Next Article in Journal
Detection and Characterization of Antibiotic-Resistant Bacteria Using Surface-Enhanced Raman Spectroscopy
Next Article in Special Issue
Engineering Charge Transfer Characteristics in Hierarchical Cu2S QDs @ ZnO Nanoneedles with p–n Heterojunctions: Towards Highly Efficient and Recyclable Photocatalysts
Previous Article in Journal
The Impact of Metallic Nanoparticles on Stem Cell Proliferation and Differentiation
 
 
Font Type:
Arial Georgia Verdana
Font Size:
Aa Aa Aa
Line Spacing:
Column Width:
Background:
Article

Vacuum Thermal Treated Ni-CeO2/SBA-15 Catalyst for CO2 Methanation

1
Department of Chemical Engineering, School of Petrochemical Technology and Energy Engineering, Zhejiang Ocean University, Zhoushan 316022, Zhejiang, China
2
School of Food and Pharmaceutical, Zhejiang Ocean University, Zhoushan 316022, Zhejiang, China
*
Author to whom correspondence should be addressed.
Nanomaterials 2018, 8(10), 759; https://doi.org/10.3390/nano8100759
Submission received: 23 August 2018 / Revised: 17 September 2018 / Accepted: 24 September 2018 / Published: 26 September 2018
(This article belongs to the Special Issue Nanostructured Catalysts for Sustainable Applications)

Abstract

:
Ni-CeO2/SBA-15-V catalyst was prepared by the impregnation method with vacuum thermal treatment and used for CO2 methanation reaction. Compared with Ni-CeO2/SBA-15-air catalyst with thermal treatment in air, the reduced Ni-CeO2/SBA-15-V catalyst with vacuum thermal treatment exhibited higher Ni dispersion and smaller Ni particle size. In CO2 methanation reaction, the Ni-CeO2/SBA-15-V catalyst was more active and selective than the Ni-CeO2/SBA-15-air catalyst. The good activity and selectivity of Ni-CeO2/SBA-15-V catalyst should be due to highly dispersed Ni in contact with small CeO2 particles.

Graphical Abstract

1. Introduction

With the increasing consumption of fossil fuel, CO2 released into the atmosphere has resulted in climate change and global warming, and the utilization of CO2 has received much attention. CO2 hydrogenation is an effective way to convert CO2 into fuels and chemicals [1,2]. CO2 methanation can convert CO2 and renewable H2 into methane, which is a promising process for CO2 conversion and the storage of renewable H2 [3].
CO2 methanation is an exothermic reaction, and the low reaction temperature is favorable for the high equilibrium conversion of CO2. Therefore, various catalysts have been developed for CO2 methanation at low temperature. Noble metal-based catalysts, such as Rh [4], Ru [5], and Pd [6], and non-noble Co [7,8] and Ni-based catalysts [9,10] are the most studied CO2 methanation catalysts. Although noble metal-based catalysts possess good activity for low-temperature CO2 methanation, Ni-based catalysts are preferred in industrial processes due to the low cost, and they have been applied for CO methanation [11,12] and CO2 methanation [13]. Ni supported on various metal oxides, such as SiO2 [13], Al2O3 [14], CeO2 [15], ZrO2 [16], and TiO2 [17], has been reported for CO2 methanation. Ni supported on SBA-15, which is a kind of mesoporous SiO2 with high specific surface area, has been reported for CO2 methanation [18,19]. Adding CeO2 to a Ni-based catalyst can enhance Ni dispersion and CO2 adsorption and dissociation [20]. CeO2-promoted Ni/SBA-15 catalyst has been used for CO2 methanation reaction and exhibits excellent catalytic performance [10,19].
However, it is difficult to obtain highly dispersed Ni particles on SBA-15 support by the conventional impregnation method, and Ni particles are mainly located on the SBA-15 outer surface [19]. Various methods, such as two solvents [21], surfactant assistant [22], and ammonia evaporation [23] methods have been used to improve the dispersion of Ni on SBA-15 support. Recently, vacuum thermal treatment was applied to synthesize highly dispersed Cu [24], Pt [25], and Pd [26] particles on mesoporous SBA-15. In the present work, the Ni-CeO2/SBA-15 catalyst was prepared by the impregnation method with vacuum thermal treatment and used for CO2 methanation. The vacuum thermal treated catalyst exhibited high dispersion of Ni and CeO2 and showed high activity and selectivity for CO2 methanation reaction.

