Abstract
In this work, cyclic voltammetry, square wave voltammetry, and chronopotentiometry were employed to systematically investigate the electrochemical behavior of O2− in LiF–BeF2 (66.7: 33.3 mol%) (FLiBe) molten salt on a gold electrode. Comparative analysis demonstrated that square wave voltammetry is more suitable than cyclic voltammetry for studying the electrochemical behavior of O2−. The square wave voltammetry results confirmed that O2− is oxidized to O2, with the electrode reaction controlled by ion diffusion. chronopotentiometry confirmed that the electrochemical behavior of O2− obeyed the Sand law. The diffusion coefficient of O2− in FLiBe by chronopotentiometry followed Arrhenius’ law. Then, a well-fitted linear relationship between O2− concentration and square wave voltammetry peak current density was established, enabling rapid determination and real-time monitoring of oxide content in an unknown FLiBe molten salt. Furthermore, the electrochemical deoxygenation of FLiBe was performed using the potentiostatic electrolysis technique, and a satisfactory removal efficiency of O2− was achieved. This study presents an in situ electrochemical quantitative analysis method to monitor the O2− concentration in FLiBe, overcoming the drawback of the long testing cycle in conventional chemical analysis. Meanwhile, this study provides new technical support for the deoxygenation and purification of the fuel salt in molten salt reactors.
1. Introduction
Fission nuclear energy, due to its high energy density, low carbon emissions, and potential for sustainable development, has become a candidate for the main clean energy source in the coming decades [1]. The molten salt reactor (MSR) has been selected as one of the six advanced fourth-generation nuclear reactors [2]. MSR has unique advantages such as inherent safety, flexible fuel-cycle characteristics, efficient transmutation of actinide elements, high thermal power density, easy realization of small-scale modularization, and less radioactive waste [3,4,5]. As the only fourth-generation reactor that uses liquid fuel, MSR adopts fluoride molten salt systems as both coolant and fuel salt due to their excellent nuclear physical properties, outstanding thermohydraulic properties, and good chemical stability [6,7].
In the Molten Salt Reactor Experiment (MSRE) and Molten Salt Breeder Reactor (MSBR) programs by Oak Ridge National Laboratory (ORNL), LiF–BeF2–ZrF4–UF4 (65–29.1–5–0.9 mol%) and LiF–BeF2–ThF4–UF4 (71.7–16–12–0.3 mol%) were used as primary fuel systems, respectively [8,9]. Recently, a 2 MWt liquid-fuel thorium molten salt experimental reactor (TMSR-LF1) led by Shanghai Institute of Applied Physics, Chinese Academy of Sciences (SINAP@CAS), has successfully realized thorium–uranium fuel conversion in the LiF–BeF2–ZrF4–ThF4–UF4 system [10]. Therefore, LiF–BeF2 (FLiBe) is the most important fuel carrier medium and coolant for MSR.
Nevertheless, fluoride salt raw materials readily absorb trace moisture from air even under low-humidity conditions [11]. The adsorbed water undergoes hydrolysis at high temperatures (Equation (1)) [12], yielding reactive oxide ions (O2−). In addition, the corrosion of the oxide passivation layer on the inner surface of the structural material also leads to an increase in the O2− content in the molten salt. Meanwhile, the active oxide can be produced through the neutron irradiation of fuel salt and the alpha-ray irradiation of carbon moderator [13]. Furthermore, the fatigue damage of loop or welding parts may bring in air and oxygen as well [14,15]. Therefore, the source of impurity O2− in MSR is extensive, and O2− has become one of the most typical impurities in fluoride molten salts.
O2− exhibits extremely high chemical activity in molten fluoride salts. Metal ions in the molten salts are highly sensitive to O2−, and the interactions between metal ions and O2− occur at high temperatures to form diverse oxide and oxyfluoride species, e.g., the fuel UF4 and ThF4 tends to combine with O2− to form insoluble oxygen-containing compounds, such as oxides (UO2, ThO2) and oxyfluorides ((UOF2)n and (ThOF2)n). These precipitates feature low solubility, high melting point, and high density compared with the molten salt medium. Continuous accumulation of nuclear fuel precipitates not only causes loss of soluble fuel, but also blocks pipelines of fuel circuits, hinders mass transfer, and disrupts the thermal-hydraulic characteristics that enable the reactor to operate stably. More severely, localized enrichment of nuclear fuel precipitates may generate overheating zones, posing severe threats to reactor safety [16]. Accordingly, strict control of oxide impurity content in fluoride salts is essential.
ORNL proposed that bubbling treatment with HF/H2 mixed gas serves as an effective approach to eliminate O2− from fluoride molten salts in MSRE and MSBR programs. Specifically, HF/H2 mixed gas with a molar ratio of 1:10 is sparged into molten salts. O2− reacts with HF to generate water vapor, thereby reducing the oxide content, as illustrated in Equation (2). Via this method, ORNL successfully controlled the oxide impurity content below 700 ppm in LiF–BeF2–ZrF4–UF4 molten salt (65–29.1–5–0.9 mol%) at 650 °C [17], and D. A. Petti et al. [18] further reduced the oxide content of FLiBe to 560 ppm. V. Afonichkin et al. [19] adopted ammonium bifluoride (NH4HF2) to replace HF for the purification of the LiF–ThF4–UF4 system and achieved favorable deoxidation performance, and the corresponding reaction is presented in Equation (3). Although both HF/H2 bubbling and ammonium bifluoride methods can effectively reduce oxide impurities, their deoxidation capacity is restricted by chemical equilibrium with inherent oxide removal limitations. Moreover, these techniques fail to eliminate trace oxide generated during reactor operation. Consequently, oxide impurities cannot be completely removed from fluoride molten salts. Since O2− cannot be avoided, it is necessary to establish the oxide content standard for the MSR. The maximum oxide content allowed in the TMSR-LF1 fuel salt is 200 ppm.
The precise analysis of oxide content in fluoride molten salts is of great significance for the safe operation of MSRs. ORNL adopted the inert gas fusion method [20], HF–H2 method [21], and the KBrF4 oxidation method [22] for oxide quantification. In the inert gas fusion method, molten fluoride specimens are heated under a high-temperature inert atmosphere, and oxide impurities are converted into carbon dioxide and water vapor, whose contents are quantitatively measured via an infrared detector. In the HF–H2 method, oxide ions react with anhydrous HF and transform into water vapor, and oxide content is calculated according to the generated vapor amount. The KBrF4 oxidation method relies on a redox reaction between molten fluoride salt and KBrF4 at 450 °C, where O2− is oxidized into oxygen gas, and oxide concentration is determined by gas pressure measurement. In recent years, LECO Corporation has developed oxide analyzers based on inert-atmosphere fusion and carbothermal reduction principles. The analyzer has a limit of detection of 0.01 μg for oxide, with analytical accuracy of 0.025 ppm or 0.5% RSD, which satisfies the analytical requirements of oxide content in fluoride salt systems.
However, all the above-mentioned O2− concentration detection methods are based on the online sampling–offline analysis mode, which has shortcomings such as time-consuming sampling, complicated sample preparation, and a long testing cycle. In addition, contamination by impurities during sample storage and transportation may interfere with test results. Moreover, there are issues such as beryllium leakage and high operational risks, making it difficult to meet the real-time monitoring and cleaning analysis requirements of trace oxide impurities in fluoride salt systems. Therefore, it is urgent to develop an in situ analysis method to achieve rapid determination of O2− concentration.
