Skip to Content
MicromachinesMicromachines
  • Article
  • Open Access

27 November 2026

23 Pages

Quasi-Static Compression Behavior and Energy Absorption of a Two-Dimensional Self-Similar Re-Entrant Auxetic Structure

,
,
,
and
1
State Key Laboratory of Advanced Equipment and Technology for Metal Forming, School of Mechanical Engineering, Shandong University, Jinan 250061, China
2
Key Laboratory of High Efficiency and Clean Mechanical Manufacture of Ministry of Education, School of Mechanical Engineering, Shandong University, Jinan 250061, China
*
Author to whom correspondence should be addressed.

Abstract

Although two-dimensional re-entrant auxetic structures exhibit negative Poisson’s ratios and promising energy absorption capabilities, their deformation stability and mechanical performance are highly dependent on cell geometry. A two-dimensional self-similar re-entrant (2D SSRE) configuration was developed and subsequently manufactured using three-dimensional printing technology. Its response to quasi-static compression was evaluated experimentally and numerically, using a conventional two-dimensional re-entrant (2D RE) structure as the reference. A parametric analysis further explored how the outer and inner re-entrant angles, their respective height-to-length ratios, and wall thickness influence the specific energy absorption (SEA) and auxetic response of the 2D SSRE structure. The finite element predictions closely matched the experimentally observed responses. At their respective densification points, the tested 2D SSRE and 2D RE configurations achieved mean SEA values of 1.368 and 0.398 J/g, respectively, corresponding to a 243.72% increase for the tested 2D SSRE configuration. The parametric study identified distinct effects of geometric variables on SEA and auxetic behavior. The SEA of the 2D SSRE structure increased with the outer re-entrant angle, wall thickness, and outer height-to-length ratio, but decreased when the inner re-entrant angle and inner height-to-length ratio became larger. In contrast, the auxetic effect became more pronounced with increases in the inner re-entrant angle and both height-to-length ratios, but was weakened by thicker cell walls. The identified relationships between geometric parameters, energy absorption capacity, and auxetic response provide useful guidance for optimizing the structural configuration of 2D SSRE designs.

1. Introduction

Auxetic behavior is distinguished by a negative Poisson’s ratio (NPR), whereby a material expands transversely under uniaxial tension and contracts transversely under uniaxial compression. Almgren [1] proposed an isotropic three-dimensional structure with a Poisson’s ratio of −1; Lakes [2] demonstrated this behavior in cellular foams; and Wojciechowski [3] identified it in a two-dimensional isotropic system through computer simulations. Evans [4] introduced the term auxetic, while Milton [5] studied composites with Poisson’s ratios approaching −1. For architected mechanical metamaterials, the geometric configuration and spatial organization of the constituent cells play a dominant role in governing the auxetic response, whereas the chemical composition of the underlying material is generally less influential. Consequently, geometric modifications provide a means of independently tailoring structural stiffness, strength, lateral deformation, and energy absorption characteristics [6,7,8]. Auxetic structures have consequently attracted interest in impact protection, lightweight transportation and aerospace components, vibration isolation, biomedical devices, and multifunctional sandwich panels [7,8]. For energy-absorbing applications, however, a large NPR alone is insufficient. The structure must also sustain an appropriate load during progressive collapse and allow sufficient deformation before densification.
Auxetic structures have been developed in a range of configurations, including re-entrant and double-arrowhead honeycombs, chiral and anti-chiral lattices, rotating-unit systems, and perforated and origami-inspired architectures [6,7,8]. Re-entrant honeycombs are particularly attractive because their deformation mechanism is readily interpreted and their geometry can be fabricated by machining, polymer processing, or additive manufacturing. Under in-plane compression, the inclined cell walls bend and rotate, causing the cells to contract laterally. The effective modulus, compressive strength, Poisson’s ratio, and energy absorption capacity depend on geometric factors such as the re-entrant angle, wall thickness, cell aspect ratio, and relative density [9,10]. Studies of modified three-dimensional re-entrant structures and hybrid configurations suggest that combining geometric features can improve load resistance and energy absorption [11,12]. Increasing geometric complexity, however, can introduce local stress concentrations and competing deformation modes [13]. The quasi-static compressive response is therefore evaluated here in terms of three related aspects: load-bearing behavior, energy absorption, and auxetic response. Load-bearing behavior is described by the nominal stress–strain response, plateau stress, and densification strain. Energy absorption is characterized by the absorbed energy (EA), energy absorption efficiency (EAE), and SEA, while the auxetic response is characterized by the evolution of Poisson’s ratio with compressive strain.
These parameters are closely interrelated. A greater wall thickness may enhance the load-bearing capacity while limiting the space available for deformation. In comparison, variations in the re-entrant angle and cell aspect ratio affect ligament rotation and buckling, which in turn can modify the strain at which densification begins. Recent research has demonstrated the potential of hierarchical honeycomb structures to enhance crushing performance [14], while hierarchical re-entrant designs can combine energy absorption with vibration insulation [15]. Fractal self-similarity and self-similar multi-cell configurations have also been used to distribute deformation across multiple length scales [16,17]. Graded beam thickness and multi-step auxetic cells provide additional means of regulating progressive collapse and transition strain [18,19]. However, conventional two-dimensional re-entrant structures may still exhibit localized buckling, lateral tilting, asymmetric collapse, and premature wall contact. These instabilities can cause stress-plateau fluctuations and weaken the measured auxetic response. The balance between structural stiffness, deformation stability, SEA, and NPR therefore remains a central design issue.
Alternative cell geometries have been proposed to address these limitations. To examine the relationship between cellular geometry, collapse response, and energy absorption, researchers have considered diverse honeycomb designs, such as multi-scale circular re-entrant [20], star-shaped [21], circular double-arrowed [22], zigzag-ligament re-entrant [23], and graded re-entrant structures [24]. Collectively, these studies highlight the role of geometry in controlling collapse sequences and energy absorption capacity. Origami-inspired auxetic meta-structures and hybrid auxetic-honeycomb lattices can further increase load-bearing capability, although their more complex architectures make parameter interactions more difficult to interpret [25,26]. Bai et al. [27] used column-wise binary encoding to vary the distribution of embedded and non-embedded cells in a staggered re-entrant lattice and also considered a fully embedded configuration. Shen et al. [28] connected corresponding vertices of inner and outer re-entrant cells by horizontal and inclined support struts. In both studies, the inner re-entrant cell was defined as a scaled copy of the outer cell. Both studies also reported nearly symmetric inward collapse with X-shaped deformation bands under compression. The baseline two-dimensional self-similar re-entrant (2D SSRE) configuration studied here shares this nested geometry. In the parametric study, however, the inner and outer re-entrant angles and height-to-length ratios are varied separately, allowing the nested cells to depart from strict geometric similarity without changing their connectivity. This makes it possible to examine whether a change at the inner cell level has the same effect as a change at the outer cell level on specific energy absorption at the onset of densification and on the evolution of Poisson’s ratio during compression.
Compared with conventional fabrication techniques, additive manufacturing offers greater flexibility in producing thin-walled structures and complex nested geometries. Recent work has examined printed re-entrant structures, impact-resistant auxetic lattices, and additively manufactured hierarchical metamaterials [29,30,31]. For polymeric lattices, dimensional deviation, surface roughness, anisotropy, incomplete fusion, and node defects can alter buckling initiation and test repeatability. These effects are relevant to polyamide 12 (PA12) fabricated by selective laser sintering (SLS), for which topology, relative density, and process-induced irregularity influence compressive behavior and energy absorption [32,33,34,35,36]. Experimental-numerical studies of additively manufactured auxetic structures further show that deformation images and finite element predictions should be evaluated together when several buckling paths are possible [37,38]. Li et al. [39] used experiments and finite element simulations to examine how the hierarchical factor and re-entrant angle influence plastic hinge development and SEA in vertex-based re-entrant honeycombs. Baroutaji et al. [40] combined in-plane compression experiments and finite element simulations to assess the effects of chevron crosslinks on deformation and auxetic response. Recent studies of hierarchical auxetic metamaterials and parameter-dependent re-entrant honeycombs also highlight the need to distinguish the geometric factors governing energy absorption from those governing NPR [41,42,43]. The mechanical response of additively manufactured auxetic structures should also be interpreted in the context of the fabrication methods employed [44].
In this work, a two-dimensional self-similar re-entrant (2D SSRE) configuration is proposed, with a conventional two-dimensional re-entrant (2D RE) structure serving as the reference design. Quasi-static uniaxial compression experiments are performed on PA12 specimens produced by selective laser sintering (SLS). Abaqus simulations and compression experiments were used jointly to examine deformation patterns, nominal stress–strain responses, SEA, and Poisson’s ratio. The effects of cell geometry were further explored by varying the outer and inner re-entrant angles (θ1, θ2), their corresponding height-to-length ratios (H1/L1, H2/L2), and wall thickness (t). This analysis explores the influence of self-similar cell geometry on deformation at the two structural levels, while assessing how geometric variations affect deformation stability, energy absorption performance, and auxetic response.

