Abstract
Ballast void formation is a known issue in railway turnouts, yet the underlying mechanisms remain insufficiently understood. This study investigates the mechanical response of a long turnout sleeper lying on a ballast bed under loading using both full-scale laboratory experiments and Discrete Element Method (DEM) simulations to study the correlation between applied load, sleeper deformation, sleeper-ballast interface pressure and residual settlement. The DEM simulations employed a deformable sleeper model using the PFacet approach in the Yade framework and an elasto-plastic contact law accounting for edge breakage (Conical Damage Model) to reproduce ballast-ballast and sleeper-ballast contact behaviour. Results show that the DEM model can replicate key experimental trends, including asymmetric sleeper bending, uplift, and the evolution of ballast pressure distribution in the short term. Under extended cyclic loading, the simulation reproduces the progressive formation of stable bedding conditions and the emergence of ballast voids, aligning with experimental observations. A simplified approach to represent USPs via reduced contact stiffness yielded realistic deformation and pressure behaviour, although residual settlement differed. The results demonstrate that DEM can reproduce and explain sleeper-ballast interaction mechanisms, providing mechanistic insight into how uneven pressure distribution and ballast rearrangement contribute to void formation in turnouts.
1. Introduction
In ballasted railway tracks, the mechanical interaction between sleeper and ballast is critical for maintaining structural stability, effective load distribution, and long-term track geometry. One well-known phenomenon that compromises track integrity is the occurrence of ballast voids.
Ballast voids refer to gaps between the sleepers and the ballast beneath the sleeper and change how load is transferred from the rail through the sleeper into the ballast and the ground. When a train passes, these gaps temporarily close, affecting the pressure onto the ballast stones and sleeper settlement as a result of it. These effects are particularly observed in railway turnouts, where sleepers are not losing contact entirely due to their extended length but exhibit localised detachment. For example, the ballast beneath the turnout’s crossing nose is frequently associated with increased degradation and a tendency to form voids near the sleeper’s centre [1,2,3,4,5,6].
The mechanical response of the track, especially in such regions, strongly depends on component-specific parameters, including sleeper stiffness, sleeper mass, and, if used, the contact behaviour of under-sleeper pads (USPs) with the ballast [1,7,8,9,10,11,12,13,14]. While numerous studies address the detection and effects of ballast voids, and more specifically full hanging sleeper conditions, the physical mechanisms underlying their initial formation and countermeasures remain insufficiently understood [15,16,17,18,19,20,21,22,23,24,25,26].
The prevailing hypothesis suggests that applied loads induce elastic deflection and bending of the long sleeper, leading to a non-uniform pressure distribution along the sleeper-ballast interface. This pressure distribution is considered to directly correlate with localised settlement and, ultimately, the formation of ballast voids [7,10,20].
Experimental investigations at full scale are indispensable for capturing real-world sleeper behaviour under controlled conditions. However, laboratory tests are resource-intensive, time-consuming to set up, and offer limited flexibility for studying parametric variations. Additionally, it is not feasible to investigate particle movement and force transmission within the ballast bed. In this context, Discrete Element Method (DEM) simulations offer a powerful complement to physical testing by enabling detailed, particle-level analysis of sleeper-ballast interaction. Still, the most valuable insights are obtained by combining both methods, as the DEM necessitates result verification for credibility, and the laboratory experiments are not well-suited for parametric studies since the initial ballast bed will always be different for each test, and statistical evaluation is especially challenging [8,11,13,14].
Various procedures exist for modelling railway ballast in DEM frameworks [8,22,23,24,25,26,27]. Each of these procedures has its advantages and disadvantages, depending on whether ballast stone shape degradation, settlement behaviour, or energy dissipation (e.g., damping, noise generation) are the main focus of the studies [8,27]. A particularly promising method involves representing ballast particles as clumps of three spheres combined with an elasto-plastic contact law, namely the Conical Damage Model (CDM). When properly parameterised, this model has demonstrated good accuracy in capturing ballast compaction, shearing behaviour and settlement under cyclic loading while maintaining manageable model complexity and particle count [28,29,30,31,32,33]. However, the original clump dimensions were tailored for relatively small-scale laboratory tests [28]. For realistic ballast representation, the particle size should ideally match the target sieve size distribution.
The same principle applies to sleeper modelling. In many studies, sleepers are implemented either as rigid geometries or as bonded particle assemblies [8,16,21,22,23,24,25,26,34]. While these approaches can be sufficient for certain studies, the inability to elastically deform or the induced artificial surface roughness due to the bonded particles can impair result accuracy. This is especially the case when the focus lies on ballast pressure and settlement correlation. Coupling the DEM with a Finite Element Method or Multi-flexible Body Dynamics solver can solve these issues but adds additional complexity to the contact computations and increases simulation effort significantly [8,13,21,23,26]. Alternatively, the use of special particle shapes in the Yade DEM framework—specifically Nodes, GridConnections, and PFacets—enables the construction of sleeper shell models. When appropriately adjusted in terms of mass and bending stiffness, this approach offers realistic deformation and contact behaviour without requiring external coupling. Moreover, staying within a single simulation ecosystem facilitates faster adaptation of contact models if needed [8,35].
The modelling of under-sleeper pads (USPs) presents particular challenges, as the polymeric materials commonly used exhibit complex mechanical behaviour, including non-linear elasticity, rate-dependent damping, and time-dependent phenomena such as creep and stress relaxation [36]. In numerical simulations, however, USPs are typically represented using the same contact laws as applied to ballast-ballast interactions, although with reduced stiffness parameters to approximate their softer response. This simplified approach has yielded satisfactory results in ballast box test and straight track simulations [11,13,28,37]. Whether this modelling strategy remains valid for more complex configurations—such as turnouts with asymmetric loading and non-uniform support conditions—remains an open question and subject of ongoing investigations.
2. Materials and Methods
2.1. Laboratory Experiments
In this work, a ballast box test setup in a laboratory is used to assess the behaviour of a long turnout sleeper under cyclic loading. A thorough description of the laboratory work is given in Grohs et al. [7], but is summarised in the following for the necessary context. To fully incorporate the long turnout sleeper and the affected ballast, a large steel box was designed with dimensions of 5 × 1.5 × 0.5 m. The box’s side walls were coated with a damping material (Ecomer ER 607) and the box’s bottom with an under sleeper pad material (Sylomer SLB 3007G) both from Getzner Werkstoffe GmbH (Bürs, Austria) to avoid resonance effects from the box walls when applying the load. The box was filled with compacted siliceous limestone up to a height of 35 cm.
Subsequently, the turnout sleeper, measuring 4.206 m in length, was positioned on the ballast bed. The concrete sleeper has a uniform trapezoidal cross-section, with a bottom width of 0.3 m and a height of 0.22 m and was equipped with four baseplates and four rail pieces. The full experimental setup is shown in Figure 1. For the initial testing sequence, the sleeper was fitted with an under-sleeper pad (USP) of type Sylomer SLB 3007G by Getzner Werkstoffe GmbH (Bürs, Austria), a product exhibiting elasto-plastic properties to mitigate ballast degradation. Between the sleeper and the USP, six pressure mapping sensor pads (Getzner Sensor Sleeper technology [38]) were installed along the sleeper’s length, allowing to measure the sleeper-ballast contact pressure. The positions of the sensor pads (enumerated from A to F) on the bottom of the sleeper are shown in Figure 2. After the full testing sequence, the USP was removed from the sleeper and the ballast bed completely renewed before the same experiments were conducted again on the “naked” sleeper, exposing the sensor pads directly to the ballast.
Figure 1.
The full large-scale ballast box test setup [7].
Figure 2.
The position of the pressure mapping sensor pads used in the laboratory experiment [7].
To monitor the movement and settlement of the sleeper over time, a total of 13 laser sensors were installed. As shown in Figure 3, L1 to L12 were used to measure vertical movement and are used in the analysis of this work. Results from L13 (lateral movement) and the inductive displacement sensors (W1–W4) will not be discussed.
Figure 3.
The position of the used displacement sensors in the laboratory experiment [7].
The vertical loads were applied on the left part of the sleeper, representing the turnouts through route. A steel beam (300 kg) was placed on the rail pieces (30 kg each) to distribute the load. The application of the load was executed using a hydraulic cylinder, which exerted a concentric force on the steel beam via a ball joint.