An electrochemical method has been proposed for the investigation of electroactive species because of its quick response and in situ monitoring. Voltammetry has been established as an accurate, in situ technique for measuring the concentration of ions in high-temperature molten salts. Relevant studies have been extensively conducted in chloride and fluoride molten salt systems. In the typical LiCl–KCl eutectic chloride melt, Serp et al. [23] studied the redox behavior of plutonium ions, while Shirai et al. [24] studied the redox and deposition behaviors of uranium and plutonium ions in LiCl–KCl eutectic melts, and determined their relevant thermodynamic parameters. Fang et al. [25] also analyzed the electrode kinetics of UCl3 in LiCl–KCl melt at 773 K via cyclic voltammetry (CV) and square wave voltammetry (SWV), acquiring key uranium kinetic parameters, validating the reliability of voltammetry for actinide speciation analysis in chloride molten salts. For fluoride molten salts, Peng et al. [12] characterized the redox and diffusion behaviors of uranium species in FLiNaK salt via CV and SWV; an electrochemical quantitative analysis method for U(IV) was then established, and the concentration of U(IV) was monitored. Furthermore, Peng et al. [26] also utilized SWV to conduct an analysis of the concentration and stability of chromium species in the FLiNaK (LiF–NaF–KF, 46.5–11.5–42 mol%) molten salt. Zhao et al. [27] investigated the redox characteristics and dissolution stability of actinide ions in FLiBe fuel salt. These studies demonstrate that voltammetric techniques are efficient and reliable for qualitative and quantitative analysis of electroactive species in molten salts.
In recent years, electrochemical detection has attained preliminary progress in oxide monitoring of high-temperature molten salts. Massot et al. [28] investigated the electrochemical behaviors of O2− in binary LiF–NaF molten salt via CV, SWV, and chronopotentiometry (CP). They found that SWV and CP are more suitable for O2− analysis than CV. Unfortunately, their research did not take into account other oxide species in molten salt and did not calibrate the actual concentration of free O2−. Shen et al. [29] systematically explored the electrochemical characteristics of O2− in the FLiNaK molten salt at 600 °C using SWV, and a linear quantitative correlation between the oxidation peak current and O2− concentration was established. However, their research lacks comparisons with other electrochemical analysis methods. Choi et al. [30] proposed that SWV could be used to monitor O2− concentration during the electrochemical reduction of uranium oxide in molten Li2O–LiCl. Manning et al. [31] determined the electrochemical behavior of O2− and O22− in LiF–BeF2–ZrF4 and LiF–BeF2–ThF4 melts by CV, and proved that the oxidation of the two ions was controlled by ion diffusion.
The above findings demonstrate the potential of SWV for O2− detection in molten salts. However, existing studies have notable limitations: most investigations focus on non-beryllium fluoride systems, which are not fully applicable to practical MSR fuel salts. Moreover, previous works lack systematic quantitative calibration, multi-method comparative analysis, and O2− impurity removal technology. To date, no complete studies have reported the electrochemical behavior, precise quantification, and electrolytic elimination of O2− in FLiBe systems, restricting the accurate monitoring and control of oxide impurities for MSR operation.
Against this background, this work systematically investigates O2− electrochemical behaviors in FLiBe salt via CV, SWV, and CP for the first time and establishes a high-precision in situ SWV quantitative method for trace O2−. Furthermore, potentiostatic electrolysis is adopted to achieve efficient removal of O2− impurities. The developed technical system can stabilize oxide content within the safe threshold of TMSR-LF1, eliminate reactor safety risks induced by oxide precipitation, and provide a reliable technical reference for the safe operation and engineering application of MSRs.
In this work, CV, SWV, and CP were employed to systematically study the electrochemical behavior of O2− in FLiBe molten salt. For the first time, the key electrochemical parameters of O2− in the FLiBe system were obtained. Then, the SWV method was employed to establish a quantitative electroanalytical method for O2−. Based on this, the O2− content in the unknown FLiBe molten salt was rapidly determined and monitored in real time. Finally, the constant potential electrolysis technique was employed to effectively remove O2− from the FLiBe system.
2. Experimental
2.1. Experimental Technical Route
Figure 1 illustrates the overall research methodology adopted in this work.
Figure 1.
Overall research methodology for this study.
2.2. Preparation of High Purity FLiBe Molten Salt
Due to the inherent hygroscopicity of fluoride salts, the FLiBe preparation process requires strict standards for deoxygenation and purification. The detailed preparation process of high-purity FLiBe molten salt used in this work is described as follows.
The raw materials, LiF (99.9%; Sigma Aldrich; Burlington, MA, USA) and BeF2 powders (99.9%; Alfa Aesar; Ward Hill, MA, USA), were placed in a high-purity nickel crucible and vacuum-dried at 300–400 °C to remove trace adsorbed free water, thereby eliminating oxide impurities introduced during the subsequent melting process. Subsequently, the pretreated LiF and BeF2 were accurately weighed at a molar ratio of 66.7:33.3 and completely melted at 650 °C. During the melting process, high-purity Ar gas (99.999%; Shanghai Louyang Gas Filling Co., Ltd., Shanghai, China) and H2/HF mixed gas (10:1 mol; Shanghai Louyang Gas Filling Co., Ltd., Shanghai, China) with constant pressure and flow rate were continuously purged into the molten salt to further eliminate residual water and oxide impurities. After purification was complete, the HF gas supply was terminated first, and the molten salt was continuously purged with ultra-pure H2 for 2–4 h to remove metallic impurity ions and trace dissolved HF in the molten salt. Following H2 purging, dry Ar gas was adopted to further remove the residual HF and H2 from the molten salt. After the preparation procedure, the liquid FLiBe molten salt was poured into a high-purity nickel crucible and cooled naturally to room temperature for use. All operations were carried out in a glove box protected by argon gas (99.999%).
2.3. Preparation of Molten Salts with Different O2− Concentrations
Li2O (99.99%; Sigma Aldrich; Burlington, MA, USA) was introduced into the FLiBe molten salt system as the source of O2−. A series of FLiBe molten salts with different O2− concentrations was prepared by adjusting the amount of Li2O. Different amounts of Li2O were added to 40 g of FLiBe molten salt, and the incremental O2− concentration was calculated according to Equation (4).
where [O2−]added is the incremental O2− concentration calculated from the added mass of Li2O; represents the added mass of Li2O; is the total mass of FLiBe molten salt, which was fixed at 40 g throughout the experiments.
Table 1 summarizes the addition amounts of Li2O in FLiBe molten salt. All subsequent electrochemical measurements were performed in the FLiBe–O2− systems listed in Table 1.
Table 1.
O2− concentrations in FLiBe molten salt with different Li2O additions.
2.4. Electrochemical Setup and Measurements
2.4.1. Electrochemical Setup
All the electrochemical experiments were performed in a glove box equipped with an electric furnace and filled with a high-purity Ar atmosphere (99.999% purity). The water and oxygen contents in the glove box were strictly controlled below 0.5 ppm. The schematic diagram of the electrochemical setup used in this study is shown in Figure 2.
Figure 2.
Schematic diagram of the molten salt electrochemical device. (1) Glove box, (2) reactor thermal insulation layer, (3) sampling channel, (4) alumina insulating electrode sleeve, (5) working electrode, (6) reference electrode, (7) water cooling coil let, (8) thermocouple, (9) auxiliary electrode, (10) vitreous carbon crucible with molten salt, (11) electric furnace, (12) alumina insulating sheet, (13) electrochemical workstation, (14) computer and data analysis software (CHI660F).