2. Materials and Methods

2.1. Geometric Configuration

The geometric parameters of the 2D SSRE structure are defined in Figure 1. The outer and inner re-entrant cells are characterized by their horizontal wall lengths (l1 and l2), heights (H1 and H2), and inclination angles (θ1 and θ2), where each angle is defined relative to the horizontal axis. The wall thickness and out-of-plane dimension are denoted by t and b, respectively. Additionally, ls1 and ls2 represent the inclined wall lengths of the outer and inner cells, while ls3 and ls4 describe the inclined and horizontal connecting wall lengths. These dimensions satisfy the following geometric equations:
l s 1 = H 1 2 sin θ 1
l s 2 = H 2 2 sin θ 2
l s 3 = ( l 1 − l 2 2 ) 2 + ( H 1 − H 2 2 ) 2
l s 4 = ( l 1 2 − H 1 2 tan θ 1 ) − ( l 2 2 − H 2 2 tan θ 2 )
Figure 1. Geometrical characteristics of the 2D SSRE structure.
Considering the geometric characteristics of the structures, a Farsoon FS401 selective laser sintering (SLS) system (Farsoon Technologies Co., Ltd., Changsha, China) was employed to fabricate specimens from polyamide 12 (PA12) powder. The system has a laser spot diameter ranging from 0.2 to 1 mm and maximum build dimensions of 700 × 380 × 580 mm. SolidWorks (2021) was employed to develop the three-dimensional geometric models, which were subsequently saved as STP files for import into the slicing software of the SLS system. During the slicing process, the powder layer thickness was specified as 100 μm.
As shown in Figure 2, the three-dimensional models and printed specimens of the two-dimensional re-entrant (2D RE) and two-dimensional self-similar re-entrant (2D SSRE) structures are presented. A 3 × 4 unit-cell array was adopted for each specimen, with three cells distributed along the x-direction and four along the y-direction. To minimize dimensional deviations and deformation associated with SLS fabrication, the geometric dimensions of the 2D SSRE structure were set to l1 = 20 mm, l2 = 10 mm, H1 = 15 mm, H2 = 7.5 mm, θ1 = θ2 = 65°, t = 1 mm, and b = 20 mm.
Figure 2. Three-dimensional models and 3D-printed specimens of the 2D RE and 2D SSRE structures.

2.2. Experimental Procedure

Standard dog-bone-shaped tensile specimens were produced from PA12 using selective laser sintering (SLS) for subsequent mechanical characterization. Identical processing conditions were adopted for the tensile and 2D SSRE specimens to maintain consistency between material characterization and structural testing. The specimen geometry was modeled in SolidWorks according to ASTM D412 [45]. The three-dimensional models were exported in STP format and imported into the slicing software for fabrication. Uniaxial tensile tests were performed on PA12 specimens using an ME50 SIT19105 electronic universal testing machine (Senkeino Technology Co., Ltd., Shenzhen, China), with the crosshead advancing at a uniform rate of 2 mm/min. The integrated data acquisition system recorded the force-displacement response throughout each test. Analysis of the three true stress–strain responses in Figure 3 yielded an average elastic modulus of 850 MPa and a yield strength of 24 MPa for PA12. A density of 0.96 g/cm3 and a Poisson’s ratio of 0.3 were adopted for PA12.
Figure 3. True stress–strain curves obtained from uniaxial tensile tests of PA12 specimens.
Quasi-static compression testing of the 2D RE and 2D SSRE specimens followed the mechanical characterization of PA12. An ME50 SIT19105 electronic universal testing machine fitted with a load cell rated at 50 kN (measurement precision: ± 0.00001 kN) was used for the experiments. As depicted in Figure 4, compression was imposed at 2 mm/min by lowering the upper platen toward the specimen resting on the lower platen. Specimen deformation was documented using an industrial camera that acquired images every 5 s. These images were subsequently analyzed in ImageJ1 to measure lateral contraction and determine the corresponding Poisson’s ratios. During compression, the testing machine’s built-in data acquisition system automatically captured the force and displacement measurements for subsequent analysis.
Figure 4. Test setup for quasi-static uniaxial compression of the 2D SSRE structure.

