Correction: Tasnim Mowri et al. Assessing the Impact of First-Life Lithium-Ion Battery Degradation on Second-Life Performance. Energies 2024, 17, 501
| Cell | Cycle | SoH | P4 | P3 | P2 | P1 |
| 1 | 120 | 94.17 | LLI | LAM | U | U |
| 355 | 90.38 | LLI | LLI | LAM | U | |
| 585 | 84.15 | LLI | LLI | LAM | LLI | |
| 596 | 80.58 | LAM | LLI | LAM | LLI | |
| 2 | 120 | 94.55 | LLI | LAM | U | U |
| 355 | 90.74 | LLI | LLI | LAM | U | |
| 585 | 84.07 | LLI | LLI | LAM | LLI | |
| 596 | 80.54 | LAM | LLI | LAM | LLI | |
| 3 | 120 | 94.07 | LLI | LAM | U | U |
| 355 | 90.28 | LLI | LLI | LAM | U | |
| 585 | 83.33 | LLI | LLI | LAM | LLI | |
| 596 | 78.76 | LAM | LLI | LAM | LLI | |
| 4 | 120 | 94.51 | LLI | LAM | U | U |
| 355 | 90.58 | LLI | LLI | U | U | |
| 505 | 85.57 | LAM | LLI | LAM | U | |
| 525 | 77.56 | LAM | LLI | LAM | LLI |
| Cell | Cycle | SoH | P4 | P3 | P2 | P1 |
| 5 | 52 | 95.59 | LLI | LAM | LAM | U |
| 230 | 79.54 | LAM | LLI | LLI | LLI | |
| 14 | 80 | 94.15 | LAM | LAM | LLI | U |
| 125 | 89.52 | LLI | LLI | LLI | U | |
| 175 | 84.47 | LAM | LLI | LLI | LLI | |
| 187 | 77.96 | LAM | LLI | LLI | LLI | |
| 15 | 80 | 94.37 | LAM | LAM | LAM | U |
| 175 | 89.18 | LLI | LLI | LLI | U | |
| 230 | 85.37 | LLI | LLI | LLI | LLI | |
| 285 | 78.36 | LAM | LLI | LLI | LLI | |
| 16 | 80 | 94.31 | LLI | LAM | LLI | U |
| 125 | 90.06 | LLI | LLI | LLI | U | |
| 175 | 83.65 | LAM | LLI | LLI | LLI | |
| 182 | 79.74 | LAM | LLI | LLI | LLI | |
| 17 | 80 | 94.11 | LAM | LAM | LLI | U |
| 125 | 89.18 | LLI | LLI | LLI | U | |
| 175 | 83.17 | LAM | LLI | LLI | LLI | |
| 183 | 79.76 | LAM | LLI | LLI | LLI | |
| 18 | 100 | 93.39 | LLI | LAM | LAM | U |
| 180 | 89.38 | LLI | LLI | LLI | U | |
| 245 | 84.37 | LAM | LLI | LLI | U | |
| 280 | 80.56 | LAM | LLI | LLI | LLI | |
| Cell | Cycle | SoH % | P4 | P3 | P2 | P1 |
| 7 | 52 | 95.25 | LAM | LAM | U | U |
| 225 | 81.30 | LLI | LLI | LLI | LLI | |
| 230 | 79.72 | PD | LLI | LLI | LLI | |
| 8 | 52 | 95.11 | LAM | LAM | U | U |
| 225 | 81.24 | LLI | LLI | LLI | LLI | |
| 230 | 79.26 | PD | LLI | LLI | LLI | |
| 9 | 150 | 94.39 | LLI | LAM | LAM | U |
| 520 | 89.98 | LLI | LAM | LLI | U | |
| 570 | 85.57 | PD | LLI | LAM | LLI | |
| 600 | 81.16 | PD | LLI | LLI | LLI | |
| 10 | 150 | 94.34 | LLI | LAM | LAM | U |
| 520 | 88.98 | LLI | LAM | LLI | LLI | |
| 570 | 84.37 | PD | LLI | LAM | LLI | |
| 600 | 79.76 | PD | LLI | LLI | LLI | |
| Cell | Cycle | SoH % | P4 | P3 | P2 | P1 |
| 6 | 52 | 95.45 | LAM | LAM | LAM | U |
| 247 | 79.56 | LLI | LLI | LLI | LLI | |
| 11 | 150 | 94.28 | LLI | LAM | LAM | U |
| 300 | 91.88 | LLI | LAM | LLI | U | |
| 370 | 85.97 | LLI | LLI | LAM | LLI | |
| 403 | 81.16 | LLI | LLI | LLI | LLI | |
| 12 | 40 | 95.87 | LAM | LAM | LAM | U |
| 120 | 89.58 | LAM | LAM | LAM | U | |
| 190 | 84.23 | LAM | LLI | LLI | LLI | |
| 201 | 80.2 | LLI | LLI | LLI | LLI | |
| 13 | 40 | 96.13 | LAM | LAM | LAM | U |
| 120 | 78.58 | LLI | LLI | LLI | LLI | |
Reference
- Mowri, S.T.; Barai, A.; Moharana, S.; Gupta, A.; Marco, J. Assessing the Impact of First-Life Lithium-Ion Battery Degradation on Second-Life Performance. Energies 2024, 17, 501. [Google Scholar] [CrossRef]
Disclaimer/Publisher’s Note: The statements, opinions and data contained in all publications are solely those of the individual author(s) and contributor(s) and not of MDPI and/or the editor(s). MDPI and/or the editor(s) disclaim responsibility for any injury to people or property resulting from any ideas, methods, instructions or products referred to in the content. |
© 2024 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/).
Share and Cite
Tasnim Mowri, S.; Barai, A.; Moharana, S.; Gupta, A.; Marco, J. Correction: Tasnim Mowri et al. Assessing the Impact of First-Life Lithium-Ion Battery Degradation on Second-Life Performance. Energies 2024, 17, 501. Energies 2024, 17, 3402. https://doi.org/10.3390/en17143402
Tasnim Mowri S, Barai A, Moharana S, Gupta A, Marco J. Correction: Tasnim Mowri et al. Assessing the Impact of First-Life Lithium-Ion Battery Degradation on Second-Life Performance. Energies 2024, 17, 501. Energies. 2024; 17(14):3402. https://doi.org/10.3390/en17143402
Chicago/Turabian StyleTasnim Mowri, Sadia, Anup Barai, Sanghamitra Moharana, Aniruddha Gupta, and James Marco. 2024. "Correction: Tasnim Mowri et al. Assessing the Impact of First-Life Lithium-Ion Battery Degradation on Second-Life Performance. Energies 2024, 17, 501" Energies 17, no. 14: 3402. https://doi.org/10.3390/en17143402
APA StyleTasnim Mowri, S., Barai, A., Moharana, S., Gupta, A., & Marco, J. (2024). Correction: Tasnim Mowri et al. Assessing the Impact of First-Life Lithium-Ion Battery Degradation on Second-Life Performance. Energies 2024, 17, 501. Energies, 17(14), 3402. https://doi.org/10.3390/en17143402