Zou, B.; Zhang, L.; Xue, X.; Tan, R.; Jiang, P.; Ma, B.; Song, Z.; Hua, W. A review on the fault and defect diagnosis of lithium-ion battery for electric vehicles. Energies 2023, 16, 5507. [Google Scholar] [CrossRef] [Scilit]
  8. Pan, T.; Yu, Z.; Ma, S.; Xu, D.; Ye, Y.; Li, J. Detection of internal short circuit in lithium-ion batteries based on electrothermal coupling model. J. Energy Storage 2025, 106, 114685. [Google Scholar] [CrossRef] [Scilit]
  9. Maleki, H.; Howard, J.N. Internal short circuit in Li-ion cells. J. Power Sources 2009, 191, 568–574. [Google Scholar] [CrossRef] [Scilit]
  10. Wang, H.; Simunovic, S.; Maleki, H.; Howard, J.N.; Hallmark, J.A. Internal configuration of prismatic lithium-ion cells at the onset of mechanically induced short circuit. J. Power Sources 2016, 306, 424–430. [Google Scholar] [CrossRef] [Scilit]
  11. Wu, C.; Wu, L.; Qiu, C.; Yang, J.; Yuan, X.; Cai, Y.; Shi, H. Experimental and numerical studies on lithium-ion battery heat generation behaviors. Energy Rep. 2023, 9, 5064–5074. [Google Scholar] [CrossRef] [Scilit]
  12. Feng, X.; Ouyang, M.; Liu, X.; Lu, L.; Xia, Y.; He, X. Thermal runaway mechanism of lithium ion battery for electric vehicles: A review. Energy Storage Mater. 2018, 10, 246–267. [Google Scholar] [CrossRef] [Scilit]
  13. Ge, S.; Leng, Y.; Liu, T.; Longchamps, R.S.; Yang, X.-G.; Gao, Y.; Wang, D.; Wang, D.; Wang, C.-Y. A new approach to both high safety and high performance of lithium-ion batteries. Sci. Adv. 2020, 6, eaay7633. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  14. Han, X.; Lu, L.; Zheng, Y.; Feng, X.; Li, Z.; Li, J.; Ouyang, M. A review on the key issues of the lithium ion battery degradation among the whole life cycle. eTransportation 2019, 1, 100005. [Google Scholar] [CrossRef] [Scilit]
  15. Yu, Q.; Wang, C.; Li, J.; Xiong, R.; Pecht, M. Challenges and outlook for lithium-ion battery fault diagnosis methods from the laboratory to real world applications. eTransportation 2023, 17, 100254. [Google Scholar] [CrossRef] [Scilit]
  16. Liu, L.; Zhang, M.; Lu, L.; Ouyang, M.; Feng, X.; Zheng, Y.; Han, X.; Pan, Y. Research progress on the mechanism and detection of internal short circuits in lithium-ion batteries. Energy Storage Sci. Technol. 2018, 7, 1003–1015. [Google Scholar]
  17. Feng, X.N. Thermal Runaway Initiation and Propagation of Lithium-Ion Traction Battery for Electric Vehicle: Test, Modeling and Prevention. Ph.D. Thesis, Tsinghua University, Beijing, China, 2016. [Google Scholar]
  18. Kong, X.; Zheng, Y.; Ouyang, M.; Lu, L.; Li, J.; Zhang, Z. Fault diagnosis and quantitative analysis of micro-short circuits for lithium-ion batteries in battery packs. J. Power Sources 2018, 395, 358–368. [Google Scholar] [CrossRef] [Scilit]
  19. Feng, X.; Pan, Y.; He, X.; Wang, L.; Ouyang, M. Detecting the internal short circuit in large-format lithium-ion battery using model-based fault-diagnosis algorithm. J. Energy Storage 2018, 18, 26–39. [Google Scholar] [CrossRef] [Scilit]
  20. Duan, B.; Zeyuan, L.; Gu, P.; Zhongkai, Z.; Zhang, C. Evaluation of battery inconsistency based on information entropy. J. Energy Storage 2018, 16, 160–166. [Google Scholar] [CrossRef] [Scilit]
  21. Zheng, Y.; Luo, Q.; Cui, Y.; Dai, H.; Han, X.; Feng, X. Fault identification and quantitative diagnosis method for series-connected lithium-ion battery packs based on capacity estimation. IEEE Trans. Ind. Electron. 2021, 69, 3059–3067. [Google Scholar] [CrossRef] [Scilit]
  22. Lei, D.; Zhang, M.; Guo, Q.; Gao, Y.; Bai, Z.; Yang, Q.; Fu, K.; Lyu, C. Model-free detection and quantitative assessment of micro short circuits in lithium-ion battery packs based on incremental capacity and unsupervised clustering. Int. J. Electrochem. Sci. 2024, 19, 100794. [Google Scholar] [CrossRef] [Scilit]
  23. Guo, Y.; Wang, Y.; Zhong, J.; Du, J.; Tian, J.; Li, Y.; Jiang, F. Fault diagnosis method for lithium-ion battery micro-internal short circuit based on incremental capacity curve. Energy Storage Sci. Technol. 2023, 12, 2536–2546. [Google Scholar] [CrossRef]
  24. Zhang, J.; Gao, X.; Zhang, L. A micro-short circuit diagnosis method for battery packs based on IC curve and charging capacity difference. Automot. Eng. 2023, 45, 191–198+230. [Google Scholar] [CrossRef]