2.3. Finite Element Simulation

Abaqus/Explicit (2022) was used to simulate the in-plane compression of the conventional 2D RE and proposed 2D SSRE structures. The explicit formulation was selected because the analysis involves large cell-wall rotations, local buckling, and evolving contact as the cells collapse. The general contact formulation was used to treat contact between the specimen and the loading platens as well as contact between cell walls. The solver also provided the kinetic and internal energy histories used to assess inertial effects during numerical compression. The complex geometries of both configurations were first modeled in three dimensions using SolidWorks and saved as STP files. Mesh generation was subsequently performed in HyperMesh (2022), after which the resulting INP files were transferred to Abaqus for numerical analysis.
The numerical compression model consists of a 2D SSRE specimen positioned between a pair of rigid loading platens, each with dimensions of 30 × 100 mm, as depicted in Figure 5. Contact interactions were modeled using the general contact formulation. A coefficient of 0.25 was assigned to tangential friction, whereas the normal contact behavior was specified as hard contact. C3D8R elements, consisting of eight-node linear bricks with reduced integration, were used to discretize the platens and the 2D SSRE structure. The structural mesh in Figure 6a had a characteristic element size of 0.4 mm, selected following a convergence assessment in which further mesh refinement yielded no appreciable change in the computed response.
Figure 5. Finite element setup for quasi-static compression of the 2D SSRE structure.
Figure 6. (a) Mesh-size sensitivity analysis of the nominal stress–strain response under quasi-static compression; (b) Kinetic and internal energy histories for the baseline 2D SSRE simulation, together with a reference curve equal to 5% of the internal energy.
The post-yield behavior of PA12 was represented in Abaqus/Explicit using a rate-independent von Mises plasticity model with tabulated isotropic hardening. The engineering stress–strain data from the uniaxial tensile tests described in Section 2.2 were first converted to true stress and total true strain. The elastic strain was then subtracted from the total true strain to obtain the true plastic strain. The resulting pairs of true stress and true plastic strain were entered as tabulated hardening data.
The numerical platen speed was set to 40 mm/s, compared with the experimental crosshead speed of 2 mm/min, to reduce the computational cost of the explicit analysis. The PA12 constitutive model was assumed to be rate-independent; neither yielding nor hardening was specified as a function of strain rate. To assess inertial effects at the selected speed, the kinetic and internal energy histories were examined for the baseline 2D SSRE configuration. Figure 6b shows these histories together with a reference curve corresponding to 5% of the internal energy. The kinetic energy remained below this reference level during loading, supporting a quasi-static interpretation of the baseline simulation. This comparison assesses structural inertia; it does not establish that PA12 is insensitive to strain rate. No lower-speed simulation was performed, so the sensitivity of the predicted response to the numerical loading speed was not quantified.

2.4. Evaluation Indicators

The force and displacement measurements obtained during compression were used to calculate the corresponding nominal stress and strain, respectively, according to the expressions below:
σ = F A , ε = δ H
where F represents the applied compressive force, while δ refers to the corresponding displacement, A and H represent the specimen’s initial cross-sectional area and height along the loading direction. Accordingly, nominal compressive stress and strain are plotted as positive quantities during compression.
The lateral deformation was evaluated using the measurement points illustrated in Figure 7. Within the area bounded by the red dashed lines, four measurement-point pairs (P1–P2, P3–P4, P5–P6, and P7–P8) were selected to characterize the transverse strain at different layers. The mean transverse strain was determined using the following expression:
ε ¯ x = 1 4 ( U P 2 x − U P 1 x D x + U P 4 x − U P 3 x D x + U P 6 x − U P 5 x D x + U P 8 x − U P 7 x D x )
where U P i x denotes the signed transverse displacement of measurement point i. With the displacement convention used in Equation (6), inward motion is negative for the left-hand points and positive for the right-hand points. The difference therefore gives the decrease in separation between P1 and P2. Dividing this difference by the initial separation (Dx) gives the transverse strain for that pair, with contraction taken as positive. The four pairwise strains are then averaged.
Figure 7. Poisson’s ratio measurement points. The red dashed lines connect the measurement points to illustrate their relative positions.
The vertical movement of the compression platen was used to determine the axial strain according to the following expression:
ε ¯ y = Δ U y D y
Poisson’s ratio was evaluated from the measured strains along the transverse and loading directions according to the following equation:
ν xy = − ε ¯ x ε ¯ y
The axial strain in Equation (7) is defined as positive in compression. Thus, under lateral contraction, both strains entering Equation (8) are positive. These strains have the opposite signs to the corresponding strains under the conventional tension-positive definition. Reversing both signs leaves their ratio unchanged, so Equation (8) retains the conventional leading minus sign and yields a negative Poisson’s ratio for lateral contraction under axial compression.
The energy absorbed by the structure up to the onset of densification (EA) was calculated by integrating the compressive load over the corresponding displacement interval, as follows:
EA = ∫ 0 δ d F ( δ ) d δ
The onset of densification was identified at the displacement associated with the last local maximum in the EAE curve. EAE was determined using the following equation:
EAE = ∫ 0 ε d F ( ε ) d ε F ( ε )
The densification strain εd is ultimately determined from the EAE curve, where εd corresponds to the last extremum point of the EAE curve.
To enable comparisons between specimens of different masses, the energy absorbed per unit mass was quantified using SEA, defined by the following equation:
SEA = EA m

3. Results

3.1. Deformation Behavior

In the deformation analysis, the longitudinal direction is aligned with the compression axis, whereas the lateral direction lies perpendicular to it within the structural plane. Figure 8 and Figure 9 document the progressive deformation of the 2D RE and 2D SSRE structures under quasi-static compression, demonstrating close correspondence between the experimentally observed and numerically predicted deformation patterns.
Figure 8. Deformation characteristics of the 2D RE structure during compression.
Figure 9. Deformation characteristics of the 2D SSRE structure during compression.
The deformation sequence in Figure 8 begins with an elastic response of the 2D RE structure, characterized by nearly symmetric inward contraction along its two sides. Mild lateral buckling emerges at a compressive strain of 0.1, followed by progressively greater deformation of the upper and lower cell regions and an increasingly pronounced lateral tilt as compression continues.
At a nominal strain of 0.1, the experimentally observed deformation pattern of the 2D SSRE structure shows a slight deviation from the numerical prediction, as illustrated in Figure 9. The simulation predicts an overall inward contraction, whereas the experimental specimen exhibits pronounced cell-wall buckling in the top cells in addition to the overall inward contraction. The observed discrepancy may arise from the uneven distribution of defects generated during additive manufacturing. At a nominal strain of 0.2, the simulated deformation pattern closely matches the experimental observations, with both results showing greater deformation in the upper and lower cells than in the central region. With continued compression, the middle cells also undergo substantial deformation, and the structure continues to contract inward while maintaining a relatively symmetric configuration. The structure continues to deform in this manner until the onset of densification.
The deformation sequences indicate that the proposed 2D SSRE structure exhibits a more stable response to quasi-static compression than the conventional 2D RE configuration. Its more coordinated deformation pattern may help maintain progressive structural collapse and sustained energy absorption throughout the compression process.