The prepared high-purity FLiBe salt (40 g) was accurately weighed and loaded into a vitreous carbon crucible (Φ = 50 mm × H 40 mm). Then, the crucible loaded with solid eutectic salt was placed and fixed in a stainless steel protective sleeve, which was further transferred inside the furnace. An alumina sheet was laid at the bottom of the sleeve for insulation. The FLiBe salt was heated by a programmed temperature control until it reached 600 °C, and then kept at this temperature to ensure that the salt was fully melted and remained in a homogeneous molten state. The actual temperature of the system was monitored in real time by a nickel–chromium thermocouple closely attached to the outer wall of the vitreous carbon crucible.
2.4.2. Electrodes
After the molten salt had fully melted and the system had reached a stable state, a three-electrode system was employed to investigate the electrochemical behavior and electrolytic removal of O2−. A gold wire (Φ = 1 mm, 99.99%; Sinopharm Chemical Reagent Co., Ltd., Shanghai, China) was used as the working electrode. The Au electrode exhibits excellent chemical inertness in the high-temperature FLiBe molten salt. Since the oxidation potential of O2− is lower than that of gold, and the oxidation product (O2) does not react with gold at the experimental temperature, the Au electrode is suitable for the electrochemical testing and electrolysis study of O2− in molten salt systems [28,29]. A graphite rod (Φ = 6 mm; Sinopharm Chemical Reagent Co., Ltd., Shanghai, China) was selected as the auxiliary electrode. The large immersion contact area of the graphite auxiliary electrode ensured stable current output. A platinum wire (Φ = 1 mm, 99.99%; Sinopharm Chemical Reagent Co., Ltd., Shanghai, China) was adopted to construct a Pt/PtOx/O2− quasi-reference electrode system [32,33], with a stable potential when the O2− concentration is constant. As shown in Figure 3, under the same O2− concentration condition, the O2− oxidation peak potential measured using the Pt quasi-reference electrode showed no drift within 5 h, indicating the feasibility of using Pt as a reference electrode in this study. After completion of the experiment, the surface area of the working electrode was determined by measuring the immersion depth of the electrode in the molten salt.
Figure 3.
SWV curves of the O2− oxidation in FLiBe–O2− (2.44 × 10−2 mol/kg) molten salt at different durations (0 h, 3 h, 5 h). Scan frequency: 10 Hz; pulse height: 25 mV; step potential: 4 mV; working electrode: Au; reference electrode: Pt; auxiliary electrode: graphite.
2.4.3. Electrochemical Methods
CV, SWV, and CP were utilized to systematically study the electrochemical behavior of O2− in the FLiBe molten salt. Particularly, SWV was employed to establish an electrochemical quantitative analysis method for O2−. The oxide removal from the FLiBe–O2− system was carried out by using the potentiostatic electrolysis method. All the electrochemical measurements were performed on a computer-controlled electrochemical workstation (Type CHI660F, Shanghai Chenhua Instruments Co., Ltd., Shanghai, China). The obtained electrochemical experimental data were processed and analyzed using the professional supporting software (CHI660F) matched with the electrochemical workstation.
2.5. Chemical Analysis Techniques
2.5.1. Determination of Total Oxide Content in Molten Salt via LECO Oxide Analyzer
The total oxide content of the molten fluoride salt was determined using an LECO oxide analyzer (Type RO600, LECO Co., Ltd., St. Joseph, MI, USA), whose structure and testing process schematic diagram are shown in Figure 4. This instrument is based on the inert gas fusion-carbon thermal reduction principle, and the obtained results represent the total oxide content of molten salt samples.
Figure 4.
Schematic diagram of the LECO oxide analyzer.
For LECO testing, approximately 50 mg of powdered molten salt sample was first wrapped with a dedicated tin capsule in a glove box. Then, the encapsulated sample was placed into a special graphite crucible in the instrument and rapidly heated to 2700 °C by current excitation. At this high temperature, the oxide in the molten salt sample would be released and react with carbon in the graphite crucible to generate CO and CO2 gases. The total oxide content was quantitatively calculated according to the infrared detection signals of the generated gases. Prior to testing, the carrier gas was deoxygenated by high-temperature copper wire and further purified by asbestos and anhydrous magnesium perchlorate to remove residual water and CO2, eliminating external oxygen interference. To reduce systematic errors and improve testing accuracy, samples were collected from five different positions of the molten salt for parallel tests, and the average value was adopted as the final result.
In order to verify the accuracy of the LECO oxide analyzer, after addition of different amounts of Li2O into the FLiBe melts, LECO was used to detect the increments of O2−, which should be consistent with the theoretical weighing values. Figure 5 shows the relationship between the theoretical O2− increments vs. detected O2− increments. The slope is approximately equal to 1, which indicates the LECO is reliable for detecting the oxide content in FLiBe salt. Meanwhile, this result also proved that the added Li2O can be completely dissolved in the FLiBe molten salt and fully release O2− ions into the melt.
Figure 5.
Linear relationship between theoretical increments of O2− concentration (calculated by Li2O addition mass) and experimental increments (measured by LECO) in FLiBe molten salt.
2.5.2. Determination of Oxygenated Anions Concentration in Molten Salt via Ion Chromatography
An ion chromatograph (ICS-2100, Dionex, Thermo Scientific, Waltham, MA, USA) was employed to determine the contents of oxygenated anions (e.g., NO3−, PO43−, SO42−) in molten salt samples, and its schematic diagram is shown in Figure 6. Considering the strong matrix interference caused by high-concentration fluoride ions in FLiBe molten salt, standardized pretreatment and column-switching separation procedures were implemented to guarantee accurate detection of trace anionic impurities. The detailed testing procedures are presented as follows. The detailed testing procedures are presented as follows.
Figure 6.
Schematic diagram of the ion chromatography.
(1) Sample preparation: All sampling vessels were pre-cleaned with ultra-pure water and thoroughly dried to prevent external anion contamination. Approximately 0.30–0.50 g of finely ground molten salt powder was accurately weighed and dissolved in ultra-pure water. The solution was diluted to a fixed volume of 25 mL, shaken evenly, and ultrasonically extracted for 40 min to fully release water-soluble oxygenated anions from the molten salt matrix. After standing to settle fine insoluble particles, the clear supernatant was collected for subsequent chromatographic testing.
(2) Pre-separation treatment: High-content fluoride ions in FLiBe molten salt can interfere with target anion separation. To eliminate such matrix interference, a valve-switching pre-separation strategy was adopted. The prepared sample solution was injected into a sulfonic acid ion-exclusion column. By precise control of switching time and flow rate, the majority of fluoride ions were diverted and discharged as waste, while trace target anions were retained and enriched in the concentration column for subsequent high-sensitivity detection.
(3) Separation and detection: The enriched anions on the concentration column were eluted with matched eluent and then delivered to an ion exchange chromatographic column. Target anions were separated based on their distinct retention characteristics and finally detected by a suppressor conductivity detector.
(4) Result analysis: Under stable chromatographic conditions, each anion exhibits a specific retention time for qualitative identification. Within the calibrated linear range, the anion peak area is linearly correlated with its concentration. Based on the pre-established standard curve, the peak areas of sample chromatograms were analyzed via professional software (ICS-2100) to calculate the concentration of each oxygenated anion, and the impurity content in the original molten salt sample was finally converted.
3. Results and Discussion
3.1. Oxide Analysis of Molten Salt
Oxygen element primarily exists in fluoride molten salts in the forms of free O2− and various oxygenated anions (e.g., NO3−, PO43−, SO42−).