To reduce the effort required for bed preparation in the laboratory experiments, a test sequence was mapped out that included a combination of quasi-static and short-term (up to 25,000 cycles) cyclic loading tests. To address a range of potential outcomes, the force magnitude was increased on multiple occasions throughout the test sequence, ranging from a total load of 80 kN up to 160 kN. Afterwards, a long-term study was started with more than 4 million cycles [7].
In this work, the results of the laboratory experiments are used to verify the outcome of Discrete Element Method simulations, which are computationally demanding. Consequently, solely the initial quasi-static loading experiments and the subsequent cyclic loading test up to 15 (and later 400) cycles will be examined in detail, as they are considered the most suitable for comparison with the simulations, given the minimal pre-compaction of the ballast bed due to the testing sequence. The long-term experiment and the complete ballast box setup including the measurement equipment is more thoroughly explained in Grohs et al. [7] and are not within the scope of this work.
2.2. Discrete Element Method Simulations
The Discrete Element Method (DEM) is a numerical technique capable of describing the mechanical behaviour of granular assemblies by modelling the interaction of individual particles through explicit contact-by-contact and particle-by-particle computations [39]. This method has been extensively applied to railway ballast modelling, where ballast particles are typically represented as clumps of spheres or complex geometries to capture their irregular shapes and simulate their mechanical response [40]. DEM simulations of railway ballast enable detailed investigation of particle-scale phenomena such as contact force distributions, particle breakage, and settlement behaviour, providing valuable insights into ballast degradation mechanisms and track performance that are difficult to obtain through experimental methods alone [11,41].
The DEM simulations in this work are set up in Yade [35], an open-source framework for discrete numerical models, following up on the approach of Kumar et al. [28] and the author’s previous work [8]. This approach is designed to combine two established strategies: one for ballast modelling and the other for a bending-elastic sleeper model.
In the simulation setup, the ballast box is modelled using wall elements to form an open steel box with the inner dimensions of 4.96 × 1.46 × 0.6 m which accounts for the reduced volume due to damping material installed in the box of the laboratory experiment.
The bulk material behaviour in DEM simulations depends on the chosen particle shape and the underlying contact law describing particle-particle interactions, typically defined as a function of particle overlap . The ballast modelling approach employed by Kumar et al. [28] and Suhr et al. [29,30] utilizes a particle representation, in which each particle is modelled as a clump of three spheres of varying sizes, as illustrated in Figure 4a. The adopted inter-particle contact law, namely the Conical Damage Model (CDM), is based on the Hertzian contact theory and incorporates the material properties Young’s modulus E, Poisson’s ratio , and friction coefficient to compute contact forces. When the normal stress exceeds a defined threshold , ideal plasticity is introduced to capture particle degradation and bulk compaction in larger assemblies. Upon reaching this threshold, the effective contact radius is increased, representing surface flattening. This results in reduced elastic overlap and consequently a limit on contact stress, representing edge breakage [29,30]. The geometric shape of the particles remains unchanged throughout the simulation. A schematic representation of the contact model is provided in Figure 4b. The simplified clump geometry preserves essential kinematic features of angular ballast, such as interlocking and restricted particle rotation, while avoiding artificial ordering effects in the assembly. Previous validation studies have demonstrated that, in combination with the CDM, this approach can reproduce both shear and compression responses with a single parameter set, supporting its suitability for macroscopic ballast behaviour simulation [28,29,30].
Figure 4.
(a) DEM ballast particle [8] and (b) schematic representation of the CDM for a sphere-sphere contact [29].
To further improve the ballast representation in the simulation, a size distribution was considered where clumps with major axes of 40 mm, 50 mm and 60 mm were used to replicate the sieve size distribution of the real ballast stones taken from ÖNORM EN 13450 category D [42,43]. The final dimensions of the ballast particles are stated in Table 1.
Table 1.
Major axis length of the clump particles present in the simulation, their respective radii of the spheres and the approximate mass fraction of the total ballast bed.
As this study employs the same ballast type (siliceous limestone, originally named Kieselkalk) as that used by Suhr et al. [29,30], for which extensive parametrisation was performed using compression and direct shear tests, it is assumed that variations in particle size do not significantly influence the overall particle behaviour and, consequently, the selected parameters. A comparable assumption was adopted by Kumar et al. [28], supporting the validity of this approach. The complete set of calibrated and validated ballast particle parameters adopted from these studies is provided in Table 2.
Table 2.
Material properties of the simulation’s components.
Studying long sleepers and the complex load transfer mechanisms present in turnouts requires the use of a suitable sleeper model that can provide realistic insights into the system. To avoid coupling the already time-consuming discrete element solver with another tool, the sleeper is best only modelled within the DEM framework. Hence, the PFacet modelling approach from previous work of the authors was used, as it provides proper bending behaviour for the sleeper while maintaining a smooth surface for the contact with ballast stones without introducing an artificial roughness [8].
This approach uses so-called nodes, cylindrical connections (termed GridConnection) and particle facets (termed PFacets) in the Yade framework. The nodes are core element of this approach and are geometrically represented as spheres. The nodes define the general grid (or mesh) of the object that is to be modelled. They are given cohesive properties (cohFrictMat in Yade) which allows for the nodes to maintain an interaction even while not in contact. When the relative position between two nodes changes, a linear reversing force or moment pulls the nodes back into their initial relative position. Additionally, the mass of the whole sleeper structure is lumped only into the nodes [8].
GridConnections are geometrically defined as a sphere that is moved along a line, resulting in a cylinder with a half sphere at the top and bottom. PFacets are a superstructure of three nodes connected with three connections, forming a triangle that is then covered with two triangular facets at the top and bottom. These elements can share nodes with other elements, which enables the design of complex shell structures like a sleeper.
To generate the sleeper model using the PFacet approach, a mesh was created with vertices along the longitudinal edges of the sleeper. This ensures structural integrity, as the model only represents a shell structure. A sketch of the sleeper’s cross-section is shown in Figure 5 where the orange spheres represent the nodes and the orange lines the surfaces of the PFacets. To ensure a similar outer surface of the PFacet model in regard to the real sleeper, the nodes are placed within the cross-sectional (black in Figure 5) and longitudinal boundaries of the real sleeper’s cross-section. The nodes were given a radius of 5 mm which entails the same radius for the GridConnections and edge radius of PFacets and hence the sleeper model. The final sleeper model is shown in Figure 6, being placed on the ballast bed.
Figure 5.
The cross-section of the PFacet sleeper model in orange and the replicated cross-section of the real sleeper in black.
Figure 6.
The final simulation setup showing the ballast bed, the sleeper model and indicators where the load is applied.
Since the mass is only lumped into the nodes and a shell model is used, the density of the node’s material needs to be adjusted appropriately to resemble the real sleeper and achieve a mass of 711 kg as for the laboratory sleeper. Unlike the nodes, the GridConnections and the PFacets cover contacts with external particles using a frictMat material in Yade seperating structural and contact behaviour.
A simulation for calibrating the sleeper’s bending properties was set up using a longer PFacet sleeper model as a cantilever beam that was loaded at the free end. The cross-section and node radius were left unchanged. By comparing the final deflection of the simulation model with an analytically computed deflection, the Young’s modulus of the cohFrictMat of the nodes (responsible for the internal mechanics of the sleeper) can be adjusted to resemble realistic bending behaviour. The elongation of the sleeper model for calibration is necessary because the assumption was made that the model behaves like an Euler-Bernoulli beam, with whose analytical computation the simulation result was compared to. Hence, this comparison is valid if the beam’s length is significantly higher than its cross-sectional dimensions and the resulting deflection is significantly smaller than the beam’s length. After calibration, it was found that the initial Young’s modulus of the sleeper nodes needs to be set to 3891 GPa to ensure correct bending behaviour. The complete calibration process for proper sleeper bending behaviour is thoroughly explained in the previous work of the author [8]. The final used parameters that ensure realistic sleeper behaviour are stated in Table 2.
Since the initial value for the sleeper’s Young’s modulus was taken from the literature for regular sleepers of a straight track that differ in shape, the turnout sleeper from the laboratory experiments was tested by bearing it on two points close to the sleeper ends and loading it with a hydraulic cylinder in the centre. Using the results of the strain-deflection curve in the linear elastic domain, it was found that the initially assumed value for the sleeper’s Young’s modulus was indeed a valid assumption.
