Handschuh-Wang, S.; Wang, T.; Zhang, Z.; Liu, F.; Han, P.; Liu, X.
Long-Term Corrosion of Eutectic Gallium, Indium, and Tin (EGaInSn) Interfacing with Diamond. Materials 2024, 17, 2683.
https://doi.org/10.3390/ma17112683
AMA Style
Handschuh-Wang S, Wang T, Zhang Z, Liu F, Han P, Liu X.
Long-Term Corrosion of Eutectic Gallium, Indium, and Tin (EGaInSn) Interfacing with Diamond. Materials. 2024; 17(11):2683.
https://doi.org/10.3390/ma17112683
Chicago/Turabian Style
Handschuh-Wang, Stephan, Tao Wang, Zongyan Zhang, Fucheng Liu, Peigang Han, and Xiaorui Liu.
2024. "Long-Term Corrosion of Eutectic Gallium, Indium, and Tin (EGaInSn) Interfacing with Diamond" Materials 17, no. 11: 2683.
https://doi.org/10.3390/ma17112683
APA Style
Handschuh-Wang, S., Wang, T., Zhang, Z., Liu, F., Han, P., & Liu, X.
(2024). Long-Term Corrosion of Eutectic Gallium, Indium, and Tin (EGaInSn) Interfacing with Diamond. Materials, 17(11), 2683.
https://doi.org/10.3390/ma17112683