A Dipping Duration Study for Optimization of Anodized-Aluminum Pressure-Sensitive Paint

Aerospace Research and Development Directorate, Japan Aerospace Exploration Agency/Chofu, Tokyo 182-8522, Japan
*
Author to whom correspondence should be addressed.
Sensors 2010, 10(11), 9799-9807; https://doi.org/10.3390/s101109799
Received: 5 September 2010 / Revised: 28 October 2010 / Accepted: 1 November 2010 / Published: 2 November 2010
(This article belongs to the Section Chemical Sensors)
Anodized-aluminum pressure-sensitive paint (AA-PSP) uses the dipping deposition method to apply a luminophore on a porous anodized-aluminum surface. We study the dipping duration, one of the parameters of the dipping deposition related to the characterization of AA-PSP. The dipping duration was varied from 1 to 100,000 s. The properties characterized are the pressure sensitivity, temperature dependency, and signal level. The maximum pressure sensitivity of 65% is obtained at the dipping duration of 100 s, the minimum temperature dependency is obtained at the duration of 1 s, and the maximum signal level is obtained at the duration of 1,000 s, respectively. Among the characteristics, the dipping duration most influences the signal level. The change in the signal level is a factor of 8.4. By introducing a weight coefficient, an optimum dipping duration can be determined. Among all the dipping parameters, such as the dipping duration, dipping solvent, and luminophore concentration, the pressure sensitivity and signal level are most influenced by the dipping solvent. View Full-Text
Keywords: anodized aluminum; pressure-sensitive paint; dipping duration anodized aluminum; pressure-sensitive paint; dipping duration
Show Figures

MDPI and ACS Style

Sakaue, H.; Ishii, K. A Dipping Duration Study for Optimization of Anodized-Aluminum Pressure-Sensitive Paint. Sensors 2010, 10, 9799-9807. https://doi.org/10.3390/s101109799

AMA Style

Sakaue H, Ishii K. A Dipping Duration Study for Optimization of Anodized-Aluminum Pressure-Sensitive Paint. Sensors. 2010; 10(11):9799-9807. https://doi.org/10.3390/s101109799

Chicago/Turabian Style

Sakaue, Hirotaka, and Keiko Ishii. 2010. "A Dipping Duration Study for Optimization of Anodized-Aluminum Pressure-Sensitive Paint" Sensors 10, no. 11: 9799-9807. https://doi.org/10.3390/s101109799

Find Other Styles

Article Access Map by Country/Region

1
Only visits after 24 November 2015 are recorded.
Back to TopTop