The approach for modelling the sleeper with PFacets in Yade currently only natively supports the use of a cohesive friction material (cohFrictMat) for internal mechanics (between nodes) and a friction material without cohesion (frictMat) for contacts of the PFacet structure with other particles. In Yade, a contact computation is always backed by so-called functors. A contact law functor uses a given geometrical functor and a physics functor to compute respective contact forces acting on the interacting particles. The initial CDM physics functor, covering the interaction between a frictMat (the PFacet’s material) and a frictMatCDM (the material for the ballast), was adapted to check which particle is an actual sphere (ballast particle) having a radius and which one is a virtual sphere (PFacet) that should be treated as a flat surface. This part is crucial for computing the correct equivalent radius for the following contact force computation. Since no contact law functor is included in Yade’s source code that uses the PFacet’s geometry functor (ScGridCoGeom) with the newly adapted CDM physics functor (MindlinPhysCDM), a new law functor was added as well. The two mentioned adaptations enable the use of an established ballast modelling approach in combination with a bending-elastic sleeper model to analyse the sleeper-ballast interaction precisely by using the CDM’s elasto-plastic contact behaviour.
2.2.1. Simulation Phases
To set up the ballast bed and the sleeper model to then apply a load, several steps are necessary. In the first phase of the simulation, the steel box is created, and a volume is defined. This volume is filled up randomly with the given clump particles of various sizes. The clumps fall into the box and spread accordingly, as the particle’s Young’s modulus and friction coefficient are significantly reduced in this phase. The time step was set to s and is based on the PWaveTimeStep() function provided by Yade. To obtain a compact ballast bed, the bottom wall of the box vibrates vertically twice with a small amplitude. In the second phase, the initially reduced friction coefficient and Young’s modulus of the particles get adjusted to their calibrated values and the time step is reduced by of its initial value to s to avoid unrealistic high forces in the updating process. Afterwards, a plate is inserted at the top of the ballast, moving downwards to compress the bed. When it reaches a stress of 333 kPa, the motion is reversed. This compression process is performed three times before particles above the wanted bed height of 35 cm are removed from the simulation.
A common problem in DEM simulations are differences in the bulk material’s density when compared to a real material sample due to geometrical differences in the particle geometries. After the ballast bed preparation phase, the density was adapted to align the bed’s volume with the supposed mass from the laboratory.
In the third phase, the previously calibrated sleeper model is inserted just above the ballast bed and then dropped under gravity. Given the insertion of new simulation elements, the time step was reevaluated and set to s for all simulations, which was the lowest common denominator for all simulations conducted in this study. After the sleeper model was inserted, a load is applied onto the sleeper on nodes on the top face where the baseplates in the laboratory experiments are located. This way, the load is distributed to six nodes per rail indicated by red dots in Figure 6. The load at both location ( and ) increases linearly until it reaches 3.53 kN which resembles the weight of components (baseplates, rail pieces, beam) that are not directly modelled in the simulation. This load is applied consistently throughout the following simulations. The full simulation setup before active loading is applied is presented in Figure 6.
The fourth phase is the loading phase, which is split up into two parts. The static and the following cycling loading phase. The maximum static load of 100 kN was identical to the laboratory experiments but was applied linearly in 0.5 s, held for 1 s and withdrawn linearly in 0.5 s to cut down on simulation time. The same sinusoidal loading was then applied on the sleeper model in the simulation as in the laboratory experiments by using a frequency of 3 Hz, a maximum total force of 80 kN and a minimum total force of 5 kN on the sleeper. The loading scheme is shown in Figure 7 and presents the total applied load onto the sleeper also considering the forces accounting for the weight of components not directly modelled in the simulation. In total, 15 loading cycles were conducted. This number of cycles is considered sufficient to assess the principal effects of loading conditions, as studies on non-cohesive materials have shown that deformation behaviour changes significantly and immediately after a load change, making a small number of cycles adequate to evaluate such influences [44].
Figure 7.
The total applied load onto the sleeper model in the simulation during the fourth phase. The dashed green line representing continous cyclic loading.
Five different but similar (due to random particle generation) ballast bed configurations were prepared and simulated this way to ensure the simulation outcome is not a singularity. The particle clump count ranged between 81,102 and 81,497 for the used particle beds.
2.2.2. Long-Term Cyclic Loading
After studying the effects of cyclic loading on multiple ballast beds, the simulation setup 4, as reasoned in the results section, was then used to start a long-term simulation covering 400 load cycles.
2.2.3. Reduction of Sleeper Contact Stiffness
In the laboratory experiments, a USP of type Sylomer SLB 3007G by Getzner Werkstoffe GmbH (Bürs, Austria) was used, which is characterised by its elasto-plastic properties. Considering the elasto-plastic approach of the Conical Damage Model (the contact model present in the DEM simulations) it was considered sufficient as a first step to decrease the sleeper’s contact stiffness to replicate the effects of a USP on the interaction between the sleeper and the ballast. Hence, no additional layer was brought into the simulation.
The Young’s modulus of the sleeper model’s material that covers the external contacts was gradually reduced by one order of magnitude. The plastic threshold value was left unchanged. The final properties for the sleepers with softer contact parameters are stated in Table 2. As for the long-term simulation, the setup of simulation 4 was used here to serve as a baseline. Reusing the identical ballast bed for different sleepers allows for straightforward comparisons and parametric studies that are not possible in the laboratory.
Additionally, the numerical damping coefficient was increased from 0.2 to 0.5. This was considered necessary to avoid unrealistic dynamics in the simulation. To verify that the change in numerical damping is feasible, another simulation with the sleeper without a reduction of the Young’s modulus was conducted. The change in numerical damping led to identical results and was therefore considered reasonable.
2.2.4. Model Validation
In this work, the laboratory experiments serve as validation for the simulation model. The focus of this study lies on sleeper bending, settlement and sleeper-ballast pressure distribution in lateral direction and the potential formation of ballast voids below the sleeper. Therefore, change in vertical sleeper position combined with the corresponding pressure distribution along the sleeper’s length is used to compare and verify simulation behaviour. The discrete nature of railway ballast makes it challenging to directly compare results across multiple setups, whether they are laboratory experiments or simulation configurations. Thus, model verification is achieved by being able to recreate similar trends in behaviour rather than exact values, as long as all results lie within reasonable ranges. Given the experimental setup using pressure mapping sensors, void formation is inferred indirectly through loss of contact pressure and uplift rather than explicitly measured geometric gaps.
3. Results
The primary focus of the study was to evaluate how load is transferred from the rails through the sleeper into the ballast. The loading and bedding conditions as well as the use of elastic layers impact sleeper bending, which impacts the pressure distribution at the sleeper-ballast interface. It is thought that the sleeper-ballast pressure distribution along the sleeper’s length directly correlates with local sleeper settlement and ballast void development. Therefore, a strong focus is set on evaluating the sleeper’s vertical position and the pressure onto the ballast over time. Given the discrete nature of ballast stones and particles, it is difficult to compare settlement results across different ballast bed configurations. Since only one testing sequence was conducted for each sleeper (with and without under-sleeper pad), it is expected that the results would scatter if multiple similar experiments had been executed. Nevertheless, it is possible to analyse the behaviour of the sleeper on the ballast bed over time and evaluate the results qualitatively. The sleeper’s vertical position in the laboratory test was measured with sensors mounted above the sleeper, which were installed after placing the sleeper on the ballast bed. Hence, possible initial settlement due to the weight of the setup while preparing the experiment is not captured. In the simulation, the absolute vertical position of each node is utilised in the analysis to provide the most unbiased evaluation possible. Consequently, the results of the laboratory experiment and the simulation are presented in separate plots.
3.1. Quasi-Static Loading
The very first experiments conducted in the laboratory were meant to test the setup and measurement equipment, while also getting a first impression on the magnitude of sleeper movement and settlement. For that reason, the load on the sleeper was slowly increased, kept constant for a short period and eventually slowly reduced again. Due to the slow change in load, this experiment will be referenced as a quasi-static loading experiment.
3.1.1. Sleeper Position and Movement—Quasi-Static Loading
To assess and compare the behaviour of a turnout sleeper subject to a quasi-static load, the sleeper’s position is captured before, during and after load application by using the measured deflection (laboratory) and the vertical position of the sleeper’s nodes (simulation) respectively along the sleeper’s length. In Figure 8, the change of the sleeper’s position is depicted for the laboratory experiment as well as the five conducted DEM simulations with different random particle configurations. In all subplots, the utilisation of light grey signifies the initial position, dark grey denotes the position during quasi-static loading with 100 kN total load, and black indicates the position after load application. The dotted red lines signal the position of the rails where the load was applied.
