28 pages, 4810 KB  
Article
Recycled Polypropylene Composites Reinforced with Microcellulose Fibres and Microcellulose-Derived Biochar: Thermal, Rheological and Mechanical Performance
by Wiktor Wyderkiewicz, Justyna Miedzianowska-Masłowska, Anna Sowińska-Baranowska and Marcin Masłowski
Materials 2026, 19(10), 1942; https://doi.org/10.3390/ma19101942 - 9 May 2026
Viewed by 592
Abstract
The mechanical recycling of mono-material biaxially oriented polypropylene (BOPP) packaging films produces recycled polypropylene (rPP) with degraded properties, limiting its use in higher-performance applications. This study investigates rPP reinforcement with 6–12 µm microcellulose fibres (MCFs, 2–10 pbw) and microcellulose-derived biochar (BC, 5–20 pbw), [...] Read more.
The mechanical recycling of mono-material biaxially oriented polypropylene (BOPP) packaging films produces recycled polypropylene (rPP) with degraded properties, limiting its use in higher-performance applications. This study investigates rPP reinforcement with 6–12 µm microcellulose fibres (MCFs, 2–10 pbw) and microcellulose-derived biochar (BC, 5–20 pbw), characterized by DSC, TGA/DTG, MVR/MFR, temperature-dependent rheology, mechanical testing and water contact angle (WCA) measurements. Both fillers acted as heterogeneous nucleating agents, shifting crystallization by up to 4 °C and increasing crystallinity by 2–4%. MCF introduced an additional low-temperature degradation step, whereas BC increased onset and peak degradation temperatures by up to 20 °C and increased char yield. Low MCF loadings increased MVR/MFR by 20–25% and reduced melt viscosity, while BC decreased flow indices by up to 50% and stiffened the melt. Tensile and flexural moduli increased by 15–25% with MCF and 40–50% with BC, with a stiffness–toughness trade-off at the highest BC contents. MCF reduced the water contact angle to 63.0° at 10 pbw, while BC increased it to 108.1° at 20 pbw, indicating opposite effects on surface wettability. Converting a single cellulosic feedstock into fibrous or carbonised fillers enables bio-based upgrading of rPP, in line with circular economy principles. Full article
(This article belongs to the Special Issue Advanced Polymer Matrix Nanocomposite Materials (3rd Edition))