3.2. Mechanical Performance Analysis

The differences in compressive mechanical behavior between the conventional 2D RE structure and the newly developed 2D SSRE configuration can be evaluated from their respective nominal stress–strain curves in Figure 10. The two repeated compression tests yielded closely matching curves, indicating good experimental repeatability. The finite element predictions reproduce the experimentally observed compression behavior with good agreement, lending additional credibility to the numerical model. For the conventional 2D RE structure, Figure 10a shows that the nominal stress initially rises during elastic deformation before decreasing when the nominal strain reaches roughly 0.06. This reduction in nominal stress can be attributed to the onset of buckling, accompanied by lateral deflection and a loss of symmetry in the deformation of the 2D RE structure. This deformation behavior persists as compression proceeds toward densification.
Figure 10. Experimental and finite element nominal stress–strain responses under compression: (a) 2D RE and (b) 2D SSRE. Two specimens were tested for each configuration (n = 2). The vertical dashed lines indicate the transitions between the deformation stages, and the green vertical line indicates the stiffness change in the 2D SSRE structure.
During the early stage of compression, the 2D SSRE structure exhibits an almost proportional increase in nominal stress with increasing strain, as indicated by the response curve in Figure 10b. The stress response reaches its plateau when the nominal strain reaches roughly 0.055. This transition is accompanied by bending and rotation of the inclined cell walls, together with the formation of plastic hinges near their ends. This relatively stable stress response persists up to a strain of approximately 0.3. Beyond this point, the stress–strain curve becomes progressively steeper as the outer re-entrant cells continue to deform inward, eventually bringing the horizontal walls of the outer and inner cells into contact. Further compression requires the inclined walls of both cell levels to undergo additional rotation and bending, increasing the structural resistance to deformation. Consequently, the nominal stress rises more rapidly with increasing strain. At a strain of approximately 0.45, a pronounced rise in nominal stress indicates the beginning of the densification stage.
Force-displacement data for both the 2D RE and 2D SSRE structures were obtained from experiments and finite-element simulations. Using Equation (9), the total energy absorption (EA) curves of both structures were calculated. These were then divided by the respective specimen masses, as expressed in Equation (11), to obtain the specific energy absorption (SEA) curves. Subsequently, Equation (10) was applied to derive the energy absorption efficiency (EAE) curves for both structures. The last extremum point of each EAE curve corresponds to the nominal strain at densification (densification strain). The SEA values at these respective densification strains were then identified from the SEA curves.
The amount of energy accumulated during compression prior to the onset of densification provides a basis for assessing the energy-absorbing performance of cellular structures. Figure 11 compares the variation in SEA with nominal strain for the 2D RE and 2D SSRE structures, with asterisks marking the SEA values corresponding to their respective densification points. For the conventional 2D RE structure, the SEA obtained experimentally was 0.398 J/g, compared with 0.416 J/g predicted by the numerical model, yielding a relative error of approximately 4.52% (Figure 11a). In contrast, the 2D SSRE structure exhibited experimental and numerical SEA values of 1.368 and 1.242 J/g, respectively, with a corresponding deviation of approximately 9.21% (Figure 11b).
Figure 11. Experimental and finite element specific energy absorption (SEA) versus nominal compressive strain: (a) 2D RE and (b) 2D SSRE. Two specimens were tested for each configuration (n = 2). The experimental SEA values reported in the text are the means of the values obtained at the respective densification points of the two tests. At the beginning of compression, the Poisson’s ratios of the conventional 2D RE and newly developed 2D SSRE configurations are roughly −1.1 and −0.52, respectively. The greater negative magnitude observed for the former indicates a more pronounced initial auxetic effect. Figure 12 shows the variation in Poisson’s ratio with nominal compressive strain, as obtained from the finite element simulations of the baseline 2D RE and 2D SSRE configurations. This difference may be attributed to the greater resistance to inward contraction of the 2D SSRE structure, which involves the deformation of more cell walls even during the initial elastic stage.
Figure 12. Poisson’s ratio versus nominal compressive strain for the baseline 2D RE and 2D SSRE configurations, obtained from finite element simulations.
For each compression test, the specific energy absorption (SEA) was evaluated at the onset of densification. The densification strains were 0.54 and 0.55 for the two 2D RE tests and 0.45 in both 2D SSRE tests. The corresponding densification strains from the finite element simulations were 0.52 for the 2D RE and 0.44 for the 2D SSRE. The SEA values obtained at these points were averaged over the two tests for each configuration. The resulting mean SEA was 1.368 J/g for the 2D SSRE and 0.398 J/g for the 2D RE, corresponding to a 243.72% increase for the tested 2D SSRE configuration. The densification strains were 0.54 and 0.55 in the two 2D RE tests and 0.45 in both 2D SSRE tests. For each configuration, the SEA values at the respective densification points were averaged over the two tests. The mean SEA was 1.368 J/g for the 2D SSRE and 0.398 J/g for the 2D RE, corresponding to a reported increase of 243.72% for the tested 2D SSRE configuration. This increase refers to the two tested configurations, which differed in relative density.
Despite its stronger initial auxetic response, the 2D RE structure shows a substantial increase in Poisson’s ratio with continued compression, while the 2D SSRE structure maintains a comparatively steady Poisson’s ratio. This divergence is associated with the instability and lateral tilting of the 2D RE structure, which weaken its auxetic response. By comparison, the 2D SSRE configuration exhibits a relatively stable negative Poisson’s ratio. The progressive deformation and eventual contact of the internal supporting walls help coordinate the inward contraction of the 2D SSRE structure, thereby contributing to its deformation stability. At higher strains, its Poisson’s ratio gradually increases as the available space for further inward contraction becomes increasingly restricted.

3.3. Comparison at Matched Relative Density

To compare the two designs at the same relative density, an additional 2D RE finite element model was constructed by increasing the wall thickness of the baseline 2D RE model. Its relative density was 0.365, matching that of the baseline 2D SSRE model. Figure 13 shows the geometries and dimensions of the three models.
Figure 13. Geometrical dimensions of the 2D RE structure; 2D RE structure (Identical relative density) and 2D SSRE structure.
Figure 14 shows the predicted deformation sequence of the density-matched 2D RE model. Despite its thicker walls, this model still tilted laterally during compression.
Figure 14. Deformation characteristics of the 2D RE structure (Identical relative density) during compression.
Figure 15 compares the predicted nominal stress–strain and SEA responses of the three models. The density-matched 2D RE exhibited a higher initial peak stress than the baseline 2D RE, followed by a decline in nominal stress as lateral tilting developed (Figure 15a). It reached densification at a nominal compressive strain of 0.30, compared with 0.44 for the baseline 2D SSRE. The corresponding SEA curves are shown in Figure 15b.
Figure 15. Comparison of 2D RE structure; 2D RE structure (Identical relative density) and 2D SSRE structure: (a) Nominal stress–strain and (b) SEA. The vertical dashed lines in (a) indicate the onset of densification for the corresponding structures.
Table 1 summarizes the masses, relative densities, densification strains, and SEA values of the three models. At their respective densification points, the density-matched 2D RE and baseline 2D SSRE achieved predicted SEA values of 1.069 and 1.242 J/g, respectively. This corresponds to approximately 16% higher SEA for the 2D SSRE in the matched-density simulations.
Table 1. Comparison of 2D RE structure; 2D RE structure (Identical relative density) and 2D SSRE structure.

4. Discussion

A systematic parametric investigation involving five geometric variables was performed to clarify their influence on the deformation patterns and mechanical response of the 2D SSRE structure during quasi-static compression, with particular consideration given to potential engineering applications. The selected parameters were the outer and inner re-entrant angles (θ1 and θ2), defined between the respective inclined cell walls and the horizontal axis; wall thickness (t); and the outer and inner height-to-length ratios (H1/L1 and H2/L2), representing the cell heights relative to their corresponding horizontal wall lengths. The two ratios were adjusted independently by varying H1 and H2, respectively, while maintaining constant values of l1 and l2. The geometric variations considered in this section may also change the relative density. The resulting trends therefore describe the configurations as modeled and should not be interpreted as comparisons at constant relative density.

