Skip to Content
PharmaceuticalsPharmaceuticals
  • Article
  • Open Access

26 January 2026

19 Pages

Soybean Polysaccharides Increase the Stability of Lansoprazole Enteric Coated Pellets

,
,
,
,
,
and
Key Laboratory of Study and Discovery of Small Targeted Molecules of Hunan Province, School of Pharmacy, Hunan Normal University, Changsha 410013, China
*
Author to whom correspondence should be addressed.
†
These authors contributed equally to this work.

Abstract

Background/Objectives: Lansoprazole (LNS) is widely used to treat and prevent stomach and intestinal ulcers and as a proton pump inhibitor with low solubility and high permeability. Soluble soybean polysaccharides (SSPS) are well-known disintegrants in food processing but are rarely used in the pharmaceutical field. In this study, we included SSPS as a disintegrant in LNS formulation for pharmaceutical use to investigate the effect of SSPS on the characteristics, dissolution curve, and stability of LNS enteric coated pellets. Methods: The screening of multiple excipients in formulation optimized the release and stability profile of enteric LNS pellets. The final enteric coated LNS pellet containing SSPS were evaluated by LNS crystal form, release profile, and stability. Results: X-ray powder diffraction revealed that this new LNS pellet and commercial reference LNS pellet had similar crystal form by X-ray powder diffraction. Under both long-term and accelerated conditions, these new SSPS-containing LNS pellets had higher release rate and better acid resistance than reference marketed LNS pellets. Conclusions: Inclusion of SSPS in LNS formulation could increase the physicochemical stability of the enteric coated capsules after storage, providing the basis of SSPS for further development and utilization in pharmaceutical formulation as a promising excipient.

1. Introduction

Lansoprazole (LNS) is a proton pump inhibitor with good permeability, belonging to Class 2 compounds in the Biopharmaceutical Classification System (BCS) [1]. With its high lipophilicity and interaction with H+/K+-ATPase, LNS in the cell membrane can be transformed into sub-sulfonic acid and sub-sulfonyl derivatives to exert its potent antibacterial activity against Helicobacter pylori (HP) and inhibit gastric acid secretion [2]. However, LNS is crystalline in nature with poor solubility, leading to low bioavailability. To improve the solubility of LNS, multiple methods to increase surface area and solubility rate of drug powder have been used [3]. For instance, hot-melt extrusion (HME) is a popular approach to increase the solubility of poorly soluble active pharmaceutical ingredients (API) for the preparation of solid dispersion, but LNS formulation by HME is challenging because LNS is a heat-liable ingredient [4]. Currently, the LNS solid pellet is prepared by a continuous coating process including a drug layer, intermediate layer, and enteric coating, followed by capsule filling. Each step of the existing technology such as centrifugal granulation technology is very time-consuming because it involves a coating step followed by a drying step, requiring the use of multiple settings and large amounts of space [5,6].
Fluidized bed bottom spray coating technology is one of the preferred approaches for coating in the preparation of drug pellets [7,8]. LNS is dispersed or dissolved in low-concentration ethanol with water-soluble materials, and this resultant drug layer is coated on the sucrose cores by the fluidized bed bottom spray coating function, and the same fluidized bed equipment is used for the intermediate layer and enteric-coated layer. Due to the high drying efficiency of the fluidized bed, the preparation process of each coating is sprayed and dried simultaneously, and there is no need to add a separate drying step, which reduces the processing time, stabilizes the preparation process, and also helps to improve the physical and chemical properties of the API [9].
Selection of water-soluble vehicles and disintegrants is necessary for the preparation of LNS pellet formulation. Soluble soybean polysaccharides (SSPS) are widely used in food processing due to their low viscosity, good solubility, and adhesion resistance, as well as excellent emulsifying, foaming, and stability properties [10,11,12]. However, there are currently a few reports on the use of SSPS as pharmaceutical excipients on enteric coated pellets.
In this study, we aim to investigating the effect of SSPS on the characteristics, dissolution curve, and stability of LNS enteric coated pellets by including SSPS as a hydrophilic carrier and disintegrant in an LNS multiparticulate-coated formulation for pharmaceutical use. Multiple excipients were screened in the formulation to optimize the release and stability profile of resultant enteric LNS pellets. The final enteric coated LNS pellets containing SSPS were evaluated by LNS crystal form, release profile, and stability and compared with marketed reference LNS pellets. The results indicated that these new SSPS-containing LNS pellets had a higher release rate and better acid resistance than reference marketed LNS pellets, providing theoretical guidance for the future application of SSPS in pharmaceutical formulations.

2. Results and Discussion

2.1. Formulation and Process Selection for the Preparation of Enteric LNS Pellets

LNS is practically insoluble in water and highly sensitive to acidic environments [13]. Ethanol, with its low surface tension, excellent wettability, and effective antifoaming properties, is therefore chosen as the solvent to enhance LNS wettability and reduce bubble formation during the suspension process [14]. And SDS is introduced to improve the solubility of LNS [15]. Water-soluble excipients including mannitol, soluble soybean polysaccharide (SSPS) and HPC are selected as the diluent, disintegrant, and adhesive, respectively, due to their ability to facilitate dispersion and enhance wettability in dissolution media [16,17]. Methyl methacrylate-ethyl acrylate copolymer (1:1) is selected as the enteric film-forming polymer, with PEG 6000 employed as the plasticizer and talc as the anti-adherent. Furthermore, talc powder is incorporated as an adsorbent on the surface of the enteric pellets [18] (Table 1). Formulation optimization is guided by the basic formulation framework. Specifically, drug-layer and intermediate-layer coatings are sequentially applied onto pellet cores, followed by the enteric coating. Multiparticulate coated systems with hydrophilic carriers are prepared using the bottom spray technique onto sucrose cores, with processing temperatures maintained below 50 °C to prevent thermal degradation of LNS (Figure 1).
Table 1. Basic formulation of LNS pellets.
Figure 1. Workflow of pellet preparation using fluidized bed bottom spray coating technology. (A) Photo of FLZB-3.0 fluidized bed bottom spray machine and its operating system. (B) Procedures and conditions of pellet coating.