The total oxide content in the molten salt was measured using a LECO oxide analyzer, denoted as [O]LECO. The oxygenated anion content was determined via ion chromatography (IC). The oxide concentration derived from all the oxygenated anions was calculated according to the oxide proportion in each oxygenated anion, defined as [O]IC. Consequently, the actual content of free O2− ions in the molten salt, expressed as [O2−], can be obtained by subtracting the oxide in oxygenated anions ([O]IC) from the total oxide content ([O]LECO), as shown in Equation (5).
The oxide analysis results of FLiBe molten salt are presented in Table 2. The total oxide concentration of the molten salt is 1.42 × 10−2 mol/kg; three types of oxygenated anions, namely NO3−, SO42−, and PO43−, were detected, with concentrations of 3.06 × 10−4, 1.25 × 10−4, and 1.05 × 10−4 mol/kg, respectively. After subtracting the total oxide content in these oxygenated anions (1.84 × 10−3 mol/kg), the actual concentration of free O2− in the original FLiBe molten salt was determined to be 1.24 × 10−2 mol/kg.
Table 2.
Oxide content analysis results of the FLiBe molten salt used in this study.
3.2. Electrochemical Behavior of O2− in FLiBe
3.2.1. Cyclic Voltammetry
CV was employed to investigate the electrochemical behavior of O2− in FLiBe molten salt, and the obtained cyclic voltammogram is presented in Figure 7A. It can be seen that the CV of the FLiBe–O2− system is somewhat disturbed by gas bubbling. The anodic run of the CV curve shows that the oxidation current begins to increase at approximately 1.1 V vs. Pt. Obvious signal disturbances emerge on the working curve when the potential rises to 1.2 V vs. Pt, which is presumably associated with gas evolution, indicating that O2− is oxidized to O2 at this potential. Within the potential range of 1.2–2.0 V vs. Pt, the continuous generation of O2 induces intense current disturbances, resulting in baseline drift and peak shape distortion. As shown in the inset of Figure 7A, the position of the oxidation peak is difficult to determine. The interference caused by oxygen bubble evolution severely compromises the accurate calibration of the oxidation peak current with the O2− content. Consequently, CV is not suitable for investigating the electrochemical behavior of O2− in FLiBe molten salt, which greatly limits its application in the electrochemical quantitative analysis of O2−.
Figure 7.
(A) Cyclic voltammogram of the FLiBe–O2− (6.18 × 10−2 mol/kg) molten salt system at a scan rate of 0.1 V/s and T = 600 °C. Inset: local magnified view of the O2− oxidation signal; working electrode: Au; reference electrode: Pt; auxiliary electrode: graphite. (B) Square wave voltammogram of the FLiBe–O2− (2.03 × 10−2 mol/kg) molten salt system. T = 600 °C. Inset: local magnified view of the O2− oxidation peak; scan frequency: 25 Hz; pulse height: 25 mV; step potential: 4 mV; working electrode: Au; reference electrode: Pt; auxiliary electrode: graphite.
3.2.2. Square Wave Voltammetry
SWV, as a high-precision electrochemical analysis technique, was employed to investigate the electrochemical behaviors of O2− in FLiBe molten salt. Figure 7B presents the typical square wave voltammogram of the FLiBe–O2− (2.03 × 10−2 mol/kg) system measured on a gold electrode at 600 °C. A distinct oxidation peak A appears at approximately 1.3 V vs. Pt. Unlike CV results, this oxidation peak exhibits a well-defined peak with a clear shape and peak position, which is hardly affected by the disturbing effects of oxygen. This phenomenon confirms that SWV is more suitable for electrochemical analysis of O2−. Evidently, peak A corresponds to the oxidation of O2−. After 2.1 V vs. Pt, the oxidation current significantly increased, which was attributed to the oxidation and dissolution of the Au working electrode into the molten salt. The oxidation of the Au electrode was also observed in CV when the potential exceeded 2.1 V vs. Pt.
Theoretically, SWV electrochemical analysis is primarily applicable to reversible electrochemical systems, while it can also be extended to systems where the peak current exhibits a linear relationship with the square root of the scanning frequency. In this study, the peak current of O2− gradually increases with increasing signal frequency, as shown in Figure 8. The peak intensity is linear with the square root of the signal frequency in the 10–40 Hz frequency range, and the fitted straight lines pass through the origin, as shown in Figure 9. This result confirms that the oxidation of O2− is controlled by ion diffusion. Therefore, SWV is suitable for further analysis of the FLiBe–O2− electrochemical system.
Figure 8.
Square wave voltammograms of the FLiBe–O2− (2.44 × 10−2 mol/kg) molten salt system at different scan frequencies of 10–40 Hz. T = 600 °C; pulse height: 25 mV; step potential: 4 mV; working electrode: Au; reference electrode: Pt; auxiliary electrode: graphite.
Figure 9.
Linear relationship between the peak current density and the square root of the frequency in the FLiBe–O2− (2.44 × 10−2 mol/kg) molten salt system. T = 600 °C; pulse height: 25 mV; step potential: 4 mV; working electrode: Au; reference electrode: Pt; auxiliary electrode: graphite.
According to the SWV theory, for diffusion-controlled electrochemical processes, the electron transfer number of the electrode reaction can be determined by measuring the half-peak width (W1/2), as shown in Equation (6).
where W1/2 is the half-peak width (V); R is the ideal gas constant (8.314 J/(mol.K)); T represents the absolute temperature (K); n is the electron transfer number; F is the Faraday constant (96,485 C/mol).
Different from the symmetric peak shape observed in conventional soluble/soluble electrochemical systems, the oxidation peak of O2− is not exactly symmetric, i.e., the increasing part of the current is sharper than the decreasing one, as shown in Figure 8. This phenomenon originates from the nucleation overpotential of oxygen gas formation. The overpotential produced during O2 gas evolution delays the current-increase response, rendering a steeper rise in the peak current. That means the decreasing part (the right half) of the peak was not affected by the nucleation overpotential. Thus, the disturbance of the signal due to the nucleation effect can be resolved by taking into account only the decreasing part (right half) of the peak for the measurement of the half peak width (W1/2). Previous literature reports similar methods for determining W1/2 in the case of the nucleation effect [28,29]. Thus, based on the obtained W1/2 and Equation (6), it was found that the number of transferred electrons for O2− oxidation at different frequencies was approximately 2, as shown in Table 3. Accordingly, the electrode reaction mechanism for O2− oxidation is ultimately determined as follows:
Table 3.
Half peak widths W1/2 and electron transfer numbers n of the FLiBe–O2− (6.18 ×10−2 mol/kg) molten salt system at different frequencies measured by SWV (T = 600 °C).
3.2.3. Chronopotentiometry
CP was employed to further investigate the electrochemical behavior and diffusion coefficient of O2− in FLiBe molten salt. The corresponding chronopotentiogram is displayed in Figure 10. For the FLiBe–O2− (3.86 ×10−2 mol/kg) system at 600 °C, a potential plateau was observed at approximately 1.3 V vs. Pt under an applied current density of 0.89 mA/cm2. The potential of this plateau was consistent with the oxidation peak potential obtained from SWV measurements, and the corresponding transition time (τ) was determined to be 0.634 s. Apparently, this plateau corresponds to the electrochemical oxidation of O2− to O2 (Equation (7)). The CP result is in good agreement with that obtained by SWV. Then, CP measurements were performed at a fixed O2− concentration (3.86 × 10−2 mol/kg), electrode area (0.121 cm2), and temperature (600 °C) by applying different current densities of 0.50, 0.66, 0.87, 0.89, 1.03, 1.12, 1.18, 1.20, and 1.28 mA/cm2. The results indicate that τ decreases with increasing current density, and the values of Iτ1/2 remain nearly constant (Figure 11c). This result is consistent with the Sand law (Equation (8)), further demonstrating that the oxidation of O2− is an ion diffusion-controlled process, which enables the determination of the diffusion coefficient of O2−. As shown in Figure 11c, the Iτ1/2 value remained stable at 8.24 × 10−5 As1/2 at 600 °C. Accordingly, the diffusion coefficient of O2− in FLiBe molten salt at 600 °C was calculated to be 2.74 × 10−9 cm2/s based on the Sand law.
where S is the electrode area, in cm2; I is the applied current, in A; τ is the transition time, in s; C is the O2− concentration, in mol/cm3; F is the Faraday constant, valued at 96,485 C/mol; n is the number of electrons transferred; D is the diffusion coefficient, in cm2/s.