2. Materials and Methods

2.1. Synthesis of Catalysts

SBA-15 was prepared by a hydrothermal method according to the literature [27]. First, 16.4 g of P123 (EO20PO70EO20, Mw = 5800; Sigma Aldrich, St. Louis, MO, USA) was dissolved in 500 mL of a 2 M HCl aqueous solution. After stirring at 40 °C for 1 h, 34.0 g tetraethoxysilane, (TEOS, Sinopharm, Shanghai, China) was dropped into the solution. Then it was stirred at 40 °C for 4 h, and aged at 100 °C for 48 h in sealed Teflon bottles. SBA-15 was obtained after filtration, drying at 80 °C overnight, and calcination at 600 °C for 4 h (heating rate of 1 °C/min).
Then, 1 g of SBA-15 was impregnated with controlled amounts of Ni(NO3)2·6H2O and Ce(NO3)3·6H2O using 5 mL of ethanol as solvent and kept at room temperature for 24 h, then it was calcinated in air or vacuum at 600 °C for 4 h with a heating rate of 1 °C/min. The resulting samples calcinated in air and vacuum are referred to as Ni-CeO2/SBA-15-air and Ni-CeO2/SBA-15-V, respectively.
For comparison, using γ-Al2O3 (241 m2/g) as support, a Ni-CeO2/Al2O3 catalyst was prepared by impregnation method and calcinated in air as described above.
In these catalysts, the theoretical Ni and CeO2 content was 10 wt % for both.

2.2. Characterization of Catalysts

N2 isotherms were measured using an Autosorb-iQ analyzer (Quantachrome Instruments, Boynton Beach, FL, USA) at −196 °C, and the pore size distribution was calculated from the desorption branch by Barrett–Joyner–Halenda (BJH) method. X-ray diffraction (XRD) patterns were measured by a DX-2700 X-ray diffractometer (Haoyuan Instrument, Dandong, China) using Cu Kα radiation. Transmission electron microscope (TEM) images were measured on a Tecnai G2 F20 microscope (FEI Company, Hillsboro, OR, USA). (XRD). H2-temperature programmed reduction (H2-TPR) patterns were measured on a TP-5080 adsorption instrument under a 5% H2/Ar flow at a rate of 10 °C/min to 900 °C. Before H2-TPR measurements, the samples were purged with an argon flow at 400 °C for 5 min. The outgas was monitored by a thermal conductivity detector (TCD) detector. Thermo gravimetric (TG) was carried out using an HCT-1 TG thermal analyzer (Henven Scientific Instrument, Beijing, China). The sample was heated from room temperature to 900 °C with a heating rate of 10 °C/min in air (20 mL/min).

2.3. Catalytic Test

The reaction was carried out in a fixed bed quartz reactor (inner diameter (ID) = 8 mm) at atmospheric pressure. The temperature of the reactor was controlled by a thermocouple inserted into the catalyst bed, and the gas flow rates were controlled by mass flow controllers. For a catalytic test, 100 mg of catalyst (60–100 mesh) diluted with 200 mg of inert SiO2 was used. The Ni-CeO2/SBA-15 catalyst was reduced to 50 mL/min of 20% H2/Ar stream at 450 °C for 40 min, and. After reduction, the reactor temperature was decreased to 200 °C in 20% H2/N2. Then the reactant gases (CO2:H2:Ar = 1:4:5, 100 mL/min) were introduced into the reactor. The reaction was conducted in the temperature range from 200 to 450 °C. The catalyst was kept for 1 h at each reaction temperature before the products were analyzed. The stability tests were performed at 350 and 400 °C. Before stability test, the Ni-CeO2/Al2O3 catalyst was reduced at 700 °C for 40 min. The exhaust and feed gas compositions were analyzed on a GC-7900 gas chromatograph (Techcomp, Kwai Chung, China) equipped with a TDX-01 column and a TCD detector. CO2 conversion, CH4 selectivity, and carbon balance were calculated using the following formulae:
CO 2   conversion = moles   of   CO 2   in moles   of   CO 2   out moles   of   CO 2   in × 100 % CH 4   selectivity = moles   of   CH 4   out moles   of   CO 2   in moles   of   CO 2   out × 100 % Carbon   balance = ( 1 moles   of   CH 4   out + moles   of   CO out + moles   of   CO 2   out moles   of   CO 2   in ) × 100 %
In this work, carbon balance was within ±3% for all the catalytic tests, indicating negligible carbon deposition on the catalysts.

