Cross-Sectional Characterization of Stain Retention and Glaze Alteration in 3D-Printed and Milled Hybrid Dental Materials

,
,
and
1
Department of Prosthodontics, Geriatric Dentistry and Craniomandibular Disorders, Charité—Universitätsmedizin Berlin, Corporate Member of Freie Universität Berlin and Humboldt-Universität zu Berlin, Aßmannshauser Str. 4–6, 14197 Berlin, Germany
2
Department of Prosthodontics, Medical Faculty and University Hospital Düsseldorf, Heinrich Heine University Düsseldorf, Moorenstraße 5, 40225 Düsseldorf, Germany
*
Author to whom correspondence should be addressed.
J. Funct. Biomater.2026, 17(12), 595;https://doi.org/10.3390/jfb17120595 
(registering DOI)
This article belongs to the Special Issue Biomaterials and 3D Printing in Dentistry: Research and Clinical Innovations

Abstract

Milled CAD/CAM and 3D-printed hybrid restorative materials are exposed to dietary staining agents, while polishing and glazing are used to optimize their surface and optical properties. This study characterized the cross-sectional location of visible staining and glaze alteration after prolonged staining exposure. Three milled and two 3D-printed hybrid materials were polished or glazed with OPTIGLAZE Color Clear HV and immersed in cola, coffee, curry, or red wine for 30 days at 37 °C. One specimen per material, surface treatment, and staining medium was sectioned (40 specimens in total). Stained glaze-layer thickness and glaze alteration were compared descriptively with previously reported color change and surface roughness. Polished specimens showed no distinct subsurface discolored zone. In glazed specimens, visible staining was located predominantly within the glaze layer and was measurable in 16 of 20 specimens (median 30.0 µm; range 14.4–63.8 µm). Curry exposure suggested near-surface yellowing in some materials, particularly beneath detached glaze. Structural defects were common, and partial detachment was observed in single specimens after curry or red wine exposure. Water-stored glazed controls showed no detachment and, where delineable, similar glaze thickness. In this descriptive analysis, cross-sectional evaluation revealed glaze alterations that were not consistently represented by surface measurements.