Haq, A.u.; Hussein, R.K.; Panchal, S.; Saeed, M.; Abubakar, H.M.; Alrub, S.A.
Solar-Driven Photocatalytic Degradation of Clothianidin Using Green NiO-GO Composite. Catalysts 2025, 15, 1078.
https://doi.org/10.3390/catal15111078
AMA Style
Haq Au, Hussein RK, Panchal S, Saeed M, Abubakar HM, Alrub SA.
Solar-Driven Photocatalytic Degradation of Clothianidin Using Green NiO-GO Composite. Catalysts. 2025; 15(11):1078.
https://doi.org/10.3390/catal15111078
Chicago/Turabian Style
Haq, Atta ul, Rageh K. Hussein, Sandeep Panchal, Muhammad Saeed, Hafiz Muhammad Abubakar, and Sharif Abu Alrub.
2025. "Solar-Driven Photocatalytic Degradation of Clothianidin Using Green NiO-GO Composite" Catalysts 15, no. 11: 1078.
https://doi.org/10.3390/catal15111078
APA Style
Haq, A. u., Hussein, R. K., Panchal, S., Saeed, M., Abubakar, H. M., & Alrub, S. A.
(2025). Solar-Driven Photocatalytic Degradation of Clothianidin Using Green NiO-GO Composite. Catalysts, 15(11), 1078.
https://doi.org/10.3390/catal15111078