3. Results and Discussion

3.1. Characterization of Catalysts

Figure 1 shows N2 adsorption–desorption isotherms and pore size distributions of SBA-15, Ni-CeO2/SBA-15-air, and Ni-CeO2/SBA-15-V. All samples showed type IV isotherm with a hysteresis loop in the relative pressure 0.65–0.80, confirming the uniform mesoporous structure in these samples. As shown in Figure 1b, the pore size of all samples was 6.5 nm, indicating the addition of Ni and CeO2 to SBA-15 without changing the mesoporous structures. As listed in Table 1, the Brunauer-Emmett-Teller (BET) surface area and pore volume decreased after the addition of NiO and CeO2 into SBA-15.
Figure 2 shows the XRD patterns of the catalysts. The reduced catalysts were reduced in a 20% H2/Ar stream (50 mL/min) for 40 min at 450 °C. As shown in Figure 2a, all the small-angle XRD patterns showed three typical peaks of mesoporous SBA-15 [27]. The result demonstrates that the mesoporous structure of SBA-15 was maintained after loading NiO and CeO2. Figure 2b shows the wide-angle XRD patterns of fresh and reduced catalysts. Compared with Ni-CeO2/SBA-15-air, Ni-CeO2/SBA-15-V exhibited obviously wider reflection peaks of NiO and CeO2, indicating that vacuum treatment can improve the dispersion of NiO and CeO2. After reduction, the reflection peaks of Ni in Ni-CeO2/SBA-15-V were also wider than those in Ni-CeO2/SBA-15-air, confirming that the Ni particle was smaller in the Ni-CeO2/SBA-15-V catalyst after reduction. As listed in Table 2, the crystal sizes of Ni and CeO2 in reduced Ni-CeO2/SBA-15-V were 8.5 and 4.2 nm, which were obviously smaller than those in reduced Ni-CeO2/SBA-15-air. The XRD results indicate that vacuum thermal treatment can improve Ni and CeO2 dispersion on SBA-15 support.
Figure 3 shows TEM images of the catalysts. For all catalysts, a well-ordered mesoporous structure could be observed. For fresh Ni-CeO2/SBA-15-air catalyst, most particles were 20–100 nm in size, which were larger than the pore size of SBA-15 and dispersed on the outside surface of SBA-15 (Figure 3a), and NiO particles larger than 20 nm could be clearly observed in Figure 3b. On the contrary, for fresh Ni-CeO2/SBA-15-V (Figure 3c), lots of particles were aligned within the mesoporous channels of SBA-15, indicating this part of particles located in the pore channels. For fresh Ni-CeO2/SBA-15-V, small particles were dispersed on the outside surface or in the nanochannel of SBA-15. NiO particles smaller than 10 nm in contact with CeO2 particles were observed (Figure 3d). TEM images of reduced Ni-CeO2/SBA-15-V catalyst are shown in Figure 3e,f. Metal Ni particles were found to be in contact with CeO2 particles, as shown in Figure 3f.
Figure 4 shows H2-TPR profiles of the catalysts. For Ni-CeO2/SBA-15-air, the sharp peak located at around 420 °C was attributed to the reduction of large bulk NiO species with no or very little interaction with SiO2 support [19]. For Ni-CeO2/SBA-15-V, a reduction peak between 300 °C and 600 °C was observed. A reduction peak beyond 500 °C corresponds to the reduction of small NiO particles strongly interacting with SiO2 support [28,29,30,31,32,33]. The result indicates that there is a strong interaction between Ni and SiO2 in Ni-CeO2/SBA-15-V catalyst.

