Meng, T.; Young, K.-h.; Koch, J.; Ouchi, T.; Yasuoka, S.
Failure Mechanisms of Nickel/Metal Hydride Batteries with Cobalt-Substituted Superlattice Hydrogen-Absorbing Alloy Anodes at 50 °C. Batteries 2016, 2, 20.
https://doi.org/10.3390/batteries2030020
AMA Style
Meng T, Young K-h, Koch J, Ouchi T, Yasuoka S.
Failure Mechanisms of Nickel/Metal Hydride Batteries with Cobalt-Substituted Superlattice Hydrogen-Absorbing Alloy Anodes at 50 °C. Batteries. 2016; 2(3):20.
https://doi.org/10.3390/batteries2030020
Chicago/Turabian Style
Meng, Tiejun, Kwo-hsiung Young, John Koch, Taihei Ouchi, and Shigekazu Yasuoka.
2016. "Failure Mechanisms of Nickel/Metal Hydride Batteries with Cobalt-Substituted Superlattice Hydrogen-Absorbing Alloy Anodes at 50 °C" Batteries 2, no. 3: 20.
https://doi.org/10.3390/batteries2030020
APA Style
Meng, T., Young, K.-h., Koch, J., Ouchi, T., & Yasuoka, S.
(2016). Failure Mechanisms of Nickel/Metal Hydride Batteries with Cobalt-Substituted Superlattice Hydrogen-Absorbing Alloy Anodes at 50 °C. Batteries, 2(3), 20.
https://doi.org/10.3390/batteries2030020