4.1. Effect of θ1

As shown in Figure 16, the three 2D SSRE structures with different θ1 values exhibit inward contraction on both sides at a strain of 0.1, while maintaining a relatively symmetric overall deformation pattern. At a strain of 0.2, differences in the deformation modes become apparent. For θ1 = 55° and 65°, buckling first occurs in the top and bottom cells, with more pronounced deformation observed at θ1 = 55°. At smaller values of θ1, the increased horizontal moment arm may promote buckling of the outer re-entrant cells’ inclined walls during compression. In contrast, the initial deformation occurs in the middle layer when θ1 reaches 75°. As compression proceeds, all three structures exhibit an overall inward contraction pattern while maintaining relatively good symmetry and deformation stability.
Figure 16. Deformation characteristics and stress distributions in 2D SSRE configurations with different outer re-entrant angles (θ1).
The influence of θ1 on the nominal stress–strain response and EAE of 2D SSRE structures is examined using the curves in Figure 17a. The asterisks identify the densification points determined from the final peak of the EAE curves. Increasing θ1 produces only minor changes in the stress plateau and densification strain, while the plateau stress exhibits a slight upward trend. Meanwhile, a gradual improvement in EAE is observed as θ1 increases. The SEA-nominal strain curves in Figure 17b exhibit increasingly steep slopes with larger θ1 values. A larger θ1 values therefore contribute to greater energy absorption per unit mass before densification, as indicated by the higher SEA values at the densification onset. Meanwhile, Figure 17c depicts that the Poisson’s ratio remains negative across the investigated compressive strain range for all 2D SSRE configurations, demonstrating their sustained auxetic behavior. Among the three 2D SSRE configurations, the design with θ1 = 65° exhibits the lowest average Poisson’s ratio, indicating the most pronounced overall auxetic behavior. Increasing θ1 from 55° to 65° allows more room for inward deformation, whereas a further increase enlarges the structural width and limits transverse strain under the same longitudinal strain. This reduction in transverse contraction causes the average Poisson’s ratio to approach zero, indicating a less pronounced auxetic effect.
Figure 17. Mechanical responses of 2D SSRE configurations at varying θ1 values: (a) nominal stress–strain curves; (b) specific energy absorption (SEA) versus nominal strain; (c) Poisson’s ratio versus nominal strain. The vertical dashed lines in (a) indicate the onset of densification for the corresponding configurations.

4.2. Effect of θ2

As shown in Figure 18, the three 2D SSRE structures with different θ2 values exhibit inward contraction from both sides at a strain of 0.1, while maintaining relatively symmetric deformation patterns. As compression proceeds, the initial buckling locations vary with θ2. For θ2 = 55°, buckling first occurs in the diagonally adjacent cells in the middle layer, whereas for θ2 = 75°, initial deformation occurs in the cells on both sides of the second layer. Despite these differences in the initial deformation locations, all three structures exhibit an overall inward contraction pattern as compression continues, while maintaining relatively good symmetry and deformation stability.
Figure 18. Deformation behavior and stress distributions of the 2D SSRE structures with different θ2 values.
The compressive responses of 2D SSRE configurations with different inner re-entrant angles (θ2) are compared in Figure 19a in terms of nominal stress–strain behavior and EAE. Both the stress plateau and EAE show relatively little sensitivity to changes in θ2. However, the densification strain decreases as θ2 increases. This behavior can be attributed to the reduced distance between the intermediate nodes of the inner and outer re-entrant cells, which limits the available space for inward contraction and causes densification to occur earlier. Across the different θ2 configurations, SEA exhibits a similar upward trend with increasing nominal strain, as reflected by the curves in Figure 19b. As θ2 increases, SEA at the onset of densification decreases mainly because the plateau region spans a narrower strain interval, while the corresponding stress level changes only slightly. Meanwhile, the Poisson’s ratio remains negative for every configuration throughout the investigated compression range (Figure 19c). An increase in θ2 results in a more negative Poisson’s ratio, indicating an enhancement in the auxetic behavior of the 2D SSRE structure.
Figure 19. Mechanical responses of 2D SSRE structures with varying θ2 values: (a) nominal stress–strain behavior; (b) specific energy absorption (SEA); (c) Poisson’s ratio. The vertical dashed lines in (a) indicate the onset of densification for the corresponding configurations.
Figure 17 and Figure 19 show why the two re-entrant angles should be examined separately. Over the investigated range, increasing the outer angle (θ1) increased SEA at the onset of densification, with only a small change in densification strain. Increasing the inner angle (θ2), by contrast, reduced the densification strain and SEA at densification while making Poisson’s ratio more negative. A parameter study in which the inner and outer angles are constrained to be equal cannot distinguish these separate effects. These trends apply to the simulated configurations considered here; the comparisons do not isolate the effects of the angles from any accompanying changes in relative density.

4.3. Effect of t

Figure 20 depicts the early-stage compressive deformation of 2D SSRE structures with varying wall thicknesses (t). All configurations undergo inward contraction on both sides, with their overall deformation remaining approximately symmetric. At a strain of 0.2, differences in the deformation modes become apparent. For t = 1.0 mm and 1.2 mm, buckling first occurs in the top and bottom cells, whereas for t = 0.8 mm, the initial deformation occurs in the middle layer. As compression proceeds, all three structures exhibit an overall inward contraction pattern while maintaining relatively good symmetry and deformation stability. When the nominal compressive strain reaches 0.5, the intermediate junctions of the unit cells are the principal regions of stress concentration in the 2D SSRE structure with t = 1.2 mm. These nodes connect multiple cell walls and are therefore prone to stress concentration. As compression continues, contact and interaction between adjacent cell walls may further increase the local stress, making these nodes potential sites for fracture initiation under practical loading conditions.
Figure 20. Deformation characteristics and stress distributions in 2D SSRE structures with varying wall thicknesses (t).
Changes in cell-wall thickness (t) produce noticeable differences in the compressive response of 2D SSRE structures, particularly in plateau stress, densification strain, and energy absorption efficiency (EAE), as reflected by the curves in Figure 21a. As t increases, the plateau stress increases because thicker cell walls require greater compressive loads to undergo buckling deformation. Meanwhile, the densification strain decreases as thicker walls limit the space available for inward contraction, leading to an earlier onset of densification. Thicker cell walls are associated with more pronounced fluctuations in the nominal stress–strain response and a reduction in EAE. At the same time, the SEA-nominal strain curves in Figure 21b become steeper as wall thickness increases, indicating a higher rate of specific energy absorption accumulation during compression.
Figure 21. Mechanical responses of 2D SSRE configurations at varying t values: (a) nominal stress–strain behavior; (b) SEA versus nominal strain; (c) Poisson’s ratio versus nominal strain. The vertical dashed lines in (a) indicate the onset of densification for the corresponding configurations.
A shorter stress plateau and greater load-bearing capacity are observed when the cell-wall thickness increases. The additional energy absorbed at the elevated stress level outweighs the effect of the shortened plateau region, resulting in a higher SEA at the onset of densification. The 2D SSRE structures with different wall thicknesses retain their auxetic behavior over the investigated compressive strain range, as reflected by the consistently negative Poisson’s ratios in Figure 21c. Increasing t reduces the available internal clearance, leading to earlier contact between neighboring cell walls during compression and a gradual weakening of the auxetic effect. This premature contact restricts further inward contraction, reducing the magnitude of transverse strain and shifting the Poisson’s ratio toward zero.