3.2. Catalytic Performance

The CO2 conversion and CH4 selectivity of the catalysts for CO2 methanation reaction are shown in Figure 5. Compared with the Ni-CeO2/SBA-15-air catalyst, the Ni-CeO2/SBA-15-V catalyst exhibited obviously higher CO2 conversion and CH4 selectivity. For the Ni-CeO2/SBA-15-V catalyst, CO2 conversion and CH4 selectivity at 400 °C were 68.8% and 99.0%, respectively. CH4 selectivity of the Ni-CeO2/SBA-15-V catalyst decreased to 97.1% at 450 °C. This is because reverse water gas shift reaction (CO2 + H2 → CO + H2O) is an endothermic reaction, and high temperatures are more conducive to producing CO and decreasing CH4 selectivity. The result shows that the Ni-CeO2/SBA-15-V catalyst was active and selective for the CO2 methanation reaction. It should be noted that the Ni-CeO2/SBA-15-air catalyst produced a large amount of CO even at low temperature. This may be due to that the large Ni particle in the Ni-CeO2/SBA-15-air catalyst was active for both CO2 methanation and reverse water–gas shift reaction, while small Ni particle in contact with CeO2 in Ni-CeO2/SBA-15-V catalyst was more selective for CO2 methanation.
Figure 6 shows the stability test of Ni-CeO2/SBA-15-V catalyst at 350 °C and 400 °C. The equilibrium conversions are also shown in Figure 6. The CO2 conversions of Ni-CeO2/SBA-15-V catalyst had a little decrease in initial 10 h on stream, then the catalyst exhibited stable catalytic performance for 50 h at 350 °C and 400 °C. After reaction for 60 h, the CO2 conversion at 350 °C and 400 °C stayed at around 49.5% and 62.5%, respectively. It is worth noticing that, during the stability test at 400 °C, CH4 selectivity achieved over the Ni-CeO2/SBA-15-air catalyst remained almost constant after 10 h on stream approaching values higher than 97%.
Among Ni-based methanation catalysts, Ni/Al2O3 catalyst is the most widely investigated and used due to its low costs and availability. Table 3 shows the CO2 conversion and selectivity of reported Ni/Al2O3 catalyst at 250 and 300 °C. Compared with the Ni/Al2O3 catalyst, the CO2 conversion of Ni-CeO2/SBA-15-V was obviously higher.
For comparison with Ni-CeO2/SBA-15-V catalyst, the stability of Ni-CeO2/Al2O3 catalyst prepared with a conventional impregnation method was tested at 350 °C. As shown in Figure 7, the CO2 conversion and CH4 selectivity of Ni-CeO2/Al2O3 catalyst were obviously lower than that of Ni-CeO2/SBA-15-V catalyst.
Carbon deposition and sintering of metal particle are the main reasons for the catalyst deactivation during CO2 methanation [10,35,36]. The spent Ni-CeO2/SBA-15-V catalyst after stability test at 400 °C was characterized by TG, XRD, and TEM. TG curve was shown in Figure 8a. There was a weight decrease below 100 °C and a weight increase in the temperature region of 180–400 °C. The weight decrease should be due to the desorption of adsorbed water and the weight increase due to the oxidation metal Ni to NiO. There was no obvious weight loss above 100 °C, indicating no obviously carbon deposition was formed on the spent Ni-CeO2/SBA-15-V catalyst. XRD patterns of reduced and spent Ni-CeO2/SBA-15-V catalysts were shown in Figure 8b. Determined by Scherrer’s equation from the (111) plane of Ni in XRD patterns, Ni crystal sizes were 8.5 and 9.1 nm for reduced and spent Ni-CeO2/SBA-15-V catalysts, respectively. XRD results indicate that the Ni particle size was slightly increased during the stability test. As shown in Figure 8c, TEM image also showed that no obviously sintering of Ni particle occurred. The TG, XRD, and TEM results indicate the slight decrease of activity and selectivity during stability test was due to the slight increase of Ni particle size.
The present work clearly demonstrates that the Ni-CeO2/SBA-15-V catalyst possessed superior activity and selectivity and exhibited excellent stability during the CO2 methanation reaction. The XRD and TEM results prove that the vacuum-thermal treated Ni-CeO2/SBA-15-V catalyst had higher Ni dispersion and smaller Ni particle size than the Ni-CeO2/SBA-15-air catalyst thermal treated in air. Based on the characterization and catalyst performance results, it can be concluded that good activity and selectivity of Ni-CeO2/SBA-15-V catalyst can be attributed to the small Ni particle size in contact with CeO2.

4. Conclusions

The effects of vacuum thermal treatment on Ni-CeO2/SBA-15 catalysts were investigated in this paper. Compared with thermal treatment in air, vacuum thermal treatment can improve the dispersion of Ni and CeO2 in the Ni-CeO2/SBA-15 catalyst. The Ni-CeO2/SBA-15-V catalyst with vacuum thermal treatment exhibited better activity and selectivity than the Ni-CeO2/SBA-15-air catalyst thermal treated in air. The excellent catalytic performance of the Ni-CeO2/SBA-15-V catalyst was mainly attributed to higher Ni and CeO2 dispersion.

Author Contributions

Conceptualization, L.W. and H.L.; Formal analysis, R.H. and S.Y.; Investigation, H.Y., G.T., K.L., and Y.Y.; Writing—original draft, L.W.; Writing—review & editing, H.L.

Funding

This research was funded by the Natural Science Foundation of China (grant number 21406206) and the national students’ innovation and entrepreneurship training program (grant number 201710340016).

Conflicts of Interest

The authors declare no conflict of interest.

