Abstract
Ultrasonic spot-welded 1060 Al/T2 Cu joints with a 0.1 mm Zn interlayer were examined through temperature measurements, microscopy, SEM/EDS, microhardness and shear testing to compare the responses to welding energy, Al thickness and post-weld holding. Increasing welding energy from 900 to 4000 J generally raised recorded peak temperatures and promoted growth of the relatively planar Cu–Zn-rich interfacial region and wavy Al–Zn-rich transition zone. In the 2 mm Al series, base-metal hardness decreased slightly, while composite near-interface hardness increased. For 2 mm Al, mean nominal shear strength reached 23.77 ± 6.70 MPa at 3000 J before decreasing at 4000 J. At the same programmed energy, 4 mm Al joints exhibited lower recorded temperatures and thinner interfacial regions; their mean strength increased throughout the tested range, reaching 20.50 ± 1.06 MPa at 4000 J. At 1400 J with 2 mm Al, Zn-assisted joints had a higher mean strength than the Zn-free control. Holding the 2 mm Al/1400 J joints at 250 °C promoted further interfacial growth, reduced the residual Zn region and increased composite near-interface hardness, while mean strength decreased to 8.23 ± 0.83 MPa after 3 h. Strengths are means ± sample standard deviations.