Wu, J.; Bai, G.; Zhao, L.; Zhang, Z.; Peng, Y.; Chu, J.; Wang, Q.
Effects of Finish Rolling Temperature on the Critical Crack Tip Opening Displacement (CTOD) of Typical 500 MPa Grade Weathering Steel. Metals 2023, 13, 1791.
https://doi.org/10.3390/met13101791
AMA Style
Wu J, Bai G, Zhao L, Zhang Z, Peng Y, Chu J, Wang Q.
Effects of Finish Rolling Temperature on the Critical Crack Tip Opening Displacement (CTOD) of Typical 500 MPa Grade Weathering Steel. Metals. 2023; 13(10):1791.
https://doi.org/10.3390/met13101791
Chicago/Turabian Style
Wu, Junping, Guangming Bai, Liyang Zhao, Zhongde Zhang, Yan Peng, Juefei Chu, and Qingfeng Wang.
2023. "Effects of Finish Rolling Temperature on the Critical Crack Tip Opening Displacement (CTOD) of Typical 500 MPa Grade Weathering Steel" Metals 13, no. 10: 1791.
https://doi.org/10.3390/met13101791
APA Style
Wu, J., Bai, G., Zhao, L., Zhang, Z., Peng, Y., Chu, J., & Wang, Q.
(2023). Effects of Finish Rolling Temperature on the Critical Crack Tip Opening Displacement (CTOD) of Typical 500 MPa Grade Weathering Steel. Metals, 13(10), 1791.
https://doi.org/10.3390/met13101791