References

  1. Centi, G.; Perathoner, S. Opportunities and prospects in the chemical recycling of carbon dioxide to fuels. Catal. Today 2009, 148, 191–205. [Google Scholar] [CrossRef]
  2. Wang, W.; Wang, S.; Ma, X.; Gong, J. Recent advances in catalytic hydrogenation of carbon dioxide. Chem. Soc. Rev. 2011, 40, 3703–3727. [Google Scholar] [CrossRef] [PubMed]
  3. Kirchner, J.; Anolleck, J.K.; Lösch, H.; Kureti, S. Methanation of CO2 on iron based catalysts. Appl. Catal. B 2018, 223, 47–59. [Google Scholar] [CrossRef]
  4. Karelovic, A.; Ruiz, P. Mechanistic study of low temperature CO2 methanation over Rh/TiO2 catalysts. J. Catal. 2013, 301, 141–153. [Google Scholar] [CrossRef]
  5. Kim, A.; Debecker, D.P.; Devred, F.; Dubois, V.; Sanchez, C.; Sassoye, C. CO2 methanation on Ru/TiO2 catalysts: On the effect of mixing anatase and rutile TiO2 supports. Appl. Catal. B 2018, 220, 615–625. [Google Scholar] [CrossRef]
  6. Park, J.-N.; McFarland, E.W. A highly dispersed Pd–Mg/SiO2 catalyst active for methanation of CO2. J. Catal. 2009, 266, 92–97. [Google Scholar] [CrossRef]
  7. Li, W.; Nie, X.; Jiang, X.; Zhang, A.; Ding, F.; Liu, M.; Liu, Z.; Guo, X.; Song, C. ZrO2 support imparts superior activity and stability of Co catalysts for CO2 methanation. Appl. Catal. B 2018, 220, 397–408. [Google Scholar] [CrossRef]
  8. Liu, H.; Xu, S.; Zhou, G.; Huang, G.; Huang, S.; Xiong, K. CO2 hydrogenation to methane over Co/KIT-6 catalyst: Effect of reduction temperature. Chem. Eng. J. 2018, 351, 65–73. [Google Scholar] [CrossRef]
  9. Ashok, J.; Ang, M.L.; Kawi, S. Enhanced activity of CO2 methanation over Ni/CeO2-ZrO2 catalysts: Influence of preparation methods. Catal. Today 2017, 281, 304–311. [Google Scholar] [CrossRef]
  10. Bian, L.; Zhang, L.; Zhu, Z.; Li, Z. Methanation of carbon oxides on Ni/Ce/SBA-15 pretreated with dielectric barrier discharge plasma. Mol. Catal. 2018, 446, 131–139. [Google Scholar] [CrossRef]
  11. Gong, D.; Li, S.; Guo, S.; Tang, H.; Wang, H.; Liu, Y. Lanthanum and cerium co-modified Ni/SiO2 catalyst for CO methanation from syngas. Appl. Surf. Sci. 2018, 434, 351–364. [Google Scholar] [CrossRef]
  12. Li, S.; Gong, D.; Tang, H.; Ma, Z.; Liu, Z.-T.; Liu, Y. Preparation of bimetallic Ni@Ru nanoparticles supported on SiO2 and their catalytic performance for CO methanation. Chem. Eng. J. 2018, 334, 2167–2178. [Google Scholar] [CrossRef]
  13. Aziz, M.A.A.; Jalil, A.A.; Triwahyono, S.; Mukti, R.R.; Taufiq-Yap, Y.H.; Sazegar, M.R. Highly active Ni-promoted mesostructured silica nanoparticles for CO2 methanation. Appl. Catal. B 2014, 147, 359–368. [Google Scholar] [CrossRef]
  14. He, L.; Lin, Q.; Liu, Y.; Huang, Y. Unique catalysis of Ni-Al hydrotalcite derived catalyst in CO2 methanation: Cooperative effect between Ni nanoparticles and a basic support. J. Energy Chem. 2014, 23, 587–592. [Google Scholar] [CrossRef]
  15. Zhou, G.; Liu, H.; Cui, K.; Jia, A.; Hu, G.; Jiao, Z.; Liu, Y.; Zhang, X. Role of surface Ni and Ce species of Ni/CeO2 catalyst in CO2 methanation. Appl. Surf. Sci. 2016, 383, 248–252. [Google Scholar] [CrossRef]
  16. Zhao, K.; Wang, W.; Li, Z. Highly efficient Ni/ZrO2 catalysts prepared via combustion method for CO2 methanation. J. CO2 Util. 2016, 16, 236–244. [Google Scholar] [CrossRef]