2.1.1. Optimal API Particle Size for Uniform Coating and Controlled Release

Particle size variation in API can critically affect suspension dispersion uniformity, ultimately influencing drug content uniformity [19]. We tested three API particle sizes (D90 = 4.9, 10.5, 18.6 μm) and found that these sizes led to similar homogeneity of the drug-layer coating solution. However, the large API particle size decreased the release rate and amount of the API from the drug layer significantly (Figure S1). Therefore, the API particle size D90 was selected to be 4.9 μm.

2.1.2. Optimal Alkalizer Identified

Distinct alkalizers result in coating solutions with varying pH values, which reflects the relative alkalinity, with the pH ranking as follows: sodium carbonate anhydrous > meglumine > magnesium carbonate > sodium bicarbonate [20]. Notably, drug layers formulated with the stronger alkalizers such as meglumine and sodium carbonate anhydrous exhibited superior stability after 30 days at 40 °C/75% RH compared to those containing sodium bicarbonate or magnesium carbonate, indicating that increased alkalinity is more favorable for API stability (Table S1). Moreover, drug layers containing sodium bicarbonate demonstrated a slightly slower release rate relative to the other three, suggesting that higher alkalinity enhances the solubilization of LNS (Figure S2). In summary, although both anhydrous sodium carbonate and meglumine perform well as alkalizers in terms of product stability and drug release, anhydrous sodium carbonate was ultimately selected for the drug layer due to its wide use as a pharmaceutical excipient.

2.1.3. Optimal Disintegrant-SSPS Loading Accelerates LNS Pellet Release

The highly fibrous soy polysaccharide material generally comprises high-molecular-weight carbohydrate polymers primarily contained in soybeans, such as arabinose, galactose, mannose, and xylose [10]. In this study, we selected SSPS and investigated the optimal dose. Drug release testing showed that incorporating 2 mg/capsule or 3 mg/capsule SSPS in both the drug and intermediate layers markedly accelerated the pellet drug release rate compared with LNS formulation lacking SSPS (Figure 2). Accordingly, 2 mg/capsule SSPS was selected for both layers.
Figure 2. Effect of SSPS on the drug release behavior of LNS. Values are expressed as mean ± SD, *** p < 0.001.

2.1.4. Optimal Surfactant-SDS in Sustaining LNS Release

SDS is a commonly used surfactant for pharmaceutical use [21]. When SDS was incorporated into the drug layer at dosages between 0.5 and 2 mg/capsule, no significant differences in the drug release rate were observed. However, lack of SDS resulted in a significantly decreased release rate, indicating that an appropriate amount of this surfactant is necessary for drug dissolution in the drug layer (Figure S3). Finally, a dosage of 0.5 mg/capsule was selected for subsequent studies.

2.1.5. Optimal Solvent for the Drug-Layer Coating Solution

Ethanol was employed as a low-concentration solvent [5]. When using either 10% or 30% ethanol as the solvent in the drug-layer coating solution, the pellets exhibited residual solvent levels below 0.1%, which is well under the formulation limit of 0.5% (Table S2). Moreover, there were no significant differences in the profile of related substances or the release curves among the pellets prepared with these solvent concentrations (Figure S4A). Given that ethanol also functions as a defoaming agent in this context—with 30% ethanol providing superior defoaming performance—the 30% ethanol solution was selected as the solvent for the drug-layer coating process (Figure S4B).

2.1.6. Optimal Coating Weight Gain for the Intermediate Layer

An excessively low intermediate layer weight may compromise product stability during storage, while an excessively high weight gain could impede drug release [22]. Therefore, selection of an appropriate intermediate layer coating weight gain is critical. When the intermediate layer coating weight gain varied between 10% and 20%, no significant differences were observed in the drug release curves of the resultant pellets (Figure S5), and stability after 30 days of storage at 40 °C/75% RH was high across this range (Table S3). Given that higher weight gains tend to increase production time, the intermediate layer weight gain was preliminarily set between 10% and 15%.

2.1.7. Optimal Enteric Coating Material for the Enteric Layer

Differences in the physicochemical properties and solubility of enteric coating materials may influence drug release profile. Particularly, commercial products are based on a methyl methacrylate/ethyl acrylate (1:1) copolymer aqueous dispersion including Eudragit® L30D-55 (Evonik Industries, Essen, Germany) and Kollicoat® MAE 30 DP (BASF SE, Ludwigshafen, Germany), whereas Kollicoat® MAE 100 P (BASF SE, Ludwigshafen, Germany), a partially neutralized variant of the same copolymer, is also commonly used. The results showed that enteric pellets prepared with various enteric coating materials all met the acid resistance requirements. Notably, the formulation using Kollicoat® MAE 100 P exhibited the highest similarity factor (f2) in its drug release profile, which was selected as the preferred enteric coating material (Figure S6).

2.1.8. Optimal Plasticizer and Anti-Adherent for Enteric Layer

Plasticizers in the enteric coating layer enhance the flexibility and plasticity of the material, thereby altering the permeability of the enteric layer [23]. Enteric pellets prepared with varying levels of plasticizer-PEG 6000 all met the acid resistance requirements. However, an increase in the PEG 6000 proportion relative to the polymer was associated with a slower drug release rate. Notably, the similarity factor (f2) peaked when PEG 6000 constituted 10% of the polymer, leading to its selection. Likewise, anti-adherents in the enteric layer can modify the viscosity of the coating solution and the relative proportion of the enteric material, with their amounts affecting both the enteric film’s permeability and dissolution rate [24]. With respect to anti-adherent talc, when its level reached 75% relative to the polymer, the acid resistance was compromised and the drug release rate was the slowest (Figure S7); By contrast, at a talc level of 25%, partial pellet adhesion and reduced yield were observed (Table S4). Based on these factors, a talc content of 50% was chosen.