4.4. Effect of H1/l1

As shown in Figure 22, the three 2D SSRE structures with different H1/l1 ratios exhibit inward contraction from both sides during the initial stage of compression, while maintaining relatively symmetric deformation patterns. At a strain of 0.2, differences in the deformation modes become apparent. For H1/l1 = 0.75 and 0.875, buckling first occurs in the top and bottom cells, with more pronounced deformation observed at H1/l1 = 0.875. An increase in H1/l1 may lengthen the inclined walls of the outer re-entrant cells, thereby extending their horizontal moment arms and increasing their susceptibility to buckling during compression. Consequently, deformation initiates in the top and bottom cells. In contrast, the structure with H1/l1 = 0.625 initially deforms in the middle layer. As compression proceeds, all three structures exhibit an overall inward contraction pattern while maintaining relatively good symmetry and deformation stability.
Figure 22. Deformation behavior and stress distributions of the 2D SSRE structures with different H1/l1 values.
The nominal stress–strain and EAE curves in Figure 23a characterize the compressive response of the 2D SSRE structure at different outer height-to-length ratios (H1/l1). Increasing H1/l1 leads to a substantial rise in densification strain, whereas the plateau stress and energy absorption efficiency remain relatively unaffected. This trend may be explained by the increased internal space available for inward contraction at higher H1/l1 ratios, allowing the stress plateau stage to extend and delaying the onset of densification. As shown in Figure 23b, changes in H1/l1 have a limited effect on the increasing slope of the SEA-nominal strain curves, consistent with the relatively small differences in the early-stage stress plateaus. However, a larger H1/l1 ratio extends the stress plateau stage and results in a higher stress at the densification point. Consequently, the SEA at densification increases substantially with increasing H1/l1. Negative Poisson’s ratios are consistently observed for the three 2D SSRE structures over the examined range of nominal compressive strain, confirming their auxetic characteristics (Figure 23c). Larger H1/l1 ratios are associated with more negative Poisson’s ratios in the 2D SSRE structure, potentially because the increased clearance within the supporting cells facilitates greater inward deformation under compression.
Figure 23. Influence of H1/l1 on the mechanical response of 2D SSRE structures: (a) nominal stress–strain curves; (b) SEA versus nominal strain; (c) Poisson’s ratio versus nominal strain. The vertical dashed lines in (a) indicate the onset of densification for the corresponding configurations.

4.5. Effect of H2/l2

As shown in Figure 24, the three 2D SSRE structures with different H2/l2 ratios exhibit inward contraction from both sides during the initial stage of compression, while maintaining relatively symmetric deformation patterns. At a strain of 0.2, differences in the deformation modes become apparent. For H2/l2 = 0.625 and 0.75, buckling first occurs in the top and bottom cells, with more pronounced deformation observed at H2/l2 = 0.625. This behavior may be attributed to the longer inclined connecting walls between the inner and outer re-entrant cells at smaller H2/l2 ratios. The relatively long horizontal moment arms of these walls increase their tendency to buckle during compression, causing deformation to initiate in the upper and lower cells. In contrast, the structure with H2/l2 = 0.875 initially deforms in the middle layer. As compression proceeds, all three structures exhibit an overall inward contraction pattern while maintaining relatively good symmetry and deformation stability.
Figure 24. Deformation patterns and stress distributions in 2D SSRE structures with varying H2/l2 values.
The dependence of the 2D SSRE structure’s nominal stress–strain response and EAE on the H2/l2 ratio is examined using the curves in Figure 25a. The results reveal that changes in H2/l2 have only a minor effect on the densification point, which remains nearly constant across the different ratios. A higher H2/l2, however, is associated with lower plateau stress but greater energy absorption efficiency. The SEA-nominal strain curves in Figure 25b become less steep as the H2/l2 ratio increases, indicating a slower rise in SEA during compression. With only minor differences in densification strain, the combination of higher plateau stress and lower structural mass at smaller H2/l2 ratios contributes to greater SEA when densification begins. The Poisson’s ratio data in Figure 25c remain negative for all 2D SSRE configurations over the investigated compressive strain range, demonstrating sustained auxetic behavior. However, larger H2/l2 ratios produce more negative Poisson’s ratios, reflecting a stronger auxetic response. This improvement may arise from the increased length of the inner inclined cell walls, which interact with the outer re-entrant walls to promote inward deformation and increase the magnitude of transverse contraction.
Figure 25. Influence of H2/l2 on the mechanical response of 2D SSRE structures: (a) nominal stress–strain curves; (b) SEA versus nominal strain; (c) Poisson’s ratio versus nominal strain. The vertical dashed lines in (a) indicate the onset of densification for the corresponding configurations.

4.6. Engineering Implications and Applicability to Other Sizes and Geometries

A potential application of the 2D SSRE structure is as a lightweight energy-absorbing core subjected to in-plane quasi-static compression. For a core with a prescribed compression stroke or load limit, candidate geometries should be assessed not only by their SEA at the onset of densification, but also by the load sustained and the energy absorbed within the available stroke. Within the investigated ranges, the finite element results showed that increasing the outer height-to-length ratio (H1/l1) delayed densification and increased SEA at its onset. This ratio is therefore a parameter to examine when a larger usable strain before densification is needed. Increasing the wall thickness also increased SEA at the onset of densification, but it raised the plateau stress and caused densification to occur earlier. A thicker-walled design is therefore not necessarily preferable when the allowable compressive load is limited. These numerical trends can guide the initial screening of candidate core geometries. Component-level performance should be verified under the intended loading and boundary conditions, and impact applications would require separate dynamic validation.
For a different cell size with the same 2D SSRE topology, a starting point is to retain the re-entrant angles and the dimensionless geometric ratios (H1/l1), (H2/l2), (l2/l1), (t/l1), and (b/l1). This preserves the nominal geometry of the repeating unit but does not establish that its compressive response is independent of size. Increasing the overall specimen size by adding more cells is also distinct from scaling all cell dimensions: the number of cells adjacent to the loading platens or free edges changes relative to the total number of cells. At smaller scales, the minimum printable wall thickness and manufacturing deviations may also limit how closely the nominal geometry can be reproduced. For a new specimen size, the collapse pattern, densification strain, and SEA should therefore be reassessed under the intended loading and boundary conditions.
For a different cell topology, the design procedure is more transferable than the specific parameter trends. A candidate geometry can be evaluated by examining how wall bending and rotation, local buckling, and wall contact affect progressive collapse, and by comparing SEA at the onset of densification together with the evolution of Poisson’s ratio during compression. Where the aim is to isolate the effect of topology, comparisons should be made at matched relative density where feasible, or the density differences should be reported explicitly. The numerical trends observed for the present 2D SSRE structure can guide the selection of candidate geometries, but their magnitude and direction should not be assumed to hold for other topologies without further evaluation.

5. Conclusions

A two-dimensional self-similar re-entrant (2D SSRE) structure was designed and fabricated through three-dimensional printing. Its mechanical response under quasi-static compression was evaluated using experiments and finite element simulations, with a conventional 2D RE structure as the reference. The effects of geometric variations were further investigated through a parametric analysis. The principal findings of this investigation can be outlined as follows:
(1) The finite element predictions agreed well with the measured compressive responses of the baseline 2D RE and 2D SSRE configurations. The 2D SSRE exhibited more stable deformation during quasi-static compression. The mean SEA values, evaluated at the respective densification points, were 1.368 J/g for the tested 2D SSRE and 0.398 J/g for the tested 2D RE. The reported increase of 243.72% applies to these two tested configurations, which differed in relative density. In a separate finite element comparison at a matched relative density of 0.365, the 2D SSRE achieved approximately 16% higher SEA than the thicker-walled 2D RE at their respective densification points.
(2) Within the investigated parameter ranges, the finite element results showed that increasing the outer re-entrant angle, wall thickness, or outer height-to-length ratio increased SEA at the onset of densification, whereas increasing the inner re-entrant angle or inner height-to-length ratio reduced it. Wall thickening increased SEA but made the Poisson’s ratio less negative. In contrast, increasing the outer height-to-length ratio increased SEA and made the Poisson’s ratio more negative over the range investigated. These trends were obtained numerically for the geometries considered and were not independently validated by compression tests on the modified configurations.