  17. Liu, J.; Li, C.; Wang, F.; He, S.; Chen, H.; Zhao, Y.; Wei, M.; Evans, D.G.; Duan, X. Enhanced low-temperature activity of CO2 methanation over highly-dispersed Ni/TiO2 catalyst. Catal. Sci. Technol. 2013, 3, 2627–2633. [Google Scholar] [CrossRef]
  18. Lu, B.; Ju, Y.; Abe, T.; Kawamoto, K. Grafting Ni particles onto SBA-15, and their enhanced performance for CO2 methanation. RSC Adv. 2015, 5, 56444–56454. [Google Scholar] [CrossRef]
  19. Bacariza, M.C.; Graça, I.; Bebiano, S.S.; Lopes, J.M.; Henriques, C. Micro- and mesoporous supports for CO2 methanation catalysts: A comparison between SBA-15, MCM-41 and USY zeolite. Chem. Eng. Sci. 2018, 175, 72–83. [Google Scholar] [CrossRef]
  20. Wang, W.; Chu, W.; Wang, N.; Yang, W.; Jiang, C. Mesoporous nickel catalyst supported on multi-walled carbon nanotubes for carbon dioxide methanation. Int. J. Hydrogen Energy 2016, 41, 967–975. [Google Scholar] [CrossRef]
  21. Kaydouh, M.N.; El Hassan, N.; Davidson, A.; Casale, S.; El Zakhem, H.; Massiani, P. Highly active and stable Ni/SBA-15 catalysts prepared by a “two solvents” method for dry reforming of methane. Microporous Mesoporous Mater. 2016, 220, 99–109. [Google Scholar] [CrossRef] [Green Version]
  22. Yang, W.; Liu, H.; Li, Y.; Wu, H.; He, D. CO2 reforming of methane to syngas over highly-stable Ni/SBA-15 catalysts prepared by P123-assisted method. Int. J. Hydrogen Energy 2016, 41, 1513–1523. [Google Scholar] [CrossRef]
  23. Zhang, Q.; Wang, M.; Zhang, T.; Wang, Y.; Tang, X.; Ning, P. A stable Ni/SBA-15 catalyst prepared by the ammonia evaporation method for dry reforming of methane. RSC Adv. 2015, 5, 94016–94024. [Google Scholar] [CrossRef]
  24. Liu, C.-H.; Lai, N.-C.; Lee, J.-F.; Chen, C.-S.; Yang, C.-M. SBA-15-supported highly dispersed copper catalysts: Vacuum–thermal preparation and catalytic studies in propylene partial oxidation to acrolein. J. Catal. 2014, 316, 231–239. [Google Scholar] [CrossRef]
  25. Wu, H.-C.; Chen, T.-C.; Lai, N.-C.; Yang, C.-M.; Wu, J.-H.; Chen, Y.-C.; Lee, J.-F.; Chen, C.-S. Synthesis of sub-nanosized Pt particles on mesoporous SBA-15 material and its application to the CO oxidation reaction. Nanoscale 2015, 7, 16848–16859. [Google Scholar] [CrossRef] [PubMed]
  26. Liu, C.-H.; Lin, C.-Y.; Chen, J.-L.; Lu, K.-T.; Lee, J.-F.; Chen, J.-M. SBA-15-supported Pd catalysts: The effect of pretreatment conditions on particle size and its application to benzyl alcohol oxidation. J. Catal. 2017, 350, 21–29. [Google Scholar] [CrossRef]
  27. Zhao, D.; Feng, J.; Huo, Q.; Melosh, N.; Fredrickson, G.H.; Chmelka, B.F.; Stucky, G.D. Triblock copolymer syntheses of mesoporous silica with periodic 50 to 300 angstrom pores. Science 1998, 279, 548–552. [Google Scholar] [CrossRef] [PubMed]
  28. He, S.; He, S.; Zhang, L.; Li, X.; Wang, J.; He, D.; Lu, J.; Luo, Y. Hydrogen production by ethanol steam reforming over Ni/SBA-15 mesoporous catalysts: Effect of Au addition. Catal. Today 2015, 258 Pt 1, 162–168. [Google Scholar] [CrossRef]
  29. Tao, M.; Xin, Z.; Meng, X.; Lv, Y.; Bian, Z. Impact of double-solvent impregnation on the Ni dispersion of Ni/SBA-15 catalysts and catalytic performance for the syngas methanation reaction. RSC Adv. 2016, 6, 35875–35883. [Google Scholar] [CrossRef]
