You are currently viewing a new version of our website. To view the old version click .
Metals
  • Correction
  • Open Access

18 September 2025

Correction: Ou et al. Manufacturing and Characterization of NiTi Alloy with Functional Properties by Selective Laser Melting. Metals 2018, 8, 342

,
,
and
1
Institute of Mold & Die Engineering, National Kaohsiung University of Applied Sciences, Kaohsiung 807, Taiwan
2
School of Dentistry, College of Oral Medicine, Taipei Medical University, Taipei 110, Taiwan
3
Division of Oral and Maxillofacial Surgery, Department of Dentistry, Taipei Medical University Hospital, Taipei 110, Taiwan
4
Casting Section, Metal Industries Research & Development Centre, Kaohsiung 811, Taiwan
In the original publication [1], there was a mistake in Figure 4. The authors plotted two curves using the same dataset. The corrected Figure 4 appears below. The authors state that the scientific conclusions are unaffected. This correction was approved by the Academic Editor. The original publication has also been updated.
Figure 4. X-ray diffractometry (XRD) spectra of NiTi powder with particle sizes of <25 μm, 25–45 μm, and >45 μm.

Reference

  1. Ou, S.-F.; Peng, B.-Y.; Chen, Y.-C.; Tsai, M.-H. Manufacturing and Characterization of NiTi Alloy with Functional Properties by Selective Laser Melting. Metals 2018, 8, 342. [Google Scholar] [CrossRef]
Disclaimer/Publisher’s Note: The statements, opinions and data contained in all publications are solely those of the individual author(s) and contributor(s) and not of MDPI and/or the editor(s). MDPI and/or the editor(s) disclaim responsibility for any injury to people or property resulting from any ideas, methods, instructions or products referred to in the content.

Article Metrics

Citations

Article Access Statistics

Multiple requests from the same IP address are counted as one view.