Figure 10.
Typical chronopotentiogram of the FLiBe–O2− (3.86 × 10−2 mol/kg) molten salt system under an applied current density of 0.89 mA/cm2. T = 600 °C; working electrode: Au (S = 0.121 cm2); reference electrode: Pt; auxiliary electrode: graphite. The density of FLiBe melt (ρFLiBe) is approximately 2 g/cm3.
Figure 11.
Evolution of Iτ1/2 vs. the applied current intensity for the FLiBe–O2− (3.86 × 10−2 mol/kg) molten salt system at different temperatures. (a) 500 °C; (b) 550 °C; (c) 600 °C; (d) 650 °C. Working electrode: Au (S = 0.121 cm2); reference electrode: Pt; auxiliary electrode: graphite. The density of FLiBe melt (ρFLiBe) is approximately 2 g/cm3.
CP were performed at different temperatures of 500 °C, 550 °C, 600 °C, and 650 °C. At all tested temperatures, the experimental results show that the transition time (τ) decreases with the increase in applied current density (I), and the values of Iτ1/2 remain constant at each temperature. In addition, the constant Iτ1/2 value increases with rising temperature, as depicted in Figure 11. These results are consistent with the Sand law, i.e., the Iτ1/2 value increases with temperature (or diffusion coefficient D) when the O2− concentration (C) and electrode area (S) remain constant. Thus, the oxidation of O2− is controlled by ion diffusion over the studied temperature range.
Based on the Sand law, the diffusion coefficients (D) of O2− in FLiBe melts were obtained at each temperature, and the resulting increases from 8.55 × 10−10 to 6.44 × 10−9 cm2/s with rising temperature from 500 °C to 650 °C. The were compared with the reported data in FLiNaK and LiF–NaF systems, as summarized in Table 4. The results indicate that the diffusion coefficient of O2− in FLiBe molten salt is about three orders of magnitude lower than that in FLiNaK and LiF–NaF molten salt systems within the investigated temperature range. The significant difference originates from the unique microstructure and thermophysical properties of FLiBe molten salt: (1) Be2+ can coordinate with F− to form [BeF4]2− (Figure 12a), which further polymerizes to construct a dense network structure [34]. These molecules have a large volume, thereby hindering the migration of O2− ions. In contrast, FLiNaK and LiF–NaF dissociate completely into free alkali metal ions and fluoride ions at high temperatures without complex formation (Figure 12b,c), resulting in a relatively high O2− diffusion coefficient. (2) Be2+ in FLiBe molten salt exhibits favorable coordination ability and can form stable Be2+-O2− complex species with O2−. The formation of such complexes with relatively large volume and relatively large hydrodynamic radius further reduces the ion migration rate and increases the viscosity of the molten salt. (3) FLiBe molten salt possesses inherently higher viscosity compared with FLiNaK and LiF–NaF systems, which is unfavorable for the mass transfer and migration of O2−. The above factors substantially reduce the diffusion rate of O2− in FLiBe molten salt. Therefore, it is reasonable that the diffusion coefficient of O2− in FLiBe (order of magnitude of ~10−9) is much lower than that in FLiNaK and LiF–NaF.
Table 4.
Comparison of O2− diffusion coefficients in various fluoride molten salts at different temperatures.
Figure 12.
XRD patterns of the (a) FLiBe, (b) FLiNaK, and (c) LiF–NaF (60:40 mol%) molten salts.
The diffusion coefficient of O2− in FLiBe molten salt increases with the elevation of temperature, and the evolution of D with temperature obeys Arrhenius’ law (Equation (9)). By fitting the experimental data based on the Arrhenius formula, as shown in Equation (10) and Figure 13, the activation energy (Ea) for O2− diffusion in FLiBe molten salt was determined to be 79.5 kJ/mol.
Figure 13.
Linear relationship between lnD and 1/T.
3.3. Establishment of Quantitative Relationship Between Peak Current Density and O2− Concentration
Theoretically, for diffusion-controlled electrode reactions, the peak current density should be linear with the reactant concentration. SWVs were performed at 600 °C with a scanning frequency of 10 Hz for FLiBe molten salt containing different O2− concentrations, and the corresponding square wave voltammograms are presented in Figure 14. As the O2− concentration increased from 1.24 × 10−2 mol/kg to 3.35 ×10−2 mol/kg, the oxidation peak current density of O2− accordingly increased from 1.740 mA/cm2 to 4.750 mA/cm2, as shown in Table 5. Then, the peak current density vs. O2− concentration is fitted, and a straight line is obtained, as shown in Figure 15. This linear relationship can be described by Equation (11). The slope equals 145.22, and the line passes through the origin of the coordinates, indicating that no O2− oxidation peak current can be detected with no O2− contained in the FLiBe melts. Equation (11) provides a quantitative relationship between the peak current and the O2− concentration. Using this equation, the O2− content in an unknown FLiBe melt can be quickly obtained based on the measured peak current.
Figure 14.
Square wave voltammograms of the FLiBe molten salt containing different O2− concentrations. T = 600 °C; scan frequency: 10 Hz; pulse height: 25 mV; step potential: 4 mV; working electrode: Au; reference electrode: Pt; auxiliary electrode: graphite.
Table 5.
Peak current densities of O2− measured by SWV in the FLiBe molten salt containing different O2− concentrations at 10 Hz and 600 °C.
Figure 15.
Linear relationship between O2− concentration and peak current density obtained by square wave voltammetry in the FLiBe molten salt containing different O2− concentrations. T = 600 °C; scan frequency: 10 Hz; pulse height: 25 mV; step potential: 4 mV; working electrode: Au; reference electrode: Pt; auxiliary electrode: graphite.
However, the peak potential of O2− positively shifts from 1.262 V to 1.302 V vs. Pt as the O2− concentration increases from 1.24 × 10−2 to 3.35 × 10−2 mol/kg, which may result from the following two reasons. One is the potential variation in the Pt/PtOx/O2− reference electrode, and the other is due to the increase in the activity of O2− according to the Nernst equation (Equation ()) expressed as follows:
where is the standard potential of O2−/O2 and is the O2− activity that can be denoted as , in which is the concentration of O2− and is its activity coefficient. is the partial pressure of O2 and is the standard atmospheric pressure. The potential of O2−/O2 with = 1.24 × 10−2 mol/kg is defined as E1, and the activity coefficient of O2− () is assumed to be 1. Thus, ΔE is the difference between E1 and the potential obtained at of 1.98 × 10−2, 2.03 × 10−2, 2.44 × 10−2, 2.71 × 10−2, 3.08 × 10−2 and 3.35 × 10−2 mol/kg can be expressed as Equation ():
where C1 is 1.24 × 10−2 mol/kg, and C is the O2− concentration at the other six concentrations, as listed in Table 6. The potential differences in obtained by using SWV and the Nernst equation are also listed in Table 6. Therefore, the potential variation caused by the Pt/PtOx/O2− reference electrode can be quantified by the difference value in the SWV measurements and the Nernst equation calculations.