2.1.9. Optimal Solid Content of Enteric Layer Coating Solution and Coating Weight Gain

Variations in the solid content of the enteric layer solution can impact the compactness of the film and alter drug release. Furthermore, higher coating weight gain in the enteric layer generally could result in a slower drug release rate and may also affect the acid resistance of the final product [25]. The result showed that drug release profiles of samples prepared with different solid contents closely resembled those of the reference product. A total of 20% solid content in the enteric-layer coating suspension posed a spray-nozzle clogging risk; balancing production efficiency with process robustness, 18% solid content was selected. Regarding the enteric coating weight gain, all samples demonstrated acceptable acid resistance, yet a progressive reduction in the drug release rate was observed with increasing weight gain. Notably, at a 40% coating weight gain, the similarity factor (f2) of the release profile dropped below 50 (Figure S8). Consequently, the optimal enteric coating weight gain was preliminarily determined to be within the range of 30–35%.

2.1.10. Final Formulation and Component Dosage Determination

The final formulation composition and ratios were determined based on a systematic evaluation of each excipient’s functional impact on critical quality attributes (CQAs) of the product (Table 2).
Table 2. Formulation of the composition in one capsule.

2.2. Powder X-Ray Diffraction

The PXRD study was designed to evaluate whether the crystal form of LNS changes with different treatments [26]. The results of Figure 3A show that the LNS API powder shared the same PXRD pattern with LNS API after spray drying with low-concentration ethanol dispersion, including the number of diffraction peaks of the samples, the position of the diffraction peaks of 2θ value, and the relative peak intensities of the diffraction peaks. In addition, the PXRD diagrams of our new LNS pellet formulation and the reference LNS pellet formulation are almost identical (Figure 3B), indicating that the crystal form of this new LNS API pellet prepared by fluidized bed coating technology is almost the same as that of the reference marketed LNS pellets.
Figure 3. PXRD graphs of LNS and its formulation. (A) Graphs of LNS API powder and LNS API after low-concentration ethanol spray drying treatment. (B) Graphs of our new LNS pellet and reference marketed LNS pellet.

2.3. Differential Scanning Calorimetry (DSC)

The DSC studies indicated a melting endothermic peak of LNS at around 179 °C, while the exothermic peak represented the decomposition of LNS (Figure 4). The reference pellet and new LNS pellet exhibited the melting peak. However, the formulation of the new pellet contains other excipient components besides LNS, which could also affect the peak appearance. Therefore, it is difficult to determine whether the crystal form of LNS in the new pellets has changed by DSC.
Figure 4. DSC analysis of API, SSPS, new LNS pellet, and reference LNS pellet.

2.4. Fourier Transform Infrared Spectroscopy (FT-IR)

FT-IR studies were conducted to evaluate the drug–polymer interaction. The results in Figure 5 demonstrate the characteristic stretching peaks of LNS at 3236.55, 2983.88, 1579.70, 1282.66, 1118.71, and 1037.70 cm−1, which represent the stretching of –NH, –CH2–, C=N, C–N, ether band, and S=O. The characteristic peaks of LNS API powder, New LNS pellet, and the physical mixture at 3236.55, 2983.88, 1579.70, 1282.66, 1118.71, and 1037.70 cm−1 were essentially identical. These findings indicated that no hydrogen bonds were formed between LNS and the carrier materials after the preparation of new LNS pellets.
Figure 5. FT-IR analysis of pure LNS, physical mixtures, new LNS pellet, and reference LNS pellet.

2.5. Quality Evaluation of the New LNS Pellet

According to the Chinese Pharmacopoeia (ChP 2020), the acid resistance and in vitro release of the new LNS pellet containing SSPS were evaluated. The results of the acid resistance study showed that the remaining dosage of the new LNS pellet was more than 90% after 2 h in 0.1 N hydrochloric acid, indicating that this LNS formulation has high acid resistance, which can effectively avoid the destruction of acid in the drug (Figure 6A). In vitro release results indicated that the release ratio of the new LNS pellet at pH 1.2 and pH 6.0 was significantly lower than that of the reference formulation, suggesting a higher stability in acidic condition of the new LNS pellet (Figure 6B,C). The relative standard deviation RSD values obtained for the new LNS pellet formulation and the reference pellet are shown in Table S5. Both LNS pellets had similar in vitro release profiles at pH 6.8, indicating that the self-made formulation could achieve in vitro release consistency with the reference formulation (f2 > 50), ensuring that it was consistent with the reference formulation in terms of quality and efficacy (Figure 6D).
Figure 6. Evaluation of the new LNS pellet. (A) Comparison of acid resistance between new LNS pellet formulation and reference formulation. (B–D) LNS release pattern between the new LNS pellet formulation and reference formulation at different pH conditions. For (A–D) (n = 3), values are expressed as mean ± SD, * p < 0.05, *** p < 0.001.
To examine the chemical stability of our new LNS pellet during shelf-life, the LNS formulation and LNS API were stored in a closed glass vial for 30 days [27,28]. The 2020 edition of the Chinese Pharmacopoeia, Part IV, 9001, defines that a content change of 5% from the initial value is a significant difference; degradation products exceeding the standard limit requirements are a significant change. The results showed that our LNS pellet had no obvious chemical degradation of the API after 30 days (Table 3). For both long-term (30 °C/60% RH) and accelerated conditions (40 °C/75% RH), these new SSPS-containing LNS pellets had a higher release rate and acid resistance than those of the reference marketed LNS pellets (Figure 7, Table 4). These results indicated that inclusion of SSPS in LNS formulation could increase the physicochemical stability of the enteric coated pellets.
Table 3. Stability test results (30 days).
Figure 7. Stability comparison between new LNS pellet formulation and reference marketed formulation. Comparison of LNS release between new LNS pellet formulation and reference formulation under long-term condition (A) and accelerated condition (B). Comparison of acid resistance between new LNS pellet formulation and reference formulation under long-term condition (C) and accelerated condition (D). For (A–D) (n = 3), values are expressed as mean ± SD, * p < 0.05, ** p < 0.01, *** p < 0.001.
Table 4. Stability test results (90 and 180 days).

