15 pages, 9796 KiB  
Article
Microstructure, Mechanical Properties and Wear Behaviors of Ultrafine-Grain WC-Based Cermets with Different Binder Phases Fabricated by Spark Plasma Sintering
by Kangwei Xu, Zhe Wang, Peipei Cao, Xiangyang Peng, Chao Chen, Qingsong Liu, Shufeng Xie, Xiaoyu Wu and Yongxin Jian
Materials 2024, 17(3), 659; https://doi.org/10.3390/ma17030659 - 29 Jan 2024
Cited by 3 | Viewed by 1556
Abstract
In this work, to explore potential substitutions for the Co binder phase, ultrafine-grain WC-based cermets with various binder phases of Co, Ni and AlCoCrNiFeCu HEA were prepared using the SPS method. Based on SPS, WC-based cermets were fabricated at higher speed, showing fine [...] Read more.
In this work, to explore potential substitutions for the Co binder phase, ultrafine-grain WC-based cermets with various binder phases of Co, Ni and AlCoCrNiFeCu HEA were prepared using the SPS method. Based on SPS, WC-based cermets were fabricated at higher speed, showing fine carbide particles less than 410 μm. The microstructure, mechanical properties and wear properties were systematically evaluated. By comparison, the grain size of WC was the lowest for WC-10Co, while WC-10 HEA cermet held the coarsest WC particles. The hardness and fracture toughness of WC-10 HEA were the best among all three samples, with values of 93.2 HRA and 11.3 MP·m1/2. However, the bending strength of WC-10HEA was about 56.1% lower than that of WC-10Co, with a value of 1349.6 MPa. The reduction in bending strength is attributed to the lower density, formation of a newly Cr-Al rich phase and coarser WC grains. In dry sliding wear conditions, WC-10 HEA showed the lowest wear rate (0.98 × 10−6 mm3/(N·m)) and coefficient of friction (0.19), indicating the best wear resistance performance. This reveals that WC-based cermet with a HEA binder phase has superior wear performance due to the higher hardness and good self-lubricating effect of the wear products. Full article