  30. Zhang, Q.; Zhang, T.; Shi, Y.; Zhao, B.; Wang, M.; Liu, Q.; Wang, J.; Long, K.; Duan, Y.; Ning, P. A sintering and carbon-resistant Ni-SBA-15 catalyst prepared by solid-state grinding method for dry reforming of methane. J. CO2 Util. 2017, 17, 10–19. [Google Scholar] [CrossRef]
  31. Zhang, Q.; Long, K.; Wang, J.; Zhang, T.; Song, Z.; Lin, Q. A novel promoting effect of chelating ligand on the dispersion of Ni species over Ni/SBA-15 catalyst for dry reforming of methane. Int. J. Hydrogen Energy 2017, 42, 14103–14114. [Google Scholar] [CrossRef]
  32. Wang, M.; Zhang, Q.; Zhang, T.; Wang, Y.; Wang, J.; Long, K.; Song, Z.; Liu, X.; Ning, P. Facile one-pot synthesis of highly dispersed Ni nanoparticles embedded in HMS for dry reforming of methane. Chem. Eng. J. 2017, 313, 1370–1381. [Google Scholar] [CrossRef]
  33. Carrero, A.; Calles, J.; García-Moreno, L.; Vizcaíno, A. Production of renewable hydrogen from glycerol steam reforming over bimetallic Ni-(Cu,Co,Cr) catalysts supported on SBA-15 silica. Catalysts 2017, 7, 55. [Google Scholar] [CrossRef]
  34. Garbarino, G.; Riani, P.; Magistri, L.; Busca, G. A study of the methanation of carbon dioxide on Ni/Al2O3 catalysts at atmospheric pressure. Int. J. Hydrogen Energy 2014, 39, 11557–11565. [Google Scholar] [CrossRef]
  35. Guo, M.; Lu, G. The effect of impregnation strategy on structural characters and CO2 methanation properties over MgO modified Ni/SiO2 catalysts. Catal. Commun. 2014, 54, 55–60. [Google Scholar] [CrossRef]
  36. Lu, X.; Gu, F.; Liu, Q.; Gao, J.; Liu, Y.; Li, H.; Jia, L.; Xu, G.; Zhong, Z.; Su, F. VOx promoted Ni catalysts supported on the modified bentonite for CO and CO2 methanation. Fuel Process. Technol. 2015, 135, 34–46. [Google Scholar] [CrossRef]
Figure 1. (a) N2 adsorption-desorption isotherms; (b) pore size distributions of SBA-15, Ni-CeO2/SBA-15-air, and Ni-CeO2/SBA-15-V.
Figure 1. (a) N2 adsorption-desorption isotherms; (b) pore size distributions of SBA-15, Ni-CeO2/SBA-15-air, and Ni-CeO2/SBA-15-V.
Nanomaterials 08 00759 g001
Figure 2. (a) Small-angle and (b) wide-angle X-ray diffraction (XRD) patterns of SBA-15, Ni-CeO2/SBA-15-air, and Ni-CeO2/SBA-15-V catalysts.
Figure 2. (a) Small-angle and (b) wide-angle X-ray diffraction (XRD) patterns of SBA-15, Ni-CeO2/SBA-15-air, and Ni-CeO2/SBA-15-V catalysts.
Nanomaterials 08 00759 g002
Figure 3. Transmission electron microscope (TEM) images of fresh and reduced catalysts: (a,b) fresh Ni-CeO2/SBA-15-air, (c,d) fresh Ni-CeO2/SBA-15-V, and (e,f) reduced Ni-CeO2/SBA-15-V.
Figure 3. Transmission electron microscope (TEM) images of fresh and reduced catalysts: (a,b) fresh Ni-CeO2/SBA-15-air, (c,d) fresh Ni-CeO2/SBA-15-V, and (e,f) reduced Ni-CeO2/SBA-15-V.
Nanomaterials 08 00759 g003
Figure 4. H2-temperature programmed reduction (H2-TPR) profile of Ni-CeO2/SBA-15-air and Ni-CeO2/SBA-15-V catalysts.
Figure 4. H2-temperature programmed reduction (H2-TPR) profile of Ni-CeO2/SBA-15-air and Ni-CeO2/SBA-15-V catalysts.
Nanomaterials 08 00759 g004
Figure 5. (a) CO2 conversion and (b) CH4 selectivity of Ni-CeO2/SBA-15-air and Ni-CeO2/SBA-15-V catalysts in methanation reaction.