2.6. Limitations

Our work investigated the in vitro dissolution behavior of lansoprazole formulations using pH 1.2, 6.0, and 6.8 buffers as dissolution media. The obtained data could preliminarily distinguish the dissolution characteristics of different formulations, providing a reference basis for preliminary quality evaluation of the formulations. However, it should be noted that the in vitro dissolution system employed in this study has significant limitations. The human gastrointestinal tract is not a simple buffer solution system but a complex biological milieu containing bile salts, phospholipids, mucoproteins, and various digestive enzymes [29,30,31]. These biological components can significantly influence the dissolution, dispersion, and transmembrane transport processes of pH-sensitive drugs by mechanisms such as solubilization and emulsification [32,33]. The classical buffer system employed in this study, lacking these critical biological components, could not mimic the actual dissolution microenvironment of drugs within the human gastrointestinal tract. For pH-dependent drugs like LNS, the correlation between in vitro dissolution profiles and in vivo absorption processes is further diminished [34,35].
Therefore, inferences drawn from our buffer-based dissolution data regarding in vivo drug performance and clinical bioavailability hold only preliminary reference value and remain speculative. Subsequent studies in the future will incorporate biologically relevant dissolution media and integrate in vivo pharmacokinetic testing to establish in vitro–in vivo correlation (IVIVC), which will yield more accurate predictions of in vivo drug behaviors, providing more reliable theoretical support for clinical formulation applications.

3. Materials and Methods

3.1. Materials

Lansoprazole (LNS) (Guilin Huaxin Pharmaceutical Ltd., Guilin, China). LNS enteric coated capsules (Tianjin Takeda Pharmaceutical Ltd., Tianjin, China). Sucrose core/710 μm~850 μm (Hangzhou Gaocheng Biological Nutrition Technology Ltd., Zhejiang, China). Magnesium Carbonate (Hebei Best Pharmaceutical Ltd., Shijiazhuang, China). Sodium carbonate anhydrous, mannitol, sodium dodecyl sulfate (SDS), polyethylene glycol 6000 (PEG6000) (Hunan Jiudian Hongyang Pharmaceutical Ltd., Changsha, China). The lipids POPC and POPG (Pharmaceutical Tech Co., Ltd., Shanghai, China). Hydroxypropyl cellulose (HPC)/SSL (Japan Soda Ltd., Tokyo, Japan). Soluble soybean polysaccharide (SSPS) (JRS Pharma, Rosenberg, Germany). Alcohol (Xinxiang Xianfeng Pharmaceutical New Materials Ltd., Xinxiang, China). Talc (Imerys Talc Italy SpA, Milan, Italy). Kollicoat® MAE100P, Kollicoat® MAE 30 DP (BASF SE, Ludwigshafen, Germany). Eudragit® L30D-55 (Evonik Industries, Essen, Germany). No. 1 hard capsules (Anhui Mount Huangshan Capsules Ltd., Anhui, China). Trisodium phosphate, sodium hydroxide, Potassium dihydrogen phosphate (Sinopharm Chemical Reagent Co., Ltd., Shanghai, China), Hydrochloric acid (Hunan Huihong Reagent Co., Changsha, China). Sodium chloride, phosphoric acid, triethylamine (Tianjin Kermel Chemical Reagent Co., Ltd., Tianjin, China). Methanol, acetonitrile (J&K Scientific Ltd., Beijing, China).

3.2. Formulation Design and Optimization

3.2.1. Optimized Conditions of Coating by Fluidized Bed Bottom Spray Technology

The spray drying conditions for each layer in this study were preliminarily determined based on past experience and exploratory trials. To optimize process conditions, a risk assessment can guide the following approach: using experimental design and establishing atomization pressure, spray velocity, airflow rate, and bed temperature as critical process parameters. The investigation of the effects of these parameters on fine particles, agglomerates, and loss on drying for the drug layer and intermediate layer, as well as on fine particles, agglomerates, loss on drying, and dissolution for the enteric layer, determines the optimal parameter ranges for spray drying each layer in Figure 1B.

3.2.2. API Particle Size Selection

Three different API D90 values were incorporated into the initial formulation and process design studies. The primary evaluation criteria were the uniformity of the drug-layer coating solution’s composition, and the drug release performance of the drug-layer micro-pellets in a pH 6.8 phosphate buffer medium was determined using a paddle apparatus (USP Apparatus 2). The rotation speed was set at 75 rpm, and the dissolution medium (900 mL of pH 6.8 phosphate buffer) was maintained at 37.0 ± 0.5 °C. Samples were withdrawn at different sampling time points, and an equal amount of the fresh medium was added back to the vessels to maintain the sink condition. It was performed in triplicate, and the samples were analyzed using UV-Vis.

3.2.3. Selection of Alkalizer

By keeping the total amount of alkalizers constant, we evaluated the impact of common alkalizers—anhydrous sodium carbonate, sodium bicarbonate, magnesium carbonate, and tromethamine—on process feasibility and product quality. The key evaluation parameters included the content of related substances in our self-made drug-layered micro pellets, measured at day 0 and after 30 days of storage under 40 °C/75% RH, as well as the drug release performance of the micro pellets assessed via a slurry-based method in pH 6.8 phosphate buffer.

3.2.4. Study on Adhesive Usage

Drawing on the reference formulation data, we selected HPC/SSL as the adhesive in both the drug layer and the intermediate layer. In the drug layer, HPC was incorporated at 2 mg, 3 mg, and 4 mg per capsule, whereas in the intermediate layer, dosages of 5 mg and 6 mg per capsule were tested. The primary evaluation criterion was the drug release profile in a pH 6.8 phosphate buffer, measured using the slurry method.

3.2.5. Study on Disintegrant

The water-soluble disintegrant SSPS was selected. Using the slurry method, we evaluated the drug release of intermediate-layer micro pellets—prepared with SSPS incorporated into both the drug and intermediate layers—in a pH 6.8 phosphate buffer medium.

