Abstract
Graphite remains the most widely used anode material for lithium-ion batteries because of its excellent reversibility, low electrochemical potential, high conductivity, and stability. Nevertheless, the relatively low mobility of lithium ions in graphite hinders the performance of cells operated at high rates. A feasible way to enhance electrochemical kinetics and achieve higher rate capabilities is to decrease graphite particle size, as it reduces diffusion path length, increases the number of intercalation sites, and lowers concentration polarization. These measures can help not only improve rate capability but also suppress lithium plating under fast-charge regimes. On the other hand, decreasing particle size increases specific surface area, the number of edges and defect sites on the surface, electrolyte reactivity, SEI formation, irreversible lithium losses, and interfacial resistance, thereby lowering initial Coulombic efficiency and cell cycling stability. This review examines the correlation among graphite particle size, morphology, crystallographic texture, specific surface area, lithium-ion transport, intercalation kinetics, fast-charging capability, and aging. Special attention is paid to the compromise between enhanced Li+ transport kinetics and additional side reactions caused by increased specific surface area. Particle shape and size distribution engineering, carbon coatings and surface treatments, and electrolytes/SEIs optimization are also considered.