Abstract
The influence of cooling rate on the solidification behavior and microstructural evolution of Al-xMg-3Zn-0.3Cu-0.1Mn-0.12Zr alloys containing 4, 8, and 12 wt.% Mg was investigated using a wedge-shaped copper mold, which provided measured cooling rates of 10–31 K s−1. Higher cooling rates refined the grains and reduced the secondary dendrite arm spacing (SDAS), producing finer and more dispersed interdendritic constituents. Power-law fitting was employed to quantify the apparent cooling rate sensitivity of SDAS. The fitted exponents were 0.415, 0.398, and 0.196 for the 4Mg, 8Mg, and 12Mg alloys, respectively. Within the investigated cooling rate range, the 4Mg and 8Mg alloys exhibited comparable apparent sensitivities, whereas the 12Mg alloy showed a trend toward a weaker SDAS response. This behavior is consistent with changes in solute-controlled coarsening in the Mg- and Zn-rich interdendritic liquid. The Mg–Zn–Cu-enriched interdendritic constituents were identified as the Mg32(Al,Zn)49-type phase. Decreasing the cooling rate promoted the coarsening and interconnection of this phase without altering the detectable major phase constitution. At comparable cooling rates, increasing Mg content resulted in higher T-phase area fractions and more interconnected morphologies.