3.2.6. Study on Surfactant Usage

SDS is a commonly employed surfactant. We examined the effect of varying dosages of sodium dodecyl sulfate in the drug layer formulation on the drug release behavior of the drug-layer micro pellets. The primary evaluation criterion was the drug release profile in a pH 6.8 phosphate buffer, measured using the slurry method.

3.2.7. Study of Solvent in the Coating Solution for the Drug Layer

Equal amounts of water, 10% ethanol, and 30% ethanol were used as solvents. The evaluation metrics for the drug-layer micro pellets included the residual solvent content, the related substance profile, and the drug release behavior in a pH 6.8 phosphate buffer, as determined by the slurry method.

3.2.8. Study of Weight Gain by Intermediate Layer Coating

We assessed the impact of intermediate layer coating weight gains of 10%, 15%, and 20% on product quality. Using the slurry method, the drug release profile of the intermediate-layer micro pellets in a pH 6.8 phosphate buffer and the related substance profile of the enteric micro pellets after 30 days of storage at 40 °C/75% RH were adopted as key evaluation criteria.

3.2.9. Identification of Enteric Coating Material

Various enteric film-forming materials were used, and the water solvent was adjusted so that the enteric coating solution maintained a fixed solid content of 18%. Key performance endpoints comprised the acid resistance of the enteric-layer micro pellets and drug release profile, evaluated with the basket apparatus in pH 4.5 phosphate buffer and, after 1 h pre-exposure to pH 1.2 hydrochloric acid, in pH 6.8 phosphate buffer.

3.2.10. Study of Plasticizer and Anti-Adherent for Enteric Layer

In line with the reference formulation, PEG 6000 was selected as the plasticizer. We investigated the impact of PEG 6000 at polymer (solid) ratios of 10%, 15%, and 20% on drug release. Likewise, talc was chosen as the anti-adherent, and its impact was studied at polymer ratios of 25%, 50%, and 75%. The primary evaluation criteria were the acid resistance of the enteric micro pellets and drug-release profile, measured with the basket method after 1 h exposure to pH 1.2 hydrochloric acid and subsequent drug release testing in pH 6.8 phosphate buffer.

3.2.11. Study on the Solid Content of Enteric Layer Coating Solution and Coating Weight Gain

Using water as the solvent for the enteric coating, we investigated how solid contents of 16%, 18%, and 20% affect drug release from the enteric-layer micro pellets. Furthermore, we evaluated weight gains of 30%, 35%, and 40% as additional formulation variables. The key evaluation endpoints were the acid resistance of the enteric micro pellets and their drug release performance in pH 6.8 phosphate buffer after acid exposure, all determined using the basket method.

3.3. Formulation Measurement by High Performance Liquid Chromatography (HPLC)

3.3.1. Test Solution Preparation

We took the contents of the LNS pellet sample, accurately weighed an appropriate amount (approximately equivalent to 15 mg of LNS) by YP-B10002 Electronic Balance (Shanghai Guangzheng Medical Instrument Ltd., Shanghai, China), placed it in a 100 mL volumetric flask, added 5 mL of 0.1 M sodium hydroxide solution and about 30 mL of methanol water (60:40) solution, sonicated for about 25 min (control water temperature not exceeding 20 °C) to dissolve LNS, and it diluted with methanol water (60:40) solution; it was shaken well and filtered, and the filtrate was obtained as LNS content test solution. In addition, an appropriate amount of the contents (about 25 mg equivalent to LNS) was accurately weighed, placed in a 100 mL measuring flask, and about 70 mL of solvent [0.1 M sodium hydroxide solution-methanol (3:1)] was added; and LNS was dissolved by mechanical shaking for about 30 min, diluted, shaken, and filtered, and the filtrate was taken as the related substances’ test solution.

3.3.2. Reference Solution Preparation

Take approximately 15 mg of LNS (chemical reference standards) and place it in a 100 mL volumetric flask, add 5 mL of 0.1 M sodium hydroxide solution and approximately 30 mL of methanol water (60:40) solution, sonicate for about 25 min (control water temperature not exceeding 20 °C) to dissolve LNS, dilute with methanol water (60:40) solution, and shake well.

3.3.3. Drug Loading and Coating Efficiency

Drug loading and coating efficiency for each coating step (drug layer, intermediate layer, and enteric layer) were calculated as the following (Table S6):
Drug loading (%) = (actual drug mass in pellets/total mass of pellets) × 100%
Coating efficiency (%) = [(pellet mass after coating − pellet mass before coating)/total solids mass
in the coating dispersion used] × 100%

3.3.4. Chromatographic Analysis

According to LNS Enteric Coated Capsules Substance Standards in the US Pharmacopeia 2023 (USP2023), the chromatographic methods and impurity limits of the relevant substances are shown in the Tables S7 and S8 [14]. The chromatographic conditions for substance determination are gradient elution with the elution method, shown in Table S9.

3.3.5. Validation Parameters for the Used UPLC Method and Separation of Degradation Products by HPLC

Based on the current standards for lansoprazole enteric coated capsules listed in the Chinese Pharmacopoeia, United States Pharmacopeia, and British Pharmacopoeia, along with the synthesis route of lansoprazole, the primary impurities in lansoprazole are identified as Impurities A, B, C, D, E, and F. Among these, Impurities A, B, C, and E are degradation impurities, while Impurities D and F are process impurities. In accordance with ICH Q3B and ICH Q2, as well as the Chinese Pharmacopoeia General Chapter 9102, a related substances analytical method was established. Validation of this method was completed based on specificity, solution stability, limit of quantification and detection, precision, accuracy, and robustness. The validated method successfully separates degradation products and is suitable for sample testing (Figure S9).

3.4. Powder X-Ray Diffraction (PXRD)

PXRD was conducted on Rigaku Smart Lab 3 kW X-ray diffractometer (Rigaku Co., Ltd., Tokyo, Japan) to evaluate whether the crystal form of LNS changes before and after spray drying with low-concentration ethanol dispersion. The instrument was equipped with a Ni filter, and the voltage of the fluorescent tube was 40 kV; the scanning angle (2θ) was 3~50° with the Cu radiation source (scanning speed:10°/min; scan step size: 0.02°).