Figure 8.
The sleeper’s position before, during and after quasi-static loading (100 kN) for the laboratory experiment and five DEM simulations without USP.
A comparison of the sleeper’s position prior to the application of load reveals a clear difference. Findings from the laboratory experiment suggest that the sleeper’s position is nearly level. This observation is attributed to the initialisation of laser sensors after the sleeper was placed on the ballast bed.
In the simulation, the absolute vertical position is used and exhibits two types of starting positions. In simulations 1 and 3, the sleeper has a slight tilt to the right side before the load was applied, while in simulation 2, 4 and 5, the sleeper exhibits a tilt to the left side. This highlights the discrete nature of railway ballast as although the ballast bed was prepared similarly in all simulations, the initial conditions for each sleeper are entirely different.
When load is applied, the experimental subject exhibits a pronounced curvature over its entire length showing deflection of −4.36 mm on the left end and −4.24 mm at the 5th measurement node from the left at box length 2.13 m. In contrast, the simulations demonstrated a more consistent behaviour, showing a W-shaped deflection profile in all cases. In the simulations, the deflection ranged from −1.32 to −2.35 mm on the left side and from −1.01 to −1.24 mm in the centre (15th node from the left at around 2.11 m box length).
Under load, the sleepers tilt to the left side where the load is applied, and an uplift is observed at the right end of the sleepers with a clear tipping point. The laboratory sleeper depicts an uplift of 0.65 mm. In the simulations, the uplift ranged from 0.45 to 0.88 mm. Once the quasi-static load is removed, the residual sleeper position becomes apparent resulting from local ballast settlement. In all cases, the sleeper’s bending has decreased significantly, showing a relatively straight line. The sleeper’s vertical position is higher than under load, which highlights the system’s elastic properties. The sleeper in the laboratory experiment depicted higher settlement than the simulations, showing −3.99 mm on the left sleeper end and −2.62 mm of settlement in the centre. In contrast to the simulations, in the laboratory experiment the sleeper also depicted settlement on the right end of −0.22 mm. All simulations have shown a rise of the right end after the load was removed again, ranging from 0.23 to 0.63 mm. Settlement on the left half of the sleeper, however, were smaller for the simulations, ranging from −1.11 to −1.99 mm on the left end and −0.78 to −1.04 mm in the centre.
3.1.2. Pressure Distribution—Quasi-Static Loading
To further clarify the distinction in deflection and sleeper bending between the laboratory box test and DEM simulations, it is essential to examine the pressure at the sleeper-ballast interface. This provides insights into the initial bedding of the sleeper and how that bedding is influenced by the applied load.
Figure 9 displays the pressure distribution summarised for each sensor pad (labeled as in Figure 2) along the length of the box. The areas in the simulations are referenced using the same letters (A to F, from left to right), but without indication in the figures for easier readability. Light grey represents the initial pressure distribution, dark grey represents the distribution during quasi-static loading with 100 kN total load, and black represents the pressure after load application. The dotted red lines signal the position of the rails where the load was applied.
Figure 9.
Pressure distribution along the sleepers length summarised for each sensor pad before, during and after static loading (100 kN) for the laboratory experiment and five simulations without USP. The areas in the simulations are referenced using the same letters (A to F, from left to right).
A clear picture is painted for the laboratory experiment: Two sensor pads (or areas), namely sensor pad A and E, carry the sleeper almost entirely. The majority of the load is carried by sensor pad A before, during, and after load application, which is consistent with the previous observations of high deflection and settlement on the left side of the sleeper. Sensor pads B and C detect no pressure before and after load application. However, when load is applied, the pressure increases to 8.3 and 9.4 kPa, respectively. Sensor pads D and F do not detect any pressure during this experiment. Sensor pad E depicts similar behaviour like sensor pad A, but unlike sensor pad A, the pressure measured after the test is slightly higher than before the test.
For the simulations, however, the situation is different. In all cases, the sleeper was carried to a significant amount in the centre at the areas of sensor pad C and D before load application, with lower pressure at the sleeper ends. However, as in the laboratory experiment, sensor pad F rarely detected substantial pressure. Under load, the situation changes. In simulation 3, 5 and to some degree also simulation 1, one area depicts significantly higher load than the other areas, namely sensor pad B for simulation 1 and 5 and sensor pad C for simulation 3. The pressure under load is more evenly distributed in simulation 2 and 4 where the areas A, B, C and D show substantial pressure. In all cases, area F does not detect any pressure, which aligns with the previously observed uplift on the right sleeper ends.
After the quasi-static load is removed, the pressure distribution changes in the simulations. In most cases, the pressure became more evenly distributed with a reduction of pressure in the centre areas. Assuming that no pressure equals no contact, the presence of two major contact areas on the left and right sides of the sleeper and almost no pressure in the middle of the sleeper explains why the sleeper in the laboratory experiment was able to show such pronounced bending. It is therefore reasonable to assume that a small gap exists between the ballast and the sleeper.
3.2. Cyclic Loading
3.2.1. Sleeper Position and Movement—Cyclic Loading
During the second stage of the active loading phase, the sleeper is subjected to a cyclic load following the initial quasi-static loading. Thus, some prestressing specific to the sleeper has already occurred in the ballast bed. To verify the DEM simulations, the very first cyclic loading experiments from the laboratory test were considered, and the first 15 full loading cycles analysed to fit the available simulation data.
In Figure 10, the sleeper’s position is shown at various stages for the laboratory experiment and the simulations. The light blue colour refers to the position at the beginning of the cyclic loading experiment at minimum load (5 kN). The dark blue line displays the position of the sleeper when the first cycle’s maximum load (80 kN) is reached. The dark green line shows the sleeper’s position at the maximum load (80 kN) of the 15th cycle, and the light green line represents the sleeper’s position after 15 cycles when loading was minimal (5 kN). The dotted red lines signal the position of the rails where the load was applied.
Figure 10.
The sleeper’s position at minimum load (5 kN) before the first cycle (light blue), under maximum load (80 kN) in the first cycle (dark blue), under maximum load (80 kN) in the 15th cycle (dark green) and under minimum load (5 kN) after 15 load cycles (light green) for the laboratory experiment and 5 DEM simulations without USP.
Under load, the sleeper experiences significant bending, and an uplift is observed on the right end. However, both observations are more pronounced for the laboratory experiment than for the simulations. The laboratory subject again shows a U-shaped bending profile, while in the simulation a W-shape profile can be seen. The deflection profile of the sleepers with and without applied load remains consistent over the analysed cycles in all cases. Nevertheless, the deflection of the sleeper changes over the load cycles. In the laboratory experiment, the sleeper’s deflection amplitude on the left end increased sightly by 0.005 mm and decreased by 0.006 mm in the centre (measurement node 5 from the left at around 2.13 m box length). In the simulations, the deflection decreased in all cases. At the left end, elastic deflection decreased by 0.10 mm on average and by 0.073 mm in the centre (at node 15 from the left at around 2.11 m box length).
The uplift on the right end is still present in all cases but became less pronounced over the load cycles, especially in the simulations. In all cases, the sleeper depicts more residual settlement on the left end than in the centre, being −0.206 mm and −0.127 mm, respectively, for the laboratory subject and on average −0.570 mm and −0.383 mm, respectively, in the simulations.
These observations imply that the ballast beds in the simulations become stiffer as the number of loading cycles increases, and the sleeper transitions to a more stable bedding condition. In the laboratory experiment, however, a stable bedding condition with two major sleeper-ballast contact areas seems to be already achieved. Only minor changes were observed in the first 15 load cycles and elastic deflection and residual settlement remain significantly lower than in the simulations.