Table 6.
The potential variations at different O2− concentrations at 600 °C.
3.4. O2− Content Determination by SWV
SWV was carried out for an unpurified FLiBe molten salt with an unknown oxide content. An example of a square wave voltammogram of a FLiBe medium obtained after the fusion without any thermal treatment to remove residual oxide ions at 600 °C with a signal frequency of 10 Hz is shown in Figure 16. This figure exhibits the oxide ions oxidation peak at about 1.35 V vs. Pt with a peak current density of 9.770 mA/cm2. Thus, the O2− concentration of this FLiBe melt was calculated to be 6.73 × 10−2 mol/kg using Equation (11). For comparison, the same FLiBe molten salt was sampled and transferred for LECO-IC analysis, and the O2− concentration was determined as 6.38 × 10−2 mol/kg. The result obtained from the in situ SWV technology is in good agreement with that obtained by the conventional offline LECO-IC analysis, with a low relative error of only 5.48%, as summarized in Table 7. The above results indicate that the SWV technology for quantitative analysis of O2− is feasible and can be applied to the rapid determination of oxide content for an unknown FLiBe molten salt.
Figure 16.
Square wave voltammogram of a FLiBe molten salt without any thermal treatment with unknown oxide concentration. T = 600 °C; scan frequency: 10 Hz; pulse height: 25 mV; step potential: 4 mV; working electrode: Au; reference electrode: Pt; auxiliary electrode: graphite.
Table 7.
Comparison of O2− content in FLiBe without thermal treatment determined by SWV and LECO-IC.
3.5. Electrolytic Removal of O2− from FLiBe
In this study, potentiostatic electrolysis was performed to remove oxide ions in the above unpurified FLiBe molten salt. The electrolysis experiments were conducted at 600 °C using a three-electrode system with a gold working electrode. The electrolytic potential was set at 1.85 V vs. Pt for a total electrolysis duration of 3.8 h. Theoretically, at this potential, O2− is oxidized to O2 while ensuring that the gold electrode does not dissolve. In order to monitor the concentration evolution of O2− ions in the electrolysis process, SWVs were conducted at different electrolysis durations. During the early stage of electrolysis, SWV scans were conducted every 0.2 h, while in the later stage, the interval was 1 h. The corresponding square wave voltammograms under different electrolysis times are displayed in Figure 17. The oxidation peak current density at around 1.3 V vs. Pt decreased significantly from the initial 9.770 mA/cm2 to 9.097 mA/cm2 after 0.2 h of electrolysis. The corresponding O2− concentration was thus decreased from 6.73 × 10−2 mol/kg to 6.26 × 10−2 mol/kg according to the quantitative equation of SWV (Equation (11)). As the electrolysis proceeds, the peak current density decreases continuously, indicating that O2− is continuously electrolyzed into O2(g) and removed. As the electrolysis time increased from 0.2 h to 2.6 h, the oxidation peak current of O2− gradually decreased, and thus the O2− concentration decreased from 6.26 × 10−2 mol/kg to 1.49 × 10−2 mol/kg. After electrolysis for 2.8 h, the peak current density decreased to 1.562 mA/cm2; the corresponding concentration of O2− at this moment is 1.08 × 10−2 mol/kg according to Equation (11). After this, the removal rate of O2− ions slowed down. Until 3.8 h, the peak current density decreased from 1.562 mA/cm2 to 1.463 mA/cm2. That is, during the last hour of the electrolysis process, the O2− concentration decreased only from 1.08 × 10−2 to 1.01 × 10−2 mol/kg. This result indicates that at low O2− concentrations, the electrolytic removal of oxide ions becomes difficult. The variation trend of residual O2− concentration as a function of electrolysis time is summarized in Figure 18.
Figure 17.
Variation in the square wave voltammograms under different electrolysis durations in the process of electrolytic removal of O2− from FLiBe melts. T = 600 °C; scan frequency: 10 Hz; pulse height: 25 mV; step potential: 4 mV; working electrode: Au; reference electrode: Pt; auxiliary electrode: graphite.
Figure 18.
Evolution of residual O2− content in FLiBe molten salt by SWV during potentiostatic electrolysis.
For comparison, molten salt samples collected at five different electrolysis durations (0 h, 0.8 h, 1.8 h, 2.8 h, and 3.8 h) were analyzed by offline LECO-IC analysis, and the oxide variation results are shown in Table 8. The SWV results are highly consistent with those obtained by LECO-IC, with relative errors within ±6%, demonstrating the reliability of SWV quantitative technology.
Table 8.
The concentration variations in O2− during the oxide removal process of FLiBe molten salt electrolysis: Comparison of SWV and LECO-IC test results.
The electrolytic removal efficiency was calculated based on the O2− concentration difference before and after electrolysis using Equation . The results show that the potentiostatic electrolysis reduces the O2− concentration from the initial 6.73 × 10−2 mol/kg to 1.01 × 10−2 mol/kg, achieving a deoxygenation efficiency of 85%. Although the electrolysis removal process of O2− seems to become difficult under low concentration conditions (between 2.8 h and 3.8 h), by means of potentiostatic electrolysis, the concentration of O2− was successfully reduced to 1.01 × 10−2 mol/kg, corresponding to 162 ppm, which met the TMSR-LF1 requirement that the O2− content in the fuel salt should be lower than 200 ppm. This work validates the feasibility of potentiostatic electrolysis for oxide removal from FLiBe molten salt.
where η is the electrolytic removal efficiency of O2−, C0 is the initial O2− concentration before electrolysis, and Cf is the final O2− concentration after electrolysis.
4. Conclusions
In this work, a three-electrode system with a gold working electrode was adopted to systematically investigate the electrochemical behavior and electrolysis removal of O2− in FLiBe molten salt. Then, an in situ electrochemical quantitative analysis method for O2− was established. Based on this, a quick determination and monitoring of O2− concentration in FLiBe was realized. Furthermore, electrochemical removal of O2− from FLiBe molten salt was performed and achieved a relatively high extraction efficiency. This study offers reliable theoretical and technical support for the in situ analysis and online monitoring of O2− impurity content in FLiBe molten salt. Meanwhile, this paper proposes an innovative route for oxide removal of FLiBe using molten salt electrolysis technology.
The main conclusions are summarized as follows:
(1) Electrochemical behavior of O2− in FLiBe molten salt. CV, SWV, and CP were employed to characterize the electrochemical behavior of O2−. Comparative analysis indicates that SWV is more suitable than CV for studying the electrochemical behavior of O2−. The SWV results confirm that O2− is oxidized to O2 at 1.3 V vs. Pt with the oxidation mechanism of O2− = 1/2O2(g) + 2e−, and the electrode reaction is controlled by ion diffusion. The CP results revealed a plateau of 1.3 V vs. Pt for O2−/O2 oxidation and proved that the electrochemical behavior of O2− complies with the Sand law, where the value of Iτ1/2 remains constant. The CP results are highly consistent with the SWV findings. The diffusion coefficients D of O2− in FLiBe at different temperatures were determined to range from 8.55 × 10−10 cm2/s to 6.44 × 10−9 cm2/s within 500–650 °C. The temperature dependence of the diffusion coefficient obeys Arrhenius’ law, and the activation energy Ea for O2− diffusion was calculated to be 79.5 kJ/mol.