3.5. Differential Scanning Calorimetry (DSC)

DSC studies were performed on the TA Instruments Discovery DSC2500 system (TA Instruments, New Castle, DE, USA). Using a temperature range of 30 °C to 200 °C, 3–5 mg of the sample was placed in an aluminum pan and heated using a heating rate of 10 °C/min.

3.6. Fourier Transform Infrared Spectroscopy (FT-IR)

FT-IR studies were conducted on an IRAffinity-1S FT-IR Spectrometer (Shimadzu Corporation, Kyoto, Japan) in the range of 4000–400 cm−1 to study the interaction between the drug and the carrier for the physical mixture, new LNS pellet samples, reference LNS pellet samples, and LNS API powder.

3.7. Acid Resistance

According to the Chinese Pharmacopoeia 2020 (ChP 2020), an automatic dissolution instrument (Shanghai Fukesi Analytical Instrument Co., Ltd., Shanghai, China) was used to study the acid resistance in vitro [15]. Fill the equivalent of 30 mg of LNS enteric coated pellets into gelatin capsules, use 1000 mL of HCl solution (0.1 M) at 100 rpm, 120 min and 37 °C, wash the pellets in the basket with water until the solution is neutralized, and determine the pellet content according to the content determination method; ensure the LNS content in each capsule is not less than 90% of the labeled amount.

3.8. In Vitro Release

R e l e a s e   % = A s a m p l e × m r e f × C r e f × V s a m p l e × 100 A r e f × V r e f × m s a m p l e
In vitro release studies were performed using a basket apparatus according to the Pharmacopoeia of the People’s Republic of China. The equivalent of 30 mg of LNS was filled into a gelatin capsule, and drug release was studied in 500 mL of phosphate buffer (pH 6.8) for 60 min at 150 rpm and 37 °C using USP Type I apparatus. The in vitro release study for the enteric coated LNS tablet was performed as described in the Pharmacopeia. The acid stage medium was 0.1 N HCl while the buffer stage medium was pH 6.8 at a basket speed of 150 rpm for 60 min at 37 °C using USP Type I apparatus for each stage. Samples were withdrawn at different sampling time points, and an equal amount of fresh medium was added back to the vessels to maintain the sink condition. It was performed in triplicate, and the samples were analyzed using UV-Vis.
C u m u l a t i v e   R e l e a s e   % = A n + A ( n − 1 ) + A ( n − 2 ) + ⋯ + A 2 + A 1   V × V s a m p l e
where Asample and Aref are the absorbances of test sample solution and reference solution, respectively; msample and mref are the weights of sample LNS and reference LNS, respectively; and Vsample and Vref are the diluting factors of test sample solution and reference solution, respectively.
To assess the similarity between the dissolution profiles, the following similarity factor equation was used:
f 2 = 50 × lg 1 + 1 n ∑ t = 1 n ( R t − T t ) 2 − 0.5 × 100
where Rt and Tt are the percentage of drug dissolved at each time point for the reference and the test solution, respectively. n is the number of dissolution sampling times. The two dissolution profiles are considered similar if f2 ≥ 50.

3.9. Stability

To study the stability of this new LNS formulation, LNS pellet samples were stored in closed glass vials using 30 °C/65% RH and 40 °C/75% RH storage conditions for up to 6 months. The appearance, in vitro release, and drug content analysis were used to investigate physical and chemical stability. In addition, LNS pellet samples were stored in closed glass vials under accelerated conditions of 40 °C/75% RH for 30 days, and their stability was compared with LNS API. The studies were performed in triplicate.

3.10. Statistical Analyses

All the experiments were tested at least three times. All data were expressed as the mean ± SD. Student’s t-test, ANOVA, and post hoc statistical analyses were used to process and analyze routine data. p < 0.05 represents statistically significant.

4. Conclusions

In this study, SSPS were selected as critical excipients for the preparation of LNS pellet in pharmaceutical processing, which improved the solubility and stability of LNS pellet. Our new SSPS-containing LNS pellets had a higher release rate and acid resistance than those of reference marketed LNS pellets under both long-term (30 °C/60% RH) and accelerated conditions (40 °C/75% RH). We conclude that inclusion of SSPS in LNS formulation could increase the physicochemical stability of the enteric coated capsules during shelf-life, laying the basis of SSPS for further use as promising soluble vehicles and disintegrants in pharmaceutical formulations.

Supplementary Materials

The following supporting information can be downloaded at: https://www.mdpi.com/article/10.3390/ph19020213/s1, Figure S1: Effect of different API D90 particle sizes. (A) Homogeneity of the drug layer coating solution. (B) Drug release behavior of LNS; Figure S2: Effect of different alkalizers on the drug release behavior of LNS; Figure S3: Effect of SDS amount on the drug release behavior of LNS; Figure S4: Effect of solvent for the drug layer coating solution on LNS pellet. (A) Effect of solvent the drug release behavior of LNS pellet. (B) Effect of solvent on the deforming performance; Figure S5: Effect of Intermediate Layer Coating Weight Gain on the drug release behavior of LNS; Figure S6: Evaluation of different enteric coating materials. (A) Acid resistance results. (B,C) Drug release behavior of LNS in different phosphate buffer; Figure S7: Evaluation of different plasticizer and anti-adherent. (A,B) Acid resistance results. (C,D) Drug release behavior of LNS; Figure S8: (A) Effect of different solid content of enteric layer coating solution on the drug release behavior of LNS. (B) Effect of different coating weight gain on the drug release behavior of LNS; Figure S9: Separation of degradation products by HPLC; Table S1: Effect of Alkalizer Type on Coating pH and Stability; Table S2: Effect of Ethanol on Stability; Table S3: Stability of Enteric pellet at 40 °C/75% RH; Table S4: Evaluation of different anti-adherent; Table S5: Dissolution Curve Data for Reference Preparation (pH 1.2–pH 6.8, 150 rpm) (n = 12); Table S6: Drug loading and coating efficiency; Table S7: Chromatographic Conditions; Table S8: Limits of Related Substances; Table S9: Gradient Elution for Related Substances.