Author Contributions

Conceptualization, B.L.; methodology, B.L.; software, B.L.; validation, S.M. and L.H.; formal analysis, B.L. and Q.L.; investigation, B.L., S.M. and L.H.; data curation, B.L., S.M. and Q.L.; writing—original draft preparation, B.L.; writing—review and editing, S.M. and J.W.; visualization, B.L. and Q.L.; supervision, J.W.; project administration, J.W.; funding acquisition, J.W. All authors have read and agreed to the published version of the manuscript.

Funding

This work was supported by the Shandong Provincial Key Research and Development Program (Grant No. 2024****0305), the Shandong Provincial Natural Science Foundation of China (Grant No. ZR2023ME150), and the National Natural Science Foundation of China (Grant No. U24A20123).

Institutional Review Board Statement

Not applicable.

Data Availability Statement

The raw data supporting the conclusions of this article will be made available by the authors on request.

Conflicts of Interest

The authors declare no conflicts of interest. The funders had no role in the design of the study; in the collection, analyses, or interpretation of data; in the writing of the manuscript; or in the decision to publish the results.

References

  1. Almgren, R.F. An isotropic three-dimensional structure with Poisson’s ratio = −1. J. Elast. 1985, 15, 427–430. [Google Scholar] [CrossRef] [Scilit]
  2. Lakes, R. Foam Structures with a Negative Poisson’s Ratio. Science 1987, 235, 1038–1040. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  3. Wojciechowski, K.W. Two-dimensional isotropic system with a negative poisson ratio. Phys. Lett. A 1989, 137, 60–64. [Google Scholar] [CrossRef] [Scilit]
  4. Evans, K.E. Auxetic polymers: A new range of materials. Endeavour 1991, 15, 170–174. [Google Scholar] [CrossRef] [Scilit]
  5. Milton, G.W. Composite materials with poisson’s ratios close to—1. J. Mech. Phys. Solids 1992, 40, 1105–1137. [Google Scholar] [CrossRef] [Scilit]
  6. Balan P, M.; Mertens A, J.; Bahubalendruni, M.V.A.R. Auxetic mechanical metamaterials and their futuristic developments: A state-of-art review. Mater. Today Commun. 2023, 34, 105285. [Google Scholar] [CrossRef] [Scilit]
  7. Francisco, M.B.; Pereira, J.L.J.; Oliver, G.A.; Roque da Silva, L.R.; Cunha, S.S.; Gomes, G.F. A review on the energy absorption response and structural applications of auxetic structures. Mech. Adv. Mater. Struct. 2022, 29, 5823–5842. [Google Scholar] [CrossRef] [Scilit]
  8. Siniauskaya, V.; Wang, H.; Liu, Y.; Chen, Y.; Zhuravkov, M.; Lyu, Y. A review on the auxetic mechanical metamaterials and their applications in the field of applied engineering. Front. Mater. 2024, 11, 1453905. [Google Scholar] [CrossRef] [Scilit]
  9. Choudhry, N.K.; Panda, B.; Kumar, S. In-plane energy absorption characteristics of a modified re-entrant auxetic structure fabricated via 3D printing. Compos. Part B Eng. 2022, 228, 109437. [Google Scholar] [CrossRef] [Scilit]
  10. Choudhry, N.K.; Panda, B.; Kumar, S. Enhanced energy absorption performance of 3D printed 2D auxetic lattices. Thin-Walled Struct. 2023, 186, 110650. [Google Scholar] [CrossRef] [Scilit]
  11. Teng, X.C.; Ren, X.; Zhang, Y.; Jiang, W.; Pan, Y.; Zhang, X.G.; Zhang, X.Y.; Xie, Y.M. A simple 3D re-entrant auxetic metamaterial with enhanced energy absorption. Int. J. Mech. Sci. 2022, 229, 107524. [Google Scholar] [CrossRef] [Scilit]
  12. Zhang, X.; Hao, H.; Tian, R.; Xue, Q.; Guan, H.; Yang, X. Quasi-static compression and dynamic crushing behaviors of novel hybrid re-entrant auxetic metamaterials with enhanced energy-absorption. Compos. Struct. 2022, 288, 115399. [Google Scholar] [CrossRef] [Scilit]
  13. Jiang, F.; Yang, S.; Qi, C.; Ding, C. Quasi-static crushing response of additive manufactured 3D reentrant circular auxetics with different polymer matrices. Mech. Adv. Mater. Struct. 2023, 30, 3826–3846. [Google Scholar] [CrossRef] [Scilit]
  14. Zhou, J.; Dong, C.; Chen, B.; Qin, R.; Li, D. Out-of-plane crushing performances of cell-based hierarchical honeycombs based on the evaluation criteria for ideal energy absorption. Thin-Walled Struct. 2023, 182, 110246. [Google Scholar] [CrossRef] [Scilit]
  15. Ma, N.; Han, Q.; Han, S.; Li, C. Hierarchical re-entrant honeycomb metamaterial for energy absorption and vibration insulation. Int. J. Mech. Sci. 2023, 250, 108307. [Google Scholar] [CrossRef] [Scilit]
  16. He, Y.; Zhang, X.; Sun, J.; Shu, X.; Li, X.; Su, B.; Xiao, G. Energy absorption of self-similar inspired multi-cell hexagonal tubes. Eng. Struct. 2023, 277, 115455. [Google Scholar] [CrossRef] [Scilit]
  17. Liu, H.; Zhang, E.T.; Ng, B.F. In-plane dynamic crushing of a novel honeycomb with functionally graded fractal self-similarity. Compos. Struct. 2021, 270, 114106. [Google Scholar] [CrossRef] [Scilit]
  18. Wang, S.; Liu, H.-T. Quasi-static compression response of a novel multi-step auxetic honeycomb with tunable transition strain. Aerosp. Sci. Technol. 2024, 155, 109730. [Google Scholar] [CrossRef] [Scilit]
  19. Zhou, J.; Wang, Y.; Luo, H.; Zhao, G.; Chen, J.; Cui, Y.; Wang, L.; Gao, Q.; Wang, X. Energy absorption of auxetic honeycomb with graded beam thickness based on Bezier curve. Aerosp. Sci. Technol. 2024, 155, 109619. [Google Scholar] [CrossRef] [Scilit]
  20. Qi, C.; Jiang, F.; Yang, S.; Remennikov, A. Multi-scale characterization of novel re-entrant circular auxetic honeycombs under quasi-static crushing. Thin-Walled Struct. 2021, 169, 108314. [Google Scholar] [CrossRef] [Scilit]
  21. Wei, L.; Zhao, X.; Yu, Q.; Zhang, W.; Zhu, G. In-plane compression behaviors of the auxetic star honeycomb: Experimental and numerical simulation. Aerosp. Sci. Technol. 2021, 115, 106797. [Google Scholar] [CrossRef] [Scilit]
  22. Jiang, F.; Yang, S.; Ding, C.; Qi, C. Quasi-static crushing behavior of novel circular double arrowed auxetic honeycombs: Experimental test and numerical simulation. Thin-Walled Struct. 2022, 177, 109434. [Google Scholar] [CrossRef] [Scilit]