(2) Establishment of an in situ electrochemical quantitative analysis method for O2−. SWV was performed on the FLiBe system with different O2− concentrations. Then, a well-fitted linear relationship between O2− concentration and peak current density was established, and the equation of the straight line is δip(mA/cm2) = 145.22 [O2−](mol/kg). This equation can be applied to the quick determination and monitoring of oxide content for an unknown FLiBe molten salt. The O2− concentration data by SWV electrochemical technology are in excellent agreement with offline results obtained by the combined LECO-IC method, with a relative error within ±6%.
(3) Electrochemical removal of O2− from FLiBe molten salt. Potentiostatic electrolysis technology was adopted for deoxygenation in FLiBe-O2− molten salt at 1.85 V vs. Pt for 3.8 h. During the electrolysis process, SWV was used for online monitoring of the variation in O2− concentration. The O2− concentration was reduced from the initial 6.73 × 10−2 mol/kg to 1.01 × 10−2 mol/kg, achieving a high oxide removal efficiency of 85%. Meanwhile, the results indicate that under the low oxide content conditions in the later stage of electrolysis, the elimination speed of O2− decreases and the electrolytic process removal of O2− becomes difficult. Nevertheless, the concentration of oxide ions after electrolysis has been successfully reduced to 1.01 × 10−2 (162 ppm), which is below the oxide content standard for the TMSR-LF1 fuel salt (200 ppm). The experimental results verify the feasibility of potentiostatic electrolysis for eliminating O2− impurities in fluoride molten salts.
This work presents three key innovations:
(1) This study fills the gap in the fundamental electrochemical parameters of O2− in the FLiBe molten salt, including peak potential, peak current, transferred electron numbers, electrode process nature, diffusion coefficient, activation energy, and electrode reaction mechanism.
(2) The linear quantitative relationship between the SWV peak current density and the O2− concentration was obtained. The established in situ electrochemical method enables quick determination and real-time monitoring of O2− content, effectively overcoming the drawbacks of time consumption, complicated pretreatment, and data hysteresis inherent to conventional offline analysis techniques. Relevant results provide a reference for the online oxide measurement of MSR fuel salt.
(3) This study verified the feasibility of O2− removal through potentiostatic electrolysis and achieved satisfactory removal efficiency. The validated high-efficiency electrochemical deoxygenation strategy provides a novel technical route for fluoride molten salt purification.
This work advances the research on oxide monitoring and purification by establishing a complete electrochemical analysis and deoxygenation system for FLiBe molten salt, which is lacking in previous beryllium-free molten salt studies. Nevertheless, several limitations remain. The electrolytic deoxygenation efficiency decreases significantly at low O2− concentrations, and the effects of trace impurities and long-term high-temperature molten salt corrosion on electrochemical detection and electrolysis performance remain unclear. Furthermore, all experiments were performed under static laboratory conditions, ignoring the flow and irradiation environments of practical MSR operation. Future studies will focus on optimizing electrolytic parameters to improve the removal efficiency of O2− at low-concentration conditions. Additionally, further research can explore the coupled effects of irradiation and hydrodynamic conditions on O2− electrochemical behaviors, and develop reliable in situ monitoring and long-term stable deoxygenation technologies adapted to actual reactor operating conditions.
Author Contributions
Conceptualization, H.P.; methodology, H.P.; software, X.F., L.W., Y.L., X.L., and H.P.; validation, H.P.; formal analysis, X.F., L.W., Y.L., and H.P.; investigation, X.F., L.W., Y.L., and H.P.; resources, Z.L., Q.D., and H.P.; data curation, X.F. and H.P.; writing—original draft, X.F.; writing—review and editing, H.P.; visualization, X.F., Y.L., X.L., Y.H., and H.P.; supervision, H.F. and Q.D.; project administration, H.F. and Q.D.; funding acquisition, Z.L., H.F., Q.D., and H.P. All authors have read and agreed to the published version of the manuscript.
Funding
This work was supported by Youth Innovation Promotion Association CAS (Grant No. 2023271), the Gansu Youth Science and Technology Fund (Grant No. 24JRRH010), the National Natural Science Foundation of China (Grant Nos. U2267226, 12341402, 22576209, 12565026 and 22006150), Xinjiang Uygur Autonomous Region Key R&D Task Special Project (Grant No. 2022B01039), and the Major Discipline Academic and Technical Leaders Training Program of Jiangxi Province (Grant No. 20232BCJ23047).
Data Availability Statement
The original contributions presented in this study are included in the article. Further inquiries can be directed to the corresponding author.
Conflicts of Interest
The authors declare no conflicts of interest.
References
- Khaleel, M.; Yusupov, Z.; Rekik, S.; Kılıç, H.; Nassar, Y.F.; El-Khozondar, H.J.; Ahmed, A.A. Harnessing nuclear power for sustainable electricity generation and achieving zero emissions. Energy Explor. Exploit. 2025, 43, 1126–1148. [Google Scholar] [CrossRef] [Scilit]
- Wu, J.; Chen, J.; Cai, X.; Zou, C.; Yu, C.; Cui, Y.; Zhang, A.; Zhao, H. A review of molten salt reactor multi-physics coupling models and development prospects. Energies 2022, 15, 8296. [Google Scholar] [CrossRef] [Scilit]
- Son, I.W.; Choi, S.; Kim, S.J.; Lee, J. Thermal-sizing of the molten salt reactor system with gas Brayton cycle. In Proceedings of the 2021 Korean Nuclear Society Autumn Meeting, Online, 21–22 October 2021. [Google Scholar]
- Ashraf, O.; Tikhomirov, G.V. Thermal-and fast-spectrum molten salt reactors for minor actinides transmutation. Ann. Nucl. Energy 2020, 148, 107751. [Google Scholar] [CrossRef] [Scilit]
- Křepel, J.; Hombourger, B.; Fiorina, C.; Mikityuk, K.; Rohde, U.; Kliem, S.; Pautz, A. Fuel cycle advantages and dynamics features of liquid fueled MSR. Ann. Nucl. Energy 2014, 64, 380–397. [Google Scholar] [CrossRef] [Scilit]
- Serp, J.; Allibert, M.; Beneš, O.; Delpech, S.; Feynberg, O.; Ghetta, V.; Heuer, D.; Holcomb, D.; Ignatiev, V.; Kloosterman, J.L.; et al. The molten salt reactor (MSR) in generation IV: Overview and perspectives. Prog. Nucl. Energy 2014, 77, 308–319. [Google Scholar] [CrossRef] [Scilit]
- Das, P.; Mukherjee, S.; Mishra, R.; Dash, S. Thermodynamic and physical properties of molten LiF-ThF4-UF4 salts mixture. J. Fluor. Chem. 2019, 226, 109349. [Google Scholar] [CrossRef] [Scilit]