Author Contributions

Conceptualization, methodology, formal analysis, writing—original draft, H.Z. and W.Y.; visualization, project administration, investigation, D.L.; software, validation, formal analysis, Y.L., X.W. and B.J.; supervision, funding acquisition, project administration, writing—review and editing, L.S. All authors have read and agreed to the published version of the manuscript.

Funding

This research was supported by the Natural Science Foundation of Hunan Province, China (Grant No. 2025JJ60775 to Leisheng Sun), the Natural Science Foundation of Changsha City, China (Grant No. kq2502182 to Leisheng Sun), the Excellent Youth Program of Hunan Provincial Department of Education (Grant No. 23B0051 to Leisheng Sun), and Innovative Training Program for Undergraduates in Hunan Province (No. S202510542425 to Xianping Wu and Leisheng Sun).

Data Availability Statement

Data are contained within the article.

Conflicts of Interest

The authors declare no conflicts of interest.

References

  1. Garnett, W.R. Lansoprazole: A Proton Pump Inhibitor. Ann. Pharmacother. 1996, 30, 1425–1436. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  2. Choi, I.J.; Kim, C.G.; Lee, J.Y.; Kim, Y.I.; Kook, M.C.; Park, B.; Joo, J. Family History of Gastric Cancer and Helicobacter pylori Treatment. N. Engl. J. Med. 2020, 382, 427–436. [Google Scholar] [CrossRef] [Scilit]
  3. Shimizu, T.; Nakano, Y.; Morimoto, S.; Tabata, T.; Hamaguchi, N.; Igari, Y. Formulation Study for Lansoprazole Fast-Disintegrating Tablet. I. Effect of Compression on Dissolution Behavior. Chem. Pharm. Bull. 2003, 51, 942–947. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  4. Alsulays, B.B.; Kulkarni, V.; Alshehri, S.M.; Almutairy, B.K.; Ashour, E.A.; Morott, J.T.; Alshetaili, A.S.; Park, J.B.; Tiwari, R.V.; Repka, M.A. Preparation and Evaluation of Enteric Coated Tablets of Hot-Melt Extruded Lansoprazole. Drug Dev. Ind. Pharm. 2017, 43, 789–796. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  5. Srebro, J.; Brniak, W.; Mendyk, A. Formulation of Dosage Forms with Proton Pump Inhibitors: State of the Art, Challenges and Future Perspectives. Pharmaceutics 2022, 14, 2043. [Google Scholar] [CrossRef] [Scilit]
  6. LiverTox: Clinical and Research Information on Drug-Induced Liver Injury; National Institute of Diabetes and Digestive and Kidney Diseases: Bethesda, MD, USA, 2012.
  7. Loh, Z.H.; Er, D.Z.; Chan, L.W.; Liew, C.V.; Heng, P.W. Spray Granulation for Drug Formulation. Expert Opin. Drug Deliv. 2011, 8, 1645–1661. [Google Scholar] [CrossRef] [Scilit]
  8. Wang, L.K.; Heng, P.W.; Liew, C.V. Classification of Annular Bed Flow Patterns and Investigation on Their Influence on the Bottom Spray Fluid Bed Coating Process. Pharm. Res. 2010, 27, 756–766. [Google Scholar] [CrossRef] [Scilit]
  9. He, W.; Yang, M.; Fan, J.H.; Feng, C.X.; Zhang, S.J.; Wang, J.X.; Guan, P.P.; Wu, W. Influences of Sodium Carbonate on Physicochemical Properties of Lansoprazole in Designed Multiple Coating Pellets. AAPS PharmSciTech 2010, 11, 1287–1293. [Google Scholar] [CrossRef] [Scilit]
  10. Hosny, K.M.; Mosli, H.A.; Hassan, A.H. Soy polysaccharide as a Novel Superdisintegrant in Sildenafil Citrate Sublingual Tablets: Preparation, Characterization, and In Vivo Evaluation. Drug Des. Dev. Ther. 2015, 9, 465–472. [Google Scholar] [CrossRef] [Scilit]
  11. Lu, Y.; Li, W.; Yang, X. Soluble Soybean Polysaccharides Enhance the Protective Effects of Genistein Against Hepatic Injury in High l-Carnitine-Fed Mice. Food Funct. 2017, 8, 4364–4373. [Google Scholar] [CrossRef] [Scilit]
  12. Anwar, S.H.; Weissbrodt, J.; Kunz, B. Microencapsulation of Fish Oil by Spray Granulation and Fluid Bed Film Coating. J. Food Sci. 2010, 75, E359–E371. [Google Scholar] [CrossRef] [Scilit]
  13. Gerloff, J.; Mignot, A.; Barth, H.; Heintze, K. Pharmacokinetics and Absolute Bioavailability of Lansoprazole. Eur. J. Clin. Pharmacol. 1996, 50, 293–297. [Google Scholar] [CrossRef] [Scilit]
  14. Little, H.J. Alcohol is a Drug; a Cautionary Note on Its Use as a Drug Solvent. Psychopharmacology 2004, 171, 234–235. [Google Scholar] [CrossRef] [Scilit]
  15. Gupta, A.; Paudwal, G.; Dolkar, R.; Lewis, S.; Gupta, P.N. Recent Advances in the Surfactant and Controlled Release Polymer-Based Solid Dispersion. Curr. Pharm. Des. 2022, 28, 1643–1659. [Google Scholar] [CrossRef] [Scilit]
  16. Liu, J.; Klinzing, G.R.; Nie, H. Effect of Material Properties and Variability of Mannitol on Tablet Formulation Development. Pharm. Res. 2023, 40, 2071–2085. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  17. Zhang, M.; Rough, S.L.; Ward, R.; Seiler, C.; Wilson, D.I. Non-Aqueous Formulations for Ram and Screen Extrusion-Spheronisation. Int. J. Pharm. 2019, 560, 394–405. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  18. Scheiffele, S.; Kolter, K.; Schepky, G. Studies comparing Kollicoat MAE 30 D with Commercial Cellulose Derivatives for Enteric Coating on Caffeine Cores. Drug Dev. Ind. Pharm. 1998, 24, 807–818. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  19. Huang, C.Y.; Ku, S.M. Prediction of Drug Particle Size and Content Uniformity in Low-Dose Solid Dosage Forms. Int. J. Pharm. 2010, 383, 70–80. [Google Scholar] [CrossRef] [Scilit]