  23. Zhu, Y.; Luo, Y.; Gao, D.; Yu, C.; Ren, X.; Zhang, C. In-plane elastic properties of a novel re-entrant auxetic honeycomb with zigzag inclined ligaments. Eng. Struct. 2022, 268, 114788. [Google Scholar] [CrossRef] [Scilit]
  24. Yu, S.; Liu, Z.; Cao, X.; Liu, J.; Huang, W.; Wang, Y. The compressive responses and failure behaviors of composite graded auxetic re-entrant honeycomb structure. Thin-Walled Struct. 2023, 187, 110721. [Google Scholar] [CrossRef] [Scilit]
  25. Hu, Q.; Lu, G.; Tse, K.M. Compressive and tensile behaviours of 3D hybrid auxetic-honeycomb lattice structures. Int. J. Mech. Sci. 2024, 263, 108767. [Google Scholar] [CrossRef] [Scilit]
  26. Yang, Q.; Li, Z.; Hao, H.; Chen, W. Compressive mechanical properties and dynamic behaviour of origami-inspired tri-directional auxetic metastructure. Eng. Struct. 2023, 281, 115751. [Google Scholar] [CrossRef] [Scilit]
  27. Bai, M.; Wang, Z.; Li, K.; Zhu, W.; Xiang, Z.; Feng, Y.; Hong, Y.; Shen, L.; Wang, D. Additively manufactured self-similar embedded honeycombs with programmable compressive response. J. Manuf. Process. 2026, 177, 580–600. [Google Scholar] [CrossRef] [Scilit]
  28. Shen, L.; Li, T.; Xu, H.; Zeng, J.; Xiang, Z.; Feng, Y.; Bai, M.; Yu, J.; Ye, T. Enhanced mechanical properties of spider web-inspired re-entrant honeycombs. Int. J. Mech. Sci. 2026, 312, 111262. [Google Scholar] [CrossRef] [Scilit]
  29. Choudhry, N.K.; Panda, B.; Dixit, U.S. Energy Absorption Characteristics of Fused Deposition Modeling 3D Printed Auxetic Re-entrant Structures: A Review. J. Mater. Eng. Perform. 2023, 32, 8981–8999. [Google Scholar] [CrossRef] [Scilit]
  30. Nam, R.; Nam, D.; Naguib, H.E. Additive manufactured 3D re-entrant auxetic structures for enhanced impact resistance. Smart Mater. Struct. 2024, 33, 125021. [Google Scholar] [CrossRef] [Scilit]
  31. Nugroho, W.T.; Dong, Y.; Pramanik, A.; Chithirai Pon Selvan, M.; Zhang, Z.; Ramakrishna, S. Additive manufacturing of re-entrant structures: Well-tailored structures, unique properties, modelling approaches and real applications. Addit. Manuf. 2023, 78, 103829. [Google Scholar] [CrossRef] [Scilit]
  32. Ghaemi Khiavi, S.; Mohammad Sadeghi, B.; Divandari, M. Effect of topology on strength and energy absorption of PA12 non-auxetic strut-based lattice structures. J. Mater. Res. Technol. 2022, 21, 1595–1613. [Google Scholar] [CrossRef] [Scilit]
  33. Iantaffi, C.; Bele, E.; McArthur, D.; Lee, P.D.; Leung, C.L.A. Auxetic response of additive manufactured cubic chiral lattices at large plastic strains. Mater. Des. 2023, 233, 112207. [Google Scholar] [CrossRef] [Scilit]
  34. K, M.K.; G, A. Quasi-static compression and energy absorption behaviour of polymeric selective laser sintered open cell lattices under varying relative densities. Rapid Prototyp. J. 2024, 30, 643–661. [Google Scholar] [CrossRef] [Scilit]
  35. Nasim, M.; Galvanetto, U. Mechanical characterisation of additively manufactured PA12 lattice structures under quasi-static compression. Mater. Today Commun. 2021, 29, 102902. [Google Scholar] [CrossRef] [Scilit]
  36. Okubo, S.; Yamauchi, Y.; Kitazono, K. Effects of random and controlled irregularity in strut lattice structure of PA12 on compression anisotropy. Addit. Manuf. 2023, 63, 103385. [Google Scholar] [CrossRef] [Scilit]
  37. Li, B.; Xin, X.; Lin, C.; Liu, L.; Liu, Y.; Leng, J. Compressive properties and energy absorption of 4D printed auxetic mechanical metamaterials. Compos. Struct. 2024, 340, 118135. [Google Scholar] [CrossRef] [Scilit]
  38. Štaffová, M.; Ondreáš, F.; Žídek, J.; Jančář, J.; Lepcio, P. Biaxial porosity gradient and cell size adjustment improve energy absorption in rigid and flexible 3D-printed reentrant honeycomb auxetic structures. Results Eng. 2024, 22, 102249. [Google Scholar] [CrossRef] [Scilit]
  39. Li, T.; Shen, L.; Xu, H.; Yu, J. In-plane quasi-static compressive response and energy absorption mechanisms of vertex-based hierarchical re-entrant honeycombs. Structures 2026, 86, 111430. [Google Scholar] [CrossRef] [Scilit]
  40. Baroutaji, A.; Nikkhah, H.; Arjunan, A.; Pirmohammad, S.; Robinson, J. In-Plane Compressive Responses of Non-Homogenous Re-Entrant Honeycombs Fabricated by Fused Deposition Modelling. Micromachines 2024, 15, 694. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  41. Gao, D.; Zhang, J.; Zhang, C.; You, Y. Dynamic Compressive and Flexural Behaviour of Re-Entrant Auxetics: A Numerical Study. Materials 2023, 16, 5219. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  42. Mazur, E.; Shishkovsky, I. Additively Manufactured Hierarchical Auxetic Mechanical Metamaterials. Materials 2022, 15, 5600. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  43. Széles, L.; Horváth, R.; Cveticanin, L. Analysis of Mechanical Properties and Parameter Dependency of Novel, Doubly Re-Entrant Auxetic Honeycomb Structures. Polymers 2024, 16, 2524. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  44. Alomarah, A.; Abbas, A.T.; Faisal, B.; Peng, Z.; Ruan, D. The Effects of Manufacturing Techniques on the Mechanical Performance of an Auxetic Structure Manufactured by Fused Filament Fabrication and Multijet Fusion Processes. Adv. Eng. Mater. 2024, 26, 2302033. [Google Scholar] [CrossRef] [Scilit]
  45. ASTM D412-16; Standard Test Methods for Vulcanized Rubber and Thermoplastic Elastomers—Tension. ASTM International: West Conshohocken, PA, USA, 2021.
Disclaimer/Publisher’s Note: The statements, opinions and data contained in all publications are solely those of the individual author(s) and contributor(s) and not of MDPI and/or the editor(s). MDPI and/or the editor(s) disclaim responsibility for any injury to people or property resulting from any ideas, methods, instructions or products referred to in the content.

Article Metrics

Citations

Article Access Statistics