3.2.2. Pressure Distribution—Cyclic Loading
Analysing the pressure distribution at the sleeper-ballast interface and its change over the cycles provides additional insights into the sleeper’s bedding condition and how this affects settlement. In Figure 11, the pressure summarised per sensor pad is shown at minimal load (5 kN) before the first cycle in light blue, at maximum load (80 kN) of the first load cycle in dark blue, at maximum load (80 kN) of the 15th cycle in dark green and after 15 load cycles at minimal load (5 kN) in light green for the laboratory experiment and the five DEM simulations. The sensor pads in the figures are labeled as in Figure 2 (A to F, from left to right). The dotted red lines signal the position of the rails where the load was applied. For the laboratory subject, the 15 load cycles did not change the pressure distribution significantly. A small increase over the cycles can be observed for sensor pad A and E under minimum as well as maximum load. Sensor pad B, C, D and F detect no pressure at minimum load. However, the pressure on sensor pad B and C increases under load, while it remains at zero for the sensor pads D and F.
Figure 11.
The pressure distribution along the sleeper’s length summarised for each sensor pad at minimum load (5 kN) before the first cycle (light blue), at maximum load (80 kN) in the first cycle (dark blue), at maximum load (80 kN) in the 15th cycle (dark green) and at minimum load (5 kN) after 15 load cycles (light green) for the laboratory experiment and 5 DEM simulations without USP. The areas in the simulations are referenced using the same letters (A to F, from left to right).
This underlines the observations from before that the laboratory sleeper already reached a stable bedding condition on the ballast with two major contact areas with a possible gap in the sleeper’s centre that closes without high impact under load.
In simulation 1, 2, 3 and 4, the sleeper’s higher settlement also leads to more change in the pressure distribution. In simulation 4, however, only minor changes, like in the laboratory, were observed. The strongest change happened below the inner loaded rail around the area of sensor pad C and D. In all simulations the pressure decreased close to the position of the inner/right loaded rail while it increased on the left side at sensor pad A and B. For simulation 2 the pressure at sensor pad C and D even dropped close to zero after 15 load cycles.
Despite the strong influence of the initial configuration on the pressure distribution, the overall bending and settlement behaviour (bending profile and higher settlement on the left side) remain similar across all five cases. Nevertheless, it is believed that a characteristic bedding condition forms after an initial consolidation phase, analogous to the laboratory experiment.
Comparisons of sleeper settlement results on randomly configured ballast beds remain qualitative in nature. To capitalise on the advantages of the simulation, the ballast bed configuration of simulation 4 is used as a baseline for further studies. This configuration has proven to be more stable than others following the initial loading cycles. Consequently, it is believed to more accurately represent the loading-to-settlement correlation as a result of ballast pressure.
3.3. Long-Term Behaviour
Comparisons between the laboratory tests and the numerical simulation reveal distinct differences in settlement behaviour and pressure distribution. However, the origin of these differences is not known. To further study the effects that might result after more loading cycles, the setup of simulation 4 is used to apply in a total of 400 load cycles.
3.3.1. Sleeper Position and Movement - Long-Term Behaviour
In Figure 12 the sleeper’s position over the box’ length is shown before and after 400 load cycles for the laboratory experiment and the simulation. The light blue colour refers to the position at the beginning of the cyclic loading experiment at minimal load (5 kN). The dark blue line displays the position of the sleeper when the first cycle’s maximum load (80 kN) is reached. The dark green line shows the sleeper’s position at the maximum load (80 kN) of the 400th cycle, and the light green line represents the sleeper’s position after 400 cycles at minimal load (5 kN). The dotted red lines signal the position of the rails where the load was applied.
Figure 12.
The sleepers position under minimum load (5 kN) before the first cycle (light blue), under maximum load (80 kN) in the first cycle (dark blue), under maximum load (80 kN) in the 400th cycle (dark green) and under minimum load (5 kN) after 400 load cycles (light green) for the laboratory experiment and simulation 4 without USP.
For the laboratory experiment, the sleeper’s bending is less pronounced after 400 load cycles than it was in the first cycle. This implies that the elastic sleeper deflection (the difference between the light and dark lines of the same colour) has decreased over time, particularly in the middle part of the sleeper. At the far left, the elastic deflection decreased from 0.23 mm to 0.14 mm, while in the centre (at the 5th node from the left in Figure 12a at around 2.1 m box length), it decreased from 1.01 mm to 0.63 mm. This implies that the ballast bed becomes more rigid as the number of loading cycles increases, and the sleeper transitions to a more stable bedding condition.
At the third node from the right, a tipping point is visible, and an uplift is still present at the right end. This uplift decreases over time from 0.41 mm to 0.27 mm. Additionally, the sleeper settles gradually on the unloaded side, depicting residual settlement (difference between the light coloured lines) of 0.39 mm at the right end. However, the residual settlement is highest on the left side of the sleeper, measuring 1.39 mm, while being 1.16 mm in the centre of the sleeper.
Figure 12b shows the sleeper’s movement over 400 load cycles in the DEM simulation (configuration 4). Significant change in elastic deflection can be observed as the sleeper develops more pronounced bending over the course of the simulation similar to the laboratory test. Elastic deflection in the centre (at the 15th node from the left side at around 2.1 m box length) increases from 0.25 mm to 0.35 mm, while it decreases at the left end from 0.23 to 0.10 mm. The uplift on the right end decreases from an initial 0.23 mm to 0.20 mm. Residual settlement depicts an approximate linear left-to-right behaviour being highest at the left end with 3.36 mm, 2.76 mm in centre and 0.48 mm at the right sleeper end.
3.3.2. Pressure Distribution—Long-Term Behaviour
In Figure 13, the pressure distribution at the sleeper-ballast interface summarised for each sensor pad is shown at minimal load (5 kN) in light blue, at maximum load (80 kN) of the first load cycle in dark blue, at maximum load (80 kN) of the 400th cycle in dark green and after 400 load cycles at minimal load (5 kN) in light green for the laboratory experiment and simulation setup 4. The sensor pads in the figures are labeled as in Figure 2 (A to F, from left to right). The dotted red lines signal the position of the rails where the load was applied.
Figure 13.
The pressure distribution along the sleeper’s length summarised for each sensor pad at minimum load (5 kN) before the first cycle (light blue), at maximum load (80 kN) in the first cycle (dark blue), at maximum load (80 kN) in the 400th cycle (dark green) and at minimum load (5 kN) after 400 load cycles (light green) for the laboratory experiment and simulation 4 without USP. The areas in the simulation are referenced using the same letters (A to F, from left to right).
In the laboratory experiment, the pressure on the left side under maximum load increases over the cycles at sensor pad A and B, while the pressure only changes slightly at the remaining sensor pads. The areas, namely sensor pad A, B, C as well as D that contribute to load transmission, persist throughout the 400 cycles. Under minimal loading sensor pads B, C, D and F do not detect any pressure.
More change in the pressure distribution can be observed in the simulation. The initially perceived stabilised situation changed significantly in the following 385 cycles. Pressure in the sleeper’s centre at sensor pad B, C and D decreased under maximum load while it increased on the extremities at sensor pad A, E and even F where previously no pressure was measured at all. The distribution itself trends towards a linear left-to-right decline under maximum load. Under minimal loading, the even distribution at the beginning of the simulation developed into a situation more similar to the laboratory experiment, where no pressure can be measured at sensor pad B, C and D while pressure increased at sensor pad A, E and even F.
3.4. Reduced Contact Stiffness
To study the effects of reduced sleeper contact stiffness, simulation setup 4 was used as a baseline and three simulations were conducted to research the effects on elastic sleeper deflection, residual settlement and pressure distribution. Similar to the studies before first quasi-static loading was applied before cyclic loading was applied for 15 cycles.
3.4.1. Quasi-Static Loading—Reduced Contact Stiffness
Sleeper Position and Movement
In Figure 14, the sleeper’s position over the box length is shown for the laboratory experiment for a sleeper equipped with a USP (Figure 14a) and three simulations (Figure 14b–d). In the simulation, the Young’s modulus of the sleeper handling external contacts was gradually reduced by one order of magnitude. The material properties of the different sleeper models are presented in Table 2. In all four subfigures, the light grey line represents the sleeper’s initial position, the dark grey line represents the sleeper’s position under quasi-static load (100 kN) and the dark line represents the sleeper’s final position. The dotted red lines signal the position of the rails where the load was applied.
Figure 14.
The sleeper’s position before, during and after quasi-static loading (100 kN) for the laboratory experiment with a sleeper equipped with a USP and three simulations with various sleeper contact stiffnesses.
The laboratory sleeper shows high elastic deflection under load, with the maximum at the left end. Similar to the case without a USP, the residual settlement with USP also occurs primarily at the left end, but its magnitude is significantly lower than in the unpadded case. A tipping point is still present, accompanied by uplift at the right end.
