Experiments and Simulations of Superalloys
- ISBN 978-3-7258-5207-9 (Hardback)
- ISBN 978-3-7258-5208-6 (PDF)
This is a Reprint of the Special Issue Experiments and Simulations of Superalloys that was published in
Summary
This Special Issue presents the latest advances in the design, processing, and performance evaluation of Ni-based superalloys. The presented articles highlight key aspects such as microstructural evolution, high-temperature tensile behavior, low-cycle fatigue, and the effects of alloying and processing on mechanical properties. Covering both single-crystal and directionally solidified superalloys, the contributions provide insights into γ/γ′ phase interactions, deformation mechanisms, and phase stability. This compilation can serve as a valuable reference for researchers and engineers working on high-performance alloys for turbine, aerospace, and power-generation applications.