Abstract
Basalt fiber-reinforced asphalt concrete (BFAC) is used in hydraulic anti-seepage structures, where sustained loading and temperature variations can compromise deformation control. This study combines triaxial creep tests with discrete element simulations to examine the effects of basalt fiber (BF), temperature, confining pressure, fiber length, and fiber content on creep and contact-scale load transfer. Under −4 °C, 0.4 MPa confining pressure and 1.5 MPa axial stress, addition of BF reduced the average creep rate from 3.55 × 10−6 s−1 to 3.21 × 10−6 s−1, a descriptive reduction of 9.58%, and increased the number of modeled contact force chains from 12,398 to 15,838 (27.75%). Increasing the confining pressure suppressed creep deformation and produced a denser modeled contact network; at 8 °C, the contact count increased from 7207 to 12,110 (68.0%) as the confining pressure increased from 0 to 0.6 MPa. In the numerical model, higher temperatures increased creep deformation through temperature-dependent viscoelastic softening of asphalt mastic; the strengths of the mastic-aggregate and mastic-fiber parallel bonds did not vary with temperature. Parametric simulations suggest that longer fibers and higher contents delayed the attainment of a common strain threshold; however, the curves crossed and no configuration had the lowest strain at every time. The 9 mm, 0.4% configuration should therefore be considered as the most favorable of the numerically investigated configurations rather than a universally optimal mixture. Only the 9 mm, 0.4% configuration was examined physically. The findings support comparative analysis of hydraulic anti-seepage materials, but long-term extrapolation requires longer experiments and three-dimensional model validation.