Although the ballast bed configuration was identical for all three simulations, the initial position of the sleeper is different for each case. This is due to the reduction in contact stiffness leading to more overlap between the ballast particles and the sleeper and hence to a lower initial height. However, the overall deflection profile before and during loading is similar in all cases. A tilt to the left side is observed and a W-shape deflection profile is seen under load. With the reduction in contact stiffness, the elastic deflection increases but, at least for this quasi-static loading experiment, the residual settlement decreases. Additionally, by reducing the stiffness, the tipping point shifts to the right while an uplift on the right end is still observed in all cases.
Pressure Distribution
Figure 15 displays the pressure distribution summarised for each sensor pad along the length of the box for the laboratory experiment with a sleeper equipped with a USP and three simulations on ballast bed configuration 4 with various contact stiffnesses. Light grey represents the initial pressure distribution, dark grey represents the distribution during quasi-static loading (100 kN), and black represents the pressure after load application. The sensor pads in the figures are labeled as in Figure 2 (A to F, from left to right). The dotted red lines signal the position of the rails where the load was applied.
Figure 15.
Pressure distribution along the sleepers length summarised for each sensor pad before, during and after static loading (100 kN) for the laboratory experiment with a sleeper equipped with a USP and three simulations with various sleeper contact stiffnesses. The areas in the simulations are referenced using the same letters (A to F, from left to right).
For the laboratory subject, the pressure under load follows an almost linear behaviour decreasing from left to right, which fits the elastic deflection behaviour previously observed. Little to no change is seen for the pressure distribution after static loading, showing the highest pressure in the centre of the sleeper at sensor pad C and D. The reduction in contact stiffness in the simulation depicts a smoothing impact. By decreasing the contact stiffness, the pressure distribution under load develops a more linear behaviour, reducing the peak at sensor pad C that is present in Figure 15b and slightly increasing the pressure at sensor pads A, B and E. While the distribution changes significantly under load, almost no change is observed for the distribution after static loading. In all cases, including the laboratory experiment, without active loading, the sleeper’s centre transfers most load into the ballast, with lower values on the extremities, as in the laboratory experiment.
3.4.2. Cyclic Loading—Reduced Contact Stiffness
Sleeper Position and Movement
After the quasi-static loading experiment, a cyclic load is applied for 15 cycles. In Figure 16, the sleeper’s position before cyclic loading at minimal load (5 kN, light blue), at maximum load (80 kN) of the first cycle (dark blue), at maximum load (80 kN) of the last cycle (dark green) and after 15 load cycles at minimal load (5 kN, light green) is shown for the laboratory experiment and the three simulations on configuration 4 with reduced contact stiffnesses. The dotted red lines signal the position of the rails where the load was applied.
Figure 16.
The sleeper’s position under minimum load (5 kN) before the first cycle (light blue), under maximum load (80 kN) in the first cycle (dark blue), under maximum load (80 kN) in the 15th cycle (dark green) and under minimum load (5 kN) after 15 load cycles (light green) for the laboratory experiment with a sleeper equipped with a USP and three simulations with various sleeper contact stiffnesses.
In the laboratory, the sleeper follows the trend from the quasi-static loading experiment, showing high elastic deflection and little residual settlement. The tipping point and uplift on the right end are present during cyclic loading as well.
In the simulation, the elastic deflection under cyclic loading increases with reduction of sleeper contact stiffness as expected. The deflection profile, however, remains consistent, showing a similar W-shape profile in all three cases. Residual settlement increases with reduction of contact stiffness showing the highest values for the simulation with the softest USP.
Pressure Distribution
The pressure distribution summarised for each sensor pad for the laboratory experiment and the three simulations with various contact stiffnesses is shown in Figure 17. The distribution before cyclic loading was applied at minimal load (5 kN) is shown in light blue, at maximum load (80 kN) of the first load cycle in dark blue, at maximum load (80 kN) of the 15th cycle in dark green and after 15 load cycles at minimal load (5 kN) in light green. The sensor pads in the figures are labeled as in Figure 2 (A to F, from left to right). The dotted red lines signal the position of the rails where the load was applied. In general, it can be observed that the softer the contact, the less change in pressure distribution over the 15 cycles. For the simulation with elastic and softer elastic USP, the pressure at sensor pad C decreases under load. When no load is applied, the sleeper is carried by sensor pad A, B, C, D and E almost equally in the simulations, while in the laboratory tests sensor pad C and D detect higher pressure than on the left side. Nevertheless, very good agreement is observed between the laboratory experiment and the simulations with reduced contact stiffness.
Figure 17.
Pressure distribution along the sleeper’s length summarised for each sensor pad before cyclic loading (light blue), under maximum load in the first cycle (dark blue), under maximum load in the 15th cycle (dark green) and after cyclic loading (light green) for the laboratory experiment with a sleeper equipped with a USP and three simulations of various sleeper contact stiffnesses. The areas in the simulations are referenced using the same letters (A to F, from left to right).
3.5. Result Interpretation Table
In order to enable easier comparison between the provided results, the following Table 3 summarizes the interprations of the studies discusssed above.
Table 3.
Result interpretation summary of the conducted studies. The symbol ↑ indicates an increase while ↓ indicates a reduction of the respective value.
4. Discussion
This study investigated the mechanical response of a long turnout sleeper bedded on ballast under asymmetric quasi-static and cyclic loading through large-scale laboratory experiments and Discrete Element Method simulations. A custom-built ballast box and high-resolution measurement instrumentation enabled detailed tracking of local sleeper deflection and local sleeper-ballast interface pressure along its length. The simulations employed a refined elastic sleeper model within the Yade framework using the PFacet approach and the Conical Damage Model to represent elasto-plastic ballast contact behaviour.
In the quasi-static laboratory tests, the sleeper exhibited pronounced U-shaped bending with an uplift on the unloaded side, attributed to uneven contact conditions and the discrete nature of the ballast. DEM simulations, in contrast, displayed more uniform W-shaped deflection profiles and a generally stiffer bedding response. The pressure distribution under quasi-static loading highlighted the existence of dominant contact zones in both laboratory and simulations, although their locations differed, reflecting the inherent variability of ballast configurations.
Cyclic loading revealed that the laboratory sleeper reached a relatively stable bedding condition within the first few cycles, with minimal change in deflection and pressure distribution. The DEM simulations required more cycles to stabilise, initially exhibiting higher residual settlement and more change in pressure redistribution. Nonetheless, trends such as the transition towards more linear pressure gradients and consistent uplift behaviour were qualitatively well reproduced.
The long-term simulation over 400 cycles further confirmed the DEM model’s capability to capture the essential consolidation behaviour observed in the laboratory. Deflection profile and pressure distribution increasingly aligned with experimental trends, including the change to a U-shaped bending profile under load and the formation of two primary contact zones when no load is applied. Hence, a voided zone forms between sleeper and ballast beneath the inner loaded rail over time. However, residual settlement remained higher in the simulation, most likely due to differences in ballast bed compaction.
Moreover, the impact of reduced contact stiffness—used to replicate the presence of an under-sleeper pad—showed increased deflection, smoother pressure distributions, and improved agreement with laboratory results in quasi-static loading. In the cyclic loading experiments, however, the differences to the laboratory increased, as residual settlement remained significantly higher than in the laboratory.
A key outcome of this work is that the DEM simulations, based on physical reasoning and a minimal calibration procedure, were able to qualitatively and to a large extent quantitatively reproduce the observed mechanical response. The simulation framework proved robust and generalisable across different loading scenarios and ballast configurations.
Key takeaways:
- The DEM model replicates sleeper bending and uplift trends observed in the laboratory under both quasi-static and cyclic loading.
- Pressure distribution under load in simulations reflects key experimental findings, such as load concentration zones and loss of contact at the sleeper’s centre and right extremity.
- Long-term loading simulations reproduce the progressive formation of stable bedding conditions and shifting contact zones, in agreement with experimental observations showing how ballast voids in turnouts can develop.
- Simplified USP modelling (via reduced contact stiffness) captures static load effects and follows consistent trends but underestimates residual settlement under cyclic loading.
- Most notably, the DEM simulations achieved high-quality agreement with laboratory results without the need for extensive parameter calibration, relying instead on physically motivated model setups and validated contact laws.
