Abstract
Prestressed concrete cylinder pipe (PCCP) experiences time-dependent prestress losses due to steel wire relaxation and corrosion during service, potentially reducing its pressure-carrying capacity. While their individual effects have been investigated, their combined impact on ultimate pressure capacity remains insufficiently understood. In this study, a three-dimensional finite element model of PCCP was developed in ABAQUS and validated against a full-scale internal water pressure test. Based on the validated model, numerical simulations were performed to evaluate the individual and combined effects of steel wire relaxation and corrosion. The results indicate that these deterioration mechanisms do not alter the PCCP failure mode: the mortar layer fails first with limited impact on capacity, followed by almost simultaneous core concrete failure. This causes rapid load redistribution to the steel cylinder and prestressing wires, resulting in increased strains and ultimate pipe failure. The ultimate capacity of the intact pipe is 2.07 MPa. A 20% relaxation ratio reduces capacity by approximately 15%, while a 30% corrosion degree causes a 64% reduction. Under 50-year combined degradation, the capacity drops to 0.70 MPa (a 66% reduction). Capacity decreases approximately linearly with relaxation, but nonlinearly with corrosion. The combined effects exhibit a staged degradation pattern: relaxation dominates early-stage capacity reduction, whereas corrosion becomes the controlling factor at later stages. The findings can provide a reference for long-term structural performance assessment and maintenance of PCCP.