Figure 5. (a) CO2 conversion and (b) CH4 selectivity of Ni-CeO2/SBA-15-air and Ni-CeO2/SBA-15-V catalysts in methanation reaction.
Nanomaterials 08 00759 g005
Figure 6. Stability of the Ni-CeO2/SBA-15-V catalyst in methanation reaction at (a) 350 °C and (b) 400 °C.
Figure 6. Stability of the Ni-CeO2/SBA-15-V catalyst in methanation reaction at (a) 350 °C and (b) 400 °C.
Nanomaterials 08 00759 g006
Figure 7. Stability of Ni-CeO2/Al2O3 catalysts in methanation reaction at 350 °C.
Figure 7. Stability of Ni-CeO2/Al2O3 catalysts in methanation reaction at 350 °C.
Nanomaterials 08 00759 g007
Figure 8. (a) Thermo gravimetric (TG) curve, (b) XRD pattern, and (c) TEM image of the spent Ni-CeO2/SBA-15-V catalyst after stability test at 400 °C.
Figure 8. (a) Thermo gravimetric (TG) curve, (b) XRD pattern, and (c) TEM image of the spent Ni-CeO2/SBA-15-V catalyst after stability test at 400 °C.
Nanomaterials 08 00759 g008
Table 1. Textural properties of SBA-15, Ni-CeO2/SBA-15-air, and Ni-CeO2/SBA-15-V.
Table 1. Textural properties of SBA-15, Ni-CeO2/SBA-15-air, and Ni-CeO2/SBA-15-V.
SamplesSBET (m2/g)Pore Volume (cm3/g)Average Pore Diameter (nm)
SBA-156901.126.56
Ni-CeO2/SBA-15-air4330.836.54
Ni-CeO2/SBA-15-V4920.836.56
Table 2. Physical properties of catalysts.
Table 2. Physical properties of catalysts.
CatalystsCeO2 Crystal Size (nm) aNiO Crystal Size (nm) bNi Crystal Size (nm) cNi Dispersion (%) d
Ni-CeO2/SBA-15-air (fresh)7.342.1--
Ni-CeO2/SBA-15-air (reduced)7.1-26.13.7
Ni-CeO2/SBA-15-V (fresh)4.610.8--
Ni-CeO2/SBA-15-V (reduced)4.2-8.511.4
a Determined by Scherrer’s equation from the (111) plane of CeO2 in X-ray diffraction (XRD) patterns; b determined by Scherrer’s equation from the (200) plane of NiO in XRD patterns; c determined by Scherrer’s equation from the (111) plane of Ni in XRD patterns; d calculated as (97.1 nm)/(particle size of Ni(nm)).
Table 3. CO2 conversion and CH4 selectivity of Ni-CeO2/SBA-15-V and reported Ni/Al2O3 catalyst.
Table 3. CO2 conversion and CH4 selectivity of Ni-CeO2/SBA-15-V and reported Ni/Al2O3 catalyst.
CatalystsNi Content (wt %)T (°C)CO2 Conversion (%)CH4 Selectivity (%)Ref.
Ni-CeO2/SBA-15-V10%25010.2100This work a
30035.499.3This work a
Ni/Al2O314%2501100[34] b
3006100[34] b
a Weight hourly space velocity(WHSV) = 60,000 mL g−1 h−1, CO2/H2/Ar = 1/4/5; b Gas hourly space velocity (GHSV) = 52,300 h−1, CO2/H2 = 1/5.

Share and Cite

MDPI and ACS Style

Wang, L.; Liu, H.; Ye, H.; Hu, R.; Yang, S.; Tang, G.; Li, K.; Yang, Y. Vacuum Thermal Treated Ni-CeO2/SBA-15 Catalyst for CO2 Methanation. Nanomaterials 2018, 8, 759. https://doi.org/10.3390/nano8100759

AMA Style

Wang L, Liu H, Ye H, Hu R, Yang S, Tang G, Li K, Yang Y. Vacuum Thermal Treated Ni-CeO2/SBA-15 Catalyst for CO2 Methanation. Nanomaterials. 2018; 8(10):759. https://doi.org/10.3390/nano8100759

Chicago/Turabian Style

Wang, Luhui, Hui Liu, Han Ye, Rong Hu, Shuqing Yang, Guoli Tang, Kunqiang Li, and Yanpeng Yang. 2018. "Vacuum Thermal Treated Ni-CeO2/SBA-15 Catalyst for CO2 Methanation" Nanomaterials 8, no. 10: 759. https://doi.org/10.3390/nano8100759

Note that from the first issue of 2016, this journal uses article numbers instead of page numbers. See further details here.

Article Metrics

Back to TopTop