- On Under Sleeper Pad Modelling
The observed differences in settlement between the laboratory experiments and the simulations under cyclic loading are attributed to the different components contributing to the overall settlement behaviour. The residual settlement of the sleeper with USP in the laboratory experiments results from the embedding of ballast stones in the USP during the initial cyclic loading phase. This behaviour in the very first loading cycles is a designed feature of the USP, which is specifically developed for ballast protection and should not be mistaken for settlement caused by ballast degradation. After sufficient load cycles, once the ballast stones are embedded in the USP, the settlement rate decreases significantly as shown in detail in Grohs et al. [7]. This behaviour of embedding the stones in the USP is not accounted for in the inter-particle contact law present in the DEM simulations, which increases the observed residual settlement in the simulation results. Consequently, the measured settlement in the laboratory represents a combination of ballast bed settlement and temporary, time-dependent (visco-elastic) USP deformation, whereas in the simulation it is a combination of ballast bed settlement and increased permanent (plastic) overlap between the sleeper model and ballast particles. The differences in settlement are therefore attributed to the modelling approach of USPs in the simulation. Purely relying on changing elastic properties is not enough to cover the full effects of this USP used in the laboratory experiments. Although residual settlement differed from the laboratory experiments, the model was able to provide valuable insights into sleeper-ballast interaction and how the stiffness of the contact influences how forces are transferred through the sleeper into the ballast. A clearer distinction between ballast settlement and USP deformation, alongside an improved contact model for ballast-USP interaction, will be the focus of future research to close the observed research gap.
Overall, this study underlines the potential of DEM simulations as a tool for gaining insights into sleeper-ballast interaction in complex scenarios such as turnouts, offering a valuable complement to physical testing for future parametric and degradation studies as well as track component development to avoid excessive ballast void development.
Author Contributions
Conceptualization: P.P., K.S. and N.K.; formal analysis: P.P.; investigation: P.P., M.Q. and F.P.; methodology: P.P., N.K. and K.S.; resources: M.Q. and N.K.; supervision: K.S. and F.P.; writing—original draft: P.P.; writing—review & editing: all authors. All authors have read and agreed to the published version of the manuscript.
Funding
The authors would like to acknowledge the financial support within the COMET K2 Competence Centers for Excellent Technologies by the Austrian Federal Ministry for Innovation, Mobility and Infrastructure (BMIMI), Austrian Federal Ministry for Economy, Energy and Tourism (BMWET), the Province of Styria (Dept. 12) and the Styrian Business Promotion Agency (SFG). Supported by TU Graz Open Access Publishing Fund.
Institutional Review Board Statement
Not applicable.
Informed Consent Statement
Not applicable.
Data Availability Statement
The datasets presented in this article are not readily available because of project guidelines. Requests to access the datasets should be directed to the author.
Acknowledgments
The publication was written at Virtual Vehicle Research GmbH in Graz, Austria. The authors would like to acknowledge the financial support within the COMET K2 Competence Centers for Excellent Technologies by the Austrian Federal Ministry for Innovation, Mobility and Infrastructure (BMIMI), Austrian Federal Ministry for Economy, Energy and Tourism (BMWET), the Province of Styria (Dept. 12) and the Styrian Business Promotion Agency (SFG). The Austrian Research Promotion Agency (FFG) has been authorised for the programme management. They would furthermore like to express thanks to their supporting industrial project partners, namely Getzner Werkstoffe GmbH, ÖBB Infrastruktur AG, SBB Infrastruktur, voestalpine Railway Systems GmbH. Supported by TU Graz Open Access Publishing Fund.
Conflicts of Interest
Authors Nishant Kumar and Martin Quirchmair were employed by the company Getzner Werkstoffe GmbH. Authors Paul Pircher and Klaus Six were employed by the company Virtual Vehicle Research GmbH (Austria). The remaining authors declare that the research was conducted in the absence of any commercial or financial relationships that could be construed as a potential conflict of interest. The funder, Getzner Werkstoffe GmbH, ÖBB Infrastruktur AG, SBB Infrastruktur and voestalpine Railway Systems GmbH, had no role in the design of the study; in the collection, analysis, or interpretation of data; in the writing of the manuscript, or in the decision to publish the results.
Abbreviations
The following abbreviations are used in this manuscript:
| DEM | Discrete Element Method |
| CDM | Conical Damage Model |
| USP | Under Sleeper Pad |
References
- Fellinger, M.; Wilfling, P.A.; Marschnig, S. CoMPAcT-Data Based Condition Monitoring and Prediction Analytics for Turnouts. In Intelligent Quality Assessment of Railway Switches and Crossings; Springer: Cham, Switzerland, 2021; pp. 129–148. [Google Scholar] [CrossRef] [Scilit]
- Pålsson, B.A.; Vilhelmson, H.; Ossberger, U.; Sehner, M.; Milosevic, M.D.G.; Loy, H.; Nielsen, J.C.O. Dynamic vehicle–track interaction and loading in a railway crossing panel–calibration of a structural track model to comprehensive field measurements. Veh. Syst. Dyn. 2024, 62, 2810–2836. [Google Scholar] [CrossRef] [Scilit]
- Loidolt, M.; Marschnig, S.; Berghold, A. Track geometry quality assessments for turnouts. Transp. Eng. 2023, 12, 100170. [Google Scholar] [CrossRef] [Scilit]
- Loidolt, M.; Marschnig, S.; Bürgler, M.; Berghold, A.; Dornig, P.; Ossberger, U. Quality Behaviour of Turnouts: Comparison, Problem Specification and Recommendation of Measures. Appl. Sci. 2023, 13, 10665. [Google Scholar] [CrossRef] [Scilit]
- Barkhordari, P.; Galeazzi, R.; Blanke, M. Monitoring of Turnout Ballast Degradation Using Statistical Low-Complexity Behavioral Models. IEEE Trans. Control Syst. Technol. 2021, 29, 278–293. [Google Scholar] [CrossRef] [Scilit]
- Shih, J.Y.; Weston, P.; Entezami, M.; Roberts, C.; O’Callaghan, M. Experiences Using MEMS Accelerometers on Railway Bearers at Switches and Crossings to Obtain Displacement—Awkward Situations. Infrastructures 2024, 9, 91. [Google Scholar] [CrossRef] [Scilit]
- Grohs, G.; Pircher, P.; Quirchmair, M.; Loy, H.; Six, K.; Pospischil, F. Behavior of turnout sleepers in a large-scale ballast box test. Sci. Rep. 2025, 15, 16717. [Google Scholar] [CrossRef] [Scilit]
- Pircher, P. A DEM Model for Elastic Sleepers to Study Dynamic Railway Track Behaviour. Master’s Thesis, Montanuniversität Leoben, Leoben, Austria, 2021. [Google Scholar] [CrossRef]
- van Belkom, A. A simplified method for calculating load distribution and rail deflections in track, incorporating the influence of sleeper stiffness. Adv. Struct. Eng. 2020, 23, 2358–2372. [Google Scholar] [CrossRef] [Scilit]
- Refahiat Nikoo, H.; Zakeri, J.; Mohammadzadeh, S. Field and laboratory investigations on the effective contact surface between sleeper and ballast particles in railway tracks. Sci. Iran. 2022, 30, 1911–1924. [Google Scholar] [CrossRef] [Scilit]
- Saeid, F.; Morteza, E.; Reza, N. Effect of rock strength on the degradation of ballast equipped with under sleeper pad using discrete element method. Int. J. Sci. Res. Arch. 2024, 11, 2579–2586. [Google Scholar] [CrossRef] [Scilit]