  25. Zhang, K.; Jiang, L.; Deng, Z.; Xie, Y.; Couture, J.; Lin, X.; Zhou, J.; Hu, X. An early soft internal short-circuit fault diagnosis method for lithium-ion battery packs in electric vehicles. IEEE/ASME Trans. Mechatron. 2023, 28, 644–655. [Google Scholar] [CrossRef] [Scilit]
  26. Sun, J.; Chen, S.; Xing, S.; Guo, Y.; Wang, S.; Wang, R.; Wu, Y.; Wu, X. A battery internal short circuit fault diagnosis method based on incremental capacity curves. J. Power Sources 2024, 602, 234381. [Google Scholar] [CrossRef] [Scilit]
  27. Zhao, X.; Wang, J.; Zhao, M.; Pan, B.; Wang, R.; Wang, L.; Yan, X. Micro-short circuit fault diagnosis of the parallel battery module based on increment capacity curve. J. Energy Storage 2024, 86, 111201. [Google Scholar] [CrossRef] [Scilit]
  28. Liao, L.; Hu, X.; Chen, H.; Wang, Z.; Wu, T.; Jiang, J. Quantitative diagnosis of micro-short circuit for lithium-ion batteries considering aging based on incremental capacity curve. J. Energy Storage 2024, 79, 110240. [Google Scholar] [CrossRef] [Scilit]
  29. Qiao, D.; Wang, X.; Lai, X.; Zheng, Y.; Wei, X.; Dai, H. Online quantitative diagnosis of internal short circuit for lithium-ion batteries using incremental capacity method. Energy 2022, 243, 123082. [Google Scholar] [CrossRef] [Scilit]
  30. Zhang, H. SOH Estimation of Lithium-Ion Batteries Based on IC Curve Characteristic Parameters and DSP Implementation. Ph.D. Thesis, Beijing Jiaotong University, Beijing, China, 2018. [Google Scholar]
  31. Liang, Y.; Wu, W.; Chen, Z.; Pan, E. Quantitative Diagnosis of Connection Fault for Lithium-Ion Batteries Based on IC Curves and Correlation Analysis. In Mechanics, Electronics, Automation and Automatic Control; IOS Press: Amsterdam, The Netherlands, 2024; pp. 137–149. [Google Scholar]
  32. Ma, Z.; Jiang, J.; Wang, Z.; Shi, W.; Zheng, L.; Zhang, Y. Research on SOC estimation method of graphite anode LiFePO4 battery based on incremental capacity analysis. Automot. Eng. 2014, 36, 1439–1444. [Google Scholar] [CrossRef]
  33. Deng, Z.; Hu, X.; Lin, X.; Che, Y.; Xu, L.; Guo, W. Data-driven state of charge estimation for lithium-ion battery packs based on Gaussian process regression. Energy 2020, 205, 118000. [Google Scholar] [CrossRef] [Scilit]
  34. Li, Y.; Abdel-Monem, M.; Gopalakrishnan, R.; Berecibar, M.; Nanini-Maury, E.; Omar, N.; van den Bossche, P.; Van Mierlo, J. A quick on-line state of health estimation method for Li-ion battery with incremental capacity curves processed by Gaussian filter. J. Power Sources 2018, 373, 40–53. [Google Scholar] [CrossRef] [Scilit]
  35. Feng, X.; Weng, C.; Ouyang, M.; Sun, J. Online internal short circuit detection for a large format lithium ion battery. Appl. Energy 2016, 161, 168–180. [Google Scholar] [CrossRef] [Scilit]
  36. Xia, B.; Chen, Z.; Mi, C.; Robert, B. External short circuit fault diagnosis for lithium-ion batteries. In Proceedings of the 2014 IEEE Transportation Electrification Conference and Expo (ITEC), Dearborn, MI, USA, 15–18 June 2014; IEEE: Piscataway, NJ, USA, 2014; pp. 1–7. [Google Scholar]
  37. Liu, L.; Feng, X.; Zhang, M.; Lu, L.; Han, X.; He, X.; Ouyang, M. Comparative study on substitute triggering approaches for internal short circuit in lithium-ion batteries. Appl. Energy 2020, 259, 114143. [Google Scholar] [CrossRef] [Scilit]
  38. Orendorff, C.J.; Roth, E.P.; Nagasubramanian, G. Experimental triggers for internal short circuits in lithium-ion cells. J. Power Sources 2011, 196, 6554–6558. [Google Scholar] [CrossRef] [Scilit]
  39. Chen, Z.; Deng, Y.; Li, H.; Liu, W. An efficient regrouping method of retired lithium-ion iron phosphate batteries based on incremental capacity curve feature extraction for echelon utilization. J. Energy Storage 2022, 56, 105917. [Google Scholar] [CrossRef] [Scilit]
  40. Ouyang, M.; Zhang, M.; Feng, X.; Lu, L.; Li, J.; He, X.; Zheng, Y. Internal short circuit detection for battery pack using equivalent parameter and consistency method. J. Power Sources 2015, 294, 272–283. [Google Scholar] [CrossRef] [Scilit]
Disclaimer/Publisher’s Note: The statements, opinions and data contained in all publications are solely those of the individual author(s) and contributor(s) and not of MDPI and/or the editor(s). MDPI and/or the editor(s) disclaim responsibility for any injury to people or property resulting from any ideas, methods, instructions or products referred to in the content.

Article Metrics

Citations

Article Access Statistics

Multiple requests from the same IP address are counted as one view.