Skip to Content
MaterialsMaterials
  • Article
  • Open Access

12 December 2022

18 Pages

Effect of Mg Powder’s Particle Size on Structure and Mechanical Properties of Ti Foam Synthesized by Space Holder Technique

,
,
,
and
1
School of Metallurgy, Northeastern University, Shenyang 110819, China
2
Engineering Technology Research Center of Ministry of Education for Materials Advanced Preparation, Shenyang 110819, China
3
School of Naval Architecture and Ocean Engineering, Guangzhou Maritime University, Guangzhou 510725, China
4
Beijing Foton Daimler Automobile Co., Ltd., Beijing 101400, China

Abstract

Titanium foam has been the focus of special attention for its specific structure and potential applications in purification, catalyst substrate, heat exchanger, biomaterial, aerospace and naval industries. However, the liquid-state foaming techniques are difficult to use in fabricating Ti foam because of its high melting temperature and strong chemical reactivity with atmospheric gases. Here, the fabrication of Ti foams via the powder metallurgy route was carried out by utilizing both magnesium powders and magnesium particles as spacer holders, and Ti powders as matrix metal. The green compacts containing Ti powder, Mg powder and Mg particles were heated to a certain temperature to remove the magnesium and obtain the Ti foam. The results show that the porosities of the obtained Ti foam are about 35–65%, and Young’s modulus and yield strength are found to be in the ranges of 22–126 MPa and 0.063–1.18 GPa, respectively. It is found that the magnesium powders play a more important role than the magnesium particles in the deformation and the densification of the green compact during the pressing, and the pore structure of Ti foam depends on the amount and the size of the magnesium spacer holders after sintering.