- Briggs, R.B. Molten-Salt Reactor Program: Semiannual Progress Report for Period Ending; ORNL-3369; Oak Ridge National Laboratory: Oak Ridge, TN, USA, 1962. [Google Scholar]
- Rosenthal, M.W.; Briggs, R.B.; Haubenreich, P.N. Molten-Salt Reactor Program: Semiannual Progress Report for Period Ending; ORNL-4782; Oak Ridge National Laboratory: Oak Ridge, TN, USA, 1972. [Google Scholar]
- Xu, H. Thorium energy and molten salt reactor R&D in China. In Thorium Energy for the World, Proceedings of the ThEC13 Conference, CERN, Globe of Science and Innovation, Geneva, Switzerland, 27–31 October 2013; Springer International Publishing: Cham, Switzerland, 2016; pp. 37–44. [Google Scholar]
- Smith, A.L.; Verleg, M.N.; Vlieland, J.; de Haas, D.; Ocadiz-Flores, J.A.; Martin, P.; Rothe, J.; Dardenne, K.; Salanne, M.; Gheribi, A.E.; et al. In situ high-temperature EXAFS measurements on radioactive and air-sensitive molten salt materials. Synchrotron Radiat. 2019, 26, 124–136. [Google Scholar] [CrossRef] [Scilit] [PubMed]
- Peng, H.; Shen, M.; Zuo, Y.; Tang, X.; Tang, R.; Xie, L. Electrochemical technique for detecting the formation of ura-nium-containing precipitates in molten fluorides. Electrochim. Acta 2016, 222, 1528–1537. [Google Scholar] [CrossRef] [Scilit]
- Robertson, R.C. MSRE Design and Operations Report: Part I. Description of Reactor Design; ORNL-TM-0728; Oak Ridge National Laboratory: Oak Ridge, TN, USA, 1965. [Google Scholar]
- Rosenthal, M.W.; Haubenreich, P.N.; Briggs, R.B. Molten-Salt Reactor Program: The Development Status of Molten Salt Breeder Reactors; ORNL-4812; Oak Ridge National Laboratory: Oak Ridge, TN, USA, 1972. [Google Scholar]
- Briggs, R.B. Molten-Salt Reactor Program: Semiannual Progress Report for Period Ending; ORNL-3708; Oak Ridge National Laboratory: Oak Ridge, TN, USA, 1964. [Google Scholar]
- Peng, H.; Ji, N.; Huang, W.; Gong, Y. Chemical Interactions between Thorium (IV) and O2− in the FLiBe and FLiNaK Molten Salt Systems. Int. J. Energy Res. 2023, 2023, 4447405. [Google Scholar] [CrossRef] [Scilit]
- Thoma, R.E. Molten-Salt Reactor Program: Chemical Aspects of MSRE Operations; ORNL-4658; Oak Ridge National Laboratory: Oak Ridge, TN, USA, 1971. [Google Scholar]
- Petti, D.A.; Smolik, G.; Simpson, M.F.; Sharpe, J.P.; Anderl, R.; Fukada, S.; Hatano, Y.; Hara, M.; Oya, Y.; Terai, T.; et al. JUPITER-II molten salt Flibe research: An up-date on tritium, mobilization and redox chemistry experiments. Fusion Eng. Des. 2006, 81, 1439–1449. [Google Scholar] [CrossRef] [Scilit]
- Afonichkin, V.; Bovet, A.; Shishkin, V. Salts purification and voltammetric study of the electroreduction of U(IV) to U(III) in molten LiF–ThF4. J. Nucl. Mater. 2011, 419, 347–352. [Google Scholar] [CrossRef] [Scilit]
- Briggs, R.B. Molten-Salt Reactor Program: Semiannual Progress Report for Period Ending; ORNL-3812; Oak Ridge National Laboratory: Oak Ridge, TN, USA, 1965. [Google Scholar]
- Briggs, R.B. Molten-Salt Reactor Program: Semiannual Progress Report for Period Ending; ORNL-3872; Oak Ridge National Laboratory: Oak Ridge, TN, USA, 1965. [Google Scholar]
- Goldberg, G.; Meyer, A.S.; White, J.C. Determination of oxides in fluoride salts by high-temperature fluorination with potassium bromotetrafluoride. Anal. Chem. 1960, 32, 314–317. [Google Scholar] [CrossRef] [Scilit]
- Serp, J.; Konings, R.J.M.; Malmbeck, R.; Rebizant, J.; Scheppler, C.; Glatz, J.-P. Electrochemical behaviour of plutonium ion in LiCl–KCl eutectic melts. J. Electroanal. Chem. 2004, 561, 143–148. [Google Scholar] [CrossRef] [Scilit]
- Shirai, O.; Iwai, T.; Suzuki, Y.; Sakamura, Y.; Tanaka, H. Electrochemical behavior of actinide ions in LiCl–KCl eutectic melts. J. Alloys Compd. 1998, 271, 685–688. [Google Scholar] [CrossRef] [Scilit]
- Fang, F.; Liu, S.; Yao, B.; Xiao, Y.; Jia, Y.; Li, B.; Ye, G.; He, H. The electrode kinetics of UCl3 in LiCl-KCl molten salt. J. Electrochem. Soc. 2024, 171, 056504. [Google Scholar] [CrossRef] [Scilit]
- Peng, H.; Shen, M.; Wang, C.; Su, T.; Zuo, Y.; Xie, L. Electrochemical investigation of the stable chromium species in molten FLINAK. Rsc Adv. 2015, 5, 76689–76695. [Google Scholar] [CrossRef] [Scilit]
- Zhao, Z.; Geng, J.; Cheng, Z.; Li, W.; Dou, Q.; Zhang, L.; Li, Q. Control and surveillance of redox potential for 233 Pa dissolution in 2LiF–BeF2 molten salt. RSC Adv. 2024, 14, 15994–16000. [Google Scholar] [CrossRef] [Scilit] [PubMed]
- Massot, L.; Cassayre, L.; Chamelot, P.; Taxil, P. On the use of electrochemical techniques to monitor free oxide content in molten fluoride media. J. Electroanal. Chem. 2007, 606, 17–23. [Google Scholar] [CrossRef] [Scilit]
- Shen, M.; Peng, H.; Ge, M.; Zuo, Y.; Xie, L. Use of square wave voltammeter for online monitoring of O2− concentration in molten fluorides at 600 °C. J. Electroanal. Chem. 2015, 748, 34–39. [Google Scholar] [CrossRef] [Scilit]
- Choi, E.Y.; Choi, I.K.; Hur, J.M.; Kang, D.-S.; Shin, H.-S.; Jeong, S.M. In situ electrochemical measurement of O2− concentration in molten Li2O/LiCl during uranium oxide reduction process. Electrochem. Solid-State Lett. 2011, 15, E11–E13. [Google Scholar] [CrossRef] [Scilit]
- Manning, D.L.; Mamantov, G. Electrochemical studies of oxide ions and related species in molten fluorides. J. Electrochem. Soc. 1977, 124, 480–483. [Google Scholar] [CrossRef] [Scilit]
- Nourry, C.; Massot, L.; Chamelot, P.; Taxil, P. Data acquisition in thermodynamic and electrochemical reduction in a Gd(III)/Gd system in LiF–CaF2 media. Electrochim. Acta 2008, 53, 2650–2655. [Google Scholar] [CrossRef] [Scilit]
- Nourry, C.; Massot, L.; Chamelot, P.; Taxil, P. Electrochemical reduction of Gd(III) and Nd(III) on reactive cathode material in molten fluoride media. J. Appl. Electrochem. 2009, 39, 927–933. [Google Scholar] [CrossRef] [Scilit]
- Fu, X.; Liu, Y.; Huang, H.; Wu, H.; Sun, J.; Han, L.; Ge, M.; Qian, Y.; Liu, H. Probing the local structure of FLiBe melts and solidified salts by in situ high-temperature NMR. Phys. Chem. Chem. Phys. 2023, 25, 19446–19452. [Google Scholar] [CrossRef] [Scilit] [PubMed]
- Peng, H. Study on Corrosive Impurities and Oxide Dissolution Behavior in Fluoride Molten Salt System; Shanghai Institute of Applied Physics, University of Chinese Academy of Sciences: Shanghai, China, 2017. [Google Scholar]
Disclaimer/Publisher’s Note: The statements, opinions and data contained in all publications are solely those of the individual author(s) and contributor(s) and not of MDPI and/or the editor(s). MDPI and/or the editor(s) disclaim responsibility for any injury to people or property resulting from any ideas, methods, instructions or products referred to in the content. |
© 2026 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license.