- Esmaeili, M.; Farsi, S.; Shamohammadi, A. Effect of rock strength on the degradation of ballast equipped with under sleeper pad. Constr. Build. Mater. 2022, 321, 126413. [Google Scholar] [CrossRef] [Scilit]
- Chi, Y.; Xiao, H.; Wang, Y.; Zhang, Z.; Nadakatti, M.M. Experimental study and numerical simulation of the impact of under-sleeper pads on the dynamic and static mechanical behavior of heavy-haul railway ballast track. Railw. Eng. Sci. 2024, 32, 384–400. [Google Scholar] [CrossRef] [Scilit]
- Berghold, A. Wirkungsweise des Schotters im Gleis Unter Verschiedenen Randbedingungen. Ph.D. Thesis, Technische Universität Graz, Graz, Austria, 2016. [Google Scholar]
- Chen, C.; McDowell, G.R. An investigation of the dynamic behaviour of track transition zones using discrete element modelling. Proc. Inst. Mech. Eng. Part F J. Rail Rapid Transit 2016, 230, 117–128. [Google Scholar] [CrossRef] [Scilit]
- Liu, D.; Su, C.; Zhang, D.; Lan, C. The Influence of an Unsupported Sleeper on the Vertical Bearing Characteristics of Heavy-Haul Railway Ballast. Materials 2024, 17, 1434. [Google Scholar] [CrossRef] [Scilit]
- Jain, A.; Metrikine, A.V.; Steenbergen, M.J.M.M.; van Dalen, K.N. Dynamic amplifications in railway transition zones: Performance evaluation of sleeper configurations using energy criterion. Front. Built Environ. 2024, 10, 1285131. [Google Scholar] [CrossRef] [Scilit]
- Holtzendorff, K. Untersuchung des Setzungsverhaltens von Bahnschotter und der Hohllagenentwicklung auf Schotterfahrbahnen. Ph.D. Thesis, Technische Universität Berlin, Berlin, Germany, 2003. [Google Scholar]
- Nielsen, J.C.; Li, X. Railway track geometry degradation due to differential settlement of ballast/subgrade–Numerical prediction by an iterative procedure. J. Sound Vib. 2018, 412, 441–456. [Google Scholar] [CrossRef] [Scilit]
- Sysyn, M.; Przybylowicz, M.; Nabochenko, O.; Liu, J. Mechanism of Sleeper–Ballast Dynamic Impact and Residual Settlements Accumulation in Zones with Unsupported Sleepers. Sustainability 2021, 13, 7740. [Google Scholar] [CrossRef] [Scilit]
- Fang, J.; Zhao, C.; Lu, X.; Xiong, W.; Shi, C. Dynamic behavior of railway Vehicle-Ballasted track system with unsupported sleepers based on the hybrid DEM-MBD method. Constr. Build. Mater. 2023, 394, 132091. [Google Scholar] [CrossRef] [Scilit]
- Guo, Y.; Jia, W.; Markine, V.; Jing, G. Rheology study of ballast-sleeper interaction with particle image Velocimetry (PIV) and discrete element modelling (DEM). Constr. Build. Mater. 2021, 282, 122710. [Google Scholar] [CrossRef] [Scilit]
- Jia, W.; Wang, H.; Jing, G.; Markine, V. Dynamic Behaviour of Ballast Under Hanging Sleepers in Railways Track Transition Zones Using Fem-Dem Method. SSRN Electron. J. 2023. [Google Scholar] [CrossRef] [Scilit]
- Jing, G.; Luo, Q.; Wang, Z.; Shen, Y. Micro-analysis of hanging sleeper dynamic interactions with ballast bed. J. Vibroeng. 2015, 17, 444–454. [Google Scholar]
- Shi, C.; Zhao, C.; Xin, L.; Wang, J. Dynamic impact of unsupported sleepers on railway infrastructure with a coupled MBD-DEM-FDM model. Transp. Geotech. 2024, 45, 101221. [Google Scholar] [CrossRef] [Scilit]
- Song, W.; Huang, B.; Shu, X.; Stránský, J.; Wu, H. Interaction between Railroad Ballast and Sleeper: A DEM-FEM Approach. Int. J. Geomech. 2019, 19, 04019030. [Google Scholar] [CrossRef] [Scilit]
- Guo, Y.; Zhao, C.; Markine, V.; Jing, G.; Zhai, W. Calibration for discrete element modelling of railway ballast: A review. Transp. Geotech. 2020, 23, 100341. [Google Scholar] [CrossRef] [Scilit]
- Kumar, N.; Suhr, B.; Marschnig, S.; Dietmaier, P.; Marte, C.; Six, K. Micro-mechanical investigation of railway ballast behavior under cyclic loading in a box test using DEM: Effects of elastic layers and ballast types. Granul. Matter 2019, 21, 106. [Google Scholar] [CrossRef] [Scilit]
- Suhr, B.; Six, K. Parametrisation of a DEM model for railway ballast under different load cases. Granul. Matter 2017, 19, 64. [Google Scholar] [CrossRef] [Scilit]
- Suhr, B.; Marschnig, S.; Six, K. Comparison of two different types of railway ballast in compression and direct shear tests: Experimental results and DEM model validation. Granul. Matter 2018, 20, 70. [Google Scholar] [CrossRef] [Scilit]
- Suhr, B.; Six, K. Simple particle shapes for DEM simulations of railway ballast: Influence of shape descriptors on packing behaviour. Granul. Matter 2020, 22, 43. [Google Scholar] [CrossRef] [Scilit]
- Suhr, B.; Skipper, W.A.; Lewis, R.; Six, K. DEM modelling of railway ballast using the Conical Damage Model: A comprehensive parametrisation strategy. Granul. Matter 2022, 24, 40. [Google Scholar] [CrossRef] [Scilit] [PubMed]
- Suhr, B.; Six, K. Efficient DEM simulations of railway ballast using simple particle shapes. Granul. Matter 2022, 24, 114. [Google Scholar] [CrossRef] [Scilit]
- Chalabii, J.; Movahedi Rad, M.; Hadizadeh Raisi, E.; Esfandiari Mehni, R. Effect of Sleeper-Ballast Particle Contact on Lateral Resistance of Concrete Sleepers in Ballasted Railway Tracks. Materials 2022, 15, 7508. [Google Scholar] [CrossRef] [Scilit]
- Angelidakis, V.; Boschi, K.; Brzeziński, K.; Caulk, R.A.; Chareyre, B.; del Valle, C.A.; Duriez, J.; Gladky, A.; van der Haven, D.L.H.; Kozicki, J.; et al. YADE—An extensible framework for the interactive simulation of multiscale, multiphase, and multiphysics particulate systems. Comput. Phys. Commun. 2024, 304, 109293. [Google Scholar] [CrossRef] [Scilit]
- Collar, E.P.; García-Martínez, J.M. Mechanical Behavior of Polymeric Materials: Recent Studies. Polymers 2024, 16, 2821. [Google Scholar] [CrossRef] [Scilit]
- Li, H.; McDowell, G.R. Discrete element modelling of under sleeper pads using a box test. Granul. Matter 2018, 20, 26. [Google Scholar] [CrossRef] [Scilit] [PubMed]
- Quirchmair, M.; Loy, H.; Sehner, M.; Pümpel, M. Schotterschonung mit Schwellensohlen: Unterschiedliche Wirksamkeiten bei gleichem Bettungsmodul. ZEVrail 2023, 147, 448–455. [Google Scholar]
- Cundall, P.A.; Strack, O.D.L. A discrete numerical model for granular assemblies. Géotechnique 1979, 29, 47–65. [Google Scholar] [CrossRef] [Scilit]
- Lu, M.; McDowell, G.R. Discrete element modelling of railway ballast under triaxial conditions. Geomech. Geoengin. 2008, 3, 257–270. [Google Scholar] [CrossRef] [Scilit]
- Villalba Sanchis, I.; Adrián, M.C.; Pablo, M.F.; Ricardo, I.F.; Salvador Zuriaga, P. Discrete elements method to model ballast behaviour under railway turnouts. Cogent Eng. 2024, 11, 2396147. [Google Scholar] [CrossRef] [Scilit]
- ÖNORM 13450; Gesteinskörnungen für Gleisschotter [Aggregates for Railway Ballast]. Austrian Standards Institute (ASI): Vienna, Austria, 2014.
- Kuttelwascher, C.; Zuzic, M. Track Ballast in Austria. Rail Infrastructure. Available online: https://www.plassertheurer.com/fileadmin/user_upload/Mediathek/Publikationen/ri_12888990.pdf (accessed on 8 July 2025).
- Baeßler, M. Lageveränderungen des Schottergleises durch Zyklische und Dynamische Beanspruchungen. Ph.D. Thesis, Technische Universität Berlin, Berlin, Germany, 2008. [Google Scholar] [CrossRef]
Disclaimer/Publisher’s Note: The statements, opinions and data contained in all publications are solely those of the individual author(s) and contributor(s) and not of MDPI and/or the editor(s). MDPI and/or the editor(s) disclaim responsibility for any injury to people or property resulting from any ideas, methods, instructions or products referred to in the content. |
© 2026 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license.