  20. Almotairy, A.; Almutairi, M.; Althobaiti, A.; Alyahya, M.; Sarabu, S.; Alzahrani, A.; Zhang, F.; Bandari, S.; Repka, M.A. Effect of pH Modifiers on the Solubility, Dissolution Rate, and Stability of Telmisartan Solid Dispersions Produced by Hot-melt Extrusion Technology. J. Drug Deliv. Sci. Technol. 2021, 65, 102674. [Google Scholar] [CrossRef] [Scilit]
  21. Balakrishnan, A.; Rege, B.D.; Amidon, G.L.; Polli, J.E. Surfactant-Mediated Dissolution: Contributions of Solubility Enhancement and Relatively Low Micelle Diffusivity. J. Pharm. Sci. 2004, 93, 2064–2075. [Google Scholar] [CrossRef] [Scilit]
  22. Xu, X.; Xu, H.; Shang, Y.; Zhu, R.; Hong, X.; Song, Z.; Yang, Z. Development of the general chapters of the Chinese Pharmacopoeia 2020 Edition: A review. J. Pharm. Anal. 2021, 11, 398–404. [Google Scholar] [CrossRef] [Scilit]
  23. Nair, A.B.; Gupta, R.; Kumria, R.; Jacob, S.; Attimarad, M. Formulation and Evaluation of Enteric Coated Tablets of Proton Pump Inhibitor. J. Basic Clin. Pharm. 2010, 1, 215–221. [Google Scholar]
  24. Kriangkrai, W.; Puttipipatkhachorn, S.; Sriamornsak, P.; Pongjanyakul, T.; Sungthongjeen, S. Impact of Anti-Tacking Agents on Properties of Gas-Entrapped Membrane and Effervescent Floating Tablets. AAPS PharmSciTech 2014, 15, 1357–1369. [Google Scholar] [CrossRef] [Scilit]
  25. Arafat, M.; Sakkal, M.; Bostanudin, M.F.; Alhanbali, O.A.; Yuvaraju, P.; Beiram, R.; Sadek, B.; Akour, A.; AbuRuz, S. Enteric-coating Film Effect on the Delayed Drug Release of Pantoprazole Gastro-Resistant Generic Tablets. F1000Research 2023, 12, 1325. [Google Scholar] [CrossRef] [Scilit]
  26. Thakral, N.K.; Zanon, R.L.; Kelly, R.C.; Thakral, S. Applications of Powder X-Ray Diffraction in Small Molecule Pharmaceuticals: Achievements and Aspirations. J. Pharm. Sci. 2018, 107, 2969–2982. [Google Scholar] [CrossRef] [Scilit]
  27. Vora, C.; Patadia, R.; Mittal, K.; Mashru, R. Formulation Development, Process Optimization, and In Vitro Characterization of Spray-Dried Lansoprazole Enteric Microparticles. Sci. Pharm. 2016, 84, 393–408. [Google Scholar] [CrossRef] [Scilit]
  28. Mehta, M.; Suryanarayanan, R. Accelerated Physical Stability Testing of Amorphous Dispersions. Mol. Pharm. 2016, 13, 2661–2666. [Google Scholar] [CrossRef] [Scilit]
  29. Zhang, M.; Zuo, Z.; Zhang, X.; Wang, L. Food Biopolymer Behaviors in the Digestive Tract: Implications for Nutrient Delivery. Crit. Rev. Food Sci. Nutr. 2024, 64, 8709–8727. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  30. Di Marzio, L.; Esposito, S.; Rinaldi, F.; Marianecci, C.; Carafa, M. Polysorbate 20 Vesicles as Oral Delivery System: In Vitro Characterization. Colloids Surf. B Biointerfaces 2013, 104, 200–206. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  31. Hundt, M.; Basit, H.; John, S. Physiology, Bile Secretion. In StatPearls; StatPearls Publishing LLC.: Treasure Island, FL, USA, 2025. [Google Scholar]
  32. Mudie, D.M.; Amidon, G.L.; Amidon, G.E. Physiological Parameters for Oral Delivery and In Vitro Testing. Mol. Pharm. 2010, 7, 1388–1405. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  33. Kleberg, K.; Jacobsen, J.; Müllertz, A. Characterising the Behaviour of Poorly Water Soluble Drugs in the Intestine: Application of Biorelevant Media for Solubility, Dissolution and Transport Studies. J. Pharm. Pharmacol. 2010, 62, 1656–1668. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  34. Liu, F.; Shokrollahi, H. In Vitro Dissolution of Proton-Pump Inhibitor Products Intended for Paediatric and Geriatric Use in Physiological Bicarbonate Buffer. Int. J. Pharm. 2015, 485, 152–159. [Google Scholar] [CrossRef] [Scilit] [PubMed]
  35. Stefanič, M.; Vrečer, F.; Rizmal, P.; Mrhar, A.; Bogataj, M. Prediction of the In Vivo Performance of Enteric Coated Pellets in the Fasted State Under Selected Biorelevant Dissolution Conditions. Eur. J. Pharm. Sci. 2014, 62, 8–15. [Google Scholar] [CrossRef] [Scilit] [PubMed]
Disclaimer/Publisher’s Note: The statements, opinions and data contained in all publications are solely those of the individual author(s) and contributor(s) and not of MDPI and/or the editor(s). MDPI and/or the editor(s) disclaim responsibility for any injury to people or property resulting from any ideas, methods, instructions or products referred to in the content.

Article Metrics

Citations

Article Access Statistics

Multiple requests from the same IP address are counted as one view.