Skip to Content
MetalsMetals
  • Article
  • Open Access

20 November 2026

23 Pages

Effects of Post-Weld Heat Treatment on Microstructural Evolution and Mechanical Properties of Friction Stir Welded 6061-T6 Aluminium Alloy Joints

and
1
School of Mechanical and Automotive Engineering, Chuzhou Polytechnic, Chuzhou 239000, China
2
College of Mechanical and Electrical Engineering, Nanjing University of Aeronautics and Astronautics, Nanjing 210016, China
*
Author to whom correspondence should be addressed.
Metals2026, 16(11), 1274;https://doi.org/10.3390/met16111274 
(registering DOI)
This article belongs to the Section Welding and Joining

Abstract

Post-weld heat treatment (PWHT) was applied to friction stir welded (FSW) 6061-T6 aluminium alloy joints to assess regional microstructural evolution and mechanical-property recovery. The treatment consisted of solution treatment at 520 °C for 1 h, water quenching, and artificial ageing at 170 °C for 7 h. Microstructural characterisation was performed using EBSD and SEM-EDS, while mechanical properties were evaluated through microhardness measurements and tensile testing. PWHT caused grain growth in the heat-affected, thermomechanically affected, and nugget zones (NZs). In the NZs, mean grain size increased from 10.17 to 16.15 μm, the fraction classified as recrystallised increased from 84.8% to 95.8%, and the high-angle grain-boundary fraction increased from 64.1% to 70.2%; KAM decreased from 0.61° to 0.54°. NZ hardness increased from 55–63 to 106–108 HV. Ultimate tensile strength and yield strength increased from 202.3 ± 2.5 to 299.8 ± 2.0 MPa and from 149.8 ± 1.4 to 249.6 ± 1.7 MPa, respectively, while elongation decreased from 13.8 ± 0.4% to 9.5 ± 0.2%. Both conditions fractured in the NZ. These findings show that PWHT restores hardness